Table of Contents
Strain-induced Stabilisation of Austenite Against Bainite Transformation
Fe - 0.12 C - 2.0 Si - 3.0 Mn (wt%)
PPT Slide
PPT Slide
PPT Slide
PPT Slide
PPT Slide
PPT Slide
PPT Slide
PPT Slide
PPT Slide
PPT Slide
PPT Slide
PPT Slide
PPT Slide
PPT Slide
PPT Slide
Conclusion
|
Author: Shiv Brat Singh
Download presentation source
Download publication
Other References
- Quantitative Evidence for the Mechanical Stabilisation of
Bainite, Materials Science and Technology, Vol. 12, 1996, pp.
610-612.
- Estimation of Bainite Plate-Thickness in Low-Alloy
Steels, Materials Science and
Engineering A, Vol. A245, 1998. pp. 72-79.
- Mechanical Stabilization of Bainite
Materials Science and Technology, Vol. 11, 1995, 1116-1128.
- The Mechanical Stabilisation of Wimanstatten Ferrite,
Materials Science and Engineering A, Vol. 223, 1997, pp.
179-185.
|