Stoichiometric substance or solution phase “end member”
GCaKCl3 = A + BT + CTlnT + DT2 + ET3 + F/T
Solution phase (Redlich-Kister model for Gex)
GLIQUID = xKCl GKCl + xCaCl2 GCaCl2
+ RT xKClln xKCl + RT xCaCl2ln xCaCl2
Gex = (L00+L01T) xKClxCaCl2
+ (L10+L11T) xKClxCaCl2 (xKCl-xCaCl2)
+ (L20+L21T) xKClxCaCl2 (xKCl-xCaCl2)2