Typical experimental data input
; Water activity data at 298.15
; Macro T/K molality act(H2O) uncert reference
"actH2O.mac" 298.15 0.1 0.998004 0.0001 "actH2O-298:74PIT/MAY"
"actH2O.mac" 298.15 0.2 0.99639 0.0001 "actH2O-298:74PIT/MAY"
"actH2O.mac" 298.15 0.3 0.994889 0.0001 "actH2O-298:74PIT/MAY"
"actH2O.mac" 298.15 0.4 0.993443 0.0001 "actH2O-298:74PIT/MAY"
"actH2O.mac" 298.15 0.5 0.99202 0.0001 "actH2O-298:74PIT/MAY"
; NiSO4 enthalpy of formation at various concentrations (82WAG/EVA)
; Macro n(H2O) DfHsol uncert reference
"DfHdil.mac" 200.0 -958505 500 "DfH-298:82WAG/EVA"
"DfHdil.mac" 300.0 -958672 500 "DfH-298:82WAG/EVA"
"DfHdil.mac" 400.0 -958797 500 "DfH-298:82WAG/EVA"
"DfHdil.mac" 500.0 -958906 200 "DfH-298:82WAG/EVA"
"DfHdil.mac" 800.0 -959169 200 "DfH-298:82WAG/EVA“
; NiSO4 solubility (65LIN, Vol II, p1219) for equilibrium aq + NiSO4(H2O)7<c>
; Macro T/K wt fraction uncert reference
"T-W1.mac" 273.15 0.216 0.005 "Solub-NH5:65LIN"
"T-W1.mac" 278.15 0.231 0.005 "Solub-NH5:65LIN"
"T-W1.mac" 283.15 0.246 0.005 "Solub-NH7:65LIN"