Two Step Practice
Two step homogenization practice may be of benefit
- Step 1: Hold at a temperature to precipitate optimum dispersoid distribution
- Step 2: Hold at final homogenization temperature
Model used to determine best conditions for step 1
Test 2 step homogenization practice