#Hubbell, J.H. and Seltzer, S.M. (2004), Tables of X-Ray Mass Attenuation Coefficients and Mass Energy-Absorption Coefficients (version 1.4). [Online] Available: http://physics.nist.gov/xaamdi [2005, March 16]. National Institute of Standards and Technology, Gaithersburg, MD. #Iron #Z = 26 #ASCII format #____________________________________ # Energy mu over rho mu e n over rho # (MeV) (cm2/g) (cm2/g) #____________________________________ 1.00000E-03 9.085E+03 9.052E+03 1.50000E-03 3.399E+03 3.388E+03 2.00000E-03 1.626E+03 1.620E+03 3.00000E-03 5.576E+02 5.535E+02 4.00000E-03 2.567E+02 2.536E+02 5.00000E-03 1.398E+02 1.372E+02 6.00000E-03 8.484E+01 8.265E+01 7.11200E-03 5.319E+01 5.133E+01 #K 7.11200E-03 4.076E+02 2.978E+02 8.00000E-03 3.056E+02 2.316E+02 1.00000E-02 1.706E+02 1.369E+02 1.50000E-02 5.708E+01 4.896E+01 2.00000E-02 2.568E+01 2.260E+01 3.00000E-02 8.176E+00 7.251E+00 4.00000E-02 3.629E+00 3.155E+00 5.00000E-02 1.958E+00 1.638E+00 6.00000E-02 1.205E+00 9.555E-01 8.00000E-02 5.952E-01 4.104E-01 1.00000E-01 3.717E-01 2.177E-01 1.50000E-01 1.964E-01 7.961E-02 2.00000E-01 1.460E-01 4.825E-02 3.00000E-01 1.099E-01 3.361E-02 4.00000E-01 9.400E-02 3.039E-02 5.00000E-01 8.414E-02 2.914E-02 6.00000E-01 7.704E-02 2.836E-02 8.00000E-01 6.699E-02 2.714E-02 1.00000E+00 5.995E-02 2.603E-02 1.25000E+00 5.350E-02 2.472E-02 1.50000E+00 4.883E-02 2.360E-02 2.00000E+00 4.265E-02 2.199E-02 3.00000E+00 3.621E-02 2.042E-02 4.00000E+00 3.312E-02 1.990E-02 5.00000E+00 3.146E-02 1.983E-02 6.00000E+00 3.057E-02 1.997E-02 8.00000E+00 2.991E-02 2.050E-02 1.00000E+01 2.994E-02 2.108E-02 1.50000E+01 3.092E-02 2.221E-02 2.00000E+01 3.224E-02 2.292E-02