AREAS BEING CONSIDERED FOR FUTURE WORK
CONTINUE TO EXTEND COVERAGE OF CURRENT OXIDES
- addition of Co, Mn, Pb to matte / metal phase
- addition of CoO, TiO2, V2O3, rare earth oxides to oxide phases
- molten salt - oxide systems
(including addition of CaF2 to oxide phases)
- inclusion of P, As
- inclusion of H2O (at high and low temperatures)
- modelling volume changes in oxide phases