#H S_W[ 1]  S_W[ 2]  S_W[ 3]  SIGMA_NU D_EN    D_X2 /NDF WX2/k1 WX2/k2 WX2/k3 GAMMA3 LOGOC3  LOGOCF  SYMS NU T_EN   MT_EB     T_X2   NDF  T_EN 2   MT_E2B   T_X2 2 NDF  EVAB    EVB     EVDENCE EVAB2   FUDGE1  FUDGE2  
12 20       20       20       0.3      2.211e-05 0.0004913 4   0.0775 0.02075 0.03743 3.048  133     -144.8  17.5 0  0.0074395 -2.5894  0.1653 4   0.0074395 -2.5894  0.1653 4   -132.91 -136.66 -136.98 0.066858 0.068589 2.1133  
12 2.707    2.707    2.707    0.3      0.003954 0.08787 4   1.405  0.04785 1.163  2.286  65.25   -70.84  17.5 7  0.010569 -0.35994 0.2349 4   0.010569 -0.35994 0.2349 4   -72.484 -75.696 -76.312 -7.2307 0.052423 1.6724  
12 1.692    0.3663   0.9283   0.067926 0.002207 0.9569 4   9.827  1.934  4.685  2.422  20.8    -27.29  17.5 11 0.0057007 4.9171   2.471  4   0.0057007 4.9171   2.471  4   -36.025 -38.825 -39.399 -15.22  0.0033454 2.6355  
12 2.883    0.409    0.5356   0.052891 0.0006372 0.4556 4   9.791  1.201  8.308  2.596  21.59   -27.86  17.5 11 0.0017349 5.6049   1.24   4   0.0017349 5.6049   1.24   4   -35.532 -38.338 -38.854 -13.94  0.0019746 2.2547  
12 4.338    0.4158   0.3999   0.030124 0.0001098 0.242 4   9.124  0.6813 12.71  2.761  22.05   -29.16  17.5 11 0.002407 6.7346   5.305  4   0.002407 6.7346   5.305  4   -34.69  -37.362 -37.816 -12.643 0.00065374 2.1555  
12 5.444    0.4269   0.3646   0.01331  1.051e-05 0.1187 4   9.055  0.5229 14.78  2.916  22      -31     17.5 10 0.0057788 7.5067   65.24  4   0.0057788 7.5067   65.24  4   -30.231 -32.842 -33.229 -8.2342 0.00013177 2.1398  
12 6.149    0.4537   0.3566   0.0044035 1.044e-05 1.076 4   7.099  0.4633 15.46  3.167  20.47   -32.91  17.5 10 0.005787 7.8549   596.9  4   0.005787 7.8549   596.9  4   -28.112 -30.957 -31.212 -7.6416 1.796e-05 3.2713  
12 5.521    0.4036   0.354    0.0050045 1.042e-05 0.8324 4   8.805  0.5862 15.69  3.108  18.21   -30.11  17.5 10 0.0057884 7.5125   462.2  4   0.0057884 7.5125   462.2  4   -25.832 -28.598 -28.888 -7.6213 2.2065e-05 2.9866  
12 5.652    0.4265   0.3542   0.0048339 1.041e-05 0.8914 4   8.4    0.5255 15.67  3.122  19.03   -31.07  17.5 10 0.0057898 7.6613   495.6  4   0.0057898 7.6613   495.6  4   -26.649 -29.459 -29.741 -7.6199 2.0844e-05 3.0557  