This library contains complete PROGRAMS for analysing and modelling the properties of nickel base alloys.
Format of documentation within this library.
[A][B][C][D] [E][F][G][H] [IJ][K][L][M] [N][O][PQ][R] [S][T][UVW][XYZ]
Programs Available
A
[Back to top]
B
[Back to top]
C
- MAP_NICKEL_CRD
- A program for the estimation of the creep rupture ductility (CRD) of nickel-base superalloys as a function of elemental composition, heat and mechanical treatments, and test conditions.
- Language: C, FORTRAN, Executables
- MAP_NICKEL_CREEP
- Calculation of the creep rupture strength of nickel-base superalloys as a function of the chemical composition and heat treatment.
- Language: C, FORTRAN, Executables
[Back to top]
D
- MAP_NICKEL_DUCT
- Calculation of the tensile ductility of nickel-base superalloys as a function of elemental composition, heat and mechanical treatments, and test temperature.
- Language: C, FORTRAN, Executables
[Back to top]
E
[Back to top]
F
[Back to top]
G
- MAP_NICKEL_GROWTH
- This MATLAB program caclulates the volume fraction of gamma-prime and the hardness or yield stress of nickel-base superalloys during precipitation ageing.
- Language: MATLAB
[Back to top]
H
[Back to top]
IJ
[Back to top]
K
[Back to top]
L
- MAP_NICKEL_LATTICE
- Calculation of the Gamma and Gamma-prime lattice parameters in nickel base superalloys as a function of the chemical composition and temperature. Based on a neural network model.
- Language: C, FORTRAN, Executables
[Back to top]
M
[Back to top]
N
- MAP_NICKEL_NIPROS
- An application of the Tpros program for calculating the yield stress of nickel-based superalloys.
- Language: C
[Back to top]
O
[Back to top]
PQ
[Back to top]
R
[Back to top]
S
[Back to top]
T
[Back to top]
UVW
- MAP_NICKEL_UTS
- A program for the estimation of the ultimate tensile stress (UTS) of nickel-base superalloys. This prediction is made as a function of elemental composition, heat and mechanical treatments, and test temperature.
- Language: C, FORTRAN, Executables
[Back to top]
XYZ
- MAP_NICKEL_YIELD
- Estimation of the yield stress of nickel-base superalloys as a function of elemental composition, heat and mechanical treatments, and test temperature.
- Language: C, FORTRAN, Executables
[Back to top]