************************************************************************ Output generated by CrystalDiffract 5.1.2 (c) 1995-2006 CrystalMaker Software Ltd ************************************************************************ (This file looks best in a mono-spaced font e.g., Monaco or Courier) Filename: Fe3C - cementite (volume fraction: 33.33%) ref no. h k l d(hkl) 2-Theta Lp F(Re) F(Im) Intensity [ 1] 0 0 1 6.7475 13.110 75.26 0.00 0.00 4.03079e-12 [ 2] 0 0 -1 6.7475 13.110 75.26 0.00 -0.00 4.03079e-12 [ 3] 0 -1 0 5.0837 17.429 42.09 0.00 0.00 4.20145e-11 [ 4] 0 1 0 5.0837 17.429 42.09 0.00 -0.00 4.20145e-11 [ 5] 1 0 0 4.5165 19.639 32.92 0.00 0.00 1.95959e-12 [ 6] -1 0 0 4.5165 19.639 32.92 0.00 -0.00 1.95959e-12 [ 7] 0 -1 1 4.0603 21.871 26.34 0.00 0.00 6.33461e-12 [ 8] 0 1 -1 4.0603 21.871 26.34 0.00 -0.00 6.33461e-12 [ 9] 0 -1 -1 4.0603 21.871 26.34 0.00 -0.00 1.50771e-11 [ 10] 0 1 1 4.0603 21.871 26.34 0.00 0.00 1.50771e-11 [ 11] 1 0 -1 3.7533 23.685 22.30 -8.21 0.00 5.49411e+00 [ 12] -1 0 1 3.7533 23.685 22.30 -8.21 -0.00 5.49411e+00 [ 13] -1 0 -1 3.7533 23.685 22.30 8.21 -0.00 5.49411e+00 [ 14] 1 0 1 3.7533 23.685 22.30 8.21 0.00 5.49411e+00 [ 15] -1 1 0 3.3764 26.373 17.79 -8.11 0.00 4.27952e+00 [ 16] 1 -1 0 3.3764 26.373 17.79 -8.11 -0.00 4.27952e+00 [ 17] 1 1 0 3.3764 26.373 17.79 -8.11 -0.00 4.27951e+00 [ 18] -1 -1 0 3.3764 26.373 17.79 -8.11 0.00 4.27951e+00 [ 19] 0 0 2 3.3737 26.395 17.76 14.95 -0.00 1.45180e+01 [ 20] 0 0 -2 3.3737 26.395 17.76 14.95 0.00 1.45180e+01 [ 21] 1 -1 -1 3.0195 29.558 13.96 8.72 -0.00 3.87766e+00 [ 22] -1 1 -1 3.0195 29.558 13.96 -8.72 0.00 3.87765e+00 [ 23] -1 1 1 3.0195 29.558 13.96 8.72 0.00 3.87766e+00 [ 24] 1 -1 1 3.0195 29.558 13.96 -8.72 -0.00 3.87765e+00 [ 25] -1 -1 1 3.0195 29.558 13.96 -8.72 0.00 3.87765e+00 [ 26] 1 1 -1 3.0195 29.558 13.96 -8.72 -0.00 3.87765e+00 [ 27] -1 -1 -1 3.0195 29.558 13.96 8.72 0.00 3.87768e+00 [ 28] 1 1 1 3.0195 29.558 13.96 8.72 -0.00 3.87768e+00 [ 29] 0 1 -2 2.8110 31.806 11.93 0.00 0.00 5.23726e-13 [ 30] 0 -1 2 2.8110 31.806 11.93 0.00 -0.00 5.23726e-13 [ 31] 0 -1 -2 2.8110 31.806 11.93 -0.00 0.00 4.06328e-11 [ 32] 0 1 2 2.8110 31.806 11.93 -0.00 -0.00 4.06328e-11 [ 33] 1 0 -2 2.7029 33.114 10.93 -0.00 -0.00 7.10149e-14 [ 34] -1 0 2 2.7029 33.114 10.93 -0.00 0.00 7.10149e-14 [ 35] -1 0 -2 2.7029 33.114 10.93 0.00 0.00 5.90191e-12 [ 36] 1 0 2 2.7029 33.114 10.93 0.00 -0.00 5.90191e-12 [ 37] 0 -2 0 2.5419 35.279 9.52 -25.04 -0.00 2.18194e+01 [ 38] 0 2 0 2.5419 35.279 9.52 -25.04 0.00 2.18194e+01 [ 39] -1 -1 2 2.3866 37.658 8.25 -53.98 0.00 8.78979e+01 [ 40] 1 -1 2 2.3866 37.658 8.25 -53.98 -0.00 8.78980e+01 [ 41] -1 1 2 2.3866 37.658 8.25 -53.98 -0.00 8.78980e+01 [ 42] -1 1 -2 2.3866 37.658 8.25 -53.98 0.00 8.78980e+01 [ 43] 1 -1 -2 2.3866 37.658 8.25 -53.98 0.00 8.78980e+01 [ 44] 1 1 -2 2.3866 37.658 8.25 -53.98 -0.00 8.78979e+01 [ 45] 1 1 2 2.3866 37.658 8.25 -53.98 -0.00 8.78982e+01 [ 46] -1 -1 -2 2.3866 37.658 8.25 -53.98 0.00 8.78982e+01 [ 47] 0 2 -1 2.3787 37.788 8.19 74.92 0.00 1.68007e+02 [ 48] 0 -2 1 2.3787 37.788 8.19 74.92 -0.00 1.68007e+02 [ 49] 0 -2 -1 2.3787 37.788 8.19 -74.92 0.00 1.68006e+02 [ 50] 0 2 1 2.3787 37.788 8.19 -74.92 -0.00 1.68006e+02 [ 51] -2 0 0 2.2582 39.886 7.26 -108.38 0.00 3.11910e+02 [ 52] 2 0 0 2.2582 39.886 7.26 -108.38 -0.00 3.11910e+02 [ 53] 0 0 3 2.2492 40.054 7.20 -0.00 -0.00 5.84008e-11 [ 54] 0 0 -3 2.2492 40.054 7.20 -0.00 0.00 5.84008e-11 [ 55] 1 -2 0 2.2151 40.696 6.95 70.07 0.00 1.24670e+02 [ 56] -1 2 0 2.2151 40.696 6.95 70.07 -0.00 1.24670e+02 [ 57] -1 -2 0 2.2151 40.696 6.95 -70.07 -0.00 1.24670e+02 [ 58] 1 2 0 2.2151 40.696 6.95 -70.07 0.00 1.24670e+02 [ 59] -2 0 1 2.1415 42.161 6.42 -0.00 -0.00 1.59741e-12 [ 60] 2 0 1 2.1415 42.161 6.42 -0.00 -0.00 9.82370e-12 [ 61] 2 0 -1 2.1415 42.161 6.42 -0.00 0.00 1.59741e-12 [ 62] -2 0 -1 2.1415 42.161 6.42 -0.00 0.00 9.82370e-12 [ 63] 1 -2 -1 2.1046 42.936 6.16 -87.79 0.00 1.73609e+02 [ 64] 1 -2 1 2.1046 42.936 6.16 87.79 -0.00 1.73609e+02 [ 65] -1 2 -1 2.1046 42.936 6.16 87.79 0.00 1.73609e+02 [ 66] 1 2 -1 2.1046 42.936 6.16 -87.79 0.00 1.73609e+02 [ 67] -1 -2 1 2.1046 42.936 6.16 -87.79 -0.00 1.73609e+02 [ 68] -1 2 1 2.1046 42.936 6.16 -87.79 -0.00 1.73609e+02 [ 69] 1 2 1 2.1046 42.936 6.16 87.79 -0.00 1.73609e+02 [ 70] -1 -2 -1 2.1046 42.936 6.16 87.79 0.00 1.73609e+02 [ 71] 2 -1 0 2.0638 43.829 5.88 -123.84 -0.00 3.29818e+02 [ 72] -2 1 0 2.0638 43.829 5.88 -123.84 0.00 3.29818e+02 [ 73] 2 1 0 2.0638 43.829 5.88 123.84 0.00 3.29818e+02 [ 74] -2 -1 0 2.0638 43.829 5.88 123.84 -0.00 3.29818e+02 [ 75] 0 1 -3 2.0569 43.984 5.84 0.00 -0.00 7.34977e-12 [ 76] 0 -1 3 2.0569 43.984 5.84 0.00 0.00 7.34977e-12 [ 77] 0 1 3 2.0569 43.984 5.84 0.00 -0.00 2.45765e-12 [ 78] 0 -1 -3 2.0569 43.984 5.84 0.00 0.00 2.45765e-12 [ 79] 0 2 -2 2.0301 44.594 5.66 -123.55 -0.00 3.15717e+02 [ 80] 0 -2 2 2.0301 44.594 5.66 -123.55 0.00 3.15717e+02 [ 81] 0 2 2 2.0301 44.594 5.66 -123.55 -0.00 3.15717e+02 [ 82] 0 -2 -2 2.0301 44.594 5.66 -123.55 0.00 3.15717e+02 [ 83] 1 0 -3 2.0133 44.987 5.55 179.02 -0.00 6.49922e+02 [ 84] -1 0 3 2.0133 44.987 5.55 179.02 0.00 6.49922e+02 [ 85] -1 0 -3 2.0133 44.987 5.55 -179.02 0.00 6.49921e+02 [ 86] 1 0 3 2.0133 44.987 5.55 -179.02 -0.00 6.49921e+02 [ 87] -2 1 1 1.9735 45.945 5.29 -89.99 0.00 1.56571e+02 [ 88] 2 -1 -1 1.9735 45.945 5.29 -89.99 -0.00 1.56571e+02 [ 89] -2 1 -1 1.9735 45.945 5.29 89.99 0.00 1.56571e+02 [ 90] 2 1 -1 1.9735 45.945 5.29 -89.99 0.00 1.56571e+02 [ 91] -2 -1 1 1.9735 45.945 5.29 -89.99 -0.00 1.56571e+02 [ 92] 2 -1 1 1.9735 45.945 5.29 89.99 -0.00 1.56571e+02 [ 93] 2 1 1 1.9735 45.945 5.29 89.99 -0.00 1.56571e+02 [ 94] -2 -1 -1 1.9735 45.945 5.29 89.99 0.00 1.56571e+02 [ 95] 2 0 -2 1.8766 48.465 4.69 -20.35 -0.00 7.09444e+00 [ 96] -2 0 2 1.8766 48.465 4.69 -20.35 0.00 7.09444e+00 [ 97] -2 0 -2 1.8766 48.465 4.69 -20.35 -0.00 7.09442e+00 [ 98] 2 0 2 1.8766 48.465 4.69 -20.35 0.00 7.09442e+00 [ 99] 1 1 -3 1.8719 48.596 4.66 -75.63 -0.00 9.73801e+01 [ 100] -1 -1 3 1.8719 48.596 4.66 -75.63 0.00 9.73801e+01 [ 101] -1 1 3 1.8719 48.596 4.66 75.63 -0.00 9.73801e+01 [ 102] -1 1 -3 1.8719 48.596 4.66 -75.63 0.00 9.73801e+01 [ 103] 1 -1 3 1.8719 48.596 4.66 -75.63 -0.00 9.73801e+01 [ 104] 1 -1 -3 1.8719 48.596 4.66 75.63 0.00 9.73801e+01 [ 105] -1 -1 -3 1.8719 48.596 4.66 75.63 -0.00 9.73801e+01 [ 106] 1 1 3 1.8719 48.596 4.66 75.63 0.00 9.73801e+01 [ 107] -1 2 -2 1.8517 49.161 4.54 102.28 0.00 1.73497e+02 [ 108] -1 -2 2 1.8517 49.161 4.54 -102.28 -0.00 1.73497e+02 [ 109] 1 -2 2 1.8517 49.161 4.54 102.28 -0.00 1.73497e+02 [ 110] 1 -2 -2 1.8517 49.161 4.54 102.28 0.00 1.73498e+02 [ 111] -1 2 2 1.8517 49.161 4.54 102.28 -0.00 1.73498e+02 [ 112] 1 2 -2 1.8517 49.161 4.54 -102.28 0.00 1.73497e+02 [ 113] -1 -2 -2 1.8517 49.161 4.54 -102.28 0.00 1.73497e+02 [ 114] 1 2 2 1.8517 49.161 4.54 -102.28 -0.00 1.73497e+02 [ 115] 2 -1 2 1.7605 51.891 4.01 -63.81 -0.00 5.97077e+01 [ 116] -2 -1 2 1.7605 51.891 4.01 63.81 0.00 5.97077e+01 [ 117] -2 1 2 1.7605 51.891 4.01 -63.81 -0.00 5.97077e+01 [ 118] 2 1 -2 1.7605 51.891 4.01 63.81 -0.00 5.97077e+01 [ 119] 2 -1 -2 1.7605 51.891 4.01 -63.81 0.00 5.97077e+01 [ 120] -2 1 -2 1.7605 51.891 4.01 -63.81 0.00 5.97077e+01 [ 121] 2 1 2 1.7605 51.891 4.01 63.81 -0.00 5.97076e+01 [ 122] -2 -1 -2 1.7605 51.891 4.01 63.81 0.00 5.97076e+01 [ 123] 0 -3 0 1.6946 54.071 3.65 0.00 -0.00 1.58602e-12 [ 124] 0 3 0 1.6946 54.071 3.65 0.00 0.00 1.58602e-12 [ 125] -2 2 0 1.6882 54.291 3.62 9.77 0.00 1.26169e+00 [ 126] 2 -2 0 1.6882 54.291 3.62 9.77 -0.00 1.26169e+00 [ 127] 2 2 0 1.6882 54.291 3.62 9.77 0.00 1.26169e+00 [ 128] -2 -2 0 1.6882 54.291 3.62 9.77 -0.00 1.26169e+00 [ 129] 0 0 4 1.6869 54.338 3.61 69.06 0.00 6.29810e+01 [ 130] 0 0 -4 1.6869 54.338 3.61 69.06 -0.00 6.29810e+01 [ 131] 0 2 -3 1.6844 54.423 3.60 80.18 -0.00 8.45894e+01 [ 132] 0 -2 3 1.6844 54.423 3.60 80.18 0.00 8.45894e+01 [ 133] 0 -2 -3 1.6844 54.423 3.60 -80.18 -0.00 8.45895e+01 [ 134] 0 2 3 1.6844 54.423 3.60 -80.18 0.00 8.45895e+01 [ 135] 0 -3 1 1.6435 55.894 3.39 0.00 0.00 3.07872e-11 [ 136] 0 3 -1 1.6435 55.894 3.39 0.00 -0.00 3.07872e-11 [ 137] 0 -3 -1 1.6435 55.894 3.39 0.00 -0.00 2.16399e-11 [ 138] 0 3 1 1.6435 55.894 3.39 0.00 0.00 2.16399e-11 [ 139] 2 -2 -1 1.6377 56.109 3.36 43.80 -0.00 2.35532e+01 [ 140] 2 -2 1 1.6377 56.109 3.36 -43.80 -0.00 2.35532e+01 [ 141] -2 2 -1 1.6377 56.109 3.36 -43.80 0.00 2.35532e+01 [ 142] -2 2 1 1.6377 56.109 3.36 43.80 0.00 2.35532e+01 [ 143] 2 2 -1 1.6377 56.109 3.36 -43.80 0.00 2.35532e+01 [ 144] -2 -2 1 1.6377 56.109 3.36 -43.80 -0.00 2.35532e+01 [ 145] 2 2 1 1.6377 56.109 3.36 43.80 0.00 2.35531e+01 [ 146] -2 -2 -1 1.6377 56.109 3.36 43.80 -0.00 2.35531e+01 [ 147] 0 -1 4 1.6010 57.514 3.18 0.00 0.00 2.42385e-13 [ 148] 0 1 -4 1.6010 57.514 3.18 0.00 -0.00 2.42385e-13 [ 149] 0 1 4 1.6010 57.514 3.18 0.00 0.00 9.36270e-12 [ 150] 0 -1 -4 1.6010 57.514 3.18 0.00 -0.00 9.36270e-12 [ 151] 2 0 -3 1.5936 57.807 3.14 0.00 -0.00 4.64899e-13 [ 152] -2 0 3 1.5936 57.807 3.14 0.00 0.00 4.64899e-13 [ 153] 2 0 3 1.5936 57.807 3.14 -0.00 -0.00 6.90277e-12 [ 154] -2 0 -3 1.5936 57.807 3.14 -0.00 0.00 6.90277e-12 [ 155] 1 -3 0 1.5866 58.088 3.10 94.36 0.00 1.01055e+02 [ 156] -1 3 0 1.5866 58.088 3.10 94.36 -0.00 1.01055e+02 [ 157] -1 -3 0 1.5866 58.088 3.10 94.36 0.00 1.01055e+02 [ 158] 1 3 0 1.5866 58.088 3.10 94.36 -0.00 1.01055e+02 [ 159] -1 0 4 1.5803 58.343 3.07 0.00 0.00 4.48203e-12 [ 160] 1 0 -4 1.5803 58.343 3.07 0.00 -0.00 4.48203e-12 [ 161] -1 0 -4 1.5803 58.343 3.07 0.00 0.00 4.81998e-12 [ 162] 1 0 4 1.5803 58.343 3.07 0.00 -0.00 4.81998e-12 [ 163] -1 -2 3 1.5782 58.424 3.06 -12.68 -0.00 1.79998e+00 [ 164] -1 2 -3 1.5782 58.424 3.06 12.68 0.00 1.79999e+00 [ 165] 1 2 -3 1.5782 58.424 3.06 -12.68 0.00 1.79998e+00 [ 166] 1 -2 3 1.5782 58.424 3.06 12.68 -0.00 1.79999e+00 [ 167] -1 2 3 1.5782 58.424 3.06 -12.68 -0.00 1.79999e+00 [ 168] 1 -2 -3 1.5782 58.424 3.06 -12.68 0.00 1.79999e+00 [ 169] -1 -2 -3 1.5782 58.424 3.06 12.68 0.00 1.80000e+00 [ 170] 1 2 3 1.5782 58.424 3.06 12.68 -0.00 1.80000e+00 [ 171] 1 -3 1 1.5445 59.831 2.91 31.17 0.00 1.03207e+01 [ 172] -1 3 -1 1.5445 59.831 2.91 31.17 -0.00 1.03207e+01 [ 173] 1 -3 -1 1.5445 59.831 2.91 -31.17 -0.00 1.03207e+01 [ 174] -1 3 1 1.5445 59.831 2.91 -31.17 0.00 1.03207e+01 [ 175] -1 -3 1 1.5445 59.831 2.91 31.17 -0.00 1.03207e+01 [ 176] 1 3 -1 1.5445 59.831 2.91 31.17 0.00 1.03207e+01 [ 177] 1 3 1 1.5444 59.831 2.91 -31.17 -0.00 1.03207e+01 [ 178] -1 -3 -1 1.5444 59.831 2.91 -31.17 0.00 1.03207e+01 [ 179] -2 1 3 1.5206 60.866 2.80 11.10 -0.00 1.25980e+00 [ 180] 2 1 -3 1.5206 60.866 2.80 11.10 -0.00 1.25980e+00 [ 181] -2 -1 3 1.5206 60.866 2.80 11.10 0.00 1.25980e+00 [ 182] 2 -1 -3 1.5206 60.866 2.80 11.10 0.00 1.25980e+00 [ 183] -2 1 -3 1.5206 60.866 2.80 -11.10 0.00 1.25979e+00 [ 184] 2 -1 3 1.5206 60.866 2.80 -11.10 -0.00 1.25979e+00 [ 185] -2 -1 -3 1.5206 60.866 2.80 -11.10 0.00 1.25979e+00 [ 186] 2 1 3 1.5206 60.866 2.80 -11.10 -0.00 1.25979e+00 [ 187] 0 3 -2 1.5143 61.149 2.77 0.00 0.00 2.73362e-11 [ 188] 0 -3 2 1.5143 61.149 2.77 0.00 -0.00 2.73362e-11 [ 189] 0 -3 -2 1.5143 61.149 2.77 -0.00 -0.00 2.05180e-11 [ 190] 0 3 2 1.5143 61.149 2.77 -0.00 0.00 2.05180e-11 [ 191] 2 -2 -2 1.5098 61.352 2.75 53.83 -0.00 2.90935e+01 [ 192] -2 2 -2 1.5098 61.352 2.75 53.83 0.00 2.90935e+01 [ 193] -2 2 2 1.5098 61.352 2.75 53.83 0.00 2.90935e+01 [ 194] 2 -2 2 1.5098 61.352 2.75 53.83 -0.00 2.90935e+01 [ 195] 2 2 -2 1.5098 61.352 2.75 53.83 -0.00 2.90935e+01 [ 196] -2 -2 2 1.5098 61.352 2.75 53.83 0.00 2.90935e+01 [ 197] -2 -2 -2 1.5098 61.352 2.75 53.83 -0.00 2.90935e+01 [ 198] 2 2 2 1.5098 61.352 2.75 53.83 0.00 2.90935e+01 [ 199] -1 -1 4 1.5090 61.385 2.74 26.61 -0.00 7.10246e+00 [ 200] 1 1 -4 1.5090 61.385 2.74 26.61 0.00 7.10246e+00 [ 201] 1 -1 4 1.5090 61.385 2.74 26.61 -0.00 7.10246e+00 [ 202] 1 -1 -4 1.5090 61.385 2.74 26.61 0.00 7.10244e+00 [ 203] -1 1 -4 1.5090 61.385 2.74 26.61 0.00 7.10246e+00 [ 204] -1 1 4 1.5090 61.385 2.74 26.61 -0.00 7.10244e+00 [ 205] 1 1 4 1.5090 61.385 2.74 26.61 -0.00 7.10247e+00 [ 206] -1 -1 -4 1.5090 61.385 2.74 26.61 0.00 7.10247e+00 [ 207] 3 0 0 1.5055 61.544 2.73 0.00 -0.00 3.22725e-14 [ 208] -3 0 0 1.5055 61.544 2.73 0.00 0.00 3.22725e-14 [ 209] -3 0 -1 1.4694 63.229 2.57 -8.70 -0.00 7.11090e-01 [ 210] -3 0 1 1.4694 63.229 2.57 8.70 -0.00 7.11090e-01 [ 211] 3 0 1 1.4694 63.229 2.57 -8.70 0.00 7.11090e-01 [ 212] 3 0 -1 1.4694 63.229 2.57 8.70 0.00 7.11090e-01 [ 213] 3 -1 0 1.4435 64.496 2.46 -5.21 -0.00 2.44131e-01 [ 214] -3 1 0 1.4435 64.496 2.46 -5.21 0.00 2.44131e-01 [ 215] -3 -1 0 1.4435 64.496 2.46 -5.21 0.00 2.44133e-01 [ 216] 3 1 0 1.4435 64.496 2.46 -5.21 -0.00 2.44133e-01 [ 217] 1 -3 2 1.4357 64.889 2.43 12.90 0.00 1.47724e+00 [ 218] 1 3 -2 1.4357 64.889 2.43 12.90 0.00 1.47723e+00 [ 219] -1 -3 2 1.4357 64.889 2.43 12.90 -0.00 1.47723e+00 [ 220] -1 3 -2 1.4357 64.889 2.43 12.90 -0.00 1.47724e+00 [ 221] -1 3 2 1.4357 64.889 2.43 12.90 -0.00 1.47724e+00 [ 222] 1 -3 -2 1.4357 64.889 2.43 12.90 0.00 1.47724e+00 [ 223] -1 -3 -2 1.4357 64.889 2.43 12.90 -0.00 1.47724e+00 [ 224] 1 3 2 1.4357 64.889 2.43 12.90 0.00 1.47724e+00 [ 225] -3 1 -1 1.4116 66.140 2.33 29.29 0.00 7.31501e+00 [ 226] -3 1 1 1.4116 66.140 2.33 -29.29 -0.00 7.31502e+00 [ 227] 3 -1 1 1.4116 66.140 2.33 29.29 -0.00 7.31501e+00 [ 228] 3 -1 -1 1.4116 66.140 2.33 -29.29 0.00 7.31502e+00 [ 229] -3 -1 1 1.4116 66.140 2.33 29.29 -0.00 7.31502e+00 [ 230] 3 1 1 1.4116 66.140 2.33 -29.29 -0.00 7.31503e+00 [ 231] 3 1 -1 1.4116 66.140 2.33 29.29 0.00 7.31502e+00 [ 232] -3 -1 -1 1.4116 66.140 2.33 -29.29 0.00 7.31503e+00 [ 233] 0 2 -4 1.4055 66.462 2.31 56.70 -0.00 2.71268e+01 [ 234] 0 -2 4 1.4055 66.462 2.31 56.70 0.00 2.71268e+01 [ 235] 0 -2 -4 1.4055 66.462 2.31 56.70 -0.00 2.71268e+01 [ 236] 0 2 4 1.4055 66.462 2.31 56.70 0.00 2.71268e+01 [ 237] -3 0 2 1.3748 68.147 2.19 0.00 -0.00 3.71400e-13 [ 238] 3 0 -2 1.3748 68.147 2.19 0.00 0.00 3.71400e-13 [ 239] 3 0 2 1.3748 68.147 2.19 -0.00 -0.00 1.23048e-11 [ 240] -3 0 -2 1.3748 68.147 2.19 -0.00 0.00 1.23048e-11 [ 241] 2 -3 0 1.3554 69.261 2.12 -14.78 0.00 1.69192e+00 [ 242] -2 3 0 1.3554 69.261 2.12 -14.78 -0.00 1.69192e+00 [ 243] -2 -3 0 1.3554 69.261 2.12 14.78 0.00 1.69193e+00 [ 244] 2 3 0 1.3554 69.261 2.12 14.78 -0.00 1.69193e+00 [ 245] 0 3 -3 1.3534 69.376 2.11 0.00 0.00 7.15561e-12 [ 246] 0 -3 3 1.3534 69.376 2.11 0.00 -0.00 7.15561e-12 [ 247] 0 3 3 1.3534 69.376 2.11 0.00 -0.00 7.99298e-13 [ 248] 0 -3 -3 1.3534 69.376 2.11 0.00 0.00 7.99298e-13 [ 249] -2 0 4 1.3515 69.492 2.10 -20.53 -0.00 3.24226e+00 [ 250] 2 0 -4 1.3515 69.492 2.10 -20.53 0.00 3.24226e+00 [ 251] -2 0 -4 1.3515 69.492 2.10 -20.53 0.00 3.24227e+00 [ 252] 2 0 4 1.3515 69.492 2.10 -20.53 -0.00 3.24227e+00 [ 253] -2 2 3 1.3502 69.567 2.10 25.44 -0.00 4.96378e+00 [ 254] -2 2 -3 1.3502 69.567 2.10 -25.44 0.00 4.96379e+00 [ 255] 2 2 -3 1.3502 69.567 2.10 -25.44 -0.00 4.96378e+00 [ 256] 2 -2 3 1.3502 69.567 2.10 -25.44 -0.00 4.96379e+00 [ 257] -2 -2 3 1.3502 69.567 2.10 -25.44 0.00 4.96378e+00 [ 258] 2 -2 -3 1.3502 69.567 2.10 25.44 0.00 4.96378e+00 [ 259] 2 2 3 1.3502 69.567 2.10 25.44 0.00 4.96378e+00 [ 260] -2 -2 -3 1.3502 69.567 2.10 25.44 -0.00 4.96378e+00 [ 261] 0 0 5 1.3495 69.607 2.10 0.00 -0.00 3.56505e-12 [ 262] 0 0 -5 1.3495 69.607 2.10 0.00 0.00 3.56505e-12 [ 263] 1 2 -4 1.3420 70.051 2.07 33.01 -0.00 8.24119e+00 [ 264] -1 -2 4 1.3420 70.051 2.07 33.01 0.00 8.24119e+00 [ 265] 1 -2 4 1.3420 70.051 2.07 -33.01 0.00 8.24117e+00 [ 266] -1 2 -4 1.3420 70.051 2.07 -33.01 -0.00 8.24117e+00 [ 267] 1 -2 -4 1.3420 70.051 2.07 -33.01 -0.00 8.24118e+00 [ 268] -1 2 4 1.3420 70.051 2.07 -33.01 0.00 8.24118e+00 [ 269] 1 2 4 1.3420 70.051 2.07 33.01 0.00 8.24117e+00 [ 270] -1 -2 -4 1.3420 70.051 2.07 33.01 -0.00 8.24117e+00 [ 271] 2 -3 1 1.3289 70.850 2.02 -7.63 -0.00 4.30682e-01 [ 272] -2 3 1 1.3289 70.850 2.02 7.63 -0.00 4.30680e-01 [ 273] 2 -3 -1 1.3289 70.850 2.02 7.63 0.00 4.30680e-01 [ 274] -2 3 -1 1.3289 70.850 2.02 -7.63 0.00 4.30682e-01 [ 275] -2 -3 -1 1.3289 70.850 2.02 -7.63 0.00 4.30683e-01 [ 276] 2 3 -1 1.3289 70.850 2.02 7.63 0.00 4.30684e-01 [ 277] -2 -3 1 1.3289 70.850 2.02 7.63 -0.00 4.30684e-01 [ 278] 2 3 1 1.3289 70.850 2.02 -7.63 -0.00 4.30683e-01 [ 279] -3 1 2 1.3272 70.954 2.02 93.40 -0.00 6.43276e+01 [ 280] 3 -1 -2 1.3272 70.954 2.02 93.40 0.00 6.43276e+01 [ 281] 3 -1 2 1.3272 70.954 2.02 93.40 0.00 6.43275e+01 [ 282] -3 1 -2 1.3272 70.954 2.02 93.40 -0.00 6.43275e+01 [ 283] 3 1 -2 1.3272 70.954 2.02 93.40 -0.00 6.43275e+01 [ 284] -3 -1 2 1.3272 70.954 2.02 93.40 0.00 6.43275e+01 [ 285] 3 1 2 1.3272 70.954 2.02 93.40 -0.00 6.43275e+01 [ 286] -3 -1 -2 1.3272 70.954 2.02 93.40 0.00 6.43275e+01 [ 287] -2 -1 4 1.3061 72.277 1.95 2.23 -0.00 3.54406e-02 [ 288] 2 1 -4 1.3061 72.277 1.95 2.23 0.00 3.54406e-02 [ 289] -2 1 -4 1.3061 72.277 1.95 -2.23 -0.00 3.54413e-02 [ 290] -2 1 4 1.3061 72.277 1.95 -2.23 0.00 3.54416e-02 [ 291] 2 -1 -4 1.3061 72.277 1.95 -2.23 -0.00 3.54416e-02 [ 292] 2 -1 4 1.3061 72.277 1.95 -2.23 0.00 3.54413e-02 [ 293] -2 -1 -4 1.3061 72.277 1.95 2.23 -0.00 3.54417e-02 [ 294] 2 1 4 1.3061 72.277 1.95 2.23 0.00 3.54417e-02 [ 295] 0 1 -5 1.3043 72.390 1.94 0.00 -0.00 3.75253e-12 [ 296] 0 -1 5 1.3043 72.390 1.94 0.00 0.00 3.75253e-12 [ 297] 0 -1 -5 1.3043 72.390 1.94 0.00 -0.00 3.33216e-12 [ 298] 0 1 5 1.3043 72.390 1.94 0.00 0.00 3.33216e-12 [ 299] -1 3 -3 1.2965 72.899 1.91 -15.68 -0.00 1.71959e+00 [ 300] 1 -3 3 1.2965 72.899 1.91 -15.68 0.00 1.71959e+00 [ 301] 1 -3 -3 1.2965 72.899 1.91 15.68 -0.00 1.71958e+00 [ 302] 1 3 -3 1.2965 72.899 1.91 -15.68 0.00 1.71958e+00 [ 303] -1 3 3 1.2965 72.899 1.91 15.68 0.00 1.71958e+00 [ 304] -1 -3 3 1.2965 72.899 1.91 -15.68 -0.00 1.71958e+00 [ 305] 1 3 3 1.2965 72.899 1.91 15.68 0.00 1.71958e+00 [ 306] -1 -3 -3 1.2965 72.899 1.91 15.68 -0.00 1.71958e+00 [ 307] 3 -2 0 1.2953 72.973 1.91 -8.15 -0.00 4.63331e-01 [ 308] -3 2 0 1.2953 72.973 1.91 -8.15 0.00 4.63331e-01 [ 309] -3 -2 0 1.2953 72.973 1.91 8.15 -0.00 4.63333e-01 [ 310] 3 2 0 1.2953 72.973 1.91 8.15 0.00 4.63333e-01 [ 311] -1 0 5 1.2930 73.125 1.90 41.90 -0.00 1.22086e+01 [ 312] 1 0 -5 1.2930 73.125 1.90 41.90 0.00 1.22086e+01 [ 313] -1 0 -5 1.2930 73.125 1.90 -41.90 0.00 1.22086e+01 [ 314] 1 0 5 1.2930 73.125 1.90 -41.90 -0.00 1.22086e+01 [ 315] -3 2 1 1.2721 74.528 1.84 -0.01 0.00 3.12189e-07 [ 316] 3 -2 -1 1.2721 74.528 1.84 -0.01 -0.00 3.12189e-07 [ 317] 3 -2 1 1.2721 74.528 1.84 0.01 0.00 3.12075e-07 [ 318] -3 2 -1 1.2721 74.528 1.84 0.01 -0.00 3.12075e-07 [ 319] 3 2 1 1.2721 74.528 1.84 0.01 0.00 3.12311e-07 [ 320] 3 2 -1 1.2721 74.528 1.84 -0.01 0.00 3.11244e-07 [ 321] -3 -2 1 1.2721 74.528 1.84 -0.01 -0.00 3.11244e-07 [ 322] -3 -2 -1 1.2721 74.528 1.84 0.01 -0.00 3.12311e-07 [ 323] 0 -4 0 1.2709 74.610 1.83 -12.44 -0.00 1.03566e+00 [ 324] 0 4 0 1.2709 74.610 1.83 -12.44 0.00 1.03566e+00 [ 325] 2 3 -2 1.2577 75.531 1.79 -39.33 -0.00 1.01329e+01 [ 326] -2 -3 2 1.2577 75.531 1.79 -39.33 0.00 1.01329e+01 [ 327] -2 3 -2 1.2577 75.531 1.79 39.33 -0.00 1.01329e+01 [ 328] -2 3 2 1.2577 75.531 1.79 39.33 0.00 1.01329e+01 [ 329] 2 -3 2 1.2577 75.531 1.79 39.33 0.00 1.01329e+01 [ 330] 2 -3 -2 1.2577 75.531 1.79 39.33 -0.00 1.01329e+01 [ 331] 2 3 2 1.2577 75.531 1.79 -39.33 -0.00 1.01329e+01 [ 332] -2 -3 -2 1.2577 75.531 1.79 -39.33 0.00 1.01329e+01 [ 333] -1 -1 5 1.2531 75.855 1.78 -31.85 -0.00 6.59241e+00 [ 334] 1 1 -5 1.2531 75.855 1.78 -31.85 0.00 6.59241e+00 [ 335] -1 1 5 1.2531 75.855 1.78 31.85 0.00 6.59245e+00 [ 336] 1 -1 -5 1.2531 75.855 1.78 31.85 -0.00 6.59245e+00 [ 337] 1 -1 5 1.2531 75.855 1.78 -31.85 -0.00 6.59243e+00 [ 338] -1 1 -5 1.2531 75.855 1.78 -31.85 0.00 6.59243e+00 [ 339] 1 1 5 1.2531 75.855 1.78 31.85 -0.00 6.59244e+00 [ 340] -1 -1 -5 1.2531 75.855 1.78 31.85 0.00 6.59244e+00 [ 341] 3 0 -3 1.2511 76.000 1.77 -8.55 0.00 4.74000e-01 [ 342] -3 0 3 1.2511 76.000 1.77 -8.55 -0.00 4.74000e-01 [ 343] 3 0 3 1.2511 76.000 1.77 8.55 0.00 4.73994e-01 [ 344] -3 0 -3 1.2511 76.000 1.77 8.55 -0.00 4.73994e-01 [ 345] 0 4 -1 1.2490 76.153 1.77 5.89 0.00 2.24231e-01 [ 346] 0 -4 1 1.2490 76.153 1.77 5.89 -0.00 2.24231e-01 [ 347] 0 -4 -1 1.2490 76.153 1.77 -5.89 0.00 2.24233e-01 [ 348] 0 4 1 1.2490 76.153 1.77 -5.89 -0.00 2.24233e-01 [ 349] 1 -4 0 1.2234 78.040 1.69 -129.24 -0.00 1.03398e+02 [ 350] -1 4 0 1.2234 78.040 1.69 -129.24 0.00 1.03398e+02 [ 351] 1 4 0 1.2234 78.040 1.69 129.24 0.00 1.03398e+02 [ 352] -1 -4 0 1.2234 78.040 1.69 129.24 -0.00 1.03398e+02 [ 353] -3 1 -3 1.2148 78.696 1.67 102.87 -0.00 6.46104e+01 [ 354] 3 -1 -3 1.2148 78.696 1.67 -102.87 0.00 6.46103e+01 [ 355] 3 -1 3 1.2148 78.696 1.67 102.87 0.00 6.46104e+01 [ 356] -3 -1 3 1.2148 78.696 1.67 102.87 0.00 6.46104e+01 [ 357] -3 1 3 1.2148 78.696 1.67 -102.87 -0.00 6.46103e+01 [ 358] 3 1 -3 1.2148 78.696 1.67 102.87 -0.00 6.46104e+01 [ 359] -3 -1 -3 1.2148 78.696 1.67 -102.87 -0.00 6.46104e+01 [ 360] 3 1 3 1.2148 78.696 1.67 -102.87 0.00 6.46104e+01 [ 361] 3 -2 2 1.2093 79.130 1.66 6.81 0.00 2.80745e-01 [ 362] -3 2 -2 1.2093 79.130 1.66 6.81 -0.00 2.80745e-01 [ 363] 3 2 -2 1.2093 79.130 1.66 -6.81 0.00 2.80745e-01 [ 364] 3 -2 -2 1.2093 79.130 1.66 6.81 0.00 2.80747e-01 [ 365] -3 2 2 1.2093 79.130 1.66 6.81 -0.00 2.80747e-01 [ 366] -3 -2 2 1.2093 79.130 1.66 -6.81 -0.00 2.80745e-01 [ 367] -3 -2 -2 1.2093 79.130 1.66 -6.81 -0.00 2.80742e-01 [ 368] 3 2 2 1.2093 79.130 1.66 -6.81 0.00 2.80742e-01 [ 369] 1 -4 1 1.2038 79.562 1.64 39.62 0.00 9.41870e+00 [ 370] -1 4 -1 1.2038 79.562 1.64 39.62 -0.00 9.41870e+00 [ 371] -1 4 1 1.2038 79.562 1.64 -39.62 0.00 9.41870e+00 [ 372] -1 -4 1 1.2038 79.562 1.64 -39.62 -0.00 9.41871e+00 [ 373] 1 -4 -1 1.2038 79.562 1.64 -39.62 -0.00 9.41870e+00 [ 374] 1 4 -1 1.2038 79.562 1.64 -39.62 0.00 9.41871e+00 [ 375] 1 4 1 1.2038 79.562 1.64 39.62 0.00 9.41871e+00 [ 376] -1 -4 -1 1.2038 79.562 1.64 39.62 -0.00 9.41871e+00 [ 377] 0 3 -4 1.1955 80.224 1.62 0.00 -0.00 2.38597e-12 [ 378] 0 -3 4 1.1955 80.224 1.62 0.00 0.00 2.38597e-12 [ 379] 0 3 4 1.1955 80.224 1.62 -0.00 -0.00 7.41172e-12 [ 380] 0 -3 -4 1.1955 80.224 1.62 -0.00 0.00 7.41172e-12 [ 381] -2 2 4 1.1933 80.405 1.61 -25.85 -0.00 3.94445e+00 [ 382] 2 -2 -4 1.1933 80.405 1.61 -25.85 0.00 3.94445e+00 [ 383] -2 2 -4 1.1933 80.405 1.61 -25.85 0.00 3.94445e+00 [ 384] -2 -2 4 1.1933 80.405 1.61 -25.85 0.00 3.94446e+00 [ 385] 2 2 -4 1.1933 80.405 1.61 -25.85 -0.00 3.94446e+00 [ 386] 2 -2 4 1.1933 80.405 1.61 -25.85 -0.00 3.94445e+00 [ 387] 2 2 4 1.1933 80.405 1.61 -25.85 -0.00 3.94443e+00 [ 388] -2 -2 -4 1.1933 80.405 1.61 -25.85 0.00 3.94443e+00 [ 389] 0 2 -5 1.1919 80.514 1.61 95.09 0.00 5.32706e+01 [ 390] 0 -2 5 1.1919 80.514 1.61 95.09 -0.00 5.32706e+01 [ 391] 0 2 5 1.1919 80.514 1.61 -95.09 -0.00 5.32706e+01 [ 392] 0 -2 -5 1.1919 80.514 1.61 -95.09 0.00 5.32706e+01 [ 393] 0 4 -2 1.1893 80.726 1.61 -43.61 -0.00 1.11589e+01 [ 394] 0 -4 2 1.1893 80.726 1.61 -43.61 0.00 1.11589e+01 [ 395] 0 -4 -2 1.1893 80.726 1.61 -43.61 -0.00 1.11589e+01 [ 396] 0 4 2 1.1893 80.726 1.61 -43.61 0.00 1.11589e+01 [ 397] 2 3 -3 1.1609 83.134 1.54 112.37 -0.00 7.10745e+01 [ 398] 2 -3 -3 1.1609 83.134 1.54 112.37 0.00 7.10746e+01 [ 399] -2 3 -3 1.1609 83.134 1.54 -112.37 0.00 7.10746e+01 [ 400] -2 -3 3 1.1609 83.134 1.54 112.37 0.00 7.10745e+01 [ 401] 2 -3 3 1.1609 83.134 1.54 -112.37 -0.00 7.10746e+01 [ 402] -2 3 3 1.1609 83.134 1.54 112.37 -0.00 7.10746e+01 [ 403] -2 -3 -3 1.1609 83.134 1.54 -112.37 0.00 7.10744e+01 [ 404] 2 3 3 1.1609 83.134 1.54 -112.37 -0.00 7.10744e+01 [ 405] 2 0 -5 1.1584 83.352 1.53 0.00 -0.00 2.96191e-12 [ 406] -2 0 5 1.1584 83.352 1.53 0.00 0.00 2.96191e-12 [ 407] 2 0 5 1.1584 83.352 1.53 0.00 -0.00 1.31480e-12 [ 408] -2 0 -5 1.1584 83.352 1.53 0.00 0.00 1.31480e-12 [ 409] 1 3 -4 1.1557 83.591 1.53 20.82 -0.00 2.42210e+00 [ 410] 1 -3 4 1.1557 83.591 1.53 20.82 -0.00 2.42211e+00 [ 411] -1 3 -4 1.1557 83.591 1.53 20.82 0.00 2.42211e+00 [ 412] -1 -3 4 1.1557 83.591 1.53 20.82 0.00 2.42210e+00 [ 413] 1 -3 -4 1.1557 83.591 1.53 20.82 -0.00 2.42210e+00 [ 414] -1 3 4 1.1557 83.591 1.53 20.82 0.00 2.42210e+00 [ 415] 1 3 4 1.1557 83.591 1.53 20.82 0.00 2.42211e+00 [ 416] -1 -3 -4 1.1557 83.591 1.53 20.82 -0.00 2.42211e+00 [ 417] 1 2 -5 1.1525 83.879 1.52 -86.80 0.00 4.19210e+01 [ 418] -1 -2 5 1.1525 83.879 1.52 -86.80 -0.00 4.19210e+01 [ 419] 1 -2 -5 1.1525 83.879 1.52 -86.80 0.00 4.19210e+01 [ 420] -1 2 5 1.1525 83.879 1.52 -86.80 -0.00 4.19210e+01 [ 421] -1 2 -5 1.1525 83.879 1.52 86.80 0.00 4.19210e+01 [ 422] 1 -2 5 1.1525 83.879 1.52 86.80 -0.00 4.19210e+01 [ 423] -1 -2 -5 1.1525 83.879 1.52 86.80 -0.00 4.19210e+01 [ 424] 1 2 5 1.1525 83.879 1.52 86.80 0.00 4.19210e+01 [ 425] -1 4 -2 1.1501 84.089 1.52 -20.97 0.00 2.43782e+00 [ 426] 1 -4 2 1.1501 84.089 1.52 -20.97 -0.00 2.43782e+00 [ 427] 1 4 -2 1.1501 84.089 1.52 20.97 -0.00 2.43782e+00 [ 428] -1 4 2 1.1501 84.089 1.52 -20.97 0.00 2.43782e+00 [ 429] -1 -4 2 1.1501 84.089 1.52 20.97 0.00 2.43782e+00 [ 430] 1 -4 -2 1.1501 84.089 1.52 -20.97 -0.00 2.43782e+00 [ 431] 1 4 2 1.1501 84.089 1.52 20.97 0.00 2.43782e+00 [ 432] -1 -4 -2 1.1501 84.089 1.52 20.97 -0.00 2.43782e+00 [ 433] -2 -1 5 1.1295 85.994 1.48 -82.26 -0.00 3.65379e+01 [ 434] 2 1 -5 1.1295 85.994 1.48 -82.26 0.00 3.65379e+01 [ 435] 2 -1 5 1.1295 85.994 1.48 82.26 0.00 3.65379e+01 [ 436] -2 1 -5 1.1295 85.994 1.48 82.26 -0.00 3.65379e+01 [ 437] 2 -1 -5 1.1295 85.994 1.48 -82.26 -0.00 3.65379e+01 [ 438] -2 1 5 1.1295 85.994 1.48 -82.26 0.00 3.65379e+01 [ 439] 2 1 5 1.1295 85.994 1.48 82.26 -0.00 3.65379e+01 [ 440] -2 -1 -5 1.1295 85.994 1.48 82.26 0.00 3.65379e+01 [ 441] -4 0 0 1.1291 86.026 1.48 -76.83 -0.00 3.18648e+01 [ 442] 4 0 0 1.1291 86.026 1.48 -76.83 0.00 3.18648e+01 [ 443] 3 -3 0 1.1255 86.373 1.47 -136.32 0.00 9.98690e+01 [ 444] -3 3 0 1.1255 86.373 1.47 -136.32 -0.00 9.98690e+01 [ 445] 3 3 0 1.1255 86.373 1.47 -136.32 0.00 9.98689e+01 [ 446] -3 -3 0 1.1255 86.373 1.47 -136.32 -0.00 9.98689e+01 [ 447] 0 0 6 1.1246 86.459 1.47 -136.54 0.00 1.00085e+02 [ 448] 0 0 -6 1.1246 86.459 1.47 -136.54 -0.00 1.00085e+02 [ 449] -3 0 4 1.1232 86.589 1.47 -0.00 0.00 9.52195e-13 [ 450] 3 0 -4 1.1232 86.589 1.47 -0.00 -0.00 9.52195e-13 [ 451] 3 0 4 1.1232 86.589 1.47 0.00 0.00 1.28940e-11 [ 452] -3 0 -4 1.1232 86.589 1.47 0.00 -0.00 1.28940e-11 [ 453] -3 2 3 1.1225 86.659 1.46 0.51 0.00 1.40791e-03 [ 454] -3 2 -3 1.1225 86.659 1.46 -0.51 -0.00 1.40785e-03 [ 455] 3 -2 -3 1.1225 86.659 1.46 0.51 -0.00 1.40791e-03 [ 456] 3 2 -3 1.1225 86.659 1.46 0.51 -0.00 1.40798e-03 [ 457] 3 -2 3 1.1225 86.659 1.46 -0.51 0.00 1.40785e-03 [ 458] -3 -2 3 1.1225 86.659 1.46 0.51 0.00 1.40798e-03 [ 459] -3 -2 -3 1.1225 86.659 1.46 -0.51 -0.00 1.40808e-03 [ 460] 3 2 3 1.1225 86.659 1.46 -0.51 0.00 1.40808e-03 [ 461] 4 0 -1 1.1136 87.522 1.45 0.00 -0.00 4.11234e-12 [ 462] -4 0 1 1.1136 87.522 1.45 0.00 0.00 4.11234e-12 [ 463] 4 0 1 1.1136 87.522 1.45 0.00 -0.00 2.66310e-12 [ 464] -4 0 -1 1.1136 87.522 1.45 0.00 0.00 2.66310e-12 [ 465] -3 3 1 1.1101 87.868 1.44 39.58 -0.00 8.27236e+00 [ 466] -3 3 -1 1.1101 87.868 1.44 -39.58 0.00 8.27236e+00 [ 467] 3 -3 -1 1.1101 87.868 1.44 39.58 0.00 8.27236e+00 [ 468] 3 -3 1 1.1101 87.868 1.44 -39.58 -0.00 8.27236e+00 [ 469] 3 3 -1 1.1101 87.868 1.44 -39.58 0.00 8.27236e+00 [ 470] -3 -3 1 1.1101 87.868 1.44 -39.58 -0.00 8.27236e+00 [ 471] -3 -3 -1 1.1101 87.868 1.44 39.58 0.00 8.27237e+00 [ 472] 3 3 1 1.1101 87.868 1.44 39.58 -0.00 8.27237e+00 [ 473] 2 -4 0 1.1076 88.125 1.44 -2.45 0.00 3.15950e-02 [ 474] -2 4 0 1.1076 88.125 1.44 -2.45 -0.00 3.15950e-02 [ 475] -2 -4 0 1.1076 88.125 1.44 -2.45 0.00 3.15942e-02 [ 476] 2 4 0 1.1076 88.125 1.44 -2.45 -0.00 3.15942e-02 [ 477] 0 -4 3 1.1065 88.233 1.44 -133.14 -0.00 9.32317e+01 [ 478] 0 4 -3 1.1065 88.233 1.44 -133.14 0.00 9.32317e+01 [ 479] 0 -4 -3 1.1065 88.233 1.44 133.14 -0.00 9.32316e+01 [ 480] 0 4 3 1.1065 88.233 1.44 133.14 0.00 9.32316e+01 [ 481] -4 -1 0 1.1023 88.660 1.43 -93.55 0.00 4.58242e+01 [ 482] 4 1 0 1.1023 88.660 1.43 -93.55 -0.00 4.58242e+01 [ 483] 4 -1 0 1.1023 88.660 1.43 93.55 -0.00 4.58242e+01 [ 484] -4 1 0 1.1023 88.660 1.43 93.55 0.00 4.58242e+01 [ 485] 0 1 -6 1.0980 89.092 1.43 -0.00 0.00 3.52455e-12 [ 486] 0 -1 6 1.0980 89.092 1.43 -0.00 -0.00 3.52455e-12 [ 487] 0 1 6 1.0980 89.092 1.43 -0.00 -0.00 8.19956e-13 [ 488] 0 -1 -6 1.0980 89.092 1.43 -0.00 0.00 8.19956e-13 [ 489] 3 -1 -4 1.0968 89.222 1.42 -52.32 0.00 1.42560e+01 [ 490] 3 1 -4 1.0968 89.222 1.42 -52.32 0.00 1.42560e+01 [ 491] -3 -1 4 1.0968 89.222 1.42 -52.32 -0.00 1.42560e+01 [ 492] -3 1 4 1.0968 89.222 1.42 -52.32 -0.00 1.42560e+01 [ 493] 3 -1 4 1.0968 89.222 1.42 -52.32 -0.00 1.42560e+01 [ 494] -3 1 -4 1.0968 89.222 1.42 -52.32 0.00 1.42560e+01 [ 495] 3 1 4 1.0968 89.222 1.42 -52.32 -0.00 1.42560e+01 [ 496] -3 -1 -4 1.0968 89.222 1.42 -52.32 0.00 1.42560e+01 [ 497] -2 4 -1 1.0929 89.618 1.42 -1.66 -0.00 1.42522e-02 [ 498] 2 -4 1 1.0929 89.618 1.42 -1.66 0.00 1.42522e-02 [ 499] 2 -4 -1 1.0929 89.618 1.42 1.66 -0.00 1.42521e-02 [ 500] -2 4 1 1.0929 89.618 1.42 1.66 0.00 1.42521e-02 [ 501] -2 -4 1 1.0929 89.618 1.42 -1.66 0.00 1.42523e-02 [ 502] -2 -4 -1 1.0929 89.618 1.42 1.66 0.00 1.42522e-02 [ 503] 2 4 1 1.0929 89.618 1.42 1.66 -0.00 1.42522e-02 [ 504] 2 4 -1 1.0929 89.618 1.42 -1.66 -0.00 1.42523e-02 [ 505] 1 0 -6 1.0913 89.794 1.42 0.00 0.00 8.69139e-12 [ 506] -1 0 6 1.0913 89.794 1.42 0.00 -0.00 8.69139e-12 [ 507] -1 0 -6 1.0913 89.794 1.42 0.00 -0.00 1.35774e-11 [ 508] 1 0 6 1.0913 89.794 1.42 0.00 0.00 1.35774e-11 [ 509] -4 -1 1 1.0878 90.153 1.41 52.49 -0.00 1.42239e+01 [ 510] 4 1 -1 1.0878 90.153 1.41 52.49 0.00 1.42239e+01 [ 511] 4 -1 1 1.0878 90.153 1.41 -52.49 -0.00 1.42239e+01 [ 512] 4 -1 -1 1.0878 90.153 1.41 52.49 0.00 1.42239e+01 [ 513] -4 1 1 1.0878 90.153 1.41 52.49 -0.00 1.42239e+01 [ 514] -4 1 -1 1.0878 90.153 1.41 -52.49 0.00 1.42239e+01 [ 515] 4 1 1 1.0878 90.153 1.41 -52.49 -0.00 1.42239e+01 [ 516] -4 -1 -1 1.0878 90.153 1.41 -52.49 0.00 1.42239e+01 [ 517] 1 -4 3 1.0747 91.566 1.40 -1.03 0.00 5.41523e-03 [ 518] 1 4 -3 1.0747 91.566 1.40 1.03 0.00 5.41540e-03 [ 519] -1 4 -3 1.0747 91.566 1.40 -1.03 -0.00 5.41523e-03 [ 520] -1 -4 3 1.0747 91.566 1.40 1.03 -0.00 5.41540e-03 [ 521] -1 4 3 1.0747 91.566 1.40 1.03 0.00 5.41551e-03 [ 522] 1 -4 -3 1.0747 91.566 1.40 1.03 -0.00 5.41551e-03 [ 523] -1 -4 -3 1.0747 91.566 1.40 -1.03 0.00 5.41539e-03 [ 524] 1 4 3 1.0747 91.566 1.40 -1.03 -0.00 5.41539e-03 [ 525] 4 0 2 1.0707 92.003 1.39 -7.57 -0.00 2.91533e-01 [ 526] -4 0 -2 1.0707 92.003 1.39 -7.57 0.00 2.91533e-01 [ 527] -4 0 2 1.0707 92.003 1.39 -7.57 -0.00 2.91532e-01 [ 528] 4 0 -2 1.0707 92.003 1.39 -7.57 0.00 2.91532e-01 [ 529] 3 3 -2 1.0676 92.349 1.39 -31.70 0.00 5.10608e+00 [ 530] -3 -3 2 1.0676 92.349 1.39 -31.70 -0.00 5.10608e+00 [ 531] -3 3 2 1.0676 92.349 1.39 -31.70 0.00 5.10609e+00 [ 532] 3 -3 -2 1.0676 92.349 1.39 -31.70 -0.00 5.10609e+00 [ 533] 3 -3 2 1.0676 92.349 1.39 -31.70 -0.00 5.10609e+00 [ 534] -3 3 -2 1.0676 92.349 1.39 -31.70 0.00 5.10609e+00 [ 535] -3 -3 -2 1.0676 92.349 1.39 -31.70 0.00 5.10609e+00 [ 536] 3 3 2 1.0676 92.349 1.39 -31.70 -0.00 5.10609e+00 [ 537] 1 1 -6 1.0670 92.425 1.39 -2.19 0.00 2.43242e-02 [ 538] -1 -1 6 1.0670 92.425 1.39 -2.19 -0.00 2.43242e-02 [ 539] 1 -1 6 1.0670 92.425 1.39 -2.19 -0.00 2.43244e-02 [ 540] 1 -1 -6 1.0670 92.425 1.39 -2.19 -0.00 2.43245e-02 [ 541] -1 1 6 1.0670 92.425 1.39 -2.19 0.00 2.43245e-02 [ 542] -1 1 -6 1.0670 92.425 1.39 -2.19 0.00 2.43244e-02 [ 543] -1 -1 -6 1.0670 92.425 1.39 -2.19 -0.00 2.43247e-02 [ 544] 1 1 6 1.0670 92.425 1.39 -2.19 0.00 2.43247e-02 [ 545] -2 -3 4 1.0566 93.605 1.38 25.96 0.00 3.39862e+00 [ 546] 2 -3 4 1.0566 93.605 1.38 -25.96 -0.00 3.39862e+00 [ 547] -2 3 -4 1.0566 93.605 1.38 -25.96 0.00 3.39862e+00 [ 548] 2 3 -4 1.0566 93.605 1.38 25.96 -0.00 3.39862e+00 [ 549] 2 -3 -4 1.0566 93.605 1.38 -25.96 -0.00 3.39861e+00 [ 550] -2 3 4 1.0566 93.605 1.38 -25.96 0.00 3.39861e+00 [ 551] -2 -3 -4 1.0566 93.605 1.38 25.96 -0.00 3.39861e+00 [ 552] 2 3 4 1.0566 93.605 1.38 25.96 0.00 3.39861e+00 [ 553] 0 -3 5 1.0556 93.713 1.38 0.00 0.00 1.59697e-12 [ 554] 0 3 -5 1.0556 93.713 1.38 0.00 -0.00 1.59697e-12 [ 555] 0 3 5 1.0556 93.713 1.38 0.00 0.00 3.32170e-12 [ 556] 0 -3 -5 1.0556 93.713 1.38 0.00 -0.00 3.32170e-12 [ 557] 2 -2 5 1.0541 93.892 1.38 -51.10 -0.00 1.31532e+01 [ 558] 2 2 -5 1.0541 93.892 1.38 -51.10 0.00 1.31532e+01 [ 559] -2 2 5 1.0541 93.892 1.38 51.10 0.00 1.31532e+01 [ 560] -2 2 -5 1.0541 93.892 1.38 -51.10 0.00 1.31532e+01 [ 561] -2 -2 5 1.0541 93.892 1.38 -51.10 -0.00 1.31532e+01 [ 562] 2 -2 -5 1.0541 93.892 1.38 51.10 -0.00 1.31532e+01 [ 563] 2 2 5 1.0541 93.892 1.38 51.10 -0.00 1.31532e+01 [ 564] -2 -2 -5 1.0541 93.892 1.38 51.10 0.00 1.31532e+01 [ 565] 2 -4 -2 1.0523 94.102 1.38 27.63 0.00 3.84113e+00 [ 566] 2 -4 2 1.0523 94.102 1.38 27.63 0.00 3.84113e+00 [ 567] -2 4 -2 1.0523 94.102 1.38 27.63 -0.00 3.84113e+00 [ 568] 2 4 -2 1.0523 94.102 1.38 27.63 0.00 3.84113e+00 [ 569] -2 -4 2 1.0523 94.102 1.38 27.63 -0.00 3.84113e+00 [ 570] -2 4 2 1.0523 94.102 1.38 27.63 -0.00 3.84113e+00 [ 571] 2 4 2 1.0523 94.102 1.38 27.63 0.00 3.84111e+00 [ 572] -2 -4 -2 1.0523 94.102 1.38 27.63 -0.00 3.84111e+00 [ 573] 4 1 -2 1.0478 94.638 1.37 -35.55 0.00 6.34752e+00 [ 574] -4 1 2 1.0478 94.638 1.37 35.55 0.00 6.34752e+00 [ 575] 4 -1 2 1.0478 94.638 1.37 35.55 -0.00 6.34750e+00 [ 576] 4 -1 -2 1.0478 94.638 1.37 35.55 -0.00 6.34752e+00 [ 577] -4 1 -2 1.0478 94.638 1.37 35.55 0.00 6.34750e+00 [ 578] -4 -1 2 1.0478 94.638 1.37 -35.55 -0.00 6.34752e+00 [ 579] 4 1 2 1.0478 94.638 1.37 -35.55 -0.00 6.34750e+00 [ 580] -4 -1 -2 1.0478 94.638 1.37 -35.55 0.00 6.34750e+00 [ 581] 4 -2 0 1.0319 96.566 1.37 7.06 -0.00 2.48681e-01 [ 582] -4 2 0 1.0319 96.566 1.37 7.06 0.00 2.48681e-01 [ 583] 4 2 0 1.0319 96.566 1.37 7.06 0.00 2.48684e-01 [ 584] -4 -2 0 1.0319 96.566 1.37 7.06 -0.00 2.48684e-01 [ 585] 0 -2 6 1.0284 97.001 1.37 1.82 0.00 1.65480e-02 [ 586] 0 2 -6 1.0284 97.001 1.37 1.82 -0.00 1.65480e-02 [ 587] 0 2 6 1.0284 97.001 1.37 1.82 -0.00 1.65474e-02 [ 588] 0 -2 -6 1.0284 97.001 1.37 1.82 0.00 1.65474e-02 [ 589] -1 -3 5 1.0279 97.061 1.37 26.58 -0.00 3.52489e+00 [ 590] 1 3 -5 1.0279 97.061 1.37 26.58 0.00 3.52489e+00 [ 591] -1 3 -5 1.0279 97.061 1.37 26.58 -0.00 3.52489e+00 [ 592] -1 3 5 1.0279 97.061 1.37 -26.58 -0.00 3.52489e+00 [ 593] 1 -3 5 1.0279 97.061 1.37 26.58 0.00 3.52489e+00 [ 594] 1 -3 -5 1.0279 97.061 1.37 -26.58 0.00 3.52489e+00 [ 595] 1 3 5 1.0279 97.061 1.37 -26.58 -0.00 3.52490e+00 [ 596] -1 -3 -5 1.0279 97.061 1.37 -26.58 0.00 3.52490e+00 [ 597] 3 -2 -4 1.0274 97.132 1.36 -6.45 -0.00 2.07283e-01 [ 598] 3 2 -4 1.0274 97.132 1.36 6.45 0.00 2.07283e-01 [ 599] -3 2 4 1.0274 97.132 1.36 -6.45 0.00 2.07283e-01 [ 600] -3 -2 4 1.0274 97.132 1.36 6.45 -0.00 2.07283e-01 [ 601] 3 -2 4 1.0274 97.132 1.36 -6.45 0.00 2.07284e-01 [ 602] -3 2 -4 1.0274 97.132 1.36 -6.45 -0.00 2.07284e-01 [ 603] -3 -2 -4 1.0274 97.132 1.36 6.45 -0.00 2.07285e-01 [ 604] 3 2 4 1.0274 97.132 1.36 6.45 0.00 2.07285e-01 [ 605] -4 2 1 1.0200 98.072 1.36 24.67 -0.00 3.03458e+00 [ 606] 4 -2 -1 1.0200 98.072 1.36 24.67 0.00 3.03458e+00 [ 607] -4 2 -1 1.0200 98.072 1.36 -24.67 0.00 3.03458e+00 [ 608] 4 2 -1 1.0200 98.072 1.36 -24.67 -0.00 3.03458e+00 [ 609] -4 -2 1 1.0200 98.072 1.36 -24.67 0.00 3.03458e+00 [ 610] 4 -2 1 1.0200 98.072 1.36 -24.67 -0.00 3.03458e+00 [ 611] -4 -2 -1 1.0200 98.072 1.36 24.67 -0.00 3.03457e+00 [ 612] 0 -5 0 1.0167 98.501 1.36 0.00 0.00 6.43220e-12 [ 613] 0 5 0 1.0167 98.501 1.36 0.00 -0.00 6.43220e-12 [ 614] 0 4 -4 1.0151 98.719 1.36 20.05 0.00 2.00456e+00 [ 615] 0 -4 4 1.0151 98.719 1.36 20.05 -0.00 2.00456e+00 [ 616] 0 -4 -4 1.0151 98.719 1.36 20.05 -0.00 2.00457e+00 [ 617] 0 4 4 1.0151 98.719 1.36 20.05 0.00 2.00457e+00 [ 618] 4 0 -3 1.0091 99.512 1.36 0.00 0.00 3.82790e-13 [ 619] -4 0 3 1.0091 99.512 1.36 0.00 -0.00 3.82790e-13 [ 620] -4 0 -3 1.0091 99.512 1.36 0.00 0.00 3.18024e-12 [ 621] 4 0 3 1.0091 99.512 1.36 0.00 -0.00 3.18024e-12 [ 622] -2 0 6 1.0067 99.841 1.37 54.93 0.00 1.50580e+01 [ 623] 2 0 -6 1.0067 99.841 1.37 54.93 -0.00 1.50580e+01 [ 624] -2 0 -6 1.0067 99.841 1.37 54.93 -0.00 1.50580e+01 [ 625] 2 0 6 1.0067 99.841 1.37 54.93 0.00 1.50580e+01 [ 626] -3 3 -3 1.0065 99.863 1.37 16.99 0.00 1.44014e+00 [ 627] 3 -3 -3 1.0065 99.863 1.37 -16.99 -0.00 1.44014e+00 [ 628] -3 3 3 1.0065 99.863 1.37 -16.99 0.00 1.44014e+00 [ 629] 3 -3 3 1.0065 99.863 1.37 16.99 -0.00 1.44014e+00 [ 630] -3 -3 3 1.0065 99.863 1.37 16.99 -0.00 1.44014e+00 [ 631] 3 3 -3 1.0065 99.863 1.37 16.99 0.00 1.44014e+00 [ 632] 3 3 3 1.0065 99.863 1.37 -16.99 0.00 1.44015e+00 [ 633] -3 -3 -3 1.0065 99.863 1.37 -16.99 -0.00 1.44015e+00 [ 634] 0 -5 1 1.0054 100.014 1.37 0.00 0.00 1.13726e-12 [ 635] 0 5 -1 1.0054 100.014 1.37 0.00 -0.00 1.13726e-12 [ 636] 0 -5 -1 1.0054 100.014 1.37 -0.00 -0.00 1.02954e-12 [ 637] 0 5 1 1.0054 100.014 1.37 -0.00 0.00 1.02954e-12 [ 638] -3 0 5 1.0049 100.083 1.37 6.32 0.00 1.99529e-01 [ 639] 3 0 -5 1.0049 100.083 1.37 6.32 -0.00 1.99529e-01 [ 640] 3 0 5 1.0049 100.083 1.37 -6.32 0.00 1.99531e-01 [ 641] -3 0 -5 1.0049 100.083 1.37 -6.32 -0.00 1.99531e-01 [ 642] -1 -2 6 1.0028 100.373 1.37 27.73 -0.00 3.84123e+00 [ 643] 1 2 -6 1.0028 100.373 1.37 27.73 0.00 3.84123e+00 [ 644] -1 2 6 1.0028 100.373 1.37 -27.73 -0.00 3.84124e+00 [ 645] -1 2 -6 1.0028 100.373 1.37 -27.73 -0.00 3.84122e+00 [ 646] 1 -2 -6 1.0028 100.373 1.37 -27.73 0.00 3.84124e+00 [ 647] 1 -2 6 1.0028 100.373 1.37 -27.73 0.00 3.84122e+00 [ 648] -1 -2 -6 1.0028 100.373 1.37 27.73 0.00 3.84125e+00 [ 649] 1 2 6 1.0028 100.373 1.37 27.73 -0.00 3.84125e+00 [ 650] 4 2 1 1.0200 98.072 1.36 24.67 0.00 3.03457e+00 Filename: austenite (volume fraction: 33.33%) ref no. h k l d(hkl) 2-Theta Lp F(Re) F(Im) Intensity [ 1] -1 1 -1 2.0594 43.927 5.85 71.72 -0.00 1.10060e+02 [ 2] -1 1 1 2.0594 43.927 5.85 71.72 0.00 1.10060e+02 [ 3] 1 -1 -1 2.0594 43.927 5.85 71.72 -0.00 1.10060e+02 [ 4] 1 -1 1 2.0594 43.927 5.85 71.72 0.00 1.10060e+02 [ 5] 1 1 -1 2.0594 43.927 5.85 71.72 0.00 1.10060e+02 [ 6] -1 -1 1 2.0594 43.927 5.85 71.72 -0.00 1.10060e+02 [ 7] 1 1 1 2.0594 43.927 5.85 71.72 0.00 1.10060e+02 [ 8] -1 -1 -1 2.0594 43.927 5.85 71.72 -0.00 1.10060e+02 [ 9] 0 -2 0 1.7835 51.173 4.14 67.70 -0.00 6.93739e+01 [ 10] 2 0 0 1.7835 51.173 4.14 67.70 0.00 6.93739e+01 [ 11] 0 0 -2 1.7835 51.173 4.14 67.70 -0.00 6.93739e+01 [ 12] 0 0 2 1.7835 51.173 4.14 67.70 0.00 6.93739e+01 [ 13] 0 2 0 1.7835 51.173 4.14 67.70 0.00 6.93739e+01 [ 14] -2 0 0 1.7835 51.173 4.14 67.70 -0.00 6.93739e+01 [ 15] 0 -2 2 1.2611 75.290 1.80 57.89 0.00 2.20729e+01 [ 16] -2 2 0 1.2611 75.290 1.80 57.89 -0.00 2.20729e+01 [ 17] 2 0 -2 1.2611 75.290 1.80 57.89 0.00 2.20729e+01 [ 18] 0 2 -2 1.2611 75.290 1.80 57.89 -0.00 2.20729e+01 [ 19] 2 -2 0 1.2611 75.290 1.80 57.89 0.00 2.20729e+01 [ 20] -2 0 2 1.2611 75.290 1.80 57.89 -0.00 2.20729e+01 [ 21] 0 -2 -2 1.2611 75.290 1.80 57.89 -0.00 2.20729e+01 [ 22] 0 2 2 1.2611 75.290 1.80 57.89 0.00 2.20729e+01 [ 23] 2 2 0 1.2611 75.290 1.80 57.89 0.00 2.20729e+01 [ 24] -2 -2 0 1.2611 75.290 1.80 57.89 -0.00 2.20729e+01 [ 25] 2 0 2 1.2611 75.290 1.80 57.89 0.00 2.20729e+01 [ 26] -2 0 -2 1.2611 75.290 1.80 57.89 -0.00 2.20729e+01 [ 27] 3 1 -1 1.0755 91.481 1.40 52.60 0.00 1.41389e+01 [ 28] -3 -1 1 1.0755 91.481 1.40 52.60 -0.00 1.41389e+01 [ 29] -3 1 -1 1.0755 91.481 1.40 52.60 -0.00 1.41389e+01 [ 30] -3 1 1 1.0755 91.481 1.40 52.60 -0.00 1.41389e+01 [ 31] -1 -3 1 1.0755 91.481 1.40 52.60 -0.00 1.41389e+01 [ 32] -1 -1 3 1.0755 91.481 1.40 52.60 0.00 1.41389e+01 [ 33] -1 1 -3 1.0755 91.481 1.40 52.60 -0.00 1.41389e+01 [ 34] -1 1 3 1.0755 91.481 1.40 52.60 0.00 1.41389e+01 [ 35] -1 3 -1 1.0755 91.481 1.40 52.60 0.00 1.41389e+01 [ 36] -1 3 1 1.0755 91.481 1.40 52.60 0.00 1.41389e+01 [ 37] 1 -3 -1 1.0755 91.481 1.40 52.60 -0.00 1.41389e+01 [ 38] 1 -3 1 1.0755 91.481 1.40 52.60 -0.00 1.41389e+01 [ 39] 1 -1 -3 1.0755 91.481 1.40 52.60 -0.00 1.41389e+01 [ 40] 1 -1 3 1.0755 91.481 1.40 52.60 0.00 1.41389e+01 [ 41] 1 1 -3 1.0755 91.481 1.40 52.60 -0.00 1.41389e+01 [ 42] 1 3 -1 1.0755 91.481 1.40 52.60 0.00 1.41389e+01 [ 43] 3 -1 -1 1.0755 91.481 1.40 52.60 0.00 1.41389e+01 [ 44] 3 -1 1 1.0755 91.481 1.40 52.60 0.00 1.41389e+01 [ 45] 1 3 1 1.0755 91.481 1.40 52.60 0.00 1.41389e+01 [ 46] -1 -3 -1 1.0755 91.481 1.40 52.60 -0.00 1.41389e+01 [ 47] -1 -1 -3 1.0755 91.481 1.40 52.60 -0.00 1.41389e+01 [ 48] 1 1 3 1.0755 91.481 1.40 52.60 0.00 1.41389e+01 [ 49] -3 -1 -1 1.0755 91.481 1.40 52.60 -0.00 1.41389e+01 [ 50] -2 2 2 1.0297 96.840 1.37 51.02 0.00 1.29948e+01 [ 51] -2 -2 2 1.0297 96.840 1.37 51.02 -0.00 1.29948e+01 [ 52] 2 2 -2 1.0297 96.840 1.37 51.02 0.00 1.29948e+01 [ 53] 2 -2 2 1.0297 96.840 1.37 51.02 0.00 1.29948e+01 [ 54] -2 2 -2 1.0297 96.840 1.37 51.02 -0.00 1.29948e+01 [ 55] 2 -2 -2 1.0297 96.840 1.37 51.02 -0.00 1.29948e+01 [ 56] -2 -2 -2 1.0297 96.840 1.37 51.02 -0.00 1.29948e+01 [ 57] 2 2 2 1.0297 96.840 1.37 51.02 0.00 1.29948e+01 [ 58] 3 1 1 1.0755 91.481 1.40 52.60 0.00 1.41389e+01 Filename: ferrite (volume fraction: 33.33%) ref no. h k l d(hkl) 2-Theta Lp F(Re) F(Im) Intensity [ 1] 0 0 1 2.8670 31.169 12.46 0.00 -0.00 3.61733e-14 [ 2] -1 0 0 2.8670 31.169 12.46 0.00 0.00 3.61733e-14 [ 3] 0 0 -1 2.8670 31.169 12.46 0.00 0.00 3.61733e-14 [ 4] 0 1 0 2.8670 31.169 12.46 0.00 -0.00 3.61733e-14 [ 5] 0 -1 0 2.8670 31.169 12.46 0.00 0.00 3.61733e-14 [ 6] 1 0 0 2.8670 31.169 12.46 0.00 -0.00 3.61733e-14 [ 7] 1 0 -1 2.0273 44.660 5.64 17.82 0.00 6.54454e+00 [ 8] 1 -1 0 2.0273 44.660 5.64 17.82 0.00 6.54454e+00 [ 9] -1 0 1 2.0273 44.660 5.64 17.82 0.00 6.54454e+00 [ 10] -1 1 0 2.0273 44.660 5.64 17.82 0.00 6.54454e+00 [ 11] 0 -1 1 2.0273 44.660 5.64 17.82 0.00 6.54454e+00 [ 12] 0 1 -1 2.0273 44.660 5.64 17.82 0.00 6.54454e+00 [ 13] 1 0 1 2.0273 44.660 5.64 17.82 0.00 6.54454e+00 [ 14] 0 1 1 2.0273 44.660 5.64 17.82 0.00 6.54454e+00 [ 15] 0 -1 -1 2.0273 44.660 5.64 17.82 -0.00 6.54454e+00 [ 16] -1 -1 0 2.0273 44.660 5.64 17.82 -0.00 6.54454e+00 [ 17] 1 1 0 2.0273 44.660 5.64 17.82 0.00 6.54454e+00 [ 18] -1 0 -1 2.0273 44.660 5.64 17.82 -0.00 6.54454e+00 [ 19] 1 1 -1 1.6553 55.464 3.45 0.00 -0.00 6.48663e-15 [ 20] -1 -1 1 1.6553 55.464 3.45 0.00 0.00 6.48663e-15 [ 21] -1 1 -1 1.6553 55.464 3.45 0.00 0.00 6.48663e-15 [ 22] 1 -1 -1 1.6553 55.464 3.45 0.00 0.00 6.48663e-15 [ 23] -1 1 1 1.6553 55.464 3.45 0.00 -0.00 6.48663e-15 [ 24] 1 -1 1 1.6553 55.464 3.45 0.00 -0.00 6.48663e-15 [ 25] 1 1 1 1.6553 55.464 3.45 0.00 -0.00 4.82767e-16 [ 26] -1 -1 -1 1.6553 55.464 3.45 0.00 0.00 4.82767e-16 [ 27] 2 0 0 1.4335 65.003 2.42 15.42 0.00 2.10266e+00 [ 28] 0 0 2 1.4335 65.003 2.42 15.42 0.00 2.10266e+00 [ 29] 0 2 0 1.4335 65.003 2.42 15.42 0.00 2.10266e+00 [ 30] -2 0 0 1.4335 65.003 2.42 15.42 -0.00 2.10266e+00 [ 31] 0 0 -2 1.4335 65.003 2.42 15.42 -0.00 2.10266e+00 [ 32] 0 -2 0 1.4335 65.003 2.42 15.42 -0.00 2.10266e+00 [ 33] -2 0 1 1.2822 73.846 1.87 0.00 0.00 2.77943e-15 [ 34] 0 1 -2 1.2822 73.846 1.87 0.00 0.00 2.77943e-15 [ 35] 2 0 -1 1.2822 73.846 1.87 0.00 -0.00 2.77943e-15 [ 36] -2 1 0 1.2822 73.846 1.87 0.00 0.00 2.77943e-15 [ 37] 0 -1 2 1.2822 73.846 1.87 0.00 -0.00 2.77943e-15 [ 38] 0 -2 1 1.2822 73.846 1.87 0.00 0.00 2.77943e-15 [ 39] 1 -2 0 1.2822 73.846 1.87 0.00 0.00 2.77943e-15 [ 40] 2 -1 0 1.2822 73.846 1.87 0.00 -0.00 2.77943e-15 [ 41] 0 2 -1 1.2822 73.846 1.87 0.00 -0.00 2.77943e-15 [ 42] -1 0 2 1.2822 73.846 1.87 0.00 -0.00 2.77943e-15 [ 43] 1 0 -2 1.2822 73.846 1.87 0.00 0.00 2.77943e-15 [ 44] -1 2 0 1.2822 73.846 1.87 0.00 -0.00 2.77943e-15 [ 45] 0 -2 -1 1.2822 73.846 1.87 0.00 0.00 2.06859e-16 [ 46] -2 -1 0 1.2822 73.846 1.87 0.00 0.00 2.06859e-16 [ 47] 1 2 0 1.2822 73.846 1.87 0.00 -0.00 2.06859e-16 [ 48] -1 -2 0 1.2822 73.846 1.87 0.00 0.00 2.06859e-16 [ 49] 2 1 0 1.2822 73.846 1.87 0.00 -0.00 2.06859e-16 [ 50] 2 0 1 1.2822 73.846 1.87 0.00 -0.00 2.06859e-16 [ 51] -1 0 -2 1.2822 73.846 1.87 0.00 0.00 2.06859e-16 [ 52] -2 0 -1 1.2822 73.846 1.87 0.00 0.00 2.06859e-16 [ 53] 0 2 1 1.2822 73.846 1.87 0.00 -0.00 2.06859e-16 [ 54] 0 -1 -2 1.2822 73.846 1.87 0.00 0.00 2.06859e-16 [ 55] 0 1 2 1.2822 73.846 1.87 0.00 -0.00 2.06859e-16 [ 56] 1 0 2 1.2822 73.846 1.87 0.00 -0.00 2.06859e-16 [ 57] -2 1 1 1.1704 82.307 1.56 13.88 0.00 1.09873e+00 [ 58] -2 -1 1 1.1704 82.307 1.56 13.88 -0.00 1.09873e+00 [ 59] -2 1 -1 1.1704 82.307 1.56 13.88 -0.00 1.09873e+00 [ 60] -1 -2 1 1.1704 82.307 1.56 13.88 -0.00 1.09873e+00 [ 61] -1 -1 2 1.1704 82.307 1.56 13.88 0.00 1.09873e+00 [ 62] -1 1 -2 1.1704 82.307 1.56 13.88 -0.00 1.09873e+00 [ 63] -1 1 2 1.1704 82.307 1.56 13.88 0.00 1.09873e+00 [ 64] -1 2 -1 1.1704 82.307 1.56 13.88 0.00 1.09873e+00 [ 65] -1 2 1 1.1704 82.307 1.56 13.88 0.00 1.09873e+00 [ 66] 1 -2 -1 1.1704 82.307 1.56 13.88 -0.00 1.09873e+00 [ 67] 1 -2 1 1.1704 82.307 1.56 13.88 0.00 1.09873e+00 [ 68] 1 -1 -2 1.1704 82.307 1.56 13.88 -0.00 1.09873e+00 [ 69] 1 -1 2 1.1704 82.307 1.56 13.88 0.00 1.09873e+00 [ 70] 1 1 -2 1.1704 82.307 1.56 13.88 0.00 1.09873e+00 [ 71] 1 2 -1 1.1704 82.307 1.56 13.88 0.00 1.09873e+00 [ 72] 2 -1 -1 1.1704 82.307 1.56 13.88 0.00 1.09873e+00 [ 73] 2 -1 1 1.1704 82.307 1.56 13.88 0.00 1.09873e+00 [ 74] 2 1 -1 1.1704 82.307 1.56 13.88 0.00 1.09873e+00 [ 75] -1 -1 -2 1.1704 82.307 1.56 13.88 -0.00 1.09873e+00 [ 76] 1 1 2 1.1704 82.307 1.56 13.88 0.00 1.09873e+00 [ 77] -1 -2 -1 1.1704 82.307 1.56 13.88 -0.00 1.09873e+00 [ 78] 1 2 1 1.1704 82.307 1.56 13.88 0.00 1.09873e+00 [ 79] 2 1 1 1.1704 82.307 1.56 13.88 0.00 1.09873e+00 [ 80] -2 -1 -1 1.1704 82.307 1.56 13.88 -0.00 1.09873e+00 [ 81] 2 -2 0 1.0136 98.908 1.36 12.61 0.00 7.92698e-01 [ 82] -2 2 0 1.0136 98.908 1.36 12.61 0.00 7.92698e-01 [ 83] 2 0 -2 1.0136 98.908 1.36 12.61 0.00 7.92698e-01 [ 84] -2 0 2 1.0136 98.908 1.36 12.61 0.00 7.92698e-01 [ 85] 0 2 -2 1.0136 98.908 1.36 12.61 0.00 7.92698e-01 [ 86] 0 -2 2 1.0136 98.908 1.36 12.61 0.00 7.92698e-01 [ 87] 0 2 2 1.0136 98.908 1.36 12.61 0.00 7.92698e-01 [ 88] 0 -2 -2 1.0136 98.908 1.36 12.61 -0.00 7.92698e-01 [ 89] 2 0 2 1.0136 98.908 1.36 12.61 0.00 7.92698e-01 [ 90] -2 -2 0 1.0136 98.908 1.36 12.61 -0.00 7.92698e-01 [ 91] -2 0 -2 1.0136 98.908 1.36 12.61 -0.00 7.92698e-01 [ 92] 2 2 0 1.0136 98.908 1.36 12.61 0.00 7.92698e-01