Current page: 25

The benches are at various stages of failure. The solution is to use a beam whose grain does not follow its length. Must be hard to get such beams. So the alternative is to screw the vertical slats in poisition, rather than create stress concentrations by forcing the vertical slats into the holes. This would create tensile stresses normal to the flow of the grain, and hence failure.