The phase transformation theory available for the modelling of microstructure in steel weld deposits is reviewed with the aim of summarising the progress, and identifying the limitations of current methods.
Modelling the Microstructure in the Fusion Zone of Steel Weld Deposits 
Recent Trends in Welding Science and Technology (TWR'89), 
eds. S. A. David and  J. M. Vitek, ASM International, 
Ohio, U. S. A., 1989, 189-198.
    
     
    
 | 