Austenitisation Kinetics
Austenite carbon content for short austenitisation
Non-equilibrium - low bainitic ferrite
Empirical relationship: Cg = 0.16 ln(t) + 0.0032T - 2.7
Volume Fraction - Dilatometry
2. N. Darwish and R. Elliott: Materials Science and Technology, 9(1993), 572.