Date and time of run 27-OCT-2006 14:36:46 > 061027143639,1 MTDATA 4.73 2002-11-15 14:22, LOG /obelix/users/mathew/mtdata-calcs-carboninaustenite/calc2/mt1.log > 061027143641,1 U-32956 on LNX-000-T (UNIX) using sgm000.exe > 061027143646,1 MODULE 3 creates MPI file /obelix/users/mathew/mtdata-calcs-carboninaustenite/calc2/def.mpi > 061027143646,1 MODULE 3 reads MPI file /obelix/users/mathew/mtdata-calcs-carboninaustenite/calc2/def.mpi > 061027143646,1 MODULE 3 creates MPR file /obelix/users/mathew/mtdata-calcs-carboninaustenite/calc2/def.mpr $(Number of lines of title) 8 * DATAFILE = /obelix/users/mathew/mtdata-calcs-carboninaustenite/calc2/def.mpi - CREATED 14:36:46 27-OCT-2006 * SYSTEM = Fe,C,Si, * NUMBER OF PHASES = 29 * NUMBER OF SPECIES = 56 * DATA FILE = /obelix/users/mathew/mtdata-calcs-carboninaustenite/calc2/def.mpi *** PROBLEM settings *** SYSTEM ELEMENTS : CFeSi NUMBER COMPONENT STATUS AMOUNT DELTA REF.P 1 Fe # TO BAL 1736.89 2 C NORMAL 83.2570 3 Si NORMAL 71.2111 NUMBER PHASE STATUS MODEL 1 DIAMOND_A4 ABSENT REDLICH-KISTER 2 GRAPHITE ABSENT PURE SUBSTANCE 3 LIQUID ABSENT REDLICH-KISTER 4 GAS ABSENT IDEAL GAS 5 BCC_A2 ABSENT SUBLATTICE 6 CBCC_A12 ABSENT SUBLATTICE 7 CEMENTITE NORMAL SUBLATTICE 8 CUB_A13 ABSENT SUBLATTICE 9 FCC_A1 NORMAL SUBLATTICE 10 FE4N ABSENT PURE SUBSTANCE 11 FECN_CHI ABSENT PURE SUBSTANCE 12 HCP_A3 ABSENT SUBLATTICE 13 KSI_CARBIDE ABSENT PURE SUBSTANCE 14 M5C2 ABSENT PURE SUBSTANCE 15 M7C3 ABSENT PURE SUBSTANCE 16 V3C2 ABSENT PURE SUBSTANCE 17 M23C6 ABSENT PURE SUBSTANCE 18 FE8SI2C ABSENT PURE SUBSTANCE 19 SIC ABSENT PURE SUBSTANCE 20 AL5FE4 ABSENT PURE SUBSTANCE 21 FE1SI1 ABSENT PURE SUBSTANCE 22 FE2SI ABSENT PURE SUBSTANCE 23 FE5SI3 ABSENT PURE SUBSTANCE 24 FESI2_H ABSENT PURE SUBSTANCE 25 FESI2_L ABSENT PURE SUBSTANCE 26 M3SI ABSENT PURE SUBSTANCE 27 CR3SI ABSENT PURE SUBSTANCE 28 CRSI2 ABSENT PURE SUBSTANCE 29 M3C2 ABSENT PURE SUBSTANCE NUMBER SUBSTANCE STATUS/CONSTRAINT 1 C NORMAL 2 Si NORMAL 3 C NORMAL 4 C NORMAL 5 Fe NORMAL 6 Si NORMAL 7 C NORMAL 8 C2 NORMAL 9 C3 NORMAL 10 C4 NORMAL 11 C5 NORMAL 12 C6 NORMAL 13 C7 NORMAL 14 Fe NORMAL 15 Fe:1 NORMAL 16 Si:1 NORMAL 17 C:2 NORMAL 18 Va:2 NORMAL 19 Fe:1 NORMAL 20 Si:1 NORMAL 21 C:2 NORMAL 22 Va:2 NORMAL 23 Fe:1 NORMAL 24 Si:1 NORMAL 25 C:2 NORMAL 26 Fe:1 NORMAL 27 Si:1 NORMAL 28 C:2 NORMAL 29 Va:2 NORMAL 30 Fe:1 NORMAL 31 Si:1 NORMAL 32 C:2 NORMAL 33 Va:2 NORMAL 34 Fe4C NORMAL 35 Fe2.2C NORMAL 36 Fe:1 NORMAL 37 Si:1 NORMAL 38 C:2 NORMAL 39 Va:2 NORMAL 40 Fe3C NORMAL 41 Fe5C2 NORMAL 42 Fe7C3 NORMAL 43 Fe3C2 NORMAL 44 Fe20Fe3C6 NORMAL 45 Fe8Si2C NORMAL 46 SiC NORMAL 47 Fe NORMAL 48 Fe.5Si.5 NORMAL 49 Fe.666667Si.333333 NORMAL 51 Fe.3Si.7 NORMAL 52 Fe.333333Si.666667 NORMAL 54 Si3Si NORMAL 55 SiSi2 NORMAL 56 Fe3C2 NORMAL UNARY SOURCE Tmin/K Tmax/K C sgte_sol 298.15 6000.00 Si sgte_sol 298.14 3600.00 C sgte_sol 298.15 6000.00 C sgte_sol 298.15 6000.00 Fe sgte_sol 298.15 6000.00 Si sgte_sol 298.14 3600.00 C sgte_sol 298.15 6000.00 C2 sgte_sol 298.15 6000.00 C3 sgte_sol 298.15 6000.00 C4 sgte_sol 298.15 6000.00 C5 sgte_sol 298.15 6000.00 C6 sgte_sol 298.15 6000.00 C7 sgte_sol 298.15 6000.00 Fe sgte_sol 298.15 6000.00 Fe:C sgte_sol 298.15 6000.00 Fe:Va sgte_sol 298.15 6000.00 Si:C sgte_sol 298.15 3600.00 Si:Va sgte_sol 298.14 3600.00 Fe:C sgte_sol 298.15 6000.00 Fe:Va sgte_sol 298.15 6000.00 Si:C sgte_sol 298.14 3000.00 Si:Va sgte_sol 298.14 3600.00 Fe:C sgte_sol 298.15 6000.00 Si:C cementite_Si 298.15 6000.00 Fe:C sgte_sol 298.15 6000.00 Fe:Va sgte_sol 298.15 6000.00 Si:C sgte_sol 298.14 3000.00 Si:Va sgte_sol 298.14 3600.00 Fe:C sgte_sol 298.15 6000.00 Fe:Va sgte_sol 298.15 6000.00 Si:C sgte_sol 298.15 3600.00 Si:Va sgte_sol 298.14 3600.00 Fe4C sgte_sol 298.15 6000.00 Fe2.2C sgte_sol 298.15 6000.00 Fe:C sgte_sol 298.15 6000.00 Fe:Va sgte_sol 298.14 6000.00 Si:C NODATA 298.15 298.00 Si:Va sgte_sol 298.14 3600.00 Fe3C sgte_sol 298.15 6000.00 Fe5C2 sgte_sol 298.15 6000.00 Fe7C3 sgte_sol 298.15 6000.00 Fe3C2 sgte_sol 298.15 6000.00 Fe20Fe3C6 sgte_sol 298.15 6000.00 Fe8Si2C sgte_sol 298.15 3600.00 SiC sgte_sol 298.14 4000.00 Fe sgte_sol 298.15 6000.00 Fe.5Si.5 sgte_sol 298.15 3600.00 Fe.666667Si.333333 sgte_sol 298.15 3600.00 Fe.625Si.375 sgte_sol 298.15 3600.00 Fe.3Si.7 sgte_sol 298.15 3600.00 Fe.333333Si.666667 sgte_sol 298.15 3600.00 Fe3Si sgte_sol 298.15 3600.00 Si3Si sgte_sol 298.15 3600.00 SiSi2 sgte_sol 298.15 3600.00 Fe3C2 plus 298.15 6000.00 TEMPERATURE : 1000.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 Stage 1* only requested *** MULTIPHASE - Stage 1* Results *** Temperature = 1000.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -4.286827E+04 5.765644E-03 1.736888E+03 9.700000E+01 C -9.175499E+03 3.316906E-01 8.325701E+01 1.000000E+00 Si -1.549295E+05 8.081998E-09 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 1.1911E+02 CEMENTITE 0.7499992 0.2500000 0.0000008 1.7723E+03 FCC_A1 0.9296422 0.0301767 0.0401811 Gibbs Energy = -8.6254024880E+07 J System Enthalpy = 4.5647457402E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1010.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1010.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -4.359264E+04 5.566164E-03 1.736888E+03 9.700000E+01 C -9.484751E+03 3.232102E-01 8.325701E+01 1.000000E+00 Si -1.554690E+05 9.114618E-09 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 1.1098E+02 CEMENTITE 0.7499992 0.2500000 0.0000008 1.7804E+03 FCC_A1 0.9288223 0.0311800 0.0399977 Gibbs Energy = -8.7576346020E+07 J System Enthalpy = 4.6311410205E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1020.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1020.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -4.432069E+04 5.374963E-03 1.736888E+03 9.700000E+01 C -9.794904E+03 3.150732E-01 8.325701E+01 1.000000E+00 Si -1.560103E+05 1.025291E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 1.0267E+02 CEMENTITE 0.7499991 0.2500000 0.0000009 1.7887E+03 FCC_A1 0.9279920 0.0321959 0.0398120 Gibbs Energy = -8.8905255557E+07 J System Enthalpy = 4.6978309424E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1030.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1030.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -4.505241E+04 5.191633E-03 1.736888E+03 9.700000E+01 C -1.010589E+04 3.072632E-01 8.325701E+01 1.000000E+00 Si -1.565532E+05 1.150477E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 9.4189E+01 CEMENTITE 0.7499991 0.2500000 0.0000009 1.7972E+03 FCC_A1 0.9271516 0.0332243 0.0396241 Gibbs Energy = -9.0240718021E+07 J System Enthalpy = 4.7648203994E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1040.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1040.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -4.578777E+04 5.015787E-03 1.736888E+03 9.700000E+01 C -1.041764E+04 2.997651E-01 8.325701E+01 1.000000E+00 Si -1.570978E+05 1.287845E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 8.5519E+01 CEMENTITE 0.7499990 0.2500000 0.0000010 1.8058E+03 FCC_A1 0.9263011 0.0342651 0.0394338 Gibbs Energy = -9.1582699118E+07 J System Enthalpy = 4.8321145527E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1050.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1050.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -4.652677E+04 4.847060E-03 1.736888E+03 9.700000E+01 C -1.073008E+04 2.925642E-01 8.325701E+01 1.000000E+00 Si -1.576441E+05 1.438250E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 7.6661E+01 CEMENTITE 0.7499990 0.2500000 0.0000010 1.8147E+03 FCC_A1 0.9254405 0.0353182 0.0392413 Gibbs Energy = -9.2931165724E+07 J System Enthalpy = 4.8997188459E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1060.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1060.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -4.726938E+04 4.685111E-03 1.736888E+03 9.700000E+01 C -1.104315E+04 2.856470E-01 8.325701E+01 1.000000E+00 Si -1.581919E+05 1.602581E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 6.7611E+01 CEMENTITE 0.7499989 0.2500000 0.0000011 1.8237E+03 FCC_A1 0.9245699 0.0363835 0.0390466 Gibbs Energy = -9.4286085880E+07 J System Enthalpy = 4.9676390109E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1070.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1070.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -4.801560E+04 4.529614E-03 1.736888E+03 9.700000E+01 C -1.135679E+04 2.790004E-01 8.325701E+01 1.000000E+00 Si -1.587414E+05 1.781761E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 5.8366E+01 CEMENTITE 0.7499989 0.2500000 0.0000011 1.8330E+03 FCC_A1 0.9236894 0.0374609 0.0388497 Gibbs Energy = -9.5647428781E+07 J System Enthalpy = 5.0358810819E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1080.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1080.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -4.876542E+04 4.380263E-03 1.736888E+03 9.700000E+01 C -1.167092E+04 2.726123E-01 8.325701E+01 1.000000E+00 Si -1.592925E+05 1.976741E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 4.8920E+01 CEMENTITE 0.7499988 0.2500000 0.0000012 1.8424E+03 FCC_A1 0.9227989 0.0385506 0.0386505 Gibbs Energy = -9.7015164780E+07 J System Enthalpy = 5.1044514078E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1090.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1090.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -4.951881E+04 4.236770E-03 1.736888E+03 9.700000E+01 C -1.198548E+04 2.664711E-01 8.325701E+01 1.000000E+00 Si -1.598451E+05 2.188504E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 3.9270E+01 CEMENTITE 0.7499987 0.2500000 0.0000013 1.8521E+03 FCC_A1 0.9218986 0.0396523 0.0384491 Gibbs Energy = -9.8389265379E+07 J System Enthalpy = 5.1733566638E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1100.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1100.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -5.027589E+04 4.098805E-03 1.736888E+03 9.700000E+01 C -1.230027E+04 2.605694E-01 8.325701E+01 1.000000E+00 Si -1.604000E+05 2.417868E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 2.9411E+01 CEMENTITE 0.7499987 0.2500000 0.0000013 1.8619E+03 FCC_A1 0.9209883 0.0407661 0.0382455 Gibbs Energy = -9.9769703233E+07 J System Enthalpy = 5.2426038660E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1110.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1110.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -5.103629E+04 3.966277E-03 1.736888E+03 9.700000E+01 C -1.261561E+04 2.548863E-01 8.325701E+01 1.000000E+00 Si -1.609549E+05 2.666466E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 1.9337E+01 CEMENTITE 0.7499986 0.2500000 0.0000014 1.8720E+03 FCC_A1 0.9200682 0.0418921 0.0380397 Gibbs Energy = -1.0115645215E+08 J System Enthalpy = 5.3122003869E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1120.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1120.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -5.180013E+04 3.838865E-03 1.736888E+03 9.700000E+01 C -1.293127E+04 2.494167E-01 8.325701E+01 1.000000E+00 Si -1.615108E+05 2.935190E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 9.0438E+00 CEMENTITE 0.7499985 0.2500000 0.0000015 1.8823E+03 FCC_A1 0.9191382 0.0430301 0.0378317 Gibbs Energy = -1.0254948708E+08 J System Enthalpy = 5.3821539710E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1130.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1130.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -5.256558E+04 3.717059E-03 1.736888E+03 9.700000E+01 C -1.329344E+04 2.429525E-01 8.325701E+01 1.000000E+00 Si -1.620743E+05 3.222908E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 1.8914E+03 FCC_A1 0.9183294 0.0440197 0.0376508 Gibbs Energy = -1.0394877684E+08 J System Enthalpy = 5.4512853769E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1140.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1140.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -5.331928E+04 3.605616E-03 1.736888E+03 9.700000E+01 C -1.394708E+04 2.295953E-01 8.325701E+01 1.000000E+00 Si -1.626597E+05 3.524876E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 1.8914E+03 FCC_A1 0.9183294 0.0440197 0.0376508 Gibbs Energy = -1.0535382712E+08 J System Enthalpy = 5.5133036763E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1150.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1150.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -5.407574E+04 3.498363E-03 1.736888E+03 9.700000E+01 C -1.460272E+04 2.171403E-01 8.325701E+01 1.000000E+00 Si -1.632473E+05 3.848218E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 1.8914E+03 FCC_A1 0.9183294 0.0440197 0.0376508 Gibbs Energy = -1.0676432448E+08 J System Enthalpy = 5.5754776821E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1160.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1160.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -5.483523E+04 3.394999E-03 1.736888E+03 9.700000E+01 C -1.526029E+04 2.055174E-01 8.325701E+01 1.000000E+00 Si -1.638374E+05 4.193829E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 1.8914E+03 FCC_A1 0.9183294 0.0440197 0.0376508 Gibbs Energy = -1.0818023510E+08 J System Enthalpy = 5.6378073363E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1170.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1170.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -5.559776E+04 3.295346E-03 1.736888E+03 9.700000E+01 C -1.591978E+04 1.946613E-01 8.325701E+01 1.000000E+00 Si -1.644298E+05 4.562646E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 1.8914E+03 FCC_A1 0.9183294 0.0440197 0.0376508 Gibbs Energy = -1.0960152571E+08 J System Enthalpy = 5.7002925859E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1180.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1180.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -5.636316E+04 3.199300E-03 1.736888E+03 9.700000E+01 C -1.658120E+04 1.845119E-01 8.325701E+01 1.000000E+00 Si -1.650246E+05 4.955648E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 1.8914E+03 FCC_A1 0.9183294 0.0440197 0.0376508 Gibbs Energy = -1.1102816364E+08 J System Enthalpy = 5.7629333831E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1190.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1190.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -5.713107E+04 3.106809E-03 1.736888E+03 9.700000E+01 C -1.724461E+04 1.750140E-01 8.325701E+01 1.000000E+00 Si -1.656215E+05 5.373861E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 1.8914E+03 FCC_A1 0.9183294 0.0440197 0.0376508 Gibbs Energy = -1.1246011674E+08 J System Enthalpy = 5.8257296859E+07 J *** PROBLEM settings *** Changes only listed under components/phases/substances NUMBER COMPONENT STATUS AMOUNT DELTA REF.P NUMBER PHASE STATUS MODEL NUMBER SUBSTANCE STATUS/CONSTRAINT TEMPERATURE : 1200.000 PRESSURE/Pa : 101325.0 VOLUME/m3 : undefined SYSTEM AMOUNT/mol : undefined COMP. AMOUNTS/mol : 1736.888 83.25701 71.21112 SYSTEM MASS/kg : 100.0000 COMP. MASSES/kg : 97.00000 1.000000 2.000000 STEPPED VARIABLE INITIAL, FINAL AND STEP VALUES OF VARIABLE TEMPERATURE 1000.00 to 1200.00 by 10.0000 *** MULTIPHASE - Stage 1* Results *** Temperature = 1200.0000 K Fixed pressure = 1.013250E+05 Pa, 1.000000E+00 atm Component Ref.Phase Chem.Pot. Activity Amount/mol Mass/kg Fe -5.790236E+04 3.017447E-03 1.736888E+03 9.700000E+01 C -1.790983E+04 1.661213E-01 8.325701E+01 1.000000E+00 Si -1.662208E+05 5.818052E-08 7.121112E+01 2.000000E+00 Total 1.891356E+03 1.000000E+02 Amount Phase Mole fraction of component within phase compnt moles Fe C Si 1.8914E+03 FCC_A1 0.9183294 0.0440197 0.0376508 Gibbs Energy = -1.1389735342E+08 J System Enthalpy = 5.8886814572E+07 J