Current Innovations in Steels
Steel Productivity in UK increased 5 fold in last 20 years
- 3 times faster than UK manufacturing
70% of steels in cars today were developed in last 10 years
Composition control in parts per million in 300 tonne casts
Advanced Process Control, Sensors and Models
Systems Solutions
- Design, Materials and Fabrication Technologies