  (c) Prof. H. K. D. H. Bhadeshia, Sree Harsha Lalam ,
      University of Cambridge, Feb, 2000


This file contains the steps to run this model.

1) Copy files onto hard disk, without disturbing the structure and remove the "READ-ONLY" status for files 'test.dat' and 'Gresult.dat'.

2) Edit the test.dat file to set input variables. The input variables are in row;


Column	 variables	
1)	Temperature (deg. C)
2)	Nickel  (at%)
3) 	Cobalt (at%)
4)	Chromium (at%)
5)	Molybdenum (at%)
6)	Tungsten (at%)
7)	Aluminium (at%)
8) 	Titantium (at%)
9) 	Niobium (at%)
10)   Tantalum (at%)
11)   Hafnium (at%)
12)   Rhenium (at%)
13)   Vanadium (at%)
14)   Iron (at%)
15)   Gallium (at%)
16)   Copper (at%)
17)   Gold (at%)

3) Click on "Gamma.exe" icon.
   
4) Finally, the results (Lattice constant (angstroms))are written in "Gresult.dat" .

5) Results are stored in a file called 'Gresult.dat'. The format of the file is;
Lattice const. (A^o)     Error Bar (A^o)      LC - Error Bar       LC + Error Bar


End of task.