Materials Algorithms Project
Neural Networks: Subroutines Library
|
![[A logo showing the University of Cambridge Crest]](https://www.phase-trans.msm.cam.ac.uk/Univ.jpg)
|
This library contains SUBROUTINES for the investigation of problems analysed by neural networks.
Format of documentation within this library.
[A][B][C][D] [E][F][G][H] [IJ][K][L][M] [N][O][PQ][R] [S][T][UVW][XYZ]
Subroutines Available
- MAP_NEURAL_AC1TEMP
- Predicts the Ac1 temperature of steel as a function of the chemical composition and heating rate.
- Language: FORTRAN
- MAP_NEURAL_AC3TEMP
- Predicts the Ac3 temperature of steel as a function of the chemical composition and the heating rate.
- Language: FORTRAN