UNIT CELL DATA a = 2.8670; b = 2.8670; c = 2.8670 Angstroms alpha = 90.000; beta = 90.000; gamma = 90.000 degrees cell volume = 23.566 A**3 Lattice type = I REFLECTIONS LIST X-ray wavelength = 1.5405 Angstroms ref no. (N) h k l d(hkl) 2-Theta Intensity I/Imax m(hkl) [ 1] 2 1 1 0 2.02728 44.9146 3.33255e+00 100.0 12 [ 2] 4 0 0 2 1.43350 65.2572 5.35348e-01 16.1 6 [ 3] 6 1 2 1 1.17045 82.5617 1.11897e+00 33.6 24 [ 4] 8 0 2 2 1.01364 99.1627 4.03651e-01 12.1 12 [ 5] 10 0 3 1 0.90663 116.5862 7.75450e-01 23.3 24 [ 6] 12 2 2 2 0.82763 137.3325 3.35084e-01 10.1 8