{} Predicted Error
-2.3025 3.065399 1.058569
-1.609 4.034503 0.750427
-1.204 5.887806 0.545741
-0.916 8.595153 0.636901
-0.693 11.974326 0.766221
-0.511 15.777820 0.775496
-0.357 19.756794 0.694035
0 30.877413 0.933913
0.693 49.164585 1.691071
1.0986 54.055214 1.270993
1.3863 55.752804 1.036097
1.6094 56.496075 0.947110
1.7918 56.876881 0.918384
1.9459 57.093967 0.911653