First page Back Continue Last page Summary Graphics
Summary
-  HCM12A has its major strength contribution from vanadium and its nitride.
-  Chromium has negligible contribution to creep strength; added for corrosion resistance.
-  Copper in HCM12A improves toughness.
-  All other precipitates would have contributed at the early stage of creep life.