<--Previous  Up  Next-->

fig2b

The same sample after creep at 980&deg;C, 200 MPa, for 85.7 hours. The microstructure is completely rafted with the ratio of the number of &gamma; terminations (white dots) to the &gamma;' terminations being identical.