{} Predicted Error
-2.3025 3.065399 1.058569
-1.609 4.034503 0.750427
-1.204 5.887806 0.545741
-0.916 8.595153 0.636901
-0.693 11.974326 0.766221
-0.511 15.777820 0.775496
-0.357 19.756794 0.694035
0 30.877413 0.933913
0.693 49.164585 1.691071
1.0986 54.055214 1.270993
1.3863 55.752804 1.036097
1.6094 56.496075 0.947110
1.7918 56.876881 0.918384
1.9459 57.093967 0.911653
-4.605170186 2.832941 1.190539
-2.995732274 2.876665 1.158156
-1.897119985 3.442706 0.912766
-1.386294361 4.848372 0.613104
-1.049822124 7.141892 0.565510
-0.798507696 10.211493 0.712691
-0.597837001 13.839503 0.786891
-0.430782916 17.767174 0.739880
-0.287682072 21.752350 0.655292
-0.162518929 25.605345 0.669443
-0.051293294 29.200069 0.826323
0.048790164 32.468472 1.046538
0.139761942 35.386494 1.260870
0.223143551 37.959591 1.439374
0.300104592 40.210556 1.573888
0.371563556 42.170387 1.666002
0.438254931 43.872803 1.721493
0.500775288 45.350811 1.747198
0.559615788 46.634895 1.749795
0.615185639 47.752346 1.735061
0.667829373 48.726860 1.707925
0.717839793 49.579048 1.672256
0.765467842 50.326347 1.631075
0.810930216 50.983757 1.586714
0.854415328 51.563896 1.540975
0.896088025 52.077412 1.495130
0.936093359 52.533478 1.450080
0.97455964 52.939724 1.406567
1.011600912 53.302666 1.364962
1.047318994 53.627930 1.325583
1.08180517 53.920223 1.288589
1.115141591 54.183578 1.254033
1.147402453 54.421604 1.221915
1.178654996 54.637207 1.192235
1.208960346 54.832989 1.164887
1.238374231 55.011173 1.139765
1.266947603 55.173779 1.116763
1.294727168 55.322392 1.095775
1.32175584 55.458599 1.076642
1.348073148 55.583683 1.059205
1.373715579 55.698692 1.043411
1.398716881 55.804691 1.029101
1.423108334 55.902580 1.016169
1.446918983 55.993053 1.004456
1.470175845 56.076897 0.993909
1.492904096 56.154701 0.984422
1.515127233 56.226997 0.975889
1.53686722 56.294304 0.968204
1.558144618 56.357006 0.961314
1.578978705 56.415516 0.955113
1.599387577 56.470158 0.949601
1.619388243 56.521305 0.944672
1.638996715 56.569267 0.940273
1.658228077 56.614212 0.936351
1.677096561 56.656403 0.932906
1.695615609 56.696098 0.929832
1.713797928 56.733410 0.927076
1.731655545 56.768600 0.924691
1.749199855 56.801781 0.922571
1.766441661 56.833050 0.920716
1.78339122 56.862625 0.919126
1.800058272 56.890610 0.917695
1.816452082 56.917053 0.916476
1.832581464 56.942123 0.915469
1.848454813 56.965923 0.914568
1.864080131 56.988445 0.913826
1.87946505 57.009861 0.913190
1.894616855 57.030209 0.912713
1.909542505 57.049606 0.912289
1.924248652 57.067997 0.911971
1.93874166 57.085541 0.911759
1.953027617 57.102238 0.911600
 57.102238 0.911600