Prediction Error Pred-Err Pred+Err
3.065399 1.058569 2.006828 4.123967
4.034503 0.750427 3.284075 4.784930
5.887806 0.545741 5.342065 6.433547
8.595153 0.636901 7.958251 9.232054
11.974326 0.766221 11.208106 12.740548
15.777820 0.775496 15.002323 16.553314
19.756794 0.694035 19.062759 20.450829
30.877413 0.933913 29.943501 31.811325
49.164585 1.691071 47.473568 50.855606
54.055214 1.270993 52.784222 55.326206
55.752804 1.036097 54.716709 56.788902
56.496075 0.947110 55.548965 57.443184
56.876881 0.918384 55.958496 57.795265
57.093967 0.911653 56.182316 58.005623
2.832941 1.190539 1.642401 4.023479
2.876665 1.158156 1.718508 4.034821
3.442706 0.912766 2.529938 4.355472
4.848372 0.613104 4.235267 5.461474
7.141892 0.565510 6.576330 7.707457
10.211493 0.712691 9.498803 10.924186
13.839503 0.786891 13.052611 14.626395
17.767174 0.739880 17.027294 18.507002
21.752350 0.655292 21.097057 22.407642
25.605345 0.669443 24.935902 26.274788
29.200069 0.826323 28.373747 30.026392
32.468472 1.046538 31.421934 33.515011
35.386494 1.260870 34.125626 36.647366
37.959591 1.439374 36.520218 39.398964
40.210556 1.573888 38.636665 41.784443
42.170387 1.666002 40.504387 43.836391
43.872803 1.721493 42.151306 45.594296
45.350811 1.747198 43.603615 47.098011
46.634895 1.749795 44.885101 48.384689
47.752346 1.735061 46.017288 49.487408
48.726860 1.707925 47.018932 50.434784
49.579048 1.672256 47.906792 51.251301
50.326347 1.631075 48.695271 51.957420
50.983757 1.586714 49.397045 52.570473
51.563896 1.540975 50.022923 53.104870
52.077412 1.495130 50.582283 53.572544
52.533478 1.450080 51.083397 53.983559
52.939724 1.406567 51.533154 54.346291
53.302666 1.364962 51.937706 54.667629
53.627930 1.325583 52.302345 54.953510
53.920223 1.288589 52.631634 55.208813
54.183578 1.254033 52.929546 55.437614
54.421604 1.221915 53.199688 55.643517
54.637207 1.192235 53.444973 55.829441
54.832989 1.164887 53.668102 55.997875
55.011173 1.139765 53.871410 56.150940
55.173779 1.116763 54.057014 56.290543
55.322392 1.095775 54.226616 56.418167
55.458599 1.076642 54.381958 56.535244
55.583683 1.059205 54.524475 56.642887
55.698692 1.043411 54.655281 56.742104
55.804691 1.029101 54.775589 56.833790
55.902580 1.016169 54.886414 56.918751
55.993053 1.004456 54.988598 56.997509
56.076897 0.993909 55.082989 57.070808
56.154701 0.984422 55.170280 57.139126
56.226997 0.975889 55.251106 57.202885
56.294304 0.968204 55.326099 57.262512
56.357006 0.961314 55.395691 57.318317
56.415516 0.955113 55.460403 57.370628
56.470158 0.949601 55.520557 57.419762
56.521305 0.944672 55.576633 57.465977
56.569267 0.940273 55.628998 57.509541
56.614212 0.936351 55.677860 57.550564
56.656403 0.932906 55.723495 57.589306
56.696098 0.929832 55.766266 57.625931
56.733410 0.927076 55.806335 57.660488
56.768600 0.924691 55.843910 57.693295
56.801781 0.922571 55.879208 57.724350
56.833050 0.920716 55.912334 57.753769
56.862625 0.919126 55.943550 57.781750
56.890610 0.917695 55.972912 57.808304
56.917053 0.916476 56.000580 57.833530
56.942123 0.915469 56.026657 57.857594
56.965923 0.914568 56.051353 57.880489
56.988445 0.913826 56.074619 57.902271
57.009861 0.913190 56.096668 57.923050
57.030209 0.912713 56.117496 57.942921
57.049606 0.912289 56.137321 57.961899
57.067997 0.911971 56.156029 57.979969
57.085541 0.911759 56.173782 57.997303
57.102238 0.911600 56.190636 58.013836
57.102238 0.911600 56.190636 58.013836