UNIT CELL DATA a = 3.5670; b = 3.5670; c = 3.5670 Angstroms alpha = 90.000; beta = 90.000; gamma = 90.000 degrees cell volume = 45.385 A**3 Lattice type = F REFLECTIONS LIST X-ray wavelength = 1.5405 Angstroms ref no. (N) h k l d(hkl) 2-Theta Intensity I/Imax m(hkl) [ 1] 3 1 1 1 2.05941 43.9269 3.10407e+02 100.0 8 [ 2] 4 2 0 0 1.78350 51.1733 1.46743e+02 47.3 6 [ 3] 8 2 2 0 1.26112 75.2896 9.33796e+01 30.1 12 [ 4] 11 1 1 3 1.07549 91.4807 1.19629e+02 38.5 24 [ 5] 12 2 2 2 1.02970 96.8401 3.66498e+01 11.8 8 [ 6] 16 0 0 4 0.89175 119.4808 2.62916e+01 8.5 6 [ 7] 19 3 1 3 0.81833 140.5254 1.43650e+02 46.3 24 [ 8] 20 2 4 0 0.79761 149.9015 1.84256e+02 59.4 24