Titanium Alloys: Aeroengine fan blade made out of Ti-6V-4Al wt%, about 40 cm in height.
Notice the structure of the root, which slots into the disc in the final assembly.
|
Titanium Alloys: Aeroengine fan blade made out of Ti-6V-4Al wt%, about 40 cm in height.
|
Titanium Alloys: Aeroengine fan blade made out of Ti-6V-4Al wt%, about 40 cm in height.
|
Titanium Alloys: Aeroengine fan blade made out of Ti-6V-4Al wt%, about 40 cm in height.
|
Titanium Alloys: Aeroengine fan blade made out of Ti-6V-4Al wt%, about 40 cm in height.
|
Titanium Alloys: Aeroengine fan blade made out of Ti-6V-4Al wt%, almost a meter in height. Notice the structure of the root.
|
Titanium Alloys: Aeroengine fan blade made out of Ti-6V-4Al wt%, almost a meter in height.
|
Titanium Alloys: Aeroengine fan blade made out of Ti-6V-4Al wt%, almost a meter in height.
|
Titanium Alloys: Aeroengine fan blade made out of Ti-6V-4Al wt%, almost a meter in height.
|