Modelling Sensitisation
Notes:
Two kind of approaches:
-empirical approaches divide the process in two stages, in a first time, precipitate growth causes the Cr depletion, in a second stage, diffusion causes self-healing. However, fitting parameters need experiments on the system to model ! And approach violates local equilibrium hypothesis.
-Thermo/kinetics