Modelling Dispersoid Precipitation
Effectiveness of dispersoids depends on their size, spacing and distribution
Develop model for dispersoid precipitation and use to optimize homogenization treatment to give best dispersoid distribution
To model dispersoid precipitation must account for both non-uniform distribution of Zr due to microsegregation during casting and Al3Zr precipitation kinetics