<--Previous Up Next-->
Higher magnification image. Pearlite in a hypoeutectoid steel Roman nail from Cordoba, dating first century B.C. to 1st century A.D. Shows cementite in the pearlite as prismatic lamellae. The original nail was 12 cm long, from a Roman thermal spring. Shows the fragmentation of the lamellae.