#H S_W[ 1]  S_W[ 2]  S_W[ 3]  SIGMA_NU D_EN    D_X2 /NDF WX2/k1 WX2/k2 WX2/k3 GAMMA3 LOGOC3  LOGOCF  SYMS NU T_EN   MT_EB     T_X2   NDF  T_EN 2   MT_E2B   T_X2 2 NDF  EVAB    EVB     EVDENCE EVAB2   FUDGE1  FUDGE2  
7  20       20       20       0.3      0.007247 0.1611 4   0.04417 0.01403 0.04009 2.795  75.7    -86.12  5040 0  0.023302 -0.98556 0.5178 4   0.023302 -0.98556 0.5178 4   -80.215 -83.835 -84.275 -4.5164 0.064692 2.0982  
7  2.707    2.707    2.707    0.3      0.006372 0.1416 4   2.169  0.03994 1.766  2.042  36.55   -42.12  24   1  0.019018 0.1675   0.4226 4   0.019018 0.1675   0.4226 4   -31.695 -34.792 -35.475 4.8542  0.047527 1.5567  
7  1.546    0.3663   0.9815   0.080664 0.002961 0.91  4   15.17  2.29   8.157  2.318  9.963   -16.09  720  6  0.0083227 4.3546   2.558  4   0.0083227 4.3546   2.558  4   -15.025 -17.745 -18.352 -5.0614 0.0045103 2.5165  
7  2.565    0.3514   0.598    0.059327 0.0009898 0.5624 4   17.2   2.025  11.65  2.543  9.203   -15.37  720  6  0.0026515 5.3544   1.507  4   0.0026515 5.3544   1.507  4   -13.112 -15.836 -16.371 -3.9087 0.0024847 2.3248  
7  4.008    0.3735   0.4161   0.036854 0.0001928 0.2839 4   15.91  1.083  19.45  2.716  9.322   -16.03  720  6  0.0016777 6.3845   2.47   4   0.0016777 6.3845   2.47   4   -11.955 -14.564 -15.036 -2.6324 0.00097048 2.1666  
7  5.197    0.3833   0.3687   0.017332 2.325e-05 0.1548 4   15.69  0.7925 23.52  2.856  8.74    -17.06  720  6  0.0045461 7.4749   30.27  4   0.0045461 7.4749   30.27  4   -10.047 -12.577 -12.99  -1.3074 0.00022031 2.1347  
7  6.055    0.4041   0.3578   0.0063766 2.305e-05 1.134 4   11.55  0.7142 25     2.996  6.917   -18.26  720  6  0.0045569 8.2112   224.1  4   0.0045569 8.2112   224.1  4   -7.6498 -10.302 -10.651 -0.73276 3.6222e-05 3.2107  
7  5.616    0.386    0.3576   0.0067775 2.301e-05 1.002 4   13.43  0.7845 25.02  2.989  6.322   -17.41  720  6  0.0045592 8.1157   198.5  4   0.0045592 8.1157   198.5  4   -7.0451 -9.7004 -10.052 -0.72362 4.0077e-05 3.0738  
7  5.641    0.3837   0.3577   0.0067471 2.299e-05 1.01  4   13.31  0.7957 25.02  2.989  6.294   -17.4   720  6  0.0045613 8.1001   200.4  4   0.0045613 8.1001   200.4  4   -7.0174 -9.6647 -10.017 -0.72303 3.9769e-05 3.0822  