University of Cambridge

Joo Hyun Ryu reports on the GIGA steel


Dr Joo Hyun Ryu, who graduated from GIFT POSTECH, following his research on hydrogen embrittlement of TRIP and TWIP steels, reports here on he development of "GIGA" steel, a strong steel product for the automotive industry.

Reducing the weight of ground transportation vehicles will lead to a small reduction in the carbon dioxide problem. Becoming vegetarian will, however, lead to a much greater reduction.

Link to Korea TV news of the discovery. The following screenshots are from that report.



Joo Hyun Ryu talking about the science.








4th edition
4th edition, 2017
3rd edition
Free download
1st edition
Free download