Amorphous phase formation during mechanical alloying of Cu and Cd powders
Zhang & Massalski
Metall. & Mater. Trans. 29A (1998) 2425
Ö.contribution from Cu/d interfaces, and accompanying increase in free energy, provide additional driving force for amorphisationÖ.