EXAMPLES OF APPLICATION INTERFACE COMMANDS
call set_temperature(gammatemp)
Subroutine call to define the temperature (K) at which the Gibbs energy minimisation will be carried out, set to the austenitising temperature (gammatemp)
call set_init_component_mass(2,wtC)
Sets mass of component ‘2’, initial component list, to the value of the variable ‘wtC’, used when equilibrium is determined
call compute_equilibrium
Call to calculate equilibrium
WtC0 = component_w_of_phase(2,7,init)
Variable ‘WtC0’ is assigned to be the amount of component ‘2’ (carbon) in phase ‘7’ (austenite) after equilibrium has been calculated (at the austenitising temperature)