Design of Creep-Resistant Steels: Success and Failure of Models

H. K. D. H. Bhadeshia and T. Sourmail

Abstract

This paper assesses the validity of mathematical models in the context of creep-resistant ferritic steels.

Japan Society for the Promotion of Science Vol. 44, 2003, 299-314

Download PDF file of paper