A database for the Ms temperature of steels as a function of chemical composition.
| Language: | NA |
| Product form: | OpenOffice or Excel spreadsheet, plain text. |
Operating System : irrelevant.
MAP_DATA_STEEL_MS
contains data for the martensite start temperature of a variety of steels as a
function of their composition. It contains, as a subset, the databases offered
by Capdevilla et al, or Pieter van der Wolk on this web site (MAP). However,
these have been thoroughly checked and a number of significant errors were found
and corrected. The present database contains an additional 700 data points
gathered from published literature.
We would therefore recommend use of the present database in all cases.
The input variables are C, Mn, Si, Cr, Ni, Mo, V, Co, Al, W, Cu, Nb, Ti, B and N.
Penultimate column contains Ms temperature in Kelvin, last column contains a
reference which is detailed on sheet 3 (References).