What is MTDATA ?
Designed to calculate phase/chemical equilibria with maximum ease and reliability
- Interactive
- User application programming
Despite reports to the contrary MTDATA does not work like other comparable programs
- A true Gibbs energy minimisation
- A non-linear optimisation problem with linear constraints
- NPL Numerical Optimisation Software Library
- No initial guess required
- Mathematical guarantee that G reduces each time it is evaluated
- Result can be proven to be a solution to the posed problem
- Very high reliability