Tm of hcp-Fe
At the P conditions existing at the inner core/outer core boundary, pure iron melts at 6400 C.
However, the presence of alloying elements such as S, Si and O will probably reduce this temperature to 5500 C.
This is very hot, comparable with temperatures on the surface of the Sun.