1. Fe-0.4C
2. Fe-0.4C-2Si
3. Fe-0.4C-1Ni
4. Fe-0.4C-1Mn
5. Fe-0.4C-1Mn-1Cr
6. Fe-0.4C-2Mn
0 1 2 3 4 5
10 10 10 10 10 10
Time / s
800
700
600
500
400
300
200
Temperature / C
calculations