MIRO(Mineral Industry Research Organisation)Projects RC54, RC81 and RC132
To develop a high quality, comprehensive thermodynamic database for oxide and sulphur containing systems of industrial interest for use in predictive phase equilibrium calculations
Facilitates calculations directly relevant to industrial processes for temperature and composition ranges outside the scope of hard copy phase diagram compilations
- Systems and priorities determined by the sponsors
- Database validated against plant / process data by sponsors