First page Back Continue Last page Summary Graphics
FE: Microscopic Modelling of FRP
Matrix and fibre material are modelled separately
Material properties: elastic or inelastic
Special problems to be solved:
- Interface: fully bonded or (partially) detached
- Nonlinear interface interactions
Notes: