Individual Phases
1 Bainite in Steels, Transformations, Microstructure and Properties
H.K.D.H. Bhadeshia, Institute of Materials.
Graphite Assume at equilibrium, MTDATA + SGTE
Bainitic ferrite Thermodynamic/Kinetic modified after Bhadeshia1
Carbides Thermodynamic/Kinetic - MTDATA?
Martensite Empirical relationships for start temperature
Carbide precipitation neglected (high Si)
Valid for Stage I of austempering process