<--Previous  Up  Next-->

Slide10

Fe-0.79C-1.59Si-1.94Mn-0.30Mo-1.33Cr-0.11V wt% Austenititised at 1000°C for 15 min. isothermally transformed at 190°C for 14 days, tempered at 400°C for 1 h.