Segregation - During Casting
Scheil modelling: Cl = C0(1-fs)k-1
- Assumes complete liquid mixing with no diffusion in the solid state, that is: Dliquid = ¥ and Dsolid = 0
- Modelling using thermodynamic data alone
Formation of carbides/phosphide remote from nodule