"YS" "O2" "Reheated" "ac_ferr" "T27J" "Reference" 605 0.0769 46 56 -27 "Line1" 605 0.074 51 48 -40 "Line2" 560 0.07 55 53 -44 "Line3" 585 0.079 43 48 -39 "Line4" 600 0.083 47 53 -32 "Line5" 495 0.081 79 61 -28 "Line6" 630 0.072 60 86 -70 "Line7" 550 0.073 42 70 -45 "Line8" 560 0.069 44 62 -31 "Line9" 550 0.071 55 55 -13 "Line10" 630 0.073 39 68 -55 "Line11" 500 0.07 54 46 -34 "Line12" 610 0.05 44 56 -80 "Line13" 590 0.052 41 59 -78 "Line14" 560 0.048 61 64 -68 "Line15" 550 0.056 51 59 -74 "Line16" 500 0.048 67 60 -68 "Line17" 530 0.12 43 45 -28 "Line18" 490 0.124 46 54 -20 "Line19" 450 0.117 53 46 -30 "Line20" 490 0.107 46 47 -26 "Line21" 420 0.11 72 21 -13 "Line22" 460 0.046 55 46 -74 "Line23" 430 0.052 48 36 -63 "Line24" 440 0.077 40 52 -57 "Line25" 410 0.05 42 63 -55 "Line26" 360 0.047 57 75 -73 "Line27" 469 0.057 40 50 -50 "Line28" 473 0.043 40 62 -65 "Line29" 499 0.055 40 58 -60 "Line30" 519 0.05 40 58 -72 "Line31" 459 0.047 40 50 -40 "Line32" 521 0.042 40 63 -40 "Line33" 507 0.053 40 61 -67 "Line34" 549 0.048 40 67 -60 "Line35" 510 0.044 40 55 -59 "Line36" 531 0.048 40 70 -37 "Line37" 500 0.045 40 55 -60 "Line38" 520 0.042 40 51 -70 "Line39" 570 0.038 40 47 -70 "Line40" 510 0.038 40 52 -70 "Line41" 550 0.04 40 44 -61 "Line42" 540 0.04 40 33 -65 "Line43" 560 0.043 40 15 -47 "Line44" 500 0.058 40 40 -47 "Line45" 510 0.065 20 54 -37 "Line46" 525 0.053 20 38 -50 "Line47" 480 0.058 20 30 -48 "Line48" 500 0.058 20 20 -37 "Line49" 440 0.048 20 5 -40 "Line50" 470 0.046 20 62 -88 "Line51" 480 0.039 20 70 -72 "Line52" 480 0.034 20 70 -60 "Line53" 500 0.031 20 63 -73 "Line54" 510 0.029 20 60 -72 "Line55" 510 0.028 20 62 -72 "Line56" 500 0.028 20 68 -75 "Line57" 540 0.029 20 74 -75 "Line58" 530 0.029 20 76 -75 "Line59"