Lay-Up of Unidirectional Composites
Angle-ply:
±Q laminates
Cross-ply laminates:
0°, 90° laminates
Mostly symmetric to avoid warping during fabrication
Include off-axis plies to prevent splitting and avoid high Poissons ratios