PPT Slide
SPINEL MODEL
(Ni2+, Al3+)1 (Ni2+, Al3+, Va)2 (Va)2 (O2-)4
“normal” NiAl2O4 - (Ni2+) (Al3+ Al3+) (Va)2 (O2-)4
“inverse” NiAl2O4 - (Al3+) (Ni2+ Al3+) (Va2) (O2-)4
“degree of inversion”
is the fraction of sites on the first sublattice occupied by Al3+