1989 Mou & Aaronson
correct Z, __ positive and large, oscillations
___negative but with wrong model
Summary:
Considerable evidence for strong repulsion between carbon atoms in ferrite. __ is large and positive, but why are there oscillations in its value?
Generally agreed that McLellan & Dunn model is the best quasichemical model for interstitial solutions.