Summary
Fundamental proof that low Mn equals high toughness at constant strength
Increasing Mn increases the strain hardening, i.e. the difference between the yield and UTS
Temperature dependence of yield strength show similar trends for low and high manganese
Explanation of manganese effect as yet unclear