UPPER BAINITE
(High Temperature)
LOWER BAINITE
(Low Temperature)
Carbon supersaturated plate
Carbon diffusion into
austenite
Carbon diffusion into
austenite and carbide
precipitation in ferrite
Carbide precipitation
from austenite