Generated by CrystalMaker 10.8.3 for macOS (https://crystalmaker.com) Coordinates for "AMS_DATA" Unit cell parameters:- a = 4.75890; b = 4.75890; c = 12.99100 Å alpha = 90.0000; beta = 90.0000; gamma = 120.0000° Listing of all 46 visible atoms: --------------------------------------------------------------------------------------- Fractional Coordinates Orthogonal Coordinates [Å] Elmt Label x y z xor yor zor --------------------------------------------------------------------------------------- O O 0.306000 0.000000 0.250000 1.26113 0.72811 -3.24775 O O 0.000000 0.306000 0.250000 -0.00000 -1.45622 -3.24775 O O 0.694000 0.694000 0.250000 2.86020 -1.65134 -3.24775 O O 0.694000 0.000000 0.750000 2.86020 1.65134 -9.74325 O O 0.000000 0.694000 0.750000 -0.00000 -3.30268 -9.74325 O O 0.306000 0.306000 0.750000 1.26113 -0.72811 -9.74325 O O 0.972667 0.333333 0.583333 4.00868 0.72811 -7.57808 O O 0.639333 0.666667 0.916667 2.63490 -1.65134 -11.90842 O O 0.666667 0.639333 0.583333 2.74755 -1.45622 -7.57808 O O 0.333333 0.972667 0.916667 1.37378 -3.83567 -11.90842 O O 0.360667 0.027333 0.583333 1.48643 0.72811 -7.57808 O O 0.027333 0.360667 0.916667 0.11265 -1.65134 -11.90842 O O 0.360667 0.333333 0.083333 1.48643 -0.72811 -1.08258 O O 0.027333 0.666667 0.416667 0.11265 -3.10756 -5.41292 O O 0.666667 0.027333 0.083333 2.74755 1.45622 -1.08258 O O 0.333333 0.360667 0.416667 1.37378 -0.92323 -5.41292 O O 0.972667 0.639333 0.083333 4.00868 -0.72811 -1.08258 O O 0.639333 0.972667 0.416667 2.63490 -3.10756 -5.41292 O O 0.306000 1.000000 0.250000 1.26113 -4.03079 -3.24775 O O 0.694000 1.000000 0.750000 2.86020 -3.10756 -9.74325 O O 1.000000 0.306000 0.250000 4.12133 0.92323 -3.24775 O O 1.000000 0.694000 0.750000 4.12133 -0.92323 -9.74325 Al Al 0.000000 0.000000 0.352000 0.00000 0.00000 -4.57283 Al Al 0.000000 0.000000 0.148000 0.00000 0.00000 -1.92267 Al Al 0.000000 0.000000 0.648000 0.00000 0.00000 -8.41817 Al Al 0.000000 0.000000 0.852000 0.00000 0.00000 -11.06833 Al Al 0.666667 0.333333 0.685333 2.74755 -0.00000 -8.90317 Al Al 0.333333 0.666667 0.018667 1.37378 -2.37945 -0.24250 Al Al 0.666667 0.333333 0.481333 2.74755 -0.00000 -6.25300 Al Al 0.333333 0.666667 0.814667 1.37378 -2.37945 -10.58333 Al Al 0.666667 0.333333 0.981333 2.74755 -0.00000 -12.74850 Al Al 0.333333 0.666667 0.314667 1.37378 -2.37945 -4.08783 Al Al 0.666667 0.333333 0.185333 2.74755 -0.00000 -2.40767 Al Al 0.333333 0.666667 0.518667 1.37378 -2.37945 -6.73800 Al Al 0.000000 1.000000 0.352000 -0.00000 -4.75890 -4.57283 Al Al 0.000000 1.000000 0.148000 -0.00000 -4.75890 -1.92267 Al Al 0.000000 1.000000 0.648000 -0.00000 -4.75890 -8.41817 Al Al 0.000000 1.000000 0.852000 -0.00000 -4.75890 -11.06833 Al Al 1.000000 0.000000 0.352000 4.12133 2.37945 -4.57283 Al Al 1.000000 0.000000 0.148000 4.12133 2.37945 -1.92267 Al Al 1.000000 0.000000 0.648000 4.12133 2.37945 -8.41817 Al Al 1.000000 0.000000 0.852000 4.12133 2.37945 -11.06833 Al Al 1.000000 1.000000 0.352000 4.12133 -2.37945 -4.57283 Al Al 1.000000 1.000000 0.148000 4.12133 -2.37945 -1.92267 Al Al 1.000000 1.000000 0.648000 4.12133 -2.37945 -8.41817 Al Al 1.000000 1.000000 0.852000 4.12133 -2.37945 -11.06833 ---------------------------------------------------------------------------------------