Each row contains an unindexed pattern, an indexed pattern and a stereogram centred on the zone axis of the diffraction pattern. The traces of the cube planes are also plotted on the stereograms.
[001] zone axis
|
[001] zone axis
|
Stereogram centred on [001]
|
[110] zone axis
|
[110] zone axis
|
Stereogram centred on [110]
|
[111] zone axis
|
[111] zone axis
|
Stereogram centred on [111]
|
[112] zone axis
|
[112] zone axis
|
Stereogram centred on [112]
|
[012] zone axis
|
[012] zone axis
|
Stereogram centred on [012]
|
[013] zone axis
|
[013] zone axis
|
Stereogram centred on [013]
|
[113] zone axis
|
[113] zone axis
|
Stereogram centred on [113]
|
[123] zone axis
|
[123] zone axis
|
Stereogram centred on [123]
|
[133] zone axis
|
[133] zone axis
|
Stereogram centred on [133]
|