1 0.29 0.09 0.74 0.002 0.007 0.66 1.3 1.02 0.292 0 0 0.001 0.0041 0 5 -0.0001798 0 7 -0.0002294 0.6738 8 -0.0002294 1.348 7 -0.0002418 2.021 7 -0.000217 2.695 9 -0.0001922 3.369 9 -0.0002294 4.043 8 -0.0002418 4.717 8 -0.0002418 5.391 9 -0.0002294 6.064 9 -0.0002418 6.738 11 -0.000217 7.412 12 -0.0001798 8.086 14 -0.0001426 8.76 15 -0.0001302 9.434 16 -0.0001302 10.11 18 -9.298e-05 10.78 18 -8.058e-05 11.46 19 -6.819e-05 12.13 20 -6.819e-05 12.8 20 -5.579e-05 13.48 21 -6.819e-05 14.15 21 -3.099e-05 14.82 22 -3.099e-05 15.5 23 -1.86e-05 16.17 23 -6.199e-06 16.85 24 6.199e-06 17.52 24 6.199e-06 18.19 25 6.199e-06 18.87 26 6.199e-06 19.54 27 6.199e-06 20.21 27 6.199e-06 20.89 27 6.199e-06 21.56 28 6.199e-06 22.24 30 6.199e-06 22.91 30 6.199e-06 23.58 30 6.199e-06 24.26 30 6.199e-06 24.93 32 1.86e-05 25.61 32 3.099e-05 26.28 34 3.099e-05 26.95 34 3.099e-05 27.63 34 3.099e-05 28.3 35 3.099e-05 28.97 35 5.579e-05 29.65 37 6.819e-05 30.32 37 8.058e-05 31 38 8.058e-05 31.67 38 0.0001178 32.34 39 0.0001054 33.02 40 0.0001302 33.69 41 0.0001302 34.37 41 0.0001426 35.04 41 0.0001302 35.71 43 0.0001302 36.39 43 0.0001302 37.06 44 0.0001426 37.73 45 0.0001674 38.41 45 0.0001798 39.08 46 0.0001922 39.76 46 0.000217 40.43 48 0.0002294 41.1 48 0.0002294 41.78 48 0.0002418 42.45 49 0.0002294 43.13 50 0.0002294 43.8 51 0.0002541 44.47 51 0.0002665 45.15 52 0.0002541 45.82 52 0.0002789 46.49 53 0.0002913 47.17 54 0.0003037 47.84 55 0.0002789 48.52 55 0.0002789 49.19 55 0.0002789 49.86 56 0.0003285 50.54 57 0.0003285 51.21 59 0.0003409 51.88 59 0.0003409 52.56 59 0.0003657 53.23 60 0.0003781 53.91 61 0.0003905 54.58 62 0.0003905 55.25 62 0.0003905 55.93 63 0.0003905 56.6 63 0.0004029 57.28 65 0.0004401 57.95 65 0.0004525 58.62 66 0.0004401 59.3 66 0.0004401 59.97 66 0.0004525 60.64 68 0.0004525 61.32 68 0.0004525 61.99 69 0.0004525 62.67 70 0.0004649 63.34 70 0.0004773 64.01 71 0.0004773 64.69 71 0.0004897 65.36 73 0.0004897 66.04 73 0.0005021 66.71 74 0.0005393 67.38 74 0.0005393 68.06 75 0.0005517 68.73 76 0.0005641 69.4 77 0.0005641 70.08 77 0.0005889 70.75 77 0.0005889 71.43 79 0.0005889 72.1 79 0.0006013 72.77 81 0.0006137 73.45 81 0.0006385 74.12 81 0.0006509 74.8 81 0.0006509 75.47 83 0.0006509 76.14 84 0.0006509 76.82 84 0.0006509 77.49 84 0.0006509 78.16 84 0.0006633 78.84 86 0.0006757 79.51 87 0.0006881 80.19 87 0.0007005 80.86 88 0.0007005 81.53 88 0.0007005 82.21 90 0.0007377 82.88 90 0.0007624 83.55 91 0.0007501 84.23 91 0.0007501 84.9 92 0.0007501 85.58 93 0.0007748 86.25 93 0.0007996 86.92 94 0.0007996 87.6 95 0.0007996 88.27 95 0.0007996 88.95 96 0.0007996 89.62 96 0.0007996 90.29 97 0.0007996 90.97 98 0.0007996 91.64 98 0.0008244 92.31 99 0.0008368 92.99 99 0.0008492 93.66 100 0.0008492 94.34 101 0.0008616 95.01 102 0.000874 95.68 102 0.000874 96.36 103 0.0008864 97.03 104 0.0008988 97.71 105 0.0008988 98.38 106 0.0008988 99.05 106 0.0008988 99.73 106 0.0009236 100.4 107 0.0009236 101.1 109 0.0009484 101.7 109 0.0009608 102.4 109 0.0009484 103.1 110 0.0009608 103.8 110 0.0009732 104.4 111 0.000998 105.1 112 0.000998 105.8 112 0.00101 106.5 113 0.00101 107.1 114 0.00101 107.8 115 0.00101 108.5 115 0.001035 109.2 116 0.001048 109.8 116 0.00106 110.5 117 0.00106 111.2 118 0.00106 111.9 119 0.00106 112.5 119 0.00106 113.2 120 0.00106 113.9 121 0.001085 114.6 121 0.00111 115.2 122 0.00111 115.9 123 0.00111 116.6 123 0.00111 117.2 124 0.001134 117.9 124 0.001159 118.6 126 0.001159 119.3 126 0.001159 119.9 127 0.001172 120.6 127 0.001172 121.3 127 0.001172 122 129 0.001184 122.6 129 0.001209 123.3 131 0.001221 124 131 0.001209 124.7 131 0.001209 125.3 132 0.001221 126 133 0.001246 126.7 134 0.001271 127.4 134 0.001271 128 135 0.001271 128.7 135 0.001271 129.4 137 0.001271 130 137 0.001296 130.7 138 0.001296 131.4 138 0.001308 132.1 140 0.00132 132.7 140 0.001333 133.4 141 0.00132 134.1 141 0.001345 134.8 141 0.001358 135.4 142 0.00137 136.1 143 0.00137 136.8 144 0.00137 137.5 145 0.00137 138.1 145 0.00137 138.8 146 0.001382 139.5 146 0.001382 140.2 146 0.00137 140.8 148 0.001382 141.5 149 0.001407 142.2 149 0.00142 142.9 149 0.00142 143.5 150 0.001457 144.2 151 0.001457 144.9 152 0.001457 145.5 152 0.001469 146.2 153 0.001469 146.9 154 0.001469 147.6 154 0.001506 148.2 156 0.001494 148.9 156 0.001494 149.6 156 0.001506 150.3 157 0.001519 150.9 159 0.001519 151.6 159 0.001506 152.3 159 0.001556 153 159 0.001556 153.6 161 0.001556 154.3 162 0.001556 155 162 0.001581 155.7 163 0.001593 156.3 163 0.001618 157 163 0.001618 157.7 165 0.001618 158.3 165 0.001618 159 166 0.001643 159.7 166 0.001655 160.4 166 0.001667 161 168 0.001667 161.7 168 0.001667 162.4 169 0.00168 163.1 170 0.001692 163.7 171 0.001717 164.4 171 0.001717 165.1 172 0.001717 165.8 173 0.001717 166.4 174 0.001717 167.1 174 0.001729 167.8 174 0.001729 168.5 175 0.001767 169.1 176 0.001767 169.8 177 0.001767 170.5 177 0.001804 171.2 178 0.001791 171.8 179 0.001816 172.5 180 0.001841 173.2 180 0.001866 173.8 181 0.001841 174.5 181 0.001853 175.2 182 0.001853 175.9 183 0.001853 176.5 184 0.001816 177.2 184 0.001853 177.9 184 0.001903 178.6 186 0.001915 179.2 187 0.001915 179.9 187 0.001915 180.6 187 0.001953 181.3 188 0.00194 181.9 189 0.001965 182.6 190 0.001965 183.3 190 0.001965 184 191 0.001965 184.6 191 0.001965 185.3 193 0.002015 186 193 0.002015 186.7 193 0.002015 187.3 194 0.002015 188 195 0.002027 188.7 196 0.002039 189.3 196 0.002064 190 197 0.002064 190.7 198 0.002064 191.4 199 0.002089 192 199 0.002089 192.7 199 0.002114 193.4 201 0.002126 194.1 201 0.002126 194.7 201 0.002139 195.4 202 0.002163 196.1 202 0.002176 196.8 204 0.002163 197.4 204 0.002176 198.1 205 0.002176 198.8 206 0.002201 199.5 206 0.002201 200.1 206 0.002213 200.8 207 0.002238 201.5 208 0.002238 202.1 209 0.002238 202.8 209 0.002238 203.5 210 0.002263 204.2 210 0.002275 204.8 211 0.002287 205.5 212 0.002287 206.2 213 0.002287 206.9 213 0.0023 207.5 213 0.002312 208.2 215 0.002337 208.9 215 0.002337 209.6 217 0.002349 210.2 217 0.002374 210.9 217 0.002374 211.6 218 0.002374 212.3 218 0.002387 212.9 218 0.002387 213.6 220 0.002399 214.3 220 0.002436 215 221 0.002411 215.6 222 0.002436 216.3 223 0.002411 217 223 0.002436 217.6 224 0.002436 218.3 224 0.002461 219 226 0.002473 219.7 226 0.002486 220.3 227 0.00251 221 227 0.00251 221.7 229 0.002523 222.4 229 0.002535 223 229 0.002548 223.7 230 0.002572 224.4 231 0.002585 225.1 231 0.002585 225.7 232 0.002585 226.4 233 0.002597 227.1 234 0.002585 227.8 234 0.002634 228.4 235 0.002647 229.1 235 0.002634 229.8 237 0.002647 230.4 237 0.002659 231.1 238 0.002672 231.8 238 0.002684 232.5 239 0.002696 233.1 239 0.002696 233.8 240 0.002709 234.5 242 0.002709 235.2 242 0.002734 235.8 243 0.002734 236.5 243 0.002746 237.2 243 0.002758 237.9 244 0.002783 238.5 245 0.002796 239.2 246 0.002796 239.9 246 0.002796 240.6 247 0.002808 241.2 248 0.002845 241.9 249 0.002845 242.6 249 0.002845 243.3 249 0.002845 243.9 250 0.002858 244.6 251 0.002895 245.3 252 0.002907 245.9 252 0.002907 246.6 252 0.002907 247.3 254 0.002907 248 254 0.002932 248.6 256 0.002944 249.3 256 0.002957 250 256 0.002957 250.7 256 0.002957 251.3 258 0.002969 252 259 0.002982 252.7 259 0.003006 253.4 260 0.003006 254 260 0.003019 254.7 261 0.003006 255.4 262 0.003019 256.1 263 0.003044 256.7 263 0.003056 257.4 264 0.003056 258.1 265 0.003056 258.8 265 0.003106 259.4 267 0.003106 260.1 267 0.003106 260.8 268 0.003106 261.4 268 0.003106 262.1 268 0.003106 262.8 269 0.00313 263.5 270 0.003143 264.1 270 0.003155 264.8 271 0.003155 265.5 272 0.003155 266.2 273 0.003155 266.8 274 0.00318 267.5 274 0.003205 268.2 274 0.003205 268.9 276 0.003217 269.5 276 0.003242 270.2 277 0.003242 270.9 277 0.003242 271.6 277 0.003254 272.2 279 0.003267 272.9 280 0.003267 273.6 281 0.003292 274.2 281 0.003304 274.9 281 0.003292 275.6 282 0.003304 276.3 283 0.003341 276.9 284 0.003329 277.6 284 0.003341 278.3 285 0.003354 279 285 0.003341 279.6 286 0.003378 280.3 287 0.003403 281 287 0.003403 281.7 288 0.003403 282.3 289 0.003403 283 290 0.003403 283.7 290 0.003428 284.4 292 0.003453 285 292 0.003453 285.7 292 0.003465 286.4 293 0.003478 287.1 293 0.00349 287.7 294 0.003502 288.4 295 0.003502 289.1 295 0.003502 289.7 296 0.003527 290.4 297 0.003539 291.1 298 0.003552 291.8 299 0.003552 292.4 299 0.003552 293.1 299 0.003552 293.8 300 0.003577 294.5 301 0.003601 295.1 302 0.003601 295.8 302 0.003601 296.5 302 0.003589 297.2 304 0.003601 297.8 304 0.003601 298.5 305 0.003639 299.2 306 0.003651 299.9 306 0.003651 300.5 306 0.003651 301.2 307 0.003663 301.9 309 0.003688 302.5 309 0.003701 303.2 310 0.003713 303.9 310 0.003713 304.6 311 0.003701 305.2 312 0.003701 305.9 312 0.003701 306.6 313 0.003725 307.3 313 0.003738 307.9 314 0.003738 308.6 315 0.00375 309.3 315 0.00375 310 317 0.003787 310.6 317 0.0038 311.3 318 0.003825 312 318 0.003825 312.7 319 0.003837 313.3 320 0.003849 314 320 0.003862 314.7 321 0.003862 315.4 321 0.003874 316 322 0.003899 316.7 323 0.003899 317.4 324 0.003911 318 324 0.003911 318.7 325 0.003949 319.4 326 0.003949 320.1 327 0.003973 320.7 328 0.003961 321.4 328 0.003961 322.1 329 0.003986 322.8 329 0.003998 323.4 330 0.004011 324.1 331 0.004011 324.8 331 0.004023 325.5 331 0.004023 326.1 332 0.004048 326.8 334 0.004035 327.5 334 0.00406 328.2 335 0.00406 328.8 335 0.004073 329.5 336 0.004097 330.2 337 0.00411 330.9 337 0.004122 331.5 338 0.00411 332.2 338 0.004122 332.9 339 0.004147 333.5 340 0.004147 334.2 342 0.004159 334.9 342 0.004159 335.6 342 0.004172 336.2 342 0.004197 336.9 343 0.004221 337.6 344 0.004221 338.3 345 0.004221 338.9 345 0.004246 339.6 346 0.004259 340.3 346 0.004246 341 347 0.004234 341.6 348 0.004259 342.3 349 0.004271 343 349 0.004271 343.7 350 0.004271 344.3 351 0.004321 345 351 0.004321 345.7 353 0.004333 346.3 353 0.004333 347 354 0.004333 347.7 354 0.004333 348.4 355 0.00437 349 356 0.00437 349.7 356 0.004383 350.4 356 0.004395 351.1 357 0.004432 351.7 359 0.004432 352.4 359 0.004432 353.1 359 0.004432 353.8 360 0.004469 354.4 361 0.004469 355.1 362 0.004469 355.8 362 0.004482 356.5 363 0.004482 357.1 363 0.004482 357.8 364 0.004519 358.5 365 0.004531 359.2 365 0.004531 359.8 367 0.004531 360.5 367 0.004531 361.2 367 0.004568 361.8 368 0.004581 362.5 369 0.004581 363.2 369 0.004593 363.9 370 0.004618 364.5 371 0.004618 365.2 371 0.00463 365.9 373 0.00463 366.6 373 0.004655 367.2 374 0.004643 367.9 374 0.004655 368.6 374 0.004668 369.3 376 0.004668 369.9 376 0.004692 370.6 377 0.004692 371.3 378 0.004717 372 378 0.00473 372.6 379 0.004754 373.3 380 0.004754 374 381 0.004754 374.6 381 0.004754 375.3 381 0.004754 376 382 0.004767 376.7 383 0.004779 377.3 384 0.004779 378 385 0.004816 378.7 385 0.004829 379.4 385 0.004829 380 386 0.004829 380.7 387 0.004841 381.4 388 0.004829 382.1 388 0.004866 382.7 389 0.004866 383.4 390 0.004878 384.1 390 0.004891 384.8 392 0.004903 385.4 392 0.004928 386.1 393 0.004928 386.8 393 0.00494 387.5 394 0.004978 388.1 395 0.004978 388.8 395 0.004978 389.5 396 0.004978 390.1 396 0.004978 390.8 397 0.00499 391.5 398 0.005027 392.2 399 0.005027 392.8 399 0.00504 393.5 399 0.00504 394.2 400 0.005027 394.9 401 0.005027 395.5 401 0.005077 396.2 402 0.005089 396.9 403 0.005102 397.6 403 0.005089 398.2 404 0.005126 398.9 404 0.005114 399.6 405 0.005126 400.3 406 0.005126 400.9 406 0.005176 401.6 407 0.005188 402.3 409 0.005188 402.9 409 0.005188 403.6 409 0.005188 404.3 410 0.005226 405 410 0.005238 405.6 411 0.005238 406.3 412 0.005263 407 413 0.005238 407.7 413 0.005238 408.3 414 0.00525 409 415 0.005275 409.7 414 0.005288 410.4 417 0.005288 411 417 0.005288 411.7 417 0.005312 412.4 418 0.005288 413.1 418 0.005325 413.7 419 0.005374 414.4 420 0.005387 415.1 421 0.005387 415.8 421 0.005387 416.4 422 0.005399 417.1 423 0.005399 417.8 424 0.005412 418.4 424 0.005436 419.1 424 0.005436 419.8 425 0.005461 420.5 426 0.005486 421.1 427 0.005498 421.8 428 0.005498 422.5 428 0.005498 423.2 429 0.005498 423.8 429 0.005511 424.5 431 0.005523 425.2 431 0.005535 425.9 431 0.005548 426.5 431 0.005548 427.2 433 0.005573 427.9 434 0.005585 428.6 434 0.00561 429.2 435 0.005622 429.9 436 0.005622 430.6 436 0.005635 431.3 437 0.005647 431.9 437 0.005647 432.6 438 0.005647 433.3 439 0.005672 433.9 439 0.005672 434.6 440 0.005697 435.3 442 0.005697 436 442 0.005734 436.6 442 0.005734 437.3 442 0.005746 438 444 0.005759 438.7 444 0.005759 439.3 445 0.005746 440 446 0.005796 440.7 446 0.005783 441.4 446 0.005808 442 448 0.005808 442.7 448 0.005821 443.4 449 0.005833 444.1 449 0.005845 444.7 450 0.005858 445.4 451 0.005858 446.1 453 0.005883 446.7 453 0.00587 447.4 453 0.005883 448.1 454 0.005883 448.8 454 0.005932 449.4 455 0.005945 450.1 456 0.005969 450.8 456 0.005957 451.5 457 0.005982 452.1 458 0.005994 452.8 459 0.006019 453.5 459 0.006019 454.2 460 0.006019 454.8 460 0.006019 455.5 461 0.006031 456.2 462 0.006019 456.9 463 0.006056 457.5 463 0.006056 458.2 464 0.006069 458.9 464 0.006069 459.6 465 0.006081 460.2 466 0.006106 460.9 467 0.006106 461.6 467 0.006118 462.2 468 0.006143 462.9 468 0.006168 463.6 469 0.006168 464.3 471 0.00618 464.9 471 0.006193 465.6 471 0.006193 466.3 472 0.006205 467 472 0.00623 467.6 473 0.006217 468.3 474 0.006217 469 474 0.006217 469.7 475 0.00623 470.3 476 0.00623 471 477 0.006255 471.7 478 0.006304 472.4 478 0.006329 473 478 0.006329 473.7 479 0.006329 474.4 480 0.006317 475 481 0.006329 475.7 481 0.006341 476.4 482 0.006354 477.1 482 0.006354 477.7 484 0.006354 478.4 484 0.006354 479.1 485 0.006379 479.8 485 0.006403 480.4 486 0.006403 481.1 487 0.006416 481.8 487 0.006416 482.5 488 0.006441 483.1 489 0.006453 483.8 489 0.006453 484.5 490 0.006453 485.2 490 0.006478 485.8 492 0.006503 486.5 492 0.006503 487.2 492 0.006515 487.9 493 0.006515 488.5 494 0.00654 489.2 495 0.006552 489.9 496 0.006564 490.5 496 0.006564 491.2 496 0.006564 491.9 498 0.006577 492.6 498 0.006614 493.2 499 0.006614 493.9 499 0.006602 494.6 500 0.006626 495.3 501 0.006651 495.9 502 0.006664 496.6 503 0.006664 497.3 503 0.006676 498 503 0.006676 498.6 504 0.006713 499.3 505 0.006713 500 505 0.006713 500.7 506 0.006726 501.3 506 0.006726 502 507 0.006763 502.7 508 0.006775 503.4 509 0.006763 504 510 0.006788 504.7 510 0.006812 505.4 510 0.006812 506 512 0.006812 506.7 512 0.006812 507.4 512 0.006812 508.1 514 0.006837 508.7 514 0.006862 509.4 515 0.006874 510.1 515 0.006887 510.8 517 0.006874 511.4 517 0.006912 512.1 517 0.006912 512.8 518 0.006924 513.5 518 0.006949 514.1 519 0.006961 514.8 521 0.006974 515.5 521 0.006974 516.2 521 0.006998 516.8 522 0.007011 517.5 523 0.007011 518.2 524 0.007011 518.8 524 0.006974 519.5 524 0.006974 520.2 526 0.007011 520.9 526 0.007023 521.5 527 0.007073 522.2 528 0.007073 522.9 528 0.007073 523.6 529 0.007085 524.2 530 0.007122 524.9 530 0.007147 525.6 531 0.007135 526.3 532 0.007122 526.9 532 0.007135 527.6 533 0.00716 528.3 534 0.007197 529 534 0.007184 529.6 535 0.007197 530.3 535 0.007222 531 536 0.007222 531.7 537 0.007246 532.3 537 0.007259 533 539 0.007246 533.7 539 0.007271 534.3 540 0.007271 535 540 0.007284 535.7 541 0.007308 536.4 542 0.007308 537 542 0.007321 537.7 543 0.007321 538.4 543 0.007321 539.1 544 0.007321 539.7 545 0.007358 540.4 546 0.00737 541.1 546 0.00737 541.8 547 0.007383 542.4 548 0.007395 543.1 549 0.007432 543.8 549 0.00742 544.5 549 0.00742 545.1 550 0.00742 545.8 551 0.007457 546.5 552 0.007482 547.1 553 0.007482 547.8 553 0.007482 548.5 554 0.007507 549.2 555 0.007531 549.8 555 0.007531 550.5 556 0.007531 551.2 557 0.007531 551.9 557 0.007544 552.5 557 0.007581 553.2 559 0.007593 553.9 559 0.007581 554.6 560 0.007593 555.2 560 0.007593 555.9 561 0.007593 556.6 562 0.007606 557.3 563 0.007631 557.9 564 0.007631 558.6 564 0.007655 559.3 565 0.007668 560 565 0.007693 560.6 566 0.00768 561.3 567 0.00768 562 567 0.00768 562.6 568 0.007705 563.3 568 0.007717 564 569 0.00773 564.7 571 0.00773 565.3 571 0.007779 566 571 0.007792 566.7 571 0.007779 567.4 573 0.007792 568 573 0.007817 568.7 574 0.007829 569.4 574 0.007841 570.1 575 0.007841 570.7 576 0.007841 571.4 577 0.007841 572.1 578 0.007841 572.8 578 0.007854 573.4 578 0.007891 574.1 579 0.007903 574.8 581 0.007928 575.4 581 0.007916 576.1 582 0.007916 576.8 582 0.007928 577.5 584 0.007953 578.1 584 0.007978 578.8 584 0.007965 579.5 585 0.007965 580.2 586 0.00799 580.8 586 0.008015 581.5 587 0.008027 582.2 588 0.00804 582.9 588 0.008027 583.5 589 0.00804 584.2 590 0.00804 584.9 590 0.01462 585.6 591 0.009391 586.2 592 0.008362 586.9 592 0.008151 587.6 593 0.008114 588.3 593 0.008114 588.9 594 0.008127 589.6 594 0.008139 590.3 596 0.008139 590.9 596 0.008139 591.6 597 0.008151 592.3 597 0.008189 593 598 0.008189 593.6 600 0.008189 594.3 600 0.008189 595 601 0.008201 595.7 601 0.008213 596.3 602 0.008238 597 602 0.008251 597.7 603 0.008288 598.4 604 0.0083 599 604 0.0083 599.7 604 0.0083 600.4 604 0.0083 601.1 606 0.008313 601.7 606 0.0083 602.4 607 0.0083 603.1 608 0.008337 603.8 609 0.008362 604.4 609 0.00835 605.1 610 0.008387 605.8 610 0.008387 606.4 611 0.008399 607.1 611 0.008399 607.8 612 0.008399 608.5 614 0.008437 609.1 615 0.008449 609.8 615 0.008449 610.5 615 0.008486 611.2 616 0.008461 611.8 616 0.008499 612.5 617 0.008499 613.2 617 0.008486 613.9 618 0.008499 614.5 619 0.008548 615.2 620 0.008499 615.9 621 0.008499 616.6 621 0.008573 617.2 621 0.008598 617.9 623 0.008585 618.6 624 0.00856 619.2 624 0.008585 619.9 625 0.00861 620.6 625 0.008647 621.3 626 0.00866 621.9 627 0.00866 622.6 628 0.008684 623.3 629 0.008684 624 629 0.008697 624.6 629 0.008684 625.3 630 0.00866 626 631 0.008697 626.7 631 0.008697 627.3 632 0.008709 628 633 0.008722 628.7 634 0.008759 629.4 635 0.008759 630 635 0.008796 630.7 636 0.008808 631.4 636 0.008808 632.1 637 0.008821 632.7 638 0.008846 633.4 639 0.008858 634.1 639 0.008858 634.7 640 0.008858 635.4 640 0.008858 636.1 642 0.008858 636.8 642 0.00887 637.4 642 0.008895 638.1 643 0.008908 638.8 643 0.008908 639.5 644 0.008932 640.1 645 0.008957 640.8 646 0.008957 641.5 646 0.008957 642.2 647 0.008957 642.8 648 0.008982 643.5 649 0.008957 644.2 649 0.008957 644.9 650 0.00897 645.5 650 0.009007 646.2 651 0.009019 646.9 652 0.009019 647.5 653 0.009019 648.2 653 0.009019 648.9 653 0.009032 649.6 654 0.009056 650.2 655 0.009069 650.9 656 0.009081 651.6 657 0.009106 652.3 657 0.009118 652.9 658 0.009118 653.6 659 0.009118 654.3 659 0.009118 655 660 0.009156 655.6 660 0.009168 656.3 661 0.009168 657 662 0.009168 657.7 663 0.009168 658.3 663 0.00918 659 664 0.009205 659.7 665 0.009218 660.4 665 0.009218 661 666 0.009255 661.7 667 0.009267 662.4 668 0.009267 663 668 0.00928 663.7 668 0.009267 664.4 669 0.009317 665.1 670 0.009317 665.7 671 0.009329 666.4 671 0.009329 667.1 672 0.009317 667.8 673 0.009354 668.4 673 0.009391 669.1 674 0.009329 669.8 675 0.009366 670.5 675 0.009379 671.1 676 0.009416 671.8 677 0.009428 672.5 678 0.009416 673.2 678 0.009416 673.8 679 0.009428 674.5 679 0.009441 675.2 680 0.00949 675.9 681 0.00949 676.5 681 0.009478 677.2 682 0.009478 677.9 682 0.009478 678.5 683 0.00949 679.2 684 0.009527 679.9 685 0.009527 680.6 685 0.009527 681.2 686 0.00954 681.9 687 0.009552 682.6 688 0.009565 683.3 688 0.009577 683.9 689 0.009565 684.6 690 0.009589 685.3 690 0.009614 686 691 0.009627 686.6 692 0.009627 687.3 692 0.009627 688 693 0.009651 688.7 693 0.009676 689.3 694 0.009664 690 695 0.009713 690.7 695 0.009713 691.3 696 0.009701 692 696 0.009689 692.7 697 0.009713 693.4 698 0.009701 694 699 0.009713 694.7 700 0.009713 695.4 700 0.009726 696.1 700 0.009763 696.7 702 0.009775 697.4 702 0.009775 698.1 703 0.009775 698.8 703 0.009813 699.4 704 0.009825 700.1 705 0.009825 700.8 706 0.009862 701.5 707 0.009862 702.1 707 0.009887 702.8 707 0.009875 703.5 709 0.009875 704.2 709 0.009887 704.8 710 0.009875 705.5 711 0.009912 706.2 711 0.009937 706.8 711 0.009924 707.5 712 0.009924 708.2 713 0.009961 708.9 714 0.009961 709.5 714 0.009974 710.2 715 0.009986 710.9 715 0.009986 711.6 717 0.01002 712.2 717 0.01004 712.9 718 0.01001 713.6 718 0.01004 714.3 718 0.01004 714.9 719 0.01005 715.6 721 0.01006 716.3 721 0.01007 717 721 0.01009 717.6 722 0.01011 718.3 723 0.01015 719 724 0.01015 719.6 725 0.01013 720.3 725 0.01015 721 726 0.01015 721.7 727 0.01018 722.3 727 0.01018 723 728 0.01018 723.7 729 0.01018 724.4 729 0.01021 725 730 0.01023 725.7 731 0.01023 726.4 732 0.01025 727.1 732 0.01026 727.7 732 0.01025 728.4 733 0.01028 729.1 734 0.01028 729.8 734 0.01028 730.4 735 0.01028 731.1 736 0.0103 731.8 736 0.01028 732.5 737 0.01032 733.1 737 0.01035 733.8 739 0.01033 734.5 739 0.01035 735.1 740 0.01037 735.8 740 0.01036 736.5 742 0.01041 737.2 742 0.01044 737.8 743 0.01044 738.5 743 0.01044 739.2 743 0.01047 739.9 744 0.01048 740.5 745 0.01049 741.2 746 0.01048 741.9 746 0.01049 742.6 747 0.01051 743.2 748 0.01053 743.9 749 0.01054 744.6 749 0.01054 745.3 749 0.01054 745.9 750 0.01058 746.6 750 0.01059 747.3 751 0.01059 748 751 0.01059 748.6 753 0.01059 749.3 753 0.01059 750 753 0.01061 750.6 753 0.01064 751.3 755 0.01069 752 756 0.01067 752.7 757 0.01066 753.3 757 0.01069 754 758 0.01069 754.7 759 0.01072 755.4 759 0.01073 756 761 0.01075 756.7 761 0.01078 757.4 762 0.01079 758.1 762 0.01079 758.7 763 0.01078 759.4 764 0.01079 760.1 764 0.01079 760.8 765 0.01078 761.4 765 0.0108 762.1 767 0.0108 762.8 768 0.01079 763.4 768 0.01078 764.1 768 0.01078 764.8 769 0.0108 765.5 770 0.01078 766.1 771 0.01075 766.8 771 0.01079 767.5 772 0.01078 768.2 773 0.01075 768.8 774 0.01074 769.5 775 0.01074 770.2 775 0.01073 770.9 775 0.01071 771.5 776 0.01068 772.2 777 0.01069 772.9 778 0.01066 773.6 778 0.01061 774.2 779 0.01061 774.9 779 0.01061 775.6 781 0.01057 776.3 781 0.01054 776.9 782 0.01054 777.6 782 0.01051 778.3 782 0.01047 778.9 784 0.01046 779.6 784 0.01042 780.3 785 0.0104 781 786 0.01038 781.6 786 0.01033 782.3 787 0.01028 783 788 0.01023 783.7 788 0.0102 784.3 789 0.01015 785 789 0.01011 785.7 791 0.01006 786.4 792 0.01002 787 792 0.009999 787.7 793 0.009949 788.4 793 0.009899 789.1 793 0.00985 789.7 794 0.009813 790.4 795 0.009738 791.1 796 0.009701 791.7 796 0.009639 792.4 796 0.009577 793.1 798 0.00954 793.8 799 0.009515 794.4 800 0.009453 795.1 800 0.009416 795.8 801 0.009342 796.5 801 0.009292 797.1 801 0.009242 797.8 801 0.009218 798.5 801 0.009193 799.2 801 0.009143 799.8 801 0.009056 800.5 801 0.009032 801.2 803 0.008982 801.9 803 0.008957 802.5 803 0.008945 803.2 804 0.008883 803.9 804 0.008821 804.6 805 0.008821 805.2 806 0.008808 805.9 807 0.008759 806.6 807 0.008746 807.2 808 0.008722 807.9 809 0.008672 808.6 809 0.00866 809.3 810 0.00866 809.9 811 0.009788 810.6 811 0.008808 811.3 812 0.00861 812 813 0.008573 812.6 814 0.00856 813.3 814 0.008523 814 814 0.008511 814.7 815 0.008511 815.3 816 0.008511 816 817 0.008474 816.7 818 0.008474 817.4 818 0.008461 818 818 0.008461 818.7 819 0.008499 819.4 819 0.008474 820 821 0.008461 820.7 821 0.008461 821.4 821 0.008461 822.1 822 0.008499 822.7 823 0.008499 823.4 824 0.008511 824.1 825 0.008499 824.8 825 0.008499 825.4 826 0.008499 826.1 827 0.008548 826.8 828 0.008548 827.5 828 0.008548 828.1 829 0.008523 828.8 829 0.008511 829.5 830 0.008511 830.2 831 0.008511 830.8 832 0.008536 831.5 832 0.008585 832.2 832 0.008635 832.9 834 0.00866 833.5 834 0.00866 834.2 835 0.00866 834.9 836 0.008697 835.5 836 0.008722 836.2 837 0.008746 836.9 838 0.008722 837.6 839 0.008746 838.2 839 0.008796 838.9 839 0.008808 839.6 840 0.008821 840.3 841 0.008846 840.9 842 0.008858 841.6 843 0.008846 842.3 843 0.008858 843 843 0.008895 843.6 844 0.008895 844.3 845 0.00892 845 846 0.00892 845.7 847 0.008957 846.3 847 0.008957 847 848 0.008982 847.7 848 0.009007 848.4 849 0.009019 849 850 0.009056 849.7 850 0.009081 850.4 851 0.009094 851 852 0.009106 851.7 853 0.009118 852.4 853 0.009118 853.1 854 0.009168 853.7 854 0.009193 854.4 855 0.009205 855.1 856 0.009218 855.8 856 0.00923 856.4 857 0.009242 857.1 857 0.009267 857.8 858 0.00928 858.5 859 0.009304 859.1 860 0.009317 859.8 861 0.009329 860.5 861 0.009342 861.2 862 0.009342 861.8 862 0.009379 862.5 863 0.009404 863.2 864 0.009416 863.8 864 0.009428 864.5 865 0.009441 865.2 866 0.009428 865.9 867 0.009453 866.5 868 0.009478 867.2 868 0.00949 867.9 868 0.009503 868.6 869 0.009527 869.2 869 0.009527 869.9 871 0.00954 870.6 872 0.009565 871.3 872 0.009589 871.9 872 0.009602 872.6 873 0.009627 873.3 874 0.009627 874 875 0.009651 874.6 876 0.009676 875.3 876 0.009676 876 876 0.009689 876.7 878 0.009713 877.3 878 0.009713 878 879 0.009701 878.7 879 0.009689 879.3 880 0.009726 880 881 0.009738 880.7 881 0.009763 881.4 882 0.0098 882 883 0.009825 882.7 883 0.009825 883.4 884 0.00985 884.1 885 0.00985 884.7 885 0.009899 885.4 886 0.009912 886.1 887 0.009924 886.8 887 0.009937 887.4 888 0.009974 888.1 889 0.009986 888.8 889 0.009986 889.5 890 0.009999 890.1 890 0.01001 890.8 892 0.01004 891.5 893 0.01004 892.1 893 0.01009 892.8 893 0.01011 893.5 894 0.01013 894.2 894 0.01017 894.8 896 0.01018 895.5 897 0.0102 896.2 897 0.01018 896.9 897 0.01017 897.5 898 0.0102 898.2 899 0.01023 898.9 900 0.01025 899.6 900 0.01025 900.2 901 0.01027 900.9 901 0.01028 901.6 903 0.0103 902.3 903 0.01028 902.9 903 0.01032 903.6 904 0.01033 904.3 904 0.01037 905 905 0.01036 905.6 906 0.0104 906.3 906 0.01042 907 907 0.01042 907.6 908 0.01044 908.3 909 0.01044 909 909 0.01047 909.7 910 0.01051 910.3 911 0.01052 911 911 0.01048 911.7 912 0.01051 912.4 912 0.01058 913 914 0.01057 913.7 914 0.01058 914.4 915 0.01059 915.1 915 0.01059 915.7 917 0.01063 916.4 917 0.01064 917.1 918 0.01066 917.8 918 0.01066 918.4 918 0.01069 919.1 919 0.01073 919.8 920 0.01075 920.5 921 0.01078 921.1 922 0.01078 921.8 922 0.0108 922.5 923 0.01079 923.1 924 0.0108 923.8 925 0.0108 924.5 925 0.01083 925.2 925 0.01085 925.8 926 0.01085 926.5 927 0.01085 927.2 928 0.0109 927.9 929 0.01097 928.5 929 0.01094 929.2 929 0.01094 929.9 930 0.01098 930.6 931 0.01098 931.2 932 0.01099 931.9 932 0.011 932.6 932 0.01103 933.3 934 0.01105 933.9 934 0.01106 934.6 935 0.01108 935.3 936 0.01108 935.9 936 0.01106 936.6 937 0.0111 937.3 937 0.01113 938 939 0.01116 938.6 939 0.01116 939.3 940 0.01119 940 940 0.01121 940.7 941 0.01124 941.3 942 0.01125 942 943 0.01124 942.7 943 0.01126 943.4 944 0.01126 944 944 0.01128 944.7 945 0.0113 945.4 946 0.01133 946.1 947 0.01135 946.7 947 0.01137 947.4 948 0.01139 948.1 949 0.01141 948.8 950 0.01144 949.4 950 0.01146 950.1 950 0.01146 950.8 950 0.01144 951.4 952 0.01146 952.1 953 0.01147 952.8 953 0.01151 953.5 954 0.01152 954.1 954 0.01151 954.8 955 0.01156 955.5 956 0.01157 956.2 957 0.01157 956.8 957 0.01162 957.5 958 0.01161 958.2 959 0.01162 958.9 959 0.01165 959.5 960 0.01167 960.2 961 0.01168 960.9 961 0.01168 961.6 962 0.01167 962.2 962 0.01168 962.9 964 0.01173 963.6 964 0.01176 964.2 965 0.01176 964.9 965 0.01177 965.6 967 0.01177 966.3 967 0.01182 966.9 968 0.01182 967.6 968 0.01183 968.3 968 0.01187 969 969 0.01185 969.6 969 0.01191 970.3 971 0.01192 971 972 0.01193 971.7 972 0.01195 972.3 973 0.01196 973 974 0.01199 973.7 974 0.01198 974.4 975 0.01203 975 975 0.01203 975.7 976 0.01199 976.4 977 0.01203 977.1 978 0.01211 977.7 978 0.01214 978.4 979 0.01213 979.1 979 0.01209 979.7 980 0.01212 980.4 981 0.01214 981.1 982 0.01216 981.8 982 0.01217 982.4 983 0.01222 983.1 984 0.01221 983.8 984 0.01222 984.5 985 0.01222 985.1 986 0.01223 985.8 986 0.0123 986.5 987 0.01229 987.2 987 0.01228 987.8 989 0.01234 988.5 990 0.01232 989.2 990 0.01237 989.9 990 0.01237 990.5 991 0.0124 991.2 992 0.01242 991.9 992 0.01245 992.6 993 0.01245 993.2 993 0.01243 993.9 994 0.01243 994.6 994 0.01244 995.2 996 0.01239 995.9 997 0.01243 996.6 997 0.01252 997.3 998 0.01253 997.9 998 0.01265 998.6 999 0.01261 999.3 1000 0.01261 1000 1000 0.01255 1001 1001 0.01261 1001 1001 0.01263 1002 1002 0.01266 1003 1002 0.01268 1003 1003 0.0127 1004 1004 0.0127 1005 1004 0.0127 1005 1005 0.0127 1006 1006 0.0127 1007 1006 0.0127 1007 1007 0.01273 1008 1008 0.01271 1009 1008 0.01273 1009 1009 0.01275 1010 1010 0.01276 1011 1011 0.01279 1011 1011 0.01278 1012 1011 0.01283 1013 1012 0.01286 1013 1013 0.01284 1014 1014 0.01284 1015 1015 0.01287 1015 1015 0.01287 1016 1015 0.0129 1017 1017 0.0129 1017 1017 0.01294 1018 1018 0.01296 1019 1018 0.01296 1020 1019 0.01299 1020 1019 0.01302 1021 1020 0.01301 1022 1021 0.01305 1022 1021 0.01305 1023 1022 0.01305 1024 1022 0.01307 1024 1022 0.0131 1025 1022 0.0131 1026 1021 0.0131 1026 1022 0.01306 1027 1023 0.01309 1028 1025 0.01315 1028 1026 0.01317 1029 1028 0.01321 1030 1029 0.0132 1030 1030 0.01322 1031 1031 0.01325 1032 1032 0.01327 1032 1033 0.01328 1033 1033 0.01332 1034 1033 0.01332 1034 1034 0.01335 1035 1035 0.01336 1036 1036 0.0134 1036 1036 0.01338 1037 1036 0.01341 1038 1037 0.01342 1038 1038 0.01343 1039 1039 0.01346 1040 1040 0.01348 1040 1040 0.01351 1041 1040 0.01351 1042 1042 0.01351 1042 1043 0.01351 1043 1043 0.01356 1044 1043 0.01354 1044 1044 0.01358 1045 1044 0.01362 1046 1046 0.01362 1046 1046 0.01366 1047 1047 0.01366 1048 1048 0.01367 1048 1048 0.01369 1049 1049 0.01371 1050 1050 0.01372 1050 1050 0.01371 1051 1051 0.01376 1052 1052 0.01376 1053 1053 0.01377 1053 1053 0.01377 1054 1054 0.01377 1055 1054 0.01378 1055 1055 0.01384 1056 1056 0.01387 1057 1056 0.0139 1057 1057 0.01392 1058 1058 0.01392 1059 1059 0.01392 1059 1059 0.01389 1060 1059 0.01394 1061 1061 0.01397 1061 1061 0.01397 1062 1062 0.01397 1063 1063 0.01399 1063 1064 0.01402 1064 1064 0.01403 1065 1065 0.01402 1065 1065 0.01405 1066 1066 0.01409 1067 1067 0.01411 1067 1068 0.01413 1068 1068 0.01413 1069 1068 0.01409 1069 1069 0.01415 1070 1069 0.01416 1071 1071 0.01416 1071 1072 0.01418 1072 1072 0.01421 1073 1072 0.01421 1073 1074 0.01423 1074 1074 0.01423 1075 1075 0.01425 1075 1075 0.01425 1076 1076 0.01428 1077 1077 0.01431 1077 1078 0.01431 1078 1078 0.01433 1079 1079 0.01433 1079 1079 0.01434 1080 1080 0.01433 1081 1081 0.01434 1081 1082 0.01435 1082 1082 0.01434 1083 1083 0.01433 1084 1083 0.01434 1084 1084 0.01437 1085 1084 0.01431 1086 1086 0.01436 1086 1086 0.01439 1087 1086 0.01433 1088 1087 0.01435 1088 1088 0.01437 1089 1089 0.01436 1090 1090 0.01437 1090 1090 0.01439 1091 1090 0.01441 1092 1092 0.01441 1092 1093 0.01441 1093 1093 0.01441 1094 1094 0.01445 1094 1094 0.01446 1095 1095 0.01441 1096 1096 0.01446 1096 1097 0.01455 1097 1097 0.01454 1098 1097 0.01451 1098 1098 0.01452 1099 1099 0.01454 1100 1100 0.01456 1100 1100 0.01457 1101 1101 0.01457 1102 1101 0.01459 1102 1103 0.01462 1103 1103 0.01462 1104 1104 0.01462 1104 1104 0.01464 1105 1104 0.01467 1106 1106 0.01467 1106 1106 0.01468 1107 1107 0.01471 1108 1108 0.01473 1108 1109 0.01473 1109 1109 0.01477 1110 1109 0.01476 1110 1111 0.01475 1111 1111 0.0148 1112 1111 0.01482 1112 1112 0.01481 1113 1112 0.01483 1114 1114 0.01483 1115 1115 0.01485 1115 1115 0.01485 1116 1115 0.01486 1117 1117 0.0149 1117 1117 0.01493 1118 1118 0.01493 1119 1118 0.01496 1119 1119 0.01497 1120 1119 0.01496 1121 1120 0.01497 1121 1121 0.01497 1122 1122 0.01501 1123 1122 0.01504 1123 1123 0.01504 1124 1124 0.01503 1125 1125 0.01504 1125 1125 0.01507 1126 1126 0.01508 1127 1127 0.01509 1127 1127 0.01513 1128 1128 0.01516 1129 1129 0.01518 1129 1129 0.01517 1130 1130 0.01512 1131 1130 0.01518 1131 1131 0.01518 1132 1132 0.01519 1133 1133 0.01519 1133 1133 0.01522 1134 1134 0.01524 1135 1134 0.01524 1135 1135 0.01526 1136 1136 0.01527 1137 1136 0.01529 1137 1137 0.0153 1138 1138 0.01533 1139 1139 0.01534 1139 1140 0.01535 1140 1140 0.01539 1141 1140 0.01537 1141 1142 0.01539 1142 1142 0.0154 1143 1143 0.0154 1143 1144 0.01543 1144 1144 0.01544 1145 1144 0.01545 1146 1145 0.01549 1146 1147 0.01549 1147 1147 0.0155 1148 1147 0.0155 1148 1148 0.01554 1149 1149 0.01555 1150 1149 0.01557 1150 1150 0.01554 1151 1151 0.01554 1152 1151 0.01564 1152 1153 0.01568 1153 1153 0.0157 1154 1154 0.01569 1154 1154 0.01568 1155 1155 0.01573 1156 1156 0.01571 1156 1156 0.01573 1157 1157 0.0157 1158 1158 0.01575 1158 1158 0.01579 1159 1159 0.0158 1160 1159 0.01581 1160 1160 0.01584 1161 1161 0.01585 1162 1162 0.01586 1162 1162 0.01588 1163 1162 0.01588 1164 1163 0.01589 1164 1164 0.0159 1165 1165 0.01592 1166 1165 0.01595 1166 1165 0.01595 1167 1168 0.01597 1168 1168 0.016 1168 1169 0.016 1169 1169 0.01604 1170 1169 0.01605 1170 1169 0.01606 1171 1171 0.01606 1172 1172 0.01605 1172 1172 0.01604 1173 1173 0.0161 1174 1173 0.01614 1174 1174 0.01615 1175 1175 0.01616 1176 1176 0.01618 1177 1176 0.01618 1177 1177 0.01616 1178 1178 0.01615 1179 1178 0.0162 1179 1179 0.01625 1180 1179 0.01625 1181 1180 0.01627 1181 1181 0.01626 1182 1182 0.0163 1183 1182 0.01631 1183 1183 0.01635 1184 1184 0.01637 1185 1184 0.0164 1185 1185 0.0164 1186 1186 0.01638 1187 1187 0.01637 1187 1187 0.01637 1188 1187 0.0164 1189 1188 0.01643 1189 1189 0.01647 1190 1190 0.01651 1191 1190 0.01649 1191 1192 0.01647 1192 1192 0.01649 1193 1193 0.01652 1193 1193 0.01653 1194 1194 0.01656 1195 1194 0.01661 1195 1195 0.01662 1196 1194 0.01664 1197 1197 0.01667 1197 1197 0.01667 1198 1198 0.01672 1199 1199 0.01672 1199 1199 0.01668 1200 1199 0.01669 1201 1200 0.01672 1201 1199 0.01671 1202 1199 0.01673 1203 1199 0.01676 1203 1199 0.01673 1204 1199 0.01673 1205 1199 0.01672 1205 1199 0.01668 1206 1199 0.01672 1207 1199 0.01672 1208 1199 0.01671 1208 1199 0.01673 1209 1199 0.01674 1210 1199 0.01673 1210 1199 0.01673 1211 1199 0.01672 1212 1199 0.01676 1212 1199 0.01672 1213 1199 0.01668 1214 1199 0.01667 1214 1199 0.01663 1215 1199 0.01662 1216 1199 0.01662 1216 1199 0.01667 1217 1199 0.01669 1218 1198 0.01669 1218 1199 0.01669 1219 1199 0.01672 1220 1199 0.01669 1220 1199 0.01671 1221 1199 0.01672 1222 1199 0.01666 1222 1199 0.01666 1223 1199 0.01667 1224 1199 0.01669 1224 1199 0.01672 1225 1199 0.01669 1226 1199 0.01672 1226 1199 0.01669 1227 1199 0.01663 1228 1199 0.01663 1228 1199 0.01668 1229 1199 0.01674 1230 1199 0.01673 1230 1199 0.01677 1231 1199 0.0168 1232 1199 0.01679 1232 1199 0.01676 1233 1199 0.01672 1234 1199 0.01673 1234 1199 0.01676 1235 1199 0.01673 1236 1199 0.01673 1236 1199 0.01669 1237 1199 0.01667 1238 1199 0.01668 1238 1199 0.01669 1239 1199 0.01672 1240 1199 0.01676 1241 1199 0.01673 1241 1199 0.01668 1242 1199 0.01666 1243 1199 0.01673 1243 1199 0.01673 1244 1199 0.01676 1245 1199 0.01676 1245 1198 0.01673 1246 1199 0.01677 1247 1199 0.01678 1247 1199 0.01677 1248 1200 0.01677 1249 1199 0.01677 1249 1199 0.01677 1250 1199 0.01673 1251 1199 0.01669 1251 1199 0.01668 1252 1198 0.01671 1253 1199 0.01672 1253 1199 0.01672 1254 1199 0.01668 1255 1199 0.01677 1255 1199 0.01678 1256 1199 0.01674 1257 1198 0.01673 1257 1199 0.01673 1258 1199 0.01672 1259 1199 0.01673 1259 1199 0.01677 1260 1200 0.01677 1261 1199 0.01679 1261 1199 0.01679 1262 1199 0.01682 1263 1199 0.01682 1263 1199 0.01673 1264 1199 0.01678 1265 1199 0.01678 1265 1200 0.01676 1266 1199 0.01674 1267 1199 0.01676 1267 1198 0.01673 1268 1199 0.01679 1269 1199 0.01673 1269 1199 0.01671 1270 1199 0.01668 1271 1199 0.01672 1272 1199 0.01674 1272 1199 0.01673 1273 1199 0.01674 1274 1200 0.01673 1274 1199 0.01673 1275 1199 0.01678 1276 1199 0.01678 1276 1199 0.01678 1277 1199 0.01677 1278 1199 0.01676 1278 1199 0.01676 1279 1199 0.01677 1280 1199 0.01677 1280 1199 0.01676 1281 1199 0.01674 1282 1199 0.01676 1282 1199 0.01677 1283 1199 0.01678 1284 1199 0.01678 1284 1199 0.01678 1285 1199 0.01677 1286 1199 0.01674 1286 1199 0.01673 1287 1199 0.01676 1288 1199 0.01677 1288 1199 0.01677 1289 1199 0.01676 1290 1199 0.01677 1290 1199 0.01678 1291 1199 0.01674 1292 1199 0.01676 1292 1199 0.01678 1293 1199 0.01678 1294 1199 0.01677 1294 1199 0.01676 1295 1199 0.01676 1296 1199 0.01676 1296 1199 0.01678 1297 1199 0.01679 1298 1199 0.01679 1298 1199 0.01678 1299 1199 0.01677 1300 1199 0.01677 1300 1199 0.01678 1301 1199 0.01678 1302 1199 0.01676 1303 1199 0.01676 1303 1199 0.01674 1304 1199 0.01674 1305 1199 0.01676 1305 1199 0.01676 1306 1199 0.01678 1307 1199 0.01677 1307 1199 0.01676 1308 1199 0.01676 1309 1199 0.01677 1309 1199 0.01678 1310 1199 0.01679 1311 1199 0.01678 1311 1199 0.01679 1312 1199 0.01678 1313 1199 0.01677 1313 1199 0.01679 1314 1199 0.01682 1315 1199 0.01679 1315 1200 0.01676 1316 1199 0.01679 1317 1199 0.01682 1317 1199 0.01679 1318 1199 0.01678 1319 1199 0.0168 1319 1199 0.01678 1320 1199 0.01679 1321 1199 0.01679 1321 1199 0.01676 1322 1199 0.01682 1323 1199 0.01682 1323 1199 0.01674 1324 1199 0.01672 1325 1199 0.01677 1325 1199 0.01683 1326 1199 0.01685 1327 1199 0.01683 1327 1199 0.01685 1328 1199 0.01682 1329 1199 0.01685 1329 1199 0.01684 1330 1199 0.01683 1331 1199 0.01685 1331 1199 0.01679 1332 1199 0.01676 1333 1199 0.0168 1334 1199 0.01678 1334 1199 0.01677 1335 1199 0.01689 1336 1199 0.01677 1336 1199 0.0168 1337 1199 0.01679 1338 1199 0.0168 1338 1199 0.01678 1339 1199 0.01679 1340 1199 0.0168 1340 1199 0.01679 1341 1199 0.01678 1342 1199 0.01679 1342 1199 0.01679 1343 1199 0.01683 1344 1199 0.01683 1344 1199 0.01682 1345 1199 0.01674 1346 1199 0.01679 1346 1199 0.01683 1347 1199 0.01684 1348 1199 0.0168 1348 1199 0.01678 1349 1199 0.01677 1350 1199 0.01679 1350 1199 0.01679 1351 1199 0.01679 1352 1199 0.0168 1352 1199 0.0168 1353 1199 0.0168 1354 1199 0.01679 1354 1199 0.01679 1355 1199 0.01684 1356 1199 0.01676 1356 1199 0.01679 1357 1199 0.01684 1358 1199 0.01684 1358 1199 0.01684 1359 1199 0.0168 1360 1199 0.01682 1360 1199 0.01682 1361 1199 0.01678 1362 1199 0.01677 1362 1199 0.01679 1363 1199 0.01683 1364 1199 0.01685 1365 1199 0.01676 1365 1199 0.01676 1366 1199 0.01676 1367 1199 0.01684 1367 1199 0.01685 1368 1199 0.01677 1369 1199 0.01673 1369 1199 0.01672 1370 1199 0.0168 1371 1199 0.01687 1371 1199 0.01687 1372 1199 0.01683 1373 1199 0.01684 1373 1199 0.01679 1374 1199 0.0168 1375 1199 0.01683 1375 1199 0.01684 1376 1199 0.01682 1377 1199 0.01671 1377 1199 0.01672 1378 1199 0.01678 1379 1199 0.01679 1379 1199 0.01682 1380 1199 0.01682 1381 1199 0.0168 1381 1199 0.01678 1382 1199 0.01682 1383 1199 0.01678 1383 1199 0.01679 1384 1199 0.01682 1385 1199 0.01683 1385 1199 0.01683 1386 1199 0.01683 1387 1199 0.0168 1387 1199 0.0168 1388 1199 0.01684 1389 1199 0.01685 1389 1199 0.01678 1390 1199 0.01684 1391 1199 0.01687 1391 1198 0.01688 1392 1199 0.01689 1393 1199 0.01687 1393 1199 0.01683 1394 1199 0.01676 1395 1199 0.01674 1395 1199 0.0168 1396 1199 0.0168 1397 1199 0.0168 1398 1199 0.0168 1398 1199 0.01684 1399 1199 0.01689 1400 1199 0.0169 1400 1199 0.01682 1401 1199 0.01683 1402 1199 0.01683 1402 1199 0.01683 1403 1199 0.01684 1404 1199 0.0168 1404 1199 0.0168 1405 1199 0.01683 1406 1199 0.01683 1406 1199 0.01669 1407 1199 0.01679 1408 1199 0.01685 1408 1199 0.01684 1409 1199 0.0168 1410 1199 0.01678 1410 1199 0.01684 1411 1199 0.01678 1412 1199 0.01674 1412 1199 0.01678 1413 1199 0.01682 1414 1199 0.01682 1414 1199 0.01683 1415 1199 0.01683 1416 1199 0.01682 1416 1199 0.01684 1417 1199 0.01683 1418 1199 0.01679 1418 1199 0.01685 1419 1199 0.01679 1420 1199 0.01682 1420 1199 0.01683 1421 1199 0.0168 1422 1199 0.01679 1422 1199 0.01678 1423 1199 0.01677 1424 1199 0.01677 1424 1199 0.0168 1425 1199 0.01682 1426 1199 0.01683 1426 1199 0.0168 1427 1199 0.01683 1428 1199 0.0168 1429 1199 0.01679 1429 1199 0.01683 1430 1199 0.01683 1431 1199 0.01682 1431 1199 0.01682 1432 1199 0.01683 1433 1199 0.01677 1433 1199 0.01679 1434 1199 0.01678 1435 1199 0.01679 1435 1199 0.01679 1436 1199 0.0168 1437 1199 0.01679 1437 1199 0.01679 1438 1199 0.01678 1439 1199 0.01673 1439 1199 0.01683 1440 1199 0.0168 1441 1199 0.01679 1441 1199 0.0168 1442 1199 0.01679 1443 1199 0.01677 1443 1199 0.01678 1444 1199 0.01678 1445 1199 0.01679 1445 1199 0.0168 1446 1199 0.01679 1447 1199 0.01678 1447 1199 0.01678 1448 1199 0.01678 1449 1199 0.01679 1449 1199 0.01678 1450 1199 0.01679 1451 1199 0.01678 1451 1199 0.01678 1452 1199 0.01676 1453 1199 0.01682 1453 1199 0.01678 1454 1199 0.01679 1455 1199 0.01677 1455 1199 0.01679 1456 1199 0.01679 1457 1199 0.01677 1457 1199 0.0168 1458 1199 0.01683 1459 1199 0.01679 1460 1199 0.01678 1460 1199 0.01677 1461 1199 0.01677 1462 1199 0.01677 1462 1199 0.01678 1463 1199 0.01677 1464 1199 0.01677 1464 1199 0.0168 1465 1199 0.0168 1466 1199 0.01679 1466 1199 0.01678 1467 1199 0.01676 1468 1199 0.01676 1468 1199 0.01678 1469 1199 0.0168 1470 1199 0.01678 1470 1199 0.01678 1471 1199 0.01677 1472 1199 0.01679 1472 1199 0.0168 1473 1199 0.01682 1474 1199 0.01682 1474 1199 0.01676 1475 1199 0.01673 1476 1199 0.01676 1476 1199 0.01678 1477 1199 0.01678 1478 1199 0.01677 1478 1199 0.01678 1479 1199 0.01678 1480 1199 0.01677 1480 1199 0.01677 1481 1199 0.01678 1482 1199 0.01677 1482 1199 0.01677 1483 1199 0.01678 1484 1199 0.01674 1484 1199 0.01673 1485 1199 0.01672 1486 1199 0.01673 1486 1199 0.01678 1487 1199 0.01679 1488 1199 0.01673 1488 1199 0.01676 1489 1199 0.01673 1490 1199 0.01674 1491 1199 0.01676 1491 1198 0.01678 1492 1199 0.01679 1493 1199 0.01677 1493 1199 0.01677 1494 1199 0.01678 1495 1199 0.01678 1495 1199 0.01678 1496 1199 0.01677 1497 1199 0.01679 1497 1199 0.01678 1498 1199 0.01677 1499 1199 0.01674 1499 1199 0.01678 1500 1194 0.01752 1501 1194 0.01718 1501 1194 0.01685 1502 1194 0.01679 1503 1194 0.01672 1503 1194 0.01676 1504 1194 0.01679 1505 1194 0.01678 1505 1193 0.01677 1506 1192 0.01676 1507 1191 0.01673 1507 1190 0.01672 1508 1190 0.01672 1509 1189 0.01672 1509 1188 0.01669 1510 1187 0.01669 1511 1187 0.01667 1511 1187 0.01659 1512 1186 0.01664 1513 1185 0.01662 1513 1184 0.01656 1514 1183 0.01656 1515 1183 0.01657 1515 1182 0.01659 1516 1181 0.01663 1517 1181 0.01658 1517 1180 0.01657 1518 1179 0.01657 1519 1179 0.01653 1519 1178 0.01652 1520 1178 0.01648 1521 1177 0.01648 1522 1176 0.01646 1522 1176 0.01642 1523 1175 0.01641 1524 1174 0.01638 1524 1173 0.01635 1525 1173 0.01643 1526 1172 0.01638 1526 1172 0.01633 1527 1171 0.01632 1528 1169 0.01632 1528 1169 0.01631 1529 1169 0.0163 1530 1169 0.01628 1530 1168 0.01626 1531 1167 0.01626 1532 1166 0.01623 1532 1165 0.01623 1533 1165 0.01622 1534 1164 0.01621 1534 1164 0.01617 1535 1163 0.01616 1536 1162 0.01615 1536 1162 0.01615 1537 1161 0.01614 1538 1160 0.01612 1538 1159 0.01612 1539 1159 0.0161 1540 1158 0.01609 1540 1157 0.01607 1541 1157 0.01607 1542 1156 0.01604 1542 1155 0.016 1543 1154 0.01599 1544 1154 0.016 1544 1153 0.016 1545 1153 0.01596 1546 1152 0.01596 1546 1151 0.01589 1547 1150 0.01592 1548 1150 0.0159 1548 1149 0.0159 1549 1149 0.01588 1550 1148 0.01584 1550 1147 0.01584 1551 1147 0.01581 1552 1146 0.01581 1553 1145 0.01581 1553 1144 0.01585 1554 1144 0.01581 1555 1143 0.01573 1555 1143 0.0157 1556 1142 0.01571 1557 1141 0.01565 1557 1140 0.01565 1558 1140 0.01566 1559 1139 0.01564 1559 1138 0.01563 1560 1138 0.01561 1561 1136 0.0156 1561 1136 0.01564 1562 1136 0.0156 1563 1135 0.01557 1563 1134 0.01554 1564 1133 0.01552 1565 1133 0.01548 1565 1133 0.01539 1566 1132 0.01539 1567 1131 0.01533 1567 1130 0.01535 1568 1129 0.01543 1569 1129 0.01548 1569 1128 0.01544 1570 1128 0.01542 1571 1127 0.01537 1571 1126 0.01537 1572 1126 0.01542 1573 1125 0.01533 1573 1125 0.01533 1574 1124 0.0153 1575 1123 0.01527 1575 1122 0.01528 1576 1122 0.01526 1577 1121 0.01524 1577 1120 0.01523 1578 1119 0.01522 1579 1119 0.01518 1579 1119 0.01516 1580 1118 0.01514 1581 1117 0.01516 1581 1116 0.01513 1582 1115 0.01513 1583 1115 0.01513 1583 1114 0.01511 1584 1114 0.01501 1585 1113 0.01507 1586 1112 0.01508 1586 1111 0.01504 1587 1111 0.01502 1588 1110 0.01499 1588 1109 0.01499 1589 1109 0.01499 1590 1108 0.01485 1590 1107 0.01488 1591 1107 0.01495 1592 1106 0.01492 1592 1105 0.01487 1593 1104 0.01485 1594 1104 0.01482 1594 1104 0.01488 1595 1103 0.01482 1596 1102 0.0148 1596 1101 0.0148 1597 1101 0.0148 1598 1101 0.01477 1598 1099 0.01475 1599 1099 0.01473 1600 1098 0.01471 1600 1097 0.01466 1601 1097 0.01464 1602 1096 0.01465 1602 1096 0.01461 1603 1094 0.01466 1604 1094 0.01464 1604 1093 0.01459 1605 1093 0.01457 1606 1092 0.01457 1606 1092 0.01457 1607 1091 0.0146 1608 1090 0.01457 1608 1090 0.01456 1609 1089 0.0145 1610 1088 0.01446 1610 1087 0.01444 1611 1086 0.01444 1612 1086 0.01442 1612 1085 0.01436 1613 1085 0.01437 1614 1084 0.01445 1614 1083 0.01435 1615 1083 0.01442 1616 1082 0.01437 1617 1080 0.01431 1617 1080 0.0143 1618 1079 0.01434 1619 1079 0.01428 1619 1079 0.01429 1620 1078 0.01426 1621 1077 0.01425 1621 1077 0.01421 1622 1076 0.0142 1623 1076 0.01419 1623 1075 0.01421 1624 1074 0.01416 1625 1073 0.01415 1625 1072 0.01413 1626 1072 0.01411 1627 1072 0.01408 1627 1071 0.01408 1628 1069 0.01406 1629 1069 0.01406 1629 1068 0.01404 1630 1068 0.01399 1631 1068 0.01402 1631 1067 0.01403 1632 1065 0.01392 1633 1065 0.01395 1633 1064 0.01397 1634 1064 0.01393 1635 1063 0.0139 1635 1062 0.01395 1636 1061 0.01389 1637 1061 0.01385 1637 1060 0.01382 1638 1060 0.01384 1639 1059 0.01384 1639 1058 0.0138 1640 1058 0.01378 1641 1057 0.01377 1641 1056 0.01377 1642 1055 0.01376 1643 1055 0.01377 1643 1054 0.01376 1644 1054 0.01374 1645 1053 0.01372 1645 1052 0.01368 1646 1052 0.01354 1647 1051 0.01366 1648 1050 0.01366 1648 1049 0.01362 1649 1049 0.01362 1650 1049 0.01362 1650 1047 0.01364 1651 1047 0.01361 1652 1046 0.01354 1652 1046 0.01346 1653 1044 0.01347 1654 1044 0.01347 1654 1043 0.01347 1655 1043 0.01347 1656 1042 0.01346 1656 1041 0.01336 1657 1040 0.01327 1658 1040 0.01322 1658 1039 0.01325 1659 1038 0.01333 1660 1038 0.0134 1660 1037 0.01337 1661 1037 0.01336 1662 1036 0.01336 1662 1036 0.01328 1663 1035 0.01328 1664 1034 0.01331 1664 1033 0.0133 1665 1033 0.01326 1666 1032 0.01326 1666 1030 0.01326 1667 1031 0.01325 1668 1029 0.01322 1668 1029 0.01317 1669 1029 0.01316 1670 1028 0.01312 1670 1028 0.01312 1671 1027 0.01311 1672 1026 0.01316 1672 1026 0.0131 1673 1025 0.01307 1674 1024 0.01306 1674 1023 0.01306 1675 1022 0.01306 1676 1022 0.01306 1676 1022 0.01302 1677 1021 0.01301 1678 1019 0.013 1679 1019 0.01304 1679 1018 0.013 1680 1018 0.01285 1681 1017 0.01299 1681 1017 0.01291 1682 1016 0.01292 1683 1015 0.01292 1683 1015 0.01291 1684 1014 0.01289 1685 1014 0.01287 1685 1012 0.01286 1686 1012 0.01285 1687 1011 0.01284 1687 1011 0.0128 1688 1010 0.01281 1689 1009 0.01279 1689 1009 0.01276 1690 1008 0.01276 1691 1007 0.01274 1691 1006 0.01271 1692 1005 0.01273 1693 1005 0.01275 1693 1004 0.0127 1694 1004 0.0127 1695 1003 0.01271 1695 1003 0.0127 1696 1002 0.0127 1697 1001 0.01269 1697 1001 0.0127 1698 1000 0.01266 1699 1000 0.01264 1699 999 0.0126 1700 999 0.0125 1701 997 0.01255 1701 997 0.01256 1702 997 0.01263 1703 996 0.01259 1703 994 0.0125 1704 994 0.01255 1705 993 0.01258 1705 993 0.01253 1706 993 0.01247 1707 992 0.01247 1707 991 0.01244 1708 990 0.01243 1709 990 0.01244 1710 990 0.01242 1710 988 0.01242 1711 988 0.01239 1712 987 0.01237 1712 986 0.01235 1713 986 0.01225 1714 985 0.0123 1714 984 0.01232 1715 984 0.01228 1716 983 0.01225 1716 983 0.01227 1717 982 0.01229 1718 981 0.01227 1718 980 0.01224 1719 979 0.01214 1720 979 0.01217 1720 979 0.01223 1721 978 0.01213 1722 977 0.01217 1722 976 0.01216 1723 976 0.01212 1724 975 0.01209 1724 974 0.01207 1725 974 0.01212 1726 973 0.01206 1726 972 0.01208 1727 972 0.01208 1728 971 0.01208 1728 969 0.01206 1729 969 0.01207 1730 968 0.01212 1730 968 0.01206 1731 968 0.01196 1732 967 0.01197 1732 967 0.01196 1733 965 0.01191 1734 965 0.0119 1734 964 0.01185 1735 964 0.01185 1736 963 0.01183 1736 962 0.01182 1737 961 0.01178 1738 961 0.01186 1738 960 0.01187 1739 959 0.01177 1740 959 0.01175 1741 958 0.01175 1741 957 0.01176 1742 957 0.01173 1743 956 0.01173 1743 955 0.01182 1744 955 0.01168 1745 954 0.01167 1745 954 0.01166 1746 953 0.0116 1747 952 0.0116 1747 950 0.01159 1748 950 0.0116 1749 950 0.0116 1749 949 0.01161 1750 949 0.01157 1751 948 0.01151 1751 947 0.01151 1752 947 0.0115 1753 946 0.01149 1753 945 0.01149 1754 944 0.01146 1755 943 0.01141 1755 943 0.01144 1756 943 0.01144 1757 942 0.01139 1757 942 0.01139 1758 940 0.01137 1759 940 0.01135 1759 940 0.01137 1760 938 0.01131 1761 938 0.01133 1761 937 0.0113 1762 936 0.01123 1763 936 0.01126 1763 935 0.01129 1764 934 0.01123 1765 934 0.01121 1765 932 0.01123 1766 932 0.0112 1767 932 0.01119 1767 931 0.01118 1768 930 0.01118 1769 930 0.01114 1769 929 0.01113 1770 929 0.0111 1771 928 0.01113 1771 927 0.01105 1772 926 0.01109 1773 926 0.01108 1774 925 0.01108 1774 924 0.01102 1775 924 0.01103 1776 923 0.011 1776 922 0.01099 1777 922 0.01099 1778 921 0.01099 1778 920 0.01097 1779 919 0.01094 1780 918 0.01093 1780 918 0.0109 1781 918 0.0109 1782 917 0.01085 1782 917 0.01087 1783 915 0.01083 1784 915 0.01082 1784 915 0.01079 1785 914 0.01079 1786 913 0.01078 1786 912 0.0108 1787 911 0.01064 1788 911 0.01071 1788 910 0.01074 1789 910 0.01069 1790 909 0.01071 1790 908 0.01067 1791 907 0.01064 1792 907 0.01067 1792 906 0.01066 1793 905 0.01062 1794 905 0.01063 1794 904 0.01061 1795 904 0.01054 1796 903 0.01058 1796 902 0.01057 1797 901 0.01053 1798 900 0.01053 1798 900 0.01052 1799 900 0.01048 1800 899 0.01048 1800 897 0.01044 1801 897 0.01046 1802 897 0.01047 1802 896 0.01038 1803 896 0.01032 1804 895 0.01037 1805 894 0.01042 1805 893 0.01044 1806 893 0.01031 1807 892 0.01033 1807 892 0.01033 1808 890 0.0103 1809 890 0.01028 1809 889 0.01025 1810 889 0.01022 1811 888 0.01021 1811 887 0.01021 1812 886 0.01018 1813 886 0.0101 1813 885 0.0101 1814 885 0.01017 1815 884 0.01016 1815 883 0.01013 1816 883 0.01002 1817 882 0.01009 1817 881 0.01007 1818 880 0.01004 1819 880 0.01004 1819 879 0.01004 1820 879 0.01001 1821 878 0.01001 1821 877 0.01001 1822 876 0.009986 1823 876 0.009924 1823 875 0.009899 1824 875 0.009899 1825 874 0.009924 1825 873 0.009937 1826 872 0.009937 1827 872 0.00985 1827 872 0.0098 1828 871 0.0098 1829 869 0.00985 1829 869 0.009788 1830 868 0.009825 1831 868 0.009788 1831 868 0.0098 1832 867 0.009775 1833 865 0.009751 1833 865 0.009689 1834 864 0.009701 1835 864 0.009738 1836 863 0.009664 1836 862 0.009614 1837 862 0.009577 1838 861 0.009552 1838 861 0.009416 1839 860 0.009565 1840 859 0.00954 1840 858 0.009565 1841 857 0.009552 1842 857 0.009552 1842 856 0.00954 1843 856 0.009503 1844 855 0.009453 1844 854 0.009441 1845 854 0.009453 1846 853 0.00949 1846 853 0.009453 1847 852 0.009416 1848 851 0.009441 1848 850 0.009404 1849 850 0.009404 1850 849 0.009342 1850 848 0.009342 1851 847 0.009342 1852 847 0.009342 1852 847 0.009292 1853 846 0.009292 1854 844 0.009292 1854 844 0.009267 1855 843 0.00923 1856 843 0.009242 1856 843 0.009205 1857 842 0.009205 1858 840 0.009193 1858 840 0.009094 1859 839 0.009131 1860 838 0.009143 1860 838 0.009106 1861 837 0.009094 1862 837 0.009044 1862 836 0.009106 1863 836 0.009056 1864 835 0.009032 1864 834 0.009007 1865 833 0.00897 1866 833 0.008957 1867 832 0.008908 1867 831 0.008982 1868 830 0.00897 1869 830 0.008932 1869 829 0.00892 1870 829 0.008858 1871 828 0.008895 1871 827 0.008858 1872 827 0.008858 1873 826 0.008846 1873 825 0.008796 1874 825 0.008771 1875 824 0.008771 1875 823 0.008771 1876 822 0.008771 1877 822 0.008734 1877 821 0.008722 1878 821 0.00866 1879 820 0.008697 1879 819 0.008722 1880 818 0.008684 1881 818 0.00861 1881 818 0.008598 1882 817 0.00861 1883 815 0.008647 1883 815 0.008622 1884 814 0.008573 1885 814 0.008424 1885 813 0.008461 1886 812 0.008499 1887 812 0.008486 1887 811 0.008474 1888 811 0.00856 1889 810 0.008585 1889 809 0.008449 1890 808 0.008412 1891 808 0.008337 1891 807 0.00835 1892 806 0.0083 1893 806 0.008213 1893 805 0.008226 1894 804 0.008275 1895 804 0.0083 1895 803 0.008288 1896 803 0.008288 1897 802 0.0083 1898 801 0.008288 1898 801 0.008275 1899 801 0.008213 1900 801 0.008114 1900 801 0.008201 1901 801 0.008164 1902 801 0.008176 1902 800 0.008151 1903 800 0.008089 1904 799 0.008065 1904 799 0.008065 1905 798 0.008052 1906 797 0.008065 1906 796 0.008015 1907 796 0.008015 1908 795 0.007965 1908 794 0.008003 1909 794 0.008015 1910 793 0.007965 1910 793 0.007928 1911 792 0.007903 1912 791 0.007928 1912 790 0.007879 1913 789 0.007879 1914 789 0.007866 1914 788 0.007866 1915 788 0.007854 1916 786 0.007779 1916 786 0.00773 1917 786 0.007804 1918 785 0.007779 1918 784 0.007767 1919 784 0.007767 1920 783 0.007705 1920 782 0.007569 1921 782 0.007742 1922 781 0.007717 1922 780 0.007668 1923 780 0.007655 1924 779 0.007631 1924 779 0.007606 1925 778 0.007606 1926 777 0.007606 1926 776 0.007581 1927 775 0.007569 1928 775 0.007581 1928 775 0.007482 1929 774 0.007494 1930 773 0.007544 1931 772 0.007507 1931 771 0.007395 1932 771 0.007321 1933 770 0.007197 1933 769 0.007209 1934 769 0.007308 1935 768 0.007395 1935 768 0.007333 1936 767 0.007346 1937 766 0.007346 1937 766 0.007308 1938 765 0.007296 1939 764 0.007296 1939 764 0.007333 1940 763 0.007271 1941 762 0.007234 1941 761 0.007308 1942 761 0.007222 1943 760 0.007184 1943 759 0.007135 1944 759 0.007135 1945 758 0.007135 1945 757 0.007122 1946 757 0.007085 1947 756 0.007085 1947 756 0.00706 1948 755 0.007073 1949 754 0.00706 1949 753 0.007036 1950 753 0.007023 1951 752 0.007011 1951 751 0.006961 1952 750 0.006998 1953 750 0.006924 1953 749 0.006936 1954 749 0.006936 1955 748 0.006924 1955 747 0.006899 1956 746 0.006837 1957 746 0.0068 1957 745 0.006825 1958 744 0.006812 1959 744 0.0068 1959 743 0.006788 1960 743 0.006763 1961 742 0.00675 1962 741 0.006676 1962 740 0.006639 1963 739 0.006676 1964 739 0.006639 1964 738 0.006676 1965 738 0.006676 1966 737 0.006639 1966 736 0.006577 1967 736 0.006577 1968 736 0.006577 1968 734 0.006614 1969 734 0.006664 1970 733 0.006676 1970 732 0.006626 1971 732 0.006577 1972 731 0.00654 1972 731 0.00649 1973 730 0.006441 1974 729 0.006391 1974 728 0.006416 1975 728 0.006441 1976 727 0.006428 1976 726 0.006403 1977 725 0.006416 1978 725 0.006354 1978 725 0.006292 1979 724 0.006354 1980 723 0.006354 1980 722 0.006341 1981 721 0.006304 1982 721 0.006304 1982 720 0.006279 1983 719 0.006255 1984 719 0.006217 1984 718 0.006205 1985 718 0.006217 1986 717 0.006217 1986 716 0.006205 1987 715 0.006155 1988 714 0.00618 1988 714 0.006069 1989 714 0.00618 1990 713 0.00618 1990 712 0.006131 1991 711 0.006118 1992 711 0.006143 1993 710 0.006069 1993 709 0.006081 1994 709 0.005982 1995 708 0.006031 1995 707 0.006056 1996 707 0.005945 1997 706 0.005932 1997 706 0.005945 1998 704 0.005945 1999 704 0.00592 1999 703 0.005858 2000 703 0.00587 2001 702 0.00587 2001 702 0.005783 2002 701 0.005808 2003 700 0.005783 2003 699 0.005783 2004 699 0.005759 2005 698 0.005771 2005 697 0.005709 2006 696 0.005709 2007 696 0.005659 2007 696 0.005622 2008 695 0.005697 2009 694 0.005721 2009 693 0.005697 2010 693 0.005672 2011 693 0.005635 2011 692 0.005635 2012 691 0.005647 2013 689 0.005684 2013 689 0.005659 2014 688 0.005635 2015 688 0.005523 2015 686 0.005523 2016 686 0.005548 2017 685 0.005474 2017 685 0.005449 2018 685 0.005436 2019 684 0.005486 2019 683 0.005486 2020 683 0.005474 2021 682 0.005424 2021 682 0.005412 2022 681 0.005337 2023 680 0.00535 2024 679 0.005226 2024 678 0.005102 2025 678 0.005114 2026 677 0.005213 2026 677 0.005325 2027 676 0.005325 2028 675 0.005288 2028 675 0.00525 2029 674 0.005263 2030 674 0.005263 2030 672 0.005238 2031 672 0.005126 2032 671 0.005139 2032 671 0.005213 2033 669 0.005164 2034 669 0.005114 2034 668 0.005052 2035 668 0.005002 2036 668 0.005077 2036 667 0.005027 2037 666 0.00504 2038 665 0.00504 2038 664 0.005015 2039 664 0.005002 2040 663 0.004978 2040 663 0.004891 2041 661 0.004878 2042 660 0.005027 2042 660 0.004878 2043 660 0.004978 2044 659 0.004928 2044 658 0.004903 2045 657 0.004866 2046 657 0.004829 2046 657 0.004816 2047 656 0.004841 2048 655 0.004841 2048 654 0.004804 2049 653 0.004779 2050 653 0.004742 2050 652 0.004754 2051 652 0.004779 2052 651 0.00473 2052 650 0.004593 2053 650 0.004531 2054 649 0.004643 2055 648 0.004705 2055 647 0.004692 2056 646 0.004643 2057 646 0.004581 2057 646 0.004593 2058 645 0.004556 2059 644 0.004618 2059 643 0.004606 2060 643 0.004618 2061 643 0.004544 2061 642 0.004507 2062 641 0.004482 2063 639 0.004469 2063 639 0.004445 2064 639 0.00442 2065 638 0.004407 2065 636 0.004383 2066 637 0.00437 2067 636 0.00437 2067 635 0.004333 2068 635 0.004283 2069 634 0.004296 2069 633 0.004358 2070 633 0.004321 2071 632 0.004308 2071 632 0.004259 2072 631 0.004221 2073 630 0.004234 2073 629 0.004209 2074 629 0.004259 2075 628 0.004246 2075 628 0.004234 2076 627 0.004221 2077 626 0.004159 2077 625 0.004097 2078 625 0.004035 2079 624 0.004023 2079 624 0.004011 2080 622 0.003998 2081 622 0.003998 2081 621 0.003998 2082 621 0.004023 2083 619 0.003998 2083 619 0.003949 2084 618 0.003961 2085 617 0.003973 2086 617 0.003936 2086 617 0.003911 2087 616 0.003936 2088 615 0.003936 2088 614 0.003837 2089 614 0.003911 2090 613 0.003849 2090 613 0.003825 2091 612 0.003812 2092 611 0.0038 2092 610 0.0038 2093 610 0.003787 2094 609 0.003787 2094 608 0.003763 2095 608 0.003725 2096 607 0.003676 2096 606 0.003639 2097 606 0.003639 2098 605 0.003676 2098 605 0.003663 2099 603 0.003651 2100 603 0.003639 2100 602 0.003589 2101 602 0.003589 2102 601 0.003552 2102 600 0.003527 2103 600 0.003515 2104 600 0.003564 2104 599 0.003527 2105 599 0.00349 2106 598 0.003478 2106 596 0.003539 2107 596 0.003515 2108 596 0.003453 2108 596 0.003391 2109 594 0.003378 2110 593 0.003341 2110 593 0.003329 2111 592 0.003341 2112 592 0.003403 2112 591 0.003366 2113 590 0.003329 2114 589 0.003254 2114 589 0.003267 2115 588 0.003267 2116 588 0.00323 2116 587 0.003242 2117 586 0.003242 2118 585 0.003205 2119 585 0.003168 2119 584 0.00318 2120 583 0.003143 2121 583 0.00313 2121 582 0.003106 2122 582 0.003118 2123 581 0.003118 2123 580 0.003106 2124 579 0.003093 2125 579 0.003068 2125 578 0.003068 2126 577 0.003044 2127 577 0.003044 2127 577 0.002994 2128 575 0.003031 2129 574 0.002957 2129 574 0.002982 2130 574 0.003006 2131 573 0.002895 2131 572 0.002932 2132 571 0.00292 2133 571 0.002994 2133 570 0.002957 2134 569 0.002895 2135 568 0.002684 2135 567 0.002746 2136 567 0.002758 2137 567 0.002758 2137 567 0.002758 2138 565 0.002771 2139 564 0.002734 2139 564 0.002721 2140 564 0.002721 2141 562 0.002696 2141 562 0.002672 2142 561 0.002672 2143 561 0.002659 2143 560 0.002647 2144 559 0.002647 2145 559 0.00261 2145 558 0.002585 2146 557 0.002572 2147 557 0.002572 2147 556 0.00256 2148 555 0.00256 2149 555 0.002548 2150 553 0.00251 2150 553 0.002399 2151 553 0.002411 2152 552 0.002449 2152 551 0.002411 2153 550 0.002387 2154 549 0.002362 2154 549 0.002399 2155 549 0.002411 2156 548 0.002349 2156 546 0.002312 2157 546 0.002275 2158 546 0.002287 2158 546 0.002312 2159 544 0.002312 2160 543 0.002275 2160 543 0.002275 2161 542 0.002275 2162 542 0.002263 2162 541 0.002275 2163 540 0.002238 2164 539 0.002188 2164 539 0.002188 2165 538 0.002188 2166 537 0.002151 2166 537 0.002114 2167 536 0.002126 2168 536 0.002114 2168 535 0.002101 2169 534 0.002064 2170 534 0.00199 2170 533 0.001903 2171 532 0.002015 2172 532 0.002015 2172 531 0.002002 2173 530 0.002002 2174 530 0.002015 2174 529 0.00194 2175 528 0.00199 2176 528 0.002052 2176 527 0.001953 2177 526 0.001928 2178 525 0.001903 2178 524 0.001853 2179 524 0.001853 2180 524 0.001915 2181 523 0.001717 2181 522 0.001742 2182 521 0.001829 2183 521 0.001779 2183 520 0.00168 2184 519 0.001717 2185 518 0.001717 2185 518 0.001705 2186 517 0.001692 2187 517 0.001705 2187 516 0.001667 2188 515 0.001667 2189 514 0.001655 2189 514 0.001618 2190 513 0.00163 2191 513 0.001556 2191 512 0.001605 2192 511 0.001581 2193 510 0.001581 2193 510 0.001543 2194 509 0.001519 2195 509 0.001506 2195 508 0.001457 2196 508 0.001457 2197 506 0.001482 2197 506 0.001482 2198 506 0.001457 2199 505 0.001457 2199 504 0.001444 2200 503 0.001407 2201 503 0.001382 2201 503 0.001382 2202 502 0.00132 2203 501 0.001358 2203 500 0.001308 2204 499 0.001283 2205 499 0.001283 2205 499 0.001283 2206 497 0.001333 2207 496 0.001283 2207 496 0.001258 2208 496 0.001258 2209 495 0.001246 2209 494 0.001209 2210 493 0.001221 2211 492 0.001172 2212 492 0.001159 2212 492 0.00111 2213 491 0.001097 2214 490 0.00106 2214 490 0.001023 2215 489 0.001122 2216 488 0.001072 2216 488 0.00106 2217 487 0.001035 2218 486 0.00101 2218 486 0.0009732 2219 485 0.00106 2220 485 0.0009856 2220 484 0.0009608 2221 483 0.0009236 2222 482 0.000874 2222 481 0.0008616 2223 481 0.0008864 2224 481 0.0008988 2224 480 0.0009112 2225 481 0.0009608 2226 482 0.000936 2226 484 0.0009608 2227 483 0.000998 2228 481 0.0009236 2228 479 0.0008864 2229 477 0.0008244 2230 475 0.0007872 2230 474 0.0007748 2231 473 0.0007377 2232 472 0.0006385 2232 471 0.0006137 2233 471 0.0006633 2234 470 0.0006881 2234 469 0.0006633 2235 469 0.0006633 2236 468 0.0006261 2236 467 0.0006137 2237 467 0.0006261 2238 467 0.0006261 2238 466 0.0006261 2239 465 0.0006013 2240 464 0.0005889 2240 464 0.0006013 2241 463 0.0006261 2242 462 0.0006385 2243 461 0.0006509 2243 460 0.0006137 2244 460 0.0005889 2245 459 0.0005517 2245 459 0.0005269 2246 458 0.0005269 2247 456 0.0005269 2247 456 0.0005145 2248 456 0.0004897 2249 455 0.0005021 2249 454 0.0004773 2250 453 0.0004897 2251 453 0.0005021 2251 453 0.0004649 2252 453 0.0004773 2253 451 0.0004773 2253 450 0.0004649 2254 449 0.0004153 2255 449 0.0004029 2255 449 0.0004029 2256 448 0.0003161 2257 447 0.0002541 2257 446 0.0003409 2258 446 0.0003657 2259 445 0.0003781 2259 444 0.0003781 2260 444 0.0003657 2261 443 0.0003285 2261 442 0.0003533 2262 442 0.0003285 2263 441 0.0002789 2263 440 0.0002789 2264 439 0.0002418 2265 439 0.0002418 2265 438 0.0002789 2266 438 0.0002541 2267 437 0.0002418 2267 436 0.0002418 2268 436 0.0001674 2269 435 0.0001426 2269 435 0.0001426 2270 434 0.0001302 2271 433 0.000155 2271 432 0.0001922 2272 431 0.0001798 2273 431 0.0001798 2273 430 0.0001426 2274 430 0.0001178 2275 428 0.0001302 2276 428 0.0001426 2276 428 0.0001674 2277 427 0.0001674 2278 426 0.0001674 2278 426 0.0001426 2279 424 0.0001426 2280 424 0.000155 2280 424 0.0001798 2281 423 0.000155 2282 422 0.0001178 2282 421 0.0001054 2283 421 0.0001054 2284 421 9.298e-05 2284 420 0.0001178 2285 418 0.0001178 2286 418 0.0001426 2286 417 0.0001674 2287 417 0.0001302 2288 416 8.058e-05 2288 415 8.058e-05 2289 414 6.199e-06 2290 414 6.199e-06 2290 413 6.199e-06 2291 412 6.819e-05 2292 412 5.579e-05 2292 411 6.819e-05 2293 410 6.819e-05 2294 410 5.579e-05 2294 409 4.339e-05 2295 409 0.0001178 2296 409 0.0001426 2296 407 5.579e-05 2297 406 1.86e-05 2298 406 6.199e-06 2298 405 6.819e-05 2299 405 6.199e-06 2300 405 1.86e-05 2300 403 6.199e-06 2301 403 6.199e-06 2302 402 6.199e-06 2302 401 6.199e-06 2303 401 6.199e-06 2304 401 6.199e-06 2304 400 6.199e-06 2305 399 6.199e-06 2306 399 3.099e-05 2307 398 6.199e-06 2307 397 -3.099e-05 2308 396 -1.86e-05 2309 396 6.199e-06 2309 396 5.579e-05 2310 394 6.199e-06 2311 394 6.199e-06 2311 393 6.199e-06 2312 392 6.199e-06 2313 392 4.339e-05 2313 392 5.579e-05 2314 391 6.819e-05 2315 390 6.819e-05 2315 389 6.819e-05 2316 388 6.819e-05 2317 388 9.298e-05 2317 387 8.058e-05 2318 386 0.0001178 2319 385 0.0001426 2319 385 0.0001798 2320 385 0.0002046 2321 384 0.0002418 2321 383 0.0002665 2322 382 0.0002789 2323 381 0.0003037 2323 381 0.0003285 2324 381 0.0003657 2325 379 0.0003781 2325 379 0.0004277 2326 378 0.0004897 2327 378 0.0005641 2327 378 0.0005889 2328 376 0.0006261 2329 376 0.0006261 2329 375 0.0006633 2330 374 0.0007377 2331 374 0.0007872 2331 373 0.0008368 2332 372 0.0008988 2333 371 0.0009236 2333 371 0.0009732 2334 370 0.001048 2335 369 0.00111 2335 369 0.001159 2336 368 0.001246 2337 368 0.001283 2338 367 0.001308 2338 367 0.001345 2339 365 0.00142 2340 365 0.001444 2340 364 0.001494 2341 363 0.001556 2342 363 0.001618 2342 362 0.001692 2343 361 0.001705 2344 361 0.001729 2344 360 0.001767 2345 359 0.001816 2346 359 0.001841 2346 358 0.001878 2347 357 0.001953 2348 356 0.001977 2348 356 0.00199 2349 355 0.002027 2350 355 0.002101 2350 354 0.002151 2351 353 0.002151 2352 353 0.002176 2352 352 0.002238 2353 350 0.002287 2354 350 0.00225 2354 350 0.002275 2355 349 0.002312 2356 349 0.0023 2356 348 0.002411 2357 347 0.002374 2358 346 0.002436 2358 346 0.002449 2359 345 0.00251 2360 345 0.002411 2360 344 0.002374 2361 343 0.002436 2362 342 0.002535 2362 342 0.002585 2363 342 0.002585 2364 340 0.002572 2364 340 0.00261 2365 339 0.002647 2366 338 0.002672 2366 338 0.002709 2367 337 0.002709 2368 336 0.00261 2369 335 0.002721 2369 335 0.002758 2370 335 0.002758 2371 334 0.002758 2371 333 0.002771 2372 332 0.002783 2373 331 0.002808 2373 331 0.002808 2374 331 0.002895 2375 330 0.002796 2375 329 0.002845 2376 328 0.002808 2377 328 0.00282 2377 327 0.00282 2378 326 0.002833 2379 326 0.002858 2379 325 0.002833 2380 324 0.002845 2381 324 0.002845 2381 323 0.002808 2382 322 0.00287 2383 321 0.002907 2383 320 0.002895 2384 320 0.002907 2385 319 0.00292 2385 319 0.00292 2386 318 0.00287 2387 317 0.00287 2387 317 0.00287 2388 317 0.002882 2389 315 0.00292 2389 315 0.002907 2390 314 0.002895 2391 313 0.002932 2391 313 0.00287 2392 312 0.002882 2393 311 0.00287 2393 310 0.00287 2394 310 0.002895 2395 310 0.00292 2395 309 0.002895 2396 308 0.002895 2397 306 0.00292 2397 306 0.002858 2398 306 0.002845 2399 305 0.00287 2400 305 0.002845 2400 304 0.002858 2401 303 0.00287 2402 302 0.00287 2402 302 0.00287 2403 301 0.002907 2404 301 0.00287 2404 300 0.002845 2405 299 0.00287 2406 299 0.002845 2406 298 0.002796 2407 297 0.002771 2408 297 0.002758 2408 296 0.002771 2409 295 0.002783 2410 295 0.002808 2410 294 0.002808 2411 293 0.002746 2412 292 0.002709 2412 292 0.002709 2413 292 0.002734 2414 291 0.002734 2414 290 0.002783 2415 289 0.002758 2416 288 0.002758 2416 288 0.002746 2417 288 0.002734 2418 287 0.002672 2418 286 0.002709 2419 285 0.002746 2420 285 0.002721 2420 284 0.002709 2421 284 0.002709 2422 282 0.002721 2422 282 0.002758 2423 281 0.002758 2424 280 0.002746 2424 280 0.002672 2425 280 0.002597 2426 278 0.002659 2426 277 0.002684 2427 277 0.002659 2428 277 0.002659 2428 276 0.002647 2429 276 0.00261 2430 274 0.002659 2431 274 0.002647 2431 274 0.002647 2432 272 0.002647 2433 271 0.002572 2433 270 0.002572 2434 270 0.002634 2435 270 0.00261 2435 269 0.002622 2436 269 0.002572 2437 267 0.00256 2437 267 0.002498 2438 267 0.002436 2439 266 0.002473 2439 265 0.002498 2440 264 0.002486 2441 264 0.002523 2441 263 0.002535 2442 263 0.002548 2443 262 0.00251 2443 261 0.002572 2444 260 0.002548 2445 260 0.002523 2445 259 0.002585 2446 259 0.002548 2447 258 0.002449 2447 256 0.002449 2448 256 0.002436 2449 256 0.002523 2449 255 0.002548 2450 255 0.002498 2451 253 0.002449 2451 253 0.002436 2452 252 0.002449 2453 252 0.002449 2453 251 0.002449 2454 250 0.002449 2455 249 0.002449 2455 249 0.002449 2456 249 0.002461 2457 247 0.002449 2457 246 0.002411 2458 246 0.002424 2459 245 0.002449 2459 245 0.002436 2460 244 0.002436 2461 243 0.002387 2461 243 0.002399 2462 242 0.002362 2463 242 0.002374 2464 241 0.002362 2464 240 0.002349 2465 239 0.002312 2466 239 0.002337 2466 238 0.002349 2467 238 0.002337 2468 237 0.002312 2468 236 0.002263 2469 235 0.002275 2470 234 0.002312 2470 234 0.002312 2471 233 0.002312 2472 233 0.002238 2472 232 0.002201 2473 231 0.002238 2474 231 0.002225 2474 230 0.002213 2475 229 0.002201 2476 229 0.002201 2476 228 0.002151 2477 227 0.002139 2478 227 0.002151 2478 226 0.002151 2479 226 0.002151 2480 224 0.002151 2480 224 0.002151 2481 224 0.002163 2482 223 0.002101 2482 222 0.002089 2483 221 0.002077 2484 220 0.002126 2484 220 0.002052 2485 219 0.002114 2486 218 0.002089 2486 218 0.002101 2487 217 0.002139 2488 217 0.001903 2488 216 0.001928 2489 215 0.002064 2490 214 0.002064 2490 214 0.002052 2491 213 0.002015 2492 213 0.002015 2492 213 0.002015 2493 211 0.00199 2494 210 0.00199 2495 209 0.001953 2495 209 0.001953 2496 209 0.001953 2497 208 0.001915 2497 206 0.001928 2498 206 0.001953 2499 206 0.001953 2499 205 0.001915 2500 204 0.001903 2501 204 0.001915 2501 202 0.001891 2502 202 0.001903 2503 202 0.001953 2503 201 0.001804 2504 201 0.001816 2505 201 0.001829 2505 199 0.001804 2506 199 0.001804 2507 199 0.001841 2507 198 0.001804 2508 197 0.001791 2509 196 0.001791 2509 195 0.001779 2510 195 0.001754 2511 194 0.001754 2511 193 0.001742 2512 193 0.001767 2513 192 0.001742 2513 191 0.001742 2514 191 0.001742 2515 190 0.001705 2515 189 0.00168 2516 189 0.001643 2517 188 0.001667 2517 188 0.00168 2518 187 0.00168 2519 186 0.001667 2519 186 0.001643 2520 184 0.001655 2521 184 0.001655 2521 184 0.001643 2522 183 0.001618 2523 182 0.001593 2523 181 0.001593 2524 181 0.001581 2525 180 0.001581 2526 179 0.001581 2526 179 0.001556 2527 177 0.001531 2528 177 0.001519 2528 177 0.001494 2529 176 0.001519 2530 175 0.001531 2530 175 0.001531 2531 174 0.001494 2532 174 0.001358 2532 173 0.001506 2533 172 0.001531 2534 171 0.001457 2534 170 0.001407 2535 170 0.001469 2536 169 0.001482 2536 168 0.001457 2537 168 0.001457 2538 167 0.001457 2538 166 0.001345 2539 166 0.001358 2540 165 0.001382 2540 165 0.00132 2541 164 0.001258 2542 164 0.001308 2542 163 0.00137 2543 162 0.001345 2544 161 0.001382 2544 161 0.001382 2545 159 0.001382 2546 159 0.001358 2546 159 0.001345 2547 158 0.001345 2548 157 0.00132 2548 156 0.001308 2549 156 0.001296 2550 155 0.001296 2550 155 0.001283 2551 154 0.001283 2552 152 0.001283 2552 152 0.001283 2553 152 0.001258 2554 150 0.001246 2554 150 0.001234 2555 149 0.001234 2556 149 0.001234 2557 149 0.001209 2557 148 0.001196 2558 147 0.001221 2559 146 0.001246 2559 145 0.001221 2560 145 0.001172 2561 144 0.001134 2561 143 0.001134 2562 143 0.001147 2563 142 0.001134 2563 141 0.001085 2564 141 0.0009608 2565 140 0.001172 2565 140 0.001159 2566 139 0.00111 2567 138 0.001097 2567 138 0.00106 2568 137 0.001072 2569 136 0.00106 2569 136 0.001048 2570 135 0.001035 2571 134 0.001035 2571 134 0.001048 2572 133 0.001035 2573 131 0.001035 2573 131 0.001035 2574 131 0.001023 2575 131 0.001023 2575 130 0.001048 2576 129 0.0009732 2577 129 0.0009608 2577 127 0.00101 2578 127 0.000998 2579 127 0.000936 2579 126 0.0009608 2580 125 0.0009732 2581 124 0.0008864 2581 123 0.0009732 2582 123 0.0009608 2583 121 0.0009112 2583 121 0.0008616 2584 121 0.0008244 2585 120 0.0008616 2585 119 0.000874 2586 119 0.000874 2587 118 0.0008492 2588 117 0.0008492 2588 116 0.000874 2589 116 0.0008492 2590 115 0.0008244 2590 115 0.0007872 2591 114 0.000812 2592 113 0.0008368 2592 113 0.0007748 2593 112 0.0007872 2594 111 0.0007996 2594 110 0.0007872 2595 109 0.0007377 2596 109 0.0007253 2596 109 0.0007253 2597 108 0.0007253 2598 107 0.0007377 2598 106 0.0007253 2599 106 0.0007253 2600 106 0.0007005 2600 105 0.0007253 2601 104 0.0007624 2602 103 0.0007377 2602 102 0.0006137 2603 102 0.0005021 2604 101 0.0005889 2604 101 0.0006509 2605 100 0.0006633 2606 98 0.0006261 2606 98 0.0006385 2607 98 0.0006261 2608 97 0.0006881 2608 96 0.0006509 2609 96 0.0006385 2610 95 0.0006013 2610 94 0.0005765 2611 94 0.0005641 2612 94 0.0005641 2612 93 0.0005641 2613 92 0.0006261 2614 91 0.0005269 2614 91 0.0005641 2615 90 0.0005517 2616 90 0.0005021 2616 88 0.0004897 2617 88 0.0005021 2618 87 0.0005145 2618 87 0.0005145 2619 86 0.0004897 2620 85 0.0004649 2621 84 0.0004897 2621 84 0.0004401 2622 84 0.0004773 2623 83 0.0004525 2623 82 0.0004153 2624 81 0.0004649 2625 80 0.0004649 2625 80 0.0003657 2626 79 0.0004277 2627 79 0.0004153 2627 77 0.0003905 2628 77 0.0003781 2629 77 0.0003657 2629 76 0.0003781 2630 76 0.0003657 2631 76 0.0003285 2631 74 0.0003409 2632 73 0.0003533 2633 73 0.0003161 2633 72 0.0002294 2634 71 9.298e-05 2635 70 0.0001302 2635 70 0.0002046 2636 69 0.0003905 2637 69 0.0004029 2637 68 0.0002541 2638 67 0.0002541 2639 66 0.0002294 2639 66 0.0002418 2640 65 0.0003037 2641 64 0.0002418 2641 64 0.0002541 2642 63 0.0001302 2643 63 0.0001426 2643 62 0.0001674 2644 61 0.0001798 2645 60 0.0001922 2645 59 0.0002046 2646 59 0.000217 2647 58 0.0002046 2647 58 0.0001674 2648 56 0.0001426 2649 56 0.0001302 2649 56 0.000155 2650 55 0.0001302 2651 54 0.0001178 2652 54 0.0001054 2652 53 9.298e-05 2653 52 8.058e-05 2654 52 0.0001054 2654 51 6.819e-05 2655 50 9.298e-05 2656 49 9.298e-05 2656 49 6.819e-05 2657 48 6.819e-05 2658 48 5.579e-05 2658 47 3.099e-05 2659 46 1.86e-05 2660 45 6.199e-06 2660 45 6.199e-06 2661 44 6.199e-06 2662 43 -3.099e-05 2662 43 6.199e-06 2663 42 -3.099e-05 2664 42 6.199e-06 2664 41 6.199e-06 2665 41 6.199e-06 2666 40 -6.199e-06 2666 39 -5.579e-05 2667 38 -0.0001302 2668 38 -5.579e-05 2668 38 -5.579e-05 2669 37 -5.579e-05 2670 37 -5.579e-05 2670 36 -4.339e-05 2671 36 -3.099e-05 2672 36 -5.579e-05 2672 34 -8.058e-05 2673 34 -5.579e-05 2674 34 -8.058e-05 2674 34 -5.579e-05 2675 34 -8.058e-05 2676 33 -0.0001054 2676 33 -8.058e-05 2677 32 -5.579e-05 2678 31 -8.058e-05 2678 31 -8.058e-05 2679 31 -0.0001178 2680 30 -9.298e-05 2680 29 -0.0001426 2681 27 -0.0002294 2682 27 -0.0002046 2683 26 -0.0002913 2683 24 -0.0001798 2684 23 -0.0001798 2685 23 -0.0002294 2685 22 -0.0002294 2686 22 -0.0001798 2687 21 -0.0002294 2687 20 -0.0002541 2688 20 -0.0002541 2689 20 -0.0002541 2689 19 -0.0002789 2690 19 -0.0002665 2691 18 -0.0003037 2691 17 -0.0003657 2692 17 -0.0003161 2693 17 -0.0002294 2693 16 -0.0002541 2694 16 -0.0003285 2695 16 -0.0003037 2695 16 -0.0003037 2696 16 -0.0002913 2697 15 -0.0002665 2697 14 -0.0002541 2698 14 -0.0003161 2699 14 -0.0002541 2699 13 -0.0003161 2700 13 -0.0003037 2701 13 -0.0003285 2701 13 -0.0003161 2702 13 -0.0002913 2703 12 -0.0003533 2703 12 -0.0003037 2704 12 -0.0003409 2705 12 -0.0003657 2705 11 -0.0003657 2706 11 -0.0003285 2707 11 -0.0004029 2707 11 -0.0005889 2708 11 -0.0004277 2709 11 -0.0003285 2709 11 -0.0003533 2710 11 -0.0003409 2711 10 -0.0003657 2711 11 -0.0003781 2712 10 -0.0003285 2713 10 -0.0003533 2714 10 -0.0003657 2714 10 -0.0003285 2715 9 -0.0002665 2716 10 -0.0003037 2716 10 -0.0004897 2717 9 -0.0004897 2718 9 -0.0003037 2718 9 -0.0003657 2719 9 -0.0004029 2720 9 -0.0003285 2720 9 -0.0003161 2721 9 -0.0003161 2722 9 -0.0003161 2722 9 -0.0003409 2723 9 -0.0003781 2724 9 -0.0003657 2724 9 -0.0003905 2725 9 -0.0003905 2726 9 -0.0003781 2726 9 -0.0003905 2727 9 -0.0003781 2728 9 -0.0003905 2728 9 -0.0003657 2729 9 -0.0003409 2730 9 -0.0003657 2730 9 -0.0004277 2731 9 -0.0003657 2732 9 -0.0003781 2732 9 -0.0003781 2733 9 -0.0003781 2734 9 -0.0003409 2734 9 -0.0003285 2735 9 -0.0003285 2736 9 -0.0003781 2736 9 -0.0003781 2737 9 -0.0003161 2738 9 -0.0003781 2738 9 -0.0003409 2739 9 -0.0003285 2740 9 -0.0003657 2740 9 -0.0003905 2741 9 -0.0004029 2742 9 -0.0003285 2742 9 -0.0003409 2743 9 -0.0003409 2744 9 -0.0003533 2745 9 -0.0003657 2745 9 -0.0003657 2746 9 -0.0003657 2747 9 -0.0003657 2747 9 -0.0003657 2748 9 -0.0003657 2749 9 -0.0003657 2749 9 -0.0003657 2750 9 -0.0003657 2751 9 -0.0003657 2751 9 -0.0003781 2752 9 -0.0003905 2753 9 -0.0003781 2753 8 -0.0003905 2754 9 -0.0003905 2755 9 -0.0003905 2755 9 -0.0003657 2756 9 -0.0003533 2757 9 -0.0003657 2757 9 -0.0003781 2758 9 -0.0003905 2759 9 -0.0003657 2759 2 0.29 0.09 0.74 0.002 0.007 0.66 1.3 1.02 0.292 0 0 0.001 0.0041 0 5 -0.000229 0 7 -0.0002414 0.3809 7 -0.0002414 0.7617 7 -0.0002414 1.143 7 -0.0002414 1.523 7 -0.0002414 1.904 7 -0.0002414 2.285 7 -0.0002414 2.666 7 -0.0002414 3.047 7 -0.0002414 3.428 9 -0.000229 3.809 9 -0.0002414 4.189 10 -0.000229 4.57 13 -0.0002042 4.951 13 -0.0001671 5.332 15 -0.0001423 5.713 17 -0.00013 6.094 18 -0.0001052 6.475 20 -8.045e-05 6.855 21 -4.332e-05 7.236 21 -3.094e-05 7.617 23 -3.094e-05 7.998 23 6.189e-06 8.379 24 6.189e-06 8.76 25 6.189e-06 9.141 26 6.189e-06 9.521 27 6.189e-06 9.902 27 6.189e-06 10.28 27 6.189e-06 10.66 29 6.189e-06 11.04 30 6.189e-06 11.43 30 6.189e-06 11.81 30 6.189e-06 12.19 31 1.857e-05 12.57 32 3.094e-05 12.95 33 3.094e-05 13.33 34 3.094e-05 13.71 34 5.57e-05 14.09 35 6.807e-05 14.47 36 8.045e-05 14.85 37 8.045e-05 15.23 38 8.045e-05 15.62 38 0.0001176 16 39 0.00013 16.38 40 0.00013 16.76 41 0.00013 17.14 41 0.0001547 17.52 42 0.0001795 17.9 43 0.0001795 18.28 44 0.0001795 18.66 45 0.0001918 19.04 45 0.0001918 19.42 46 0.0002166 19.8 46 0.000229 20.19 48 0.000229 20.57 48 0.0002414 20.95 49 0.0002414 21.33 49 0.0002414 21.71 51 0.0002537 22.09 52 0.0002785 22.47 52 0.0002785 22.85 52 0.0002909 23.23 54 0.0002909 23.61 54 0.0003156 23.99 55 0.000328 24.38 55 0.0003404 24.76 56 0.0003404 25.14 57 0.0003527 25.52 59 0.0003404 25.9 59 0.0003404 26.28 59 0.0003651 26.66 60 0.0003775 27.04 62 0.0003899 27.42 62 0.0003899 27.8 63 0.000427 28.18 63 0.0004394 28.56 65 0.0004518 28.95 65 0.0004518 29.33 66 0.0004518 29.71 66 0.0004641 30.09 67 0.0004765 30.47 68 0.0004889 30.85 69 0.0005013 31.23 70 0.0005013 31.61 70 0.0005013 31.99 71 0.0005013 32.37 72 0.000526 32.75 73 0.0005384 33.13 73 0.0005508 33.52 74 0.0005508 33.9 75 0.0005632 34.28 76 0.0005632 34.66 77 0.0005879 35.04 77 0.0005879 35.42 78 0.0006003 35.8 79 0.0006003 36.18 80 0.000625 36.56 81 0.0006498 36.94 81 0.0006498 37.32 81 0.0006622 37.71 83 0.0006746 38.09 84 0.0006746 38.47 84 0.0006622 38.85 84 0.0006869 39.23 85 0.0006993 39.61 87 0.0006993 39.99 87 0.0006993 40.37 88 0.0007241 40.75 88 0.0007364 41.13 90 0.0007488 41.51 90 0.0007612 41.89 91 0.0007859 42.28 92 0.0007612 42.66 92 0.0007612 43.04 93 0.0007859 43.42 94 0.0007859 43.8 95 0.0007983 44.18 95 0.0008107 44.56 96 0.0007983 44.94 97 0.0008355 45.32 98 0.0008478 45.7 99 0.0008478 46.08 99 0.0008478 46.46 100 0.0008478 46.85 101 0.0008602 47.23 102 0.0008602 47.61 102 0.000885 47.99 103 0.0008973 48.37 104 0.0008973 48.75 105 0.0009345 49.13 106 0.0009468 49.51 106 0.0009468 49.89 106 0.0009716 50.27 107 0.0009716 50.65 109 0.000984 51.04 109 0.000984 51.42 109 0.0009964 51.8 110 0.001009 52.18 112 0.001009 52.56 112 0.001021 52.94 113 0.001046 53.32 113 0.001058 53.7 115 0.001058 54.08 115 0.001058 54.46 116 0.001071 54.84 116 0.001095 55.22 117 0.001108 55.61 118 0.001108 55.99 119 0.00112 56.37 120 0.001108 56.75 121 0.00112 57.13 121 0.001145 57.51 122 0.001133 57.89 123 0.001133 58.27 123 0.001145 58.65 124 0.001157 59.03 125 0.001157 59.41 126 0.001157 59.8 127 0.001194 60.18 127 0.001207 60.56 127 0.001207 60.94 129 0.001219 61.32 130 0.001207 61.7 131 0.001219 62.08 131 0.001219 62.46 132 0.001244 62.84 133 0.001256 63.22 134 0.001269 63.6 134 0.001256 63.98 135 0.001269 64.37 136 0.001269 64.75 137 0.001281 65.13 137 0.001306 65.51 138 0.001306 65.89 138 0.001306 66.27 140 0.001318 66.65 141 0.001355 67.03 141 0.001368 67.41 142 0.001368 67.79 143 0.001368 68.17 144 0.001368 68.55 144 0.001392 68.94 145 0.001417 69.32 146 0.001442 69.7 146 0.001454 70.08 148 0.001479 70.46 149 0.001491 70.84 149 0.001491 71.22 149 0.001504 71.6 150 0.001516 71.98 151 0.001516 72.36 152 0.001516 72.74 152 0.001541 73.13 153 0.001553 73.51 154 0.001566 73.89 155 0.001566 74.27 156 0.001566 74.65 156 0.001578 75.03 157 0.001578 75.41 159 0.00159 75.79 159 0.001603 76.17 159 0.001615 76.55 160 0.001615 76.93 161 0.00164 77.31 162 0.001652 77.7 163 0.001652 78.08 163 0.001665 78.46 164 0.001665 78.84 165 0.001665 79.22 165 0.001677 79.6 166 0.001689 79.98 167 0.001714 80.36 168 0.001714 80.74 168 0.001714 81.12 170 0.001714 81.5 170 0.001739 81.88 171 0.001764 82.27 171 0.001764 82.65 172 0.001764 83.03 174 0.001764 83.41 174 0.001764 83.79 174 0.001764 84.17 176 0.001764 84.55 176 0.001788 84.93 177 0.001813 85.31 177 0.001813 85.69 179 0.001813 86.07 180 0.001838 86.46 180 0.001863 86.84 181 0.001863 87.22 181 0.001863 87.6 182 0.001863 87.98 184 0.001875 88.36 184 0.001912 88.74 184 0.001912 89.12 185 0.001912 89.5 187 0.001912 89.88 187 0.001937 90.26 188 0.001962 90.64 188 0.001962 91.03 190 0.001974 91.41 190 0.001999 91.79 191 0.001999 92.17 191 0.001987 92.55 192 0.001999 92.93 193 0.002011 93.31 194 0.002011 93.69 195 0.002011 94.07 195 0.002024 94.45 196 0.002048 94.83 196 0.002061 95.22 198 0.002073 95.6 199 0.002073 95.98 199 0.002073 96.36 199 0.00211 96.74 201 0.00211 97.12 201 0.002123 97.5 201 0.002135 97.88 202 0.002147 98.26 202 0.00216 98.64 204 0.002172 99.02 204 0.002172 99.4 206 0.002185 99.79 206 0.002209 100.2 207 0.002222 100.5 208 0.002234 100.9 209 0.002259 101.3 209 0.002246 101.7 210 0.002246 102.1 211 0.002259 102.5 212 0.002271 102.8 212 0.002308 103.2 213 0.002321 103.6 213 0.002321 104 215 0.002333 104.4 215 0.002333 104.7 217 0.002333 105.1 217 0.002333 105.5 218 0.002358 105.9 218 0.002358 106.3 218 0.002395 106.6 220 0.002383 107 221 0.002383 107.4 221 0.002407 107.8 223 0.00242 108.2 223 0.002432 108.5 224 0.002432 108.9 224 0.00242 109.3 225 0.002457 109.7 226 0.002444 110.1 227 0.002469 110.4 227 0.002482 110.8 228 0.002482 111.2 229 0.002482 111.6 230 0.002506 112 231 0.002531 112.4 231 0.002531 112.7 232 0.002556 113.1 233 0.002581 113.5 234 0.002581 113.9 234 0.002593 114.3 235 0.002593 114.6 236 0.002593 115 237 0.002605 115.4 237 0.002618 115.8 238 0.00263 116.2 238 0.002643 116.5 240 0.002655 116.9 240 0.002667 117.3 242 0.002667 117.7 242 0.002692 118.1 243 0.002692 118.4 243 0.002692 118.8 244 0.002692 119.2 245 0.002704 119.6 246 0.002692 120 246 0.002692 120.4 247 0.002704 120.7 248 0.002717 121.1 249 0.002742 121.5 249 0.002754 121.9 250 0.002779 122.3 251 0.002803 122.6 252 0.002828 123 252 0.002841 123.4 254 0.002841 123.8 254 0.002853 124.2 255 0.002878 124.5 256 0.002865 124.9 256 0.002865 125.3 257 0.002878 125.7 258 0.002865 126.1 259 0.002878 126.4 259 0.002902 126.8 260 0.002902 127.2 261 0.002902 127.6 262 0.002902 128 263 0.002927 128.3 263 0.00294 128.7 264 0.002964 129.1 265 0.002989 129.5 265 0.003001 129.9 267 0.003001 130.3 267 0.003001 130.6 268 0.003014 131 268 0.003026 131.4 270 0.003051 131.8 270 0.003051 132.2 271 0.003051 132.5 271 0.003051 132.9 273 0.003051 133.3 273 0.003063 133.7 274 0.003076 134.1 274 0.003076 134.4 276 0.003088 134.8 276 0.0031 135.2 277 0.0031 135.6 277 0.0031 136 279 0.0031 136.3 280 0.003138 136.7 280 0.003138 137.1 281 0.00315 137.5 281 0.00315 137.9 282 0.003138 138.3 284 0.00315 138.6 284 0.003162 139 285 0.003162 139.4 286 0.003175 139.8 286 0.003187 140.2 287 0.003199 140.5 288 0.003224 140.9 288 0.003274 141.3 289 0.00336 141.7 290 0.00341 142.1 290 0.003459 142.4 292 0.003484 142.8 292 0.003422 143.2 293 0.003298 143.6 294 0.003249 144 294 0.003249 144.3 295 0.003224 144.7 296 0.003224 145.1 297 0.003237 145.5 298 0.003237 145.9 299 0.003237 146.3 299 0.003249 146.6 300 0.003237 147 301 0.003237 147.4 302 0.003261 147.8 302 0.003261 148.2 302 0.003274 148.5 304 0.003286 148.9 305 0.003286 149.3 306 0.003298 149.7 306 0.003348 150.1 306 0.003348 150.4 307 0.003348 150.8 308 0.003373 151.2 309 0.003435 151.6 310 0.003472 152 310 0.003509 152.3 312 0.003509 152.7 312 0.003521 153.1 313 0.003534 153.5 313 0.003546 153.9 314 0.003546 154.2 315 0.003546 154.6 317 0.003546 155 317 0.003546 155.4 317 0.003571 155.8 318 0.003571 156.2 319 0.003596 156.5 319 0.003596 156.9 320 0.003596 157.3 321 0.00362 157.7 322 0.00362 158.1 323 0.003645 158.4 323 0.003645 158.8 324 0.003645 159.2 325 0.003645 159.6 326 0.00367 160 326 0.003695 160.3 328 0.003695 160.7 328 0.003695 161.1 329 0.003695 161.5 330 0.003695 161.9 331 0.003695 162.2 331 0.003695 162.6 331 0.003732 163 332 0.003744 163.4 334 0.003744 163.8 334 0.003744 164.2 335 0.003744 164.5 336 0.003756 164.9 337 0.003794 165.3 337 0.003794 165.7 338 0.003794 166.1 338 0.003806 166.4 340 0.003831 166.8 340 0.003843 167.2 342 0.003855 167.6 342 0.00388 168 342 0.003868 168.3 343 0.00388 168.7 344 0.003893 169.1 345 0.003905 169.5 345 0.003905 169.9 346 0.003905 170.2 347 0.003905 170.6 348 0.00393 171 349 0.003942 171.4 349 0.003954 171.8 350 0.003967 172.1 351 0.003954 172.5 351 0.003954 172.9 353 0.003979 173.3 353 0.003992 173.7 354 0.004029 174.1 356 0.004029 174.4 356 0.004041 174.8 356 0.004054 175.2 356 0.004066 175.6 358 0.004054 176 359 0.004078 176.3 360 0.004066 176.7 360 0.004091 177.1 361 0.004103 177.5 362 0.004103 177.9 363 0.004115 178.2 363 0.004115 178.6 364 0.00414 179 365 0.004153 179.4 365 0.004153 179.8 367 0.004153 180.1 367 0.004165 180.5 368 0.004165 180.9 368 0.00419 181.3 369 0.00419 181.7 370 0.00419 182.1 371 0.004214 182.4 371 0.004214 182.8 373 0.004239 183.2 373 0.004264 183.6 374 0.004264 184 374 0.004276 184.3 375 0.004276 184.7 376 0.004276 185.1 377 0.004301 185.5 378 0.004313 185.9 379 0.004326 186.2 379 0.004326 186.6 380 0.004326 187 381 0.004351 187.4 381 0.004363 187.8 382 0.004363 188.1 383 0.004375 188.5 383 0.004363 188.9 384 0.0044 189.3 385 0.004412 189.7 386 0.004412 190 387 0.004412 190.4 387 0.004425 190.8 388 0.004425 191.2 388 0.00445 191.6 390 0.004474 192 390 0.004474 192.3 392 0.004474 192.7 392 0.004474 193.1 393 0.004499 193.5 393 0.004511 193.9 395 0.004524 194.2 395 0.004524 194.6 396 0.004524 195 396 0.004536 195.4 398 0.004549 195.8 398 0.004573 196.1 399 0.004573 196.5 399 0.004573 196.9 400 0.004573 197.3 401 0.004573 197.7 401 0.004573 198 403 0.004598 198.4 403 0.004586 198.8 404 0.00461 199.2 404 0.004623 199.6 405 0.004623 200 406 0.004635 200.3 406 0.004635 200.7 407 0.004635 201.1 408 0.00466 201.5 409 0.00466 201.9 410 0.004709 202.2 410 0.004722 202.6 411 0.004722 203 412 0.004722 203.4 413 0.004722 203.8 413 0.004722 204.1 414 0.004722 204.5 415 0.004722 204.9 416 0.004722 205.3 417 0.004759 205.7 417 0.004759 206 418 0.004759 206.4 418 0.004771 206.8 419 0.004784 207.2 420 0.004821 207.6 421 0.004858 207.9 421 0.004858 208.3 423 0.00487 208.7 423 0.004883 209.1 424 0.004908 209.5 424 0.00492 209.9 425 0.00492 210.2 426 0.00492 210.6 428 0.004957 211 428 0.004957 211.4 429 0.004969 211.8 430 0.004982 212.1 430 0.005007 212.5 431 0.005019 212.9 431 0.005019 213.3 432 0.005031 213.7 434 0.005031 214 434 0.005056 214.4 435 0.005068 214.8 435 0.005081 215.2 436 0.005081 215.6 437 0.005106 215.9 438 0.005093 216.3 438 0.005093 216.7 439 0.005106 217.1 440 0.005093 217.5 441 0.005081 217.9 442 0.005081 218.2 442 0.005106 218.6 443 0.005155 219 444 0.005205 219.4 445 0.005217 219.8 446 0.005229 220.1 446 0.005229 220.5 447 0.005229 220.9 448 0.005266 221.3 449 0.005279 221.7 449 0.005279 222 450 0.005279 222.4 451 0.005279 222.8 452 0.005279 223.2 453 0.005304 223.6 453 0.005328 223.9 454 0.005328 224.3 455 0.005353 224.7 456 0.005353 225.1 456 0.005378 225.5 458 0.005378 225.8 457 0.005378 226.2 459 0.005403 226.6 459 0.005427 227 460 0.005427 227.4 460 0.00544 227.8 462 0.005477 228.1 462 0.005477 228.5 463 0.005477 228.9 464 0.005489 229.3 464 0.005502 229.7 465 0.005489 230 466 0.005514 230.4 467 0.005539 230.8 467 0.005539 231.2 468 0.005564 231.6 469 0.005576 231.9 470 0.005588 232.3 471 0.005588 232.7 471 0.005588 233.1 472 0.005613 233.5 473 0.005613 233.8 474 0.005625 234.2 474 0.005638 234.6 475 0.005638 235 476 0.00565 235.4 476 0.005675 235.8 478 0.005687 236.1 478 0.0057 236.5 479 0.005724 236.9 480 0.005737 237.3 481 0.005724 237.7 481 0.005737 238 481 0.005762 238.4 483 0.005774 238.8 484 0.005774 239.2 484 0.005799 239.6 485 0.005799 239.9 486 0.005823 240.3 487 0.005836 240.7 487 0.005848 241.1 488 0.005848 241.5 489 0.005873 241.8 490 0.005898 242.2 490 0.005898 242.6 492 0.005898 243 492 0.005922 243.4 492 0.005947 243.8 493 0.005947 244.1 494 0.005972 244.5 495 0.005972 244.9 496 0.005997 245.3 496 0.005997 245.7 497 0.005997 246 498 0.005997 246.4 499 0.005997 246.8 499 0.006009 247.2 500 0.006034 247.6 501 0.006059 247.9 501 0.006071 248.3 503 0.006083 248.7 503 0.006096 249.1 504 0.006108 249.5 505 0.00612 249.8 506 0.006108 250.2 506 0.006108 250.6 506 0.00612 251 508 0.00617 251.4 509 0.006195 251.7 509 0.006207 252.1 510 0.006207 252.5 511 0.006207 252.9 512 0.006207 253.3 512 0.006207 253.7 513 0.006232 254 514 0.006257 254.4 514 0.006269 254.8 515 0.006294 255.2 516 0.006294 255.6 517 0.006281 255.9 517 0.006306 256.3 518 0.006343 256.7 519 0.006343 257.1 519 0.006368 257.5 521 0.006356 257.8 521 0.006356 258.2 522 0.00638 258.6 523 0.006393 259 524 0.006393 259.4 524 0.006393 259.7 525 0.006405 260.1 526 0.00643 260.5 527 0.006442 260.9 528 0.006467 261.3 528 0.006479 261.7 529 0.006492 262 530 0.006492 262.4 530 0.006492 262.8 531 0.006517 263.2 532 0.006529 263.6 533 0.006541 263.9 534 0.006541 264.3 534 0.006554 264.7 535 0.006566 265.1 535 0.006591 265.5 537 0.006591 265.8 537 0.006603 266.2 539 0.006616 266.6 539 0.00664 267 540 0.00664 267.4 541 0.006653 267.7 542 0.006665 268.1 542 0.00669 268.5 542 0.006702 268.9 543 0.006702 269.3 544 0.006715 269.6 545 0.006715 270 546 0.006739 270.4 546 0.006752 270.8 547 0.006776 271.2 548 0.006801 271.6 549 0.006814 271.9 549 0.006838 272.3 550 0.006814 272.7 551 0.006801 273.1 553 0.006814 273.5 553 0.006838 273.8 554 0.006851 274.2 554 0.006888 274.6 555 0.0069 275 556 0.0069 275.4 556 0.0069 275.7 557 0.006913 276.1 558 0.00695 276.5 559 0.00695 276.9 560 0.00695 277.3 560 0.006974 277.6 561 0.007012 278 562 0.007024 278.4 562 0.007049 278.8 564 0.007061 279.2 564 0.007061 279.6 565 0.007061 279.9 566 0.007061 280.3 567 0.007098 280.7 567 0.007086 281.1 568 0.007086 281.5 568 0.007098 281.8 569 0.007111 282.2 570 0.007111 282.6 571 0.007135 283 571 0.00716 283.4 572 0.00716 283.7 574 0.007173 284.1 574 0.007197 284.5 574 0.00721 284.9 576 0.00721 285.3 576 0.007234 285.6 577 0.007259 286 578 0.007259 286.4 578 0.007284 286.8 579 0.007309 287.2 580 0.007296 287.5 581 0.007296 287.9 582 0.007309 288.3 582 0.007321 288.7 583 0.007358 289.1 584 0.007358 289.5 585 0.007371 289.8 585 0.007358 290.2 586 0.007395 290.6 587 0.007408 291 588 0.007408 291.4 589 0.007432 291.7 589 0.007457 292.1 590 0.007457 292.5 592 0.00747 292.9 592 0.00747 293.3 592 0.007482 293.6 593 0.007494 294 593 0.007494 294.4 594 0.007507 294.8 596 0.007519 295.2 596 0.007519 295.5 596 0.007519 295.9 598 0.007531 296.3 599 0.007531 296.7 600 0.007556 297.1 600 0.007593 297.5 601 0.007618 297.8 601 0.007618 298.2 601 0.00763 298.6 603 0.00763 299 603 0.007655 299.4 605 0.00768 299.7 604 0.007668 300.1 606 0.007692 300.5 607 0.007692 300.9 607 0.007717 301.3 607 0.007742 301.6 609 0.007742 302 609 0.007742 302.4 610 0.007754 302.8 610 0.007779 303.2 611 0.007779 303.5 612 0.007779 303.9 613 0.007804 304.3 614 0.007816 304.7 614 0.007841 305.1 615 0.007866 305.4 617 0.007878 305.8 617 0.00789 306.2 617 0.007915 306.6 618 0.007903 307 619 0.00789 307.4 620 0.00789 307.7 621 0.00789 308.1 621 0.007903 308.5 622 0.007952 308.9 623 0.007952 309.3 624 0.007977 309.6 625 0.007989 310 626 0.008002 310.4 626 0.008002 310.8 627 0.008002 311.2 628 0.008039 311.5 628 0.008064 311.9 629 0.008101 312.3 630 0.008113 312.7 631 0.008113 313.1 631 0.008126 313.4 632 0.008126 313.8 633 0.008126 314.2 634 0.008163 314.6 634 0.008175 315 635 0.008175 315.4 636 0.008187 315.7 637 0.0082 316.1 637 0.008212 316.5 639 0.008225 316.9 639 0.008225 317.3 640 0.008225 317.6 640 0.008249 318 642 0.008262 318.4 642 0.008274 318.8 643 0.008299 319.2 643 0.008324 319.5 644 0.008336 319.9 645 0.008336 320.3 646 0.008373 320.7 646 0.008385 321.1 647 0.008385 321.4 648 0.008385 321.8 650 0.008398 322.2 650 0.008423 322.6 650 0.008423 323 651 0.008435 323.4 652 0.008447 323.7 653 0.008447 324.1 654 0.008472 324.5 654 0.008472 324.9 655 0.008485 325.3 656 0.008509 325.6 657 0.008522 326 657 0.008534 326.4 658 0.008534 326.8 659 0.008534 327.2 660 0.008534 327.5 660 0.008571 327.9 661 0.008584 328.3 662 0.008584 328.7 663 0.008596 329.1 664 0.008596 329.4 664 0.008621 329.8 665 0.00867 330.2 666 0.008683 330.6 667 0.008683 331 668 0.008695 331.3 668 0.008695 331.7 669 0.008707 332.1 669 0.008732 332.5 670 0.008744 332.9 671 0.008757 333.3 671 0.008782 333.6 673 0.008794 334 673 0.008794 334.4 674 0.008794 334.8 675 0.008819 335.2 675 0.008806 335.5 676 0.008843 335.9 677 0.008843 336.3 678 0.008843 336.7 679 0.008843 337.1 679 0.008843 337.4 680 0.008819 337.8 681 0.008843 338.2 681 0.008893 338.6 682 0.00893 339 683 0.008967 339.3 684 0.00898 339.7 685 0.008992 340.1 685 0.008992 340.5 686 0.008992 340.9 687 0.008992 341.3 688 0.009029 341.6 689 0.009041 342 689 0.009041 342.4 690 0.009054 342.8 691 0.009066 343.2 692 0.009091 343.5 693 0.009103 343.9 693 0.009116 344.3 694 0.00914 344.7 694 0.009153 345.1 695 0.009153 345.4 696 0.009165 345.8 696 0.009165 346.2 697 0.009178 346.6 697 0.00919 347 699 0.00919 347.3 700 0.009215 347.7 700 0.00924 348.1 700 0.009252 348.5 701 0.009264 348.9 702 0.009264 349.2 703 0.009264 349.6 703 0.009252 350 704 0.009289 350.4 705 0.009301 350.8 706 0.009314 351.2 707 0.009301 351.5 707 0.009301 351.9 708 0.009326 352.3 709 0.009339 352.7 709 0.009339 353.1 711 0.009326 353.4 711 0.009314 353.8 712 0.009339 354.2 712 0.009351 354.6 714 0.009363 355 714 0.009363 355.3 715 0.009376 355.7 715 0.009376 356.1 716 0.009388 356.5 717 0.0094 356.9 718 0.0094 357.2 718 0.009438 357.6 719 0.009438 358 720 0.009438 358.4 721 0.009438 358.8 721 0.009438 359.2 721 0.00945 359.5 723 0.009462 359.9 724 0.009475 360.3 725 0.009462 360.7 726 0.009475 361.1 727 0.009512 361.4 728 0.009487 361.8 728 0.009512 362.2 729 0.009512 362.6 730 0.009512 363 730 0.009512 363.3 731 0.009512 363.7 732 0.009524 364.1 732 0.009549 364.5 733 0.009561 364.9 734 0.009561 365.2 735 0.009561 365.6 736 0.009561 366 736 0.009561 366.4 737 0.009574 366.8 738 0.009586 367.1 738 0.009586 367.5 739 0.009586 367.9 739 0.009586 368.3 740 0.009574 368.7 741 0.009574 369.1 742 0.009561 369.4 743 0.009549 369.8 743 0.009561 370.2 744 0.009574 370.6 745 0.009561 371 746 0.009561 371.3 747 0.009537 371.7 748 0.009524 372.1 749 0.009512 372.5 750 0.009512 372.9 750 0.009487 373.2 752 0.009487 373.6 752 0.009462 374 753 0.009438 374.4 753 0.009413 374.8 753 0.009388 375.1 754 0.009351 375.5 755 0.009301 375.9 756 0.009277 376.3 757 0.00924 376.7 757 0.009202 377.1 758 0.009178 377.4 759 0.00914 377.8 760 0.009091 378.2 761 0.009029 378.6 761 0.00898 379 762 0.008942 379.3 763 0.008893 379.7 764 0.008819 380.1 764 0.008769 380.5 765 0.008707 380.9 766 0.008645 381.2 767 0.008571 381.6 768 0.008497 382 768 0.008423 382.4 769 0.008348 382.8 771 0.008274 383.1 771 0.0082 383.5 771 0.008138 383.9 772 0.008064 384.3 774 0.007989 384.7 775 0.007915 385 775 0.007853 385.4 776 0.007791 385.8 778 0.00773 386.2 779 0.007668 386.6 779 0.007618 387 780 0.007593 387.3 781 0.007556 387.7 782 0.007544 388.1 783 0.007531 388.5 784 0.007507 388.9 785 0.007507 389.2 786 0.007494 389.6 786 0.007494 390 787 0.007494 390.4 788 0.007507 390.8 789 0.007531 391.1 789 0.007569 391.5 789 0.007569 391.9 790 0.007593 392.3 792 0.007618 392.7 792 0.007606 393 792 0.007606 393.4 793 0.00763 393.8 793 0.00763 394.2 793 0.007655 394.6 794 0.007643 395 796 0.007655 395.3 796 0.007692 395.7 796 0.007705 396.1 798 0.007742 396.5 799 0.007767 396.9 799 0.007791 397.2 800 0.007791 397.6 800 0.007841 398 801 0.007853 398.4 801 0.007853 398.8 801 0.007878 399.1 801 0.007866 399.5 801 0.007853 399.9 801 0.007866 400.3 801 0.007903 400.7 803 0.007915 401 803 0.00794 401.4 804 0.007977 401.8 804 0.008014 402.2 805 0.008039 402.6 806 0.008051 402.9 807 0.008076 403.3 807 0.008088 403.7 808 0.008113 404.1 809 0.008126 404.5 809 0.008113 404.9 811 0.008101 405.2 811 0.008126 405.6 811 0.008163 406 812 0.008225 406.4 814 0.008286 406.8 814 0.008299 407.1 815 0.008311 407.5 816 0.008336 407.9 817 0.008348 408.3 818 0.008385 408.7 818 0.00841 409 818 0.008398 409.4 819 0.008435 409.8 820 0.008472 410.2 821 0.008485 410.6 821 0.008497 410.9 822 0.008497 411.3 824 0.008534 411.7 824 0.008546 412.1 825 0.008571 412.5 826 0.008608 412.9 826 0.008608 413.2 828 0.008608 413.6 828 0.008658 414 829 0.008683 414.4 829 0.008683 414.8 830 0.008695 415.1 831 0.008732 415.5 832 0.008769 415.9 832 0.008782 416.3 833 0.008794 416.7 834 0.008819 417 836 0.008819 417.4 836 0.008806 417.8 836 0.008843 418.2 837 0.008881 418.6 838 0.008893 418.9 839 0.008918 419.3 839 0.00893 419.7 840 0.008967 420.1 842 0.008942 420.5 842 0.00898 420.9 843 0.008992 421.2 843 0.009004 421.6 844 0.009004 422 845 0.009017 422.4 846 0.009041 422.8 847 0.009041 423.1 847 0.009091 423.5 848 0.009091 423.9 849 0.00914 424.3 850 0.009153 424.7 850 0.009178 425 851 0.00919 425.4 852 0.00919 425.8 853 0.009215 426.2 854 0.009227 426.6 854 0.009227 426.9 855 0.009252 427.3 856 0.009277 427.7 857 0.009277 428.1 857 0.009277 428.5 858 0.009326 428.8 859 0.009339 429.2 860 0.009363 429.6 861 0.009339 430 861 0.009326 430.4 862 0.009351 430.8 862 0.009376 431.1 864 0.009388 431.5 864 0.0094 431.9 865 0.009388 432.3 865 0.009388 432.7 867 0.009376 433 868 0.009376 433.4 868 0.009388 433.8 869 0.009388 434.2 870 0.009438 434.6 871 0.00945 434.9 872 0.009499 435.3 873 0.009499 435.7 875 0.009487 436.1 876 0.009512 436.5 877 0.009475 436.8 877 0.009438 437.2 877 0.009462 437.6 876 0.00945 438 877 0.009413 438.4 877 0.009413 438.8 878 0.009388 439.1 878 0.0094 439.5 878 0.009413 439.9 879 0.009425 440.3 879 0.009425 440.7 880 0.009438 441 881 0.009462 441.4 882 0.009512 441.8 883 0.009512 442.2 884 0.009524 442.6 885 0.009561 442.9 886 0.009574 443.3 887 0.009574 443.7 888 0.009586 444.1 889 0.009636 444.5 889 0.009648 444.8 890 0.009673 445.2 891 0.009697 445.6 893 0.00971 446 893 0.009697 446.4 893 0.00971 446.7 894 0.009735 447.1 895 0.009722 447.5 897 0.009747 447.9 897 0.009759 448.3 898 0.009759 448.7 898 0.009735 449 899 0.009759 449.4 900 0.009759 449.8 900 0.009796 450.2 900 0.009821 450.6 901 0.009871 450.9 901 0.009908 451.3 901 0.009908 451.7 901 0.009933 452.1 901 0.00992 452.5 901 0.009945 452.8 901 0.009933 453.2 903 0.009945 453.6 904 0.00997 454 904 0.009995 454.4 906 0.01002 454.7 907 0.01003 455.1 909 0.01006 455.5 911 0.01009 455.9 912 0.01013 456.3 913 0.01018 456.7 915 0.0102 457 915 0.01025 457.4 916 0.01027 457.8 917 0.01028 458.2 918 0.01032 458.6 918 0.01033 458.9 919 0.01037 459.3 920 0.01038 459.7 921 0.01039 460.1 922 0.01043 460.5 922 0.01043 460.8 923 0.01044 461.2 924 0.01046 461.6 924 0.01049 462 925 0.01051 462.4 925 0.0105 462.7 926 0.01049 463.1 928 0.01054 463.5 928 0.01059 463.9 929 0.01061 464.3 929 0.01063 464.6 930 0.01064 465 931 0.01065 465.4 932 0.01068 465.8 932 0.01068 466.2 934 0.01069 466.6 934 0.0107 466.9 934 0.01072 467.3 936 0.01074 467.7 936 0.01076 468.1 937 0.01077 468.5 937 0.01081 468.8 939 0.01084 469.2 939 0.01084 469.6 940 0.01086 470 940 0.0109 470.4 942 0.01096 470.7 943 0.01101 471.1 943 0.01103 471.5 944 0.01105 471.9 944 0.01106 472.3 945 0.01106 472.6 947 0.01108 473 947 0.0111 473.4 948 0.01112 473.8 948 0.01115 474.2 950 0.01116 474.6 950 0.01116 474.9 950 0.01117 475.3 952 0.0112 475.7 953 0.01121 476.1 953 0.01123 476.5 954 0.01127 476.8 954 0.01128 477.2 956 0.01132 477.6 956 0.01134 478 957 0.01134 478.4 957 0.01134 478.7 958 0.01137 479.1 959 0.01136 479.5 960 0.01138 479.9 961 0.01139 480.3 961 0.01143 480.6 962 0.01144 481 963 0.01147 481.4 964 0.01149 481.8 965 0.01152 482.2 965 0.01154 482.5 966 0.01155 482.9 967 0.01153 483.3 968 0.01158 483.7 968 0.01163 484.1 969 0.01165 484.5 969 0.01165 484.8 971 0.01168 485.2 972 0.0117 485.6 972 0.01171 486 973 0.01171 486.4 974 0.01174 486.7 975 0.01178 487.1 975 0.01179 487.5 975 0.01181 487.9 976 0.01181 488.3 978 0.01185 488.6 978 0.01185 489 979 0.01188 489.4 980 0.01191 489.8 981 0.01193 490.2 982 0.01195 490.5 983 0.01195 490.9 983 0.01197 491.3 984 0.01201 491.7 984 0.01202 492.1 985 0.01205 492.5 986 0.01206 492.8 986 0.0121 493.2 987 0.01211 493.6 988 0.01211 494 989 0.01215 494.4 990 0.01216 494.7 990 0.01216 495.1 991 0.0122 495.5 992 0.01221 495.9 993 0.01222 496.3 993 0.01226 496.6 994 0.01227 497 995 0.01231 497.4 996 0.01232 497.8 997 0.01233 498.2 997 0.01235 498.5 998 0.01237 498.9 999 0.01238 499.3 1000 0.0124 499.7 1000 0.01242 500.1 1001 0.01245 500.5 1001 0.01247 500.8 1002 0.01249 501.2 1003 0.01253 501.6 1003 0.01253 502 1004 0.01253 502.4 1005 0.01257 502.7 1006 0.01258 503.1 1007 0.01263 503.5 1008 0.01266 503.9 1008 0.01267 504.3 1009 0.01268 504.6 1009 0.01268 505 1011 0.01268 505.4 1011 0.01269 505.8 1011 0.01269 506.2 1012 0.01272 506.5 1014 0.01273 506.9 1014 0.01275 507.3 1015 0.01277 507.7 1015 0.01278 508.1 1017 0.0128 508.4 1017 0.01282 508.8 1018 0.01282 509.2 1018 0.01283 509.6 1019 0.01285 510 1019 0.0129 510.4 1021 0.0129 510.7 1022 0.01294 511.1 1022 0.01294 511.5 1024 0.01293 511.9 1024 0.01295 512.3 1025 0.01295 512.6 1025 0.01297 513 1026 0.01297 513.4 1027 0.01297 513.8 1028 0.01297 514.2 1029 0.01297 514.5 1030 0.01297 514.9 1030 0.01297 515.3 1031 0.013 515.7 1032 0.01301 516.1 1033 0.01304 516.4 1033 0.01306 516.8 1034 0.01306 517.2 1035 0.01308 517.6 1036 0.0131 518 1036 0.0131 518.4 1037 0.01311 518.7 1037 0.0131 519.1 1039 0.01313 519.5 1039 0.01313 519.9 1040 0.01315 520.3 1040 0.01318 520.6 1042 0.01321 521 1042 0.01322 521.4 1043 0.01325 521.8 1043 0.01326 522.2 1044 0.01327 522.5 1045 0.01331 522.9 1047 0.01332 523.3 1047 0.01332 523.7 1048 0.01335 524.1 1049 0.01337 524.4 1050 0.01337 524.8 1051 0.0134 525.2 1051 0.01342 525.6 1052 0.01344 526 1053 0.01344 526.3 1053 0.01345 526.7 1054 0.01347 527.1 1054 0.01348 527.5 1055 0.01352 527.9 1056 0.01353 528.3 1057 0.01355 528.6 1058 0.01358 529 1058 0.0136 529.4 1059 0.0136 529.8 1060 0.0136 530.2 1061 0.0136 530.5 1061 0.01363 530.9 1062 0.01367 531.3 1063 0.01368 531.7 1064 0.01372 532.1 1065 0.01373 532.4 1065 0.01373 532.8 1066 0.01377 533.2 1067 0.01378 533.6 1068 0.01379 534 1068 0.01381 534.3 1069 0.01383 534.7 1069 0.01384 535.1 1071 0.01386 535.5 1072 0.01388 535.9 1072 0.01389 536.3 1073 0.01394 536.6 1074 0.01398 537 1074 0.01399 537.4 1075 0.01399 537.8 1076 0.01399 538.2 1076 0.014 538.5 1078 0.01403 538.9 1078 0.01404 539.3 1079 0.01404 539.7 1079 0.01408 540.1 1080 0.01409 540.4 1081 0.01412 540.8 1082 0.01413 541.2 1083 0.01414 541.6 1083 0.01418 542 1084 0.01419 542.3 1086 0.01423 542.7 1086 0.01424 543.1 1086 0.01425 543.5 1087 0.01428 543.9 1088 0.01429 544.2 1089 0.01431 544.6 1090 0.01434 545 1090 0.01434 545.4 1090 0.01435 545.8 1092 0.01438 546.2 1093 0.01439 546.5 1094 0.01441 546.9 1094 0.01444 547.3 1095 0.01446 547.7 1096 0.01449 548.1 1097 0.01449 548.4 1097 0.01451 548.8 1098 0.01454 549.2 1099 0.01454 549.6 1100 0.01455 550 1101 0.01456 550.3 1101 0.01459 550.7 1102 0.0146 551.1 1103 0.01462 551.5 1104 0.01466 551.9 1104 0.01469 552.2 1105 0.01471 552.6 1106 0.01473 553 1106 0.01475 553.4 1107 0.01478 553.8 1108 0.01477 554.2 1109 0.0148 554.5 1109 0.01482 554.9 1111 0.01482 555.3 1111 0.01486 555.7 1112 0.01487 556.1 1112 0.0149 556.4 1114 0.01491 556.8 1114 0.01491 557.2 1115 0.01493 557.6 1115 0.01498 558 1117 0.01499 558.3 1117 0.01503 558.7 1119 0.01504 559.1 1119 0.01507 559.5 1119 0.01509 559.9 1119 0.01508 560.2 1121 0.01511 560.6 1122 0.01511 561 1122 0.01512 561.4 1123 0.01512 561.8 1123 0.01512 562.1 1125 0.01513 562.5 1125 0.01516 562.9 1126 0.01518 563.3 1127 0.01522 563.7 1128 0.01524 564.1 1129 0.01527 564.4 1129 0.01529 564.8 1129 0.01532 565.2 1131 0.01533 565.6 1131 0.01535 566 1133 0.01538 566.3 1133 0.0154 566.7 1134 0.0154 567.1 1134 0.01542 567.5 1136 0.01545 567.9 1136 0.01547 568.2 1136 0.01547 568.6 1137 0.01549 569 1139 0.01553 569.4 1140 0.01555 569.8 1140 0.01558 570.1 1140 0.0156 570.5 1142 0.01563 570.9 1143 0.01564 571.3 1143 0.01564 571.7 1144 0.01565 572.1 1144 0.0157 572.4 1145 0.01571 572.8 1147 0.01576 573.2 1147 0.01577 573.6 1148 0.01577 574 1148 0.01577 574.3 1149 0.0158 574.7 1150 0.01582 575.1 1151 0.01585 575.5 1151 0.01586 575.9 1152 0.0159 576.2 1153 0.01591 576.6 1154 0.01591 577 1154 0.01595 577.4 1155 0.01597 577.8 1156 0.01599 578.1 1157 0.01599 578.5 1158 0.01601 578.9 1158 0.01601 579.3 1159 0.01602 579.7 1160 0.01603 580 1161 0.01606 580.4 1162 0.0161 580.8 1162 0.0161 581.2 1162 0.01612 581.6 1164 0.01612 582 1165 0.01615 582.3 1165 0.01617 582.7 1166 0.01617 583.1 1167 0.0162 583.5 1167 0.01622 583.9 1168 0.01623 584.2 1169 0.01623 584.6 1169 0.01626 585 1170 0.01628 585.4 1172 0.01629 585.8 1172 0.01632 586.1 1173 0.01633 586.5 1173 0.01634 586.9 1174 0.01634 587.3 1175 0.01638 587.7 1176 0.01639 588 1177 0.01642 588.4 1178 0.01647 588.8 1178 0.01649 589.2 1179 0.01649 589.6 1179 0.01649 590 1180 0.01652 590.3 1181 0.01653 590.7 1181 0.01653 591.1 1183 0.01658 591.5 1183 0.0166 591.9 1184 0.01662 592.2 1185 0.01664 592.6 1186 0.01668 593 1187 0.0167 593.4 1187 0.01672 593.8 1188 0.01673 594.1 1189 0.01674 594.5 1190 0.01673 594.9 1190 0.01674 595.3 1190 0.01678 595.7 1192 0.01679 596 1193 0.0168 596.4 1194 0.01683 596.8 1194 0.01684 597.2 1194 0.01686 597.6 1196 0.01686 598 1197 0.01689 598.3 1197 0.01691 598.7 1198 0.01693 599.1 1199 0.01695 599.5 1199 0.01695 599.9 1200 0.01696 600.2 1200 0.01699 600.6 1200 0.017 601 1200 0.017 601.4 1200 0.01701 601.8 1200 0.01701 602.1 1200 0.017 602.5 1200 0.017 602.9 1200 0.01696 603.3 1199 0.01696 603.7 1200 0.01695 604 1199 0.01695 604.4 1200 0.01695 604.8 1200 0.01695 605.2 1199 0.01694 605.6 1199 0.01694 605.9 1199 0.01694 606.3 1199 0.01695 606.7 1199 0.01693 607.1 1199 0.01691 607.5 1199 0.01694 607.9 1199 0.01694 608.2 1199 0.01691 608.6 1199 0.01693 609 1199 0.01691 609.4 1200 0.01686 609.8 1199 0.01684 610.1 1199 0.01686 610.5 1200 0.01693 610.9 1200 0.01691 611.3 1199 0.0169 611.7 1199 0.0169 612 1199 0.0169 612.4 1199 0.01689 612.8 1199 0.0169 613.2 1199 0.01689 613.6 1199 0.0169 613.9 1199 0.01686 614.3 1199 0.01684 614.7 1200 0.01681 615.1 1199 0.01681 615.5 1199 0.01681 615.9 1199 0.01684 616.2 1199 0.01683 616.6 1200 0.01681 617 1199 0.01681 617.4 1200 0.0168 617.8 1199 0.01681 618.1 1199 0.01681 618.5 1199 0.0168 618.9 1200 0.0168 619.3 1199 0.0168 619.7 1199 0.01679 620 1199 0.0168 620.4 1199 0.0168 620.8 1200 0.0168 621.2 1199 0.0168 621.6 1199 0.0168 621.9 1199 0.0168 622.3 1199 0.0168 622.7 1199 0.01679 623.1 1199 0.01676 623.5 1199 0.01676 623.8 1200 0.01675 624.2 1199 0.01675 624.6 1200 0.01676 625 1200 0.01676 625.4 1199 0.01678 625.8 1199 0.01676 626.1 1199 0.01674 626.5 1199 0.01673 626.9 1199 0.01672 627.3 1200 0.0167 627.7 1199 0.01669 628 1199 0.01672 628.4 1199 0.0167 628.8 1199 0.0167 629.2 1199 0.01672 629.6 1200 0.0167 629.9 1199 0.0167 630.3 1199 0.01672 630.7 1199 0.0167 631.1 1199 0.01669 631.5 1199 0.01669 631.8 1200 0.01668 632.2 1200 0.01665 632.6 1199 0.01665 633 1199 0.01668 633.4 1199 0.01669 633.8 1200 0.01667 634.1 1199 0.01668 634.5 1199 0.01667 634.9 1199 0.01667 635.3 1199 0.01663 635.7 1199 0.01663 636 1199 0.01662 636.4 1199 0.0166 636.8 1199 0.01659 637.2 1200 0.01657 637.6 1199 0.01655 637.9 1200 0.0166 638.3 1199 0.01663 638.7 1199 0.01663 639.1 1200 0.0166 639.5 1199 0.0166 639.8 1199 0.0166 640.2 1200 0.0166 640.6 1199 0.01662 641 1200 0.0166 641.4 1199 0.01659 641.7 1199 0.01659 642.1 1199 0.01659 642.5 1199 0.01657 642.9 1199 0.01655 643.3 1199 0.01654 643.7 1199 0.01654 644 1200 0.01654 644.4 1200 0.01654 644.8 1200 0.01654 645.2 1200 0.01655 645.6 1199 0.01652 645.9 1199 0.0165 646.3 1199 0.01652 646.7 1199 0.0165 647.1 1200 0.0165 647.5 1199 0.0165 647.8 1199 0.01649 648.2 1199 0.01649 648.6 1199 0.01646 649 1199 0.01647 649.4 1199 0.01648 649.7 1199 0.0165 650.1 1199 0.01652 650.5 1199 0.0165 650.9 1200 0.01649 651.3 1199 0.01649 651.7 1200 0.0165 652 1200 0.01648 652.4 1199 0.01646 652.8 1199 0.01644 653.2 1200 0.01643 653.6 1199 0.01644 653.9 1200 0.01643 654.3 1199 0.01643 654.7 1199 0.01646 655.1 1199 0.01644 655.5 1200 0.01643 655.8 1199 0.01642 656.2 1199 0.01642 656.6 1199 0.01641 657 1199 0.01642 657.4 1199 0.01642 657.7 1199 0.01642 658.1 1200 0.01642 658.5 1199 0.01642 658.9 1200 0.01641 659.3 1199 0.01639 659.6 1200 0.01637 660 1200 0.01637 660.4 1199 0.01638 660.8 1199 0.01639 661.2 1199 0.01639 661.6 1200 0.01637 661.9 1199 0.01637 662.3 1199 0.01638 662.7 1200 0.01636 663.1 1199 0.01634 663.5 1200 0.01634 663.8 1199 0.01633 664.2 1199 0.01633 664.6 1199 0.01633 665 1200 0.01634 665.4 1199 0.01632 665.7 1200 0.01631 666.1 1199 0.01629 666.5 1199 0.01629 666.9 1199 0.01627 667.3 1199 0.01624 667.6 1199 0.01626 668 1199 0.01627 668.4 1199 0.01628 668.8 1200 0.01631 669.2 1199 0.01629 669.6 1199 0.01628 669.9 1199 0.01631 670.3 1199 0.01632 670.7 1200 0.01629 671.1 1199 0.01627 671.5 1199 0.01624 671.8 1199 0.01627 672.2 1199 0.01627 672.6 1199 0.01629 673 1199 0.01627 673.4 1199 0.01624 673.7 1200 0.01624 674.1 1200 0.01626 674.5 1200 0.01627 674.9 1199 0.01626 675.3 1199 0.01628 675.6 1200 0.01628 676 1200 0.01626 676.4 1199 0.01626 676.8 1199 0.01626 677.2 1200 0.01624 677.5 1199 0.01626 677.9 1200 0.01622 678.3 1199 0.01621 678.7 1200 0.01617 679.1 1199 0.01617 679.5 1200 0.01613 679.8 1200 0.01617 680.2 1199 0.01621 680.6 1200 0.01624 681 1199 0.01621 681.4 1199 0.01618 681.7 1200 0.01616 682.1 1199 0.01615 682.5 1199 0.01616 682.9 1199 0.01615 683.3 1199 0.01616 683.6 1199 0.01616 684 1199 0.01613 684.4 1200 0.01612 684.8 1199 0.01611 685.2 1199 0.01611 685.5 1199 0.01612 685.9 1199 0.01613 686.3 1199 0.01615 686.7 1199 0.01615 687.1 1199 0.01616 687.5 1200 0.01615 687.8 1199 0.01612 688.2 1200 0.01611 688.6 1199 0.0161 689 1199 0.0161 689.4 1199 0.01611 689.7 1200 0.01611 690.1 1199 0.0161 690.5 1199 0.01611 690.9 1199 0.0161 691.3 1199 0.0161 691.6 1200 0.0161 692 1199 0.01611 692.4 1199 0.01611 692.8 1199 0.0161 693.2 1200 0.0161 693.5 1199 0.0161 693.9 1199 0.01611 694.3 1199 0.0161 694.7 1200 0.0161 695.1 1199 0.01611 695.5 1199 0.0161 695.8 1200 0.0161 696.2 1199 0.01612 696.6 1199 0.0161 697 1199 0.01607 697.4 1199 0.01607 697.7 1199 0.01611 698.1 1199 0.0161 698.5 1199 0.01601 698.9 1199 0.01602 699.3 1199 0.0161 699.6 1199 0.0161 700 1199 0.0161 700.4 1200 0.01608 700.8 1200 0.01608 701.2 1199 0.01608 701.5 1199 0.0161 701.9 1199 0.01608 702.3 1199 0.0161 702.7 1199 0.01607 703.1 1200 0.01608 703.4 1199 0.0161 703.8 1199 0.01608 704.2 1199 0.01608 704.6 1199 0.01607 705 1199 0.01608 705.4 1199 0.01607 705.7 1199 0.01605 706.1 1200 0.01607 706.5 1199 0.01607 706.9 1199 0.01607 707.3 1199 0.01608 707.6 1199 0.01607 708 1200 0.01607 708.4 1200 0.01607 708.8 1199 0.01607 709.2 1199 0.01606 709.5 1199 0.01606 709.9 1200 0.01607 710.3 1199 0.01606 710.7 1199 0.01607 711.1 1200 0.01606 711.4 1199 0.01605 711.8 1200 0.01607 712.2 1199 0.01605 712.6 1199 0.01606 713 1199 0.01605 713.4 1199 0.01606 713.7 1199 0.01602 714.1 1199 0.01606 714.5 1199 0.01605 714.9 1199 0.01602 715.3 1200 0.016 715.6 1199 0.01601 716 1199 0.01597 716.4 1199 0.01597 716.8 1199 0.01599 717.2 1200 0.01596 717.5 1199 0.01599 717.9 1199 0.01602 718.3 1199 0.01606 718.7 1199 0.01606 719.1 1199 0.01606 719.4 1199 0.01603 719.8 1199 0.01606 720.2 1199 0.01606 720.6 1199 0.01605 721 1199 0.01605 721.3 1200 0.01603 721.7 1199 0.01602 722.1 1199 0.01601 722.5 1199 0.016 722.9 1199 0.01601 723.3 1199 0.01601 723.6 1199 0.01602 724 1199 0.01602 724.4 1199 0.01602 724.8 1200 0.01603 725.2 1199 0.01602 725.5 1199 0.01605 725.9 1199 0.01602 726.3 1200 0.01603 726.7 1199 0.01601 727.1 1199 0.01602 727.4 1199 0.01601 727.8 1199 0.01602 728.2 1199 0.01602 728.6 1199 0.01602 729 1199 0.01602 729.3 1199 0.016 729.7 1199 0.016 730.1 1199 0.01602 730.5 1199 0.016 730.9 1199 0.01601 731.3 1199 0.01602 731.6 1199 0.01601 732 1199 0.016 732.4 1199 0.01601 732.8 1199 0.01603 733.2 1199 0.01602 733.5 1200 0.01601 733.9 1199 0.016 734.3 1200 0.016 734.7 1199 0.01599 735.1 1199 0.016 735.4 1199 0.016 735.8 1199 0.01599 736.2 1199 0.01597 736.6 1199 0.01599 737 1199 0.01599 737.3 1199 0.01597 737.7 1199 0.01601 738.1 1199 0.01601 738.5 1199 0.01602 738.9 1199 0.016 739.2 1199 0.01599 739.6 1200 0.016 740 1199 0.01599 740.4 1199 0.01597 740.8 1199 0.01599 741.2 1199 0.01597 741.5 1200 0.01597 741.9 1199 0.01597 742.3 1199 0.01599 742.7 1199 0.01594 743.1 1199 0.0159 743.4 1199 0.01592 743.8 1199 0.0159 744.2 1199 0.01591 744.6 1199 0.01592 745 1199 0.01595 745.3 1200 0.01591 745.7 1199 0.01594 746.1 1200 0.01597 746.5 1199 0.01596 746.9 1200 0.01599 747.2 1199 0.01597 747.6 1199 0.01597 748 1200 0.016 748.4 1199 0.01597 748.8 1199 0.01599 749.2 1199 0.01595 749.5 1199 0.01599 749.9 1199 0.01597 750.3 1199 0.01597 750.7 1199 0.01594 751.1 1199 0.01596 751.4 1199 0.01597 751.8 1199 0.01594 752.2 1200 0.01596 752.6 1199 0.01596 753 1199 0.01597 753.3 1199 0.01599 753.7 1199 0.01599 754.1 1199 0.01597 754.5 1199 0.01597 754.9 1199 0.01597 755.2 1199 0.01596 755.6 1199 0.01597 756 1199 0.01597 756.4 1199 0.01599 756.8 1199 0.01597 757.1 1199 0.01592 757.5 1199 0.01594 757.9 1199 0.01597 758.3 1199 0.01601 758.7 1199 0.01597 759.1 1200 0.01596 759.4 1199 0.01599 759.8 1199 0.01597 760.2 1199 0.01599 760.6 1200 0.01596 761 1199 0.01596 761.3 1199 0.01597 761.7 1199 0.01596 762.1 1199 0.01597 762.5 1200 0.01601 762.9 1199 0.01601 763.2 1199 0.016 763.6 1199 0.01591 764 1200 0.01594 764.4 1199 0.0159 764.8 1199 0.0159 765.1 1199 0.01594 765.5 1199 0.01589 765.9 1199 0.01592 766.3 1199 0.01597 766.7 1199 0.01592 767.1 1199 0.01594 767.4 1199 0.01599 767.8 1199 0.01597 768.2 1199 0.01592 768.6 1199 0.01591 769 1199 0.01596 769.3 1199 0.01597 769.7 1199 0.01597 770.1 1199 0.01596 770.5 1199 0.01591 770.9 1199 0.0159 771.2 1199 0.01591 771.6 1200 0.01592 772 1199 0.01592 772.4 1199 0.01596 772.8 1199 0.01594 773.1 1199 0.0159 773.5 1199 0.01594 773.9 1199 0.01591 774.3 1199 0.01595 774.7 1199 0.01594 775.1 1199 0.01594 775.4 1199 0.01595 775.8 1199 0.01596 776.2 1199 0.01596 776.6 1199 0.01592 777 1200 0.0159 777.3 1199 0.01591 777.7 1199 0.01594 778.1 1199 0.01594 778.5 1199 0.0159 778.9 1199 0.01585 779.2 1199 0.01592 779.6 1199 0.01596 780 1199 0.0159 780.4 1199 0.0159 780.8 1199 0.01594 781.1 1199 0.01587 781.5 1199 0.01594 781.9 1200 0.01592 782.3 1199 0.01587 782.7 1200 0.01595 783 1199 0.01587 783.4 1199 0.01597 783.8 1199 0.0159 784.2 1199 0.01592 784.6 1199 0.01587 785 1199 0.01594 785.3 1199 0.01589 785.7 1199 0.01597 786.1 1200 0.01595 786.5 1199 0.01599 786.9 1199 0.01602 787.2 1199 0.01596 787.6 1199 0.01595 788 1199 0.0159 788.4 1199 0.01585 788.8 1199 0.01591 789.1 1199 0.01592 789.5 1199 0.01592 789.9 1199 0.01594 790.3 1199 0.01592 790.7 1199 0.01591 791 1199 0.01592 791.4 1199 0.01592 791.8 1199 0.01591 792.2 1199 0.01592 792.6 1200 0.01597 793 1199 0.01591 793.3 1199 0.01585 793.7 1199 0.01596 794.1 1199 0.01594 794.5 1199 0.01585 794.9 1199 0.01595 795.2 1200 0.01581 795.6 1199 0.01591 796 1199 0.0159 796.4 1199 0.0159 796.8 1199 0.01594 797.1 1200 0.01592 797.5 1199 0.01597 797.9 1199 0.01594 798.3 1199 0.01594 798.7 1199 0.01597 799 1199 0.01585 799.4 1199 0.016 799.8 1199 0.01581 800.2 1199 0.01595 800.6 1199 0.01602 800.9 1199 0.0158 801.3 1199 0.01599 801.7 1199 0.01601 802.1 1199 0.01577 802.5 1199 0.01586 802.9 1199 0.01605 803.2 1200 0.01596 803.6 1199 0.01573 804 1199 0.01579 804.4 1199 0.01606 804.8 1199 0.01618 805.1 1200 0.01612 805.5 1199 0.01592 805.9 1199 0.01571 806.3 1199 0.01564 806.7 1199 0.01571 807 1199 0.01585 807.4 1199 0.01597 807.8 1199 0.01605 808.2 1199 0.01612 808.6 1199 0.01612 808.9 1199 0.01611 809.3 1199 0.01603 809.7 1199 0.01596 810.1 1199 0.01586 810.5 1200 0.0157 810.9 1199 0.01558 811.2 1199 0.01553 811.6 1199 0.01564 812 1199 0.01587 812.4 1199 0.0161 812.8 1199 0.0161 813.1 1199 0.01584 813.5 1199 0.01566 813.9 1199 0.01582 814.3 1199 0.01606 814.7 1199 0.01596 815 1199 0.01571 815.4 1199 0.01584 815.8 1199 0.01601 816.2 1199 0.0158 816.6 1199 0.01582 816.9 1199 0.01601 817.3 1200 0.01581 817.7 1199 0.01587 818.1 1199 0.01597 818.5 1199 0.01577 818.8 1199 0.01597 819.2 1199 0.01582 819.6 1199 0.01587 820 1199 0.01586 820.4 1199 0.01586 820.8 1199 0.01587 821.1 1199 0.01587 821.5 1200 0.01586 821.9 1200 0.01591 822.3 1199 0.01585 822.7 1199 0.01594 823 1199 0.01582 823.4 1199 0.0159 823.8 1199 0.01589 824.2 1199 0.01582 824.6 1199 0.01591 824.9 1199 0.01591 825.3 1199 0.01587 825.7 1199 0.01595 826.1 1199 0.01592 826.5 1199 0.01585 826.8 1199 0.0158 827.2 1199 0.01585 827.6 1199 0.01589 828 1199 0.01585 828.4 1199 0.01581 828.8 1199 0.01587 829.1 1199 0.01587 829.5 1199 0.01584 829.9 1199 0.01585 830.3 1199 0.01587 830.7 1199 0.01582 831 1199 0.01585 831.4 1200 0.01586 831.8 1199 0.0158 832.2 1199 0.01587 832.6 1199 0.01582 832.9 1199 0.01587 833.3 1199 0.01582 833.7 1199 0.01585 834.1 1199 0.01582 834.5 1199 0.01586 834.8 1199 0.01584 835.2 1199 0.01587 835.6 1199 0.01581 836 1199 0.01589 836.4 1200 0.01585 836.7 1199 0.01584 837.1 1199 0.0159 837.5 1199 0.01581 837.9 1199 0.01581 838.3 1199 0.01587 838.7 1199 0.01582 839 1199 0.01585 839.4 1199 0.0159 839.8 1199 0.01587 840.2 1199 0.01582 840.6 1199 0.01582 840.9 1199 0.01587 841.3 1199 0.01587 841.7 1199 0.01585 842.1 1199 0.01582 842.5 1199 0.01582 842.8 1199 0.01585 843.2 1199 0.01586 843.6 1199 0.01585 844 1199 0.01586 844.4 1199 0.01585 844.7 1200 0.01586 845.1 1199 0.01585 845.5 1199 0.01585 845.9 1199 0.01585 846.3 1200 0.01585 846.7 1199 0.01585 847 1199 0.01582 847.4 1199 0.01584 847.8 1199 0.01582 848.2 1199 0.01584 848.6 1199 0.01582 848.9 1199 0.01582 849.3 1199 0.01584 849.7 1199 0.01585 850.1 1199 0.01585 850.5 1200 0.01582 850.8 1199 0.01581 851.2 1199 0.01581 851.6 1200 0.01585 852 1199 0.01585 852.4 1199 0.01581 852.7 1200 0.01582 853.1 1199 0.01585 853.5 1200 0.01582 853.9 1199 0.0158 854.3 1199 0.01585 854.6 1199 0.0158 855 1199 0.01584 855.4 1199 0.01585 855.8 1199 0.01581 856.2 1199 0.01585 856.6 1199 0.01581 856.9 1199 0.01585 857.3 1199 0.01582 857.7 1199 0.01584 858.1 1199 0.0158 858.5 1199 0.01581 858.8 1199 0.01576 859.2 1199 0.01582 859.6 1199 0.0158 860 1199 0.01585 860.4 1199 0.01582 860.7 1199 0.01579 861.1 1200 0.01581 861.5 1199 0.0158 861.9 1199 0.0158 862.3 1199 0.01582 862.6 1199 0.01581 863 1199 0.01584 863.4 1199 0.01581 863.8 1199 0.01579 864.2 1199 0.01577 864.6 1199 0.01576 864.9 1199 0.01576 865.3 1199 0.01577 865.7 1200 0.01581 866.1 1199 0.01581 866.5 1199 0.01579 866.8 1199 0.01581 867.2 1199 0.01582 867.6 1199 0.01579 868 1199 0.01582 868.4 1199 0.01582 868.7 1199 0.01579 869.1 1199 0.0158 869.5 1199 0.01577 869.9 1199 0.01581 870.3 1199 0.01582 870.6 1199 0.01582 871 1199 0.0158 871.4 1199 0.01579 871.8 1199 0.01577 872.2 1199 0.01579 872.6 1199 0.01577 872.9 1200 0.01581 873.3 1199 0.01579 873.7 1199 0.0158 874.1 1199 0.0158 874.5 1199 0.01576 874.8 1199 0.01579 875.2 1199 0.01579 875.6 1199 0.01577 876 1199 0.01581 876.4 1199 0.01581 876.7 1199 0.01576 877.1 1199 0.01577 877.5 1199 0.01577 877.9 1199 0.01577 878.3 1199 0.01577 878.6 1199 0.01575 879 1199 0.01577 879.4 1199 0.01581 879.8 1199 0.01581 880.2 1199 0.0158 880.5 1199 0.01579 880.9 1199 0.01575 881.3 1200 0.01574 881.7 1199 0.01574 882.1 1199 0.01574 882.5 1199 0.01577 882.8 1199 0.01577 883.2 1199 0.01577 883.6 1199 0.0158 884 1199 0.01579 884.4 1199 0.01579 884.7 1199 0.01577 885.1 1199 0.01577 885.5 1199 0.01575 885.9 1199 0.01577 886.3 1200 0.01579 886.6 1199 0.01581 887 1200 0.0158 887.4 1199 0.01577 887.8 1199 0.01577 888.2 1200 0.01579 888.5 1199 0.0158 888.9 1200 0.01576 889.3 1199 0.01577 889.7 1199 0.0158 890.1 1199 0.01582 890.5 1199 0.0158 890.8 1199 0.01581 891.2 1199 0.01582 891.6 1199 0.01582 892 1199 0.0158 892.4 1199 0.01582 892.7 1199 0.01581 893.1 1199 0.01581 893.5 1199 0.01581 893.9 1199 0.0158 894.3 1199 0.01581 894.6 1199 0.01577 895 1199 0.01577 895.4 1199 0.01577 895.8 1199 0.01577 896.2 1200 0.01576 896.5 1199 0.01577 896.9 1199 0.01577 897.3 1199 0.01579 897.7 1199 0.01577 898.1 1199 0.01577 898.4 1199 0.01577 898.8 1199 0.01576 899.2 1199 0.01577 899.6 1199 0.01577 900 1187 0.01575 900.4 1194 0.01581 900.7 1194 0.01585 901.1 1194 0.01585 901.5 1194 0.01579 901.9 1194 0.01577 902.3 1193 0.0158 902.6 1192 0.0158 903 1192 0.01576 903.4 1190 0.01576 903.8 1190 0.01573 904.2 1190 0.0157 904.5 1188 0.01566 904.9 1188 0.01568 905.3 1187 0.01568 905.7 1186 0.0157 906.1 1186 0.01566 906.4 1184 0.01563 906.8 1183 0.01561 907.2 1183 0.01558 907.6 1182 0.01556 908 1181 0.01553 908.4 1180 0.01548 908.7 1180 0.0155 909.1 1179 0.01548 909.5 1178 0.01548 909.9 1177 0.01543 910.3 1176 0.0154 910.6 1176 0.01538 911 1176 0.01534 911.4 1175 0.01533 911.8 1174 0.0153 912.2 1173 0.01527 912.5 1172 0.01523 912.9 1172 0.01523 913.3 1171 0.01524 913.7 1169 0.01522 914.1 1169 0.01519 914.4 1169 0.01522 914.8 1168 0.01523 915.2 1167 0.01518 915.6 1165 0.01519 916 1165 0.01517 916.3 1165 0.01517 916.7 1164 0.01514 917.1 1162 0.01514 917.5 1162 0.01514 917.9 1162 0.01507 918.3 1161 0.01504 918.6 1160 0.01501 919 1159 0.01499 919.4 1158 0.01496 919.8 1158 0.01495 920.2 1157 0.01493 920.5 1156 0.01492 920.9 1155 0.01491 921.3 1154 0.01485 921.7 1154 0.01486 922.1 1153 0.01483 922.4 1152 0.0148 922.8 1152 0.0148 923.2 1151 0.01478 923.6 1150 0.01475 924 1149 0.01472 924.3 1148 0.01473 924.7 1148 0.01469 925.1 1147 0.01469 925.5 1146 0.01469 925.9 1146 0.01464 926.3 1144 0.01461 926.6 1144 0.01461 927 1143 0.0146 927.4 1142 0.01457 927.8 1142 0.01456 928.2 1141 0.01454 928.5 1140 0.01452 928.9 1140 0.0145 929.3 1139 0.01448 929.7 1137 0.01445 930.1 1137 0.01443 930.4 1136 0.01443 930.8 1136 0.01439 931.2 1135 0.01439 931.6 1134 0.01438 932 1133 0.01438 932.3 1132 0.01434 932.7 1131 0.01429 933.1 1131 0.01425 933.5 1130 0.01425 933.9 1129 0.01423 934.2 1129 0.01419 934.6 1128 0.01415 935 1127 0.01415 935.4 1126 0.01413 935.8 1126 0.0141 936.2 1125 0.01409 936.5 1124 0.01407 936.9 1123 0.01409 937.3 1123 0.01409 937.7 1122 0.01404 938.1 1122 0.01403 938.4 1120 0.01399 938.8 1119 0.01399 939.2 1119 0.01397 939.6 1119 0.01396 940 1117 0.01393 940.3 1117 0.01391 940.7 1115 0.01389 941.1 1115 0.01384 941.5 1114 0.01384 941.9 1113 0.01382 942.2 1113 0.01381 942.6 1111 0.01381 943 1111 0.01376 943.4 1110 0.01372 943.8 1110 0.01372 944.2 1109 0.01373 944.5 1108 0.01367 944.9 1107 0.01361 945.3 1106 0.01362 945.7 1106 0.01365 946.1 1105 0.01365 946.4 1104 0.01361 946.8 1104 0.01361 947.2 1103 0.01358 947.6 1102 0.01356 948 1101 0.01353 948.3 1101 0.01352 948.7 1100 0.01348 949.1 1099 0.01346 949.5 1098 0.01347 949.9 1097 0.01345 950.2 1097 0.01345 950.6 1096 0.01339 951 1095 0.01339 951.4 1095 0.01332 951.8 1094 0.0133 952.1 1093 0.01327 952.5 1092 0.01324 952.9 1092 0.01325 953.3 1090 0.01321 953.7 1090 0.01322 954.1 1090 0.01321 954.4 1088 0.01319 954.8 1087 0.01316 955.2 1086 0.01319 955.6 1086 0.01314 956 1085 0.01314 956.3 1084 0.01313 956.7 1083 0.01306 957.1 1083 0.01305 957.5 1082 0.01304 957.9 1082 0.01304 958.2 1080 0.013 958.6 1079 0.01299 959 1079 0.01297 959.4 1079 0.01294 959.8 1077 0.01294 960.1 1077 0.01294 960.5 1076 0.0129 960.9 1075 0.01285 961.3 1074 0.01285 961.7 1074 0.01285 962.1 1073 0.01283 962.4 1072 0.0128 962.8 1072 0.01278 963.2 1070 0.01277 963.6 1069 0.01277 964 1069 0.01275 964.3 1068 0.01275 964.7 1068 0.01271 965.1 1067 0.01271 965.5 1065 0.01268 965.9 1065 0.01268 966.2 1064 0.01268 966.6 1064 0.01268 967 1063 0.01267 967.4 1062 0.01264 967.8 1061 0.01263 968.1 1061 0.01259 968.5 1060 0.01261 968.9 1059 0.01259 969.3 1058 0.01258 969.7 1058 0.01256 970.1 1057 0.01254 970.4 1056 0.01252 970.8 1055 0.01249 971.2 1054 0.01248 971.6 1054 0.01246 972 1053 0.01243 972.3 1053 0.01242 972.7 1051 0.01241 973.1 1051 0.0124 973.5 1050 0.01237 973.9 1049 0.01235 974.2 1049 0.01235 974.6 1048 0.01232 975 1047 0.0123 975.4 1047 0.0123 975.8 1046 0.01228 976.1 1044 0.01226 976.5 1044 0.01221 976.9 1043 0.0122 977.3 1043 0.01219 977.7 1042 0.01217 978 1041 0.01215 978.4 1040 0.01214 978.8 1040 0.01211 979.2 1039 0.01207 979.6 1038 0.01209 980 1037 0.01206 980.3 1036 0.01205 980.7 1036 0.01205 981.1 1035 0.01202 981.5 1034 0.01201 981.9 1034 0.012 982.2 1033 0.01197 982.6 1032 0.01194 983 1031 0.01193 983.4 1030 0.0119 983.8 1029 0.01191 984.1 1029 0.01189 984.5 1028 0.01185 984.9 1028 0.01185 985.3 1026 0.0118 985.7 1026 0.01179 986 1025 0.01176 986.4 1025 0.01175 986.8 1024 0.01175 987.2 1023 0.01175 987.6 1022 0.01174 988 1022 0.0117 988.3 1021 0.01168 988.7 1019 0.01168 989.1 1019 0.01165 989.5 1018 0.01163 989.9 1018 0.01162 990.2 1017 0.0116 990.6 1016 0.01158 991 1015 0.01158 991.4 1015 0.01155 991.8 1014 0.01155 992.1 1013 0.01149 992.5 1012 0.01149 992.9 1011 0.01146 993.3 1011 0.01142 993.7 1010 0.01138 994 1009 0.01141 994.4 1008 0.01144 994.8 1008 0.01142 995.2 1007 0.01137 995.6 1006 0.01136 995.9 1005 0.01132 996.3 1004 0.01132 996.7 1004 0.01131 997.1 1003 0.01128 997.5 1002 0.01127 997.9 1001 0.01127 998.2 1001 0.01126 998.6 1001 0.01123 999 1000 0.01122 999.4 999 0.0112 999.8 999 0.01118 1000 998 0.01118 1001 997 0.01117 1001 997 0.01116 1001 996 0.01113 1002 994 0.0111 1002 993 0.01108 1002 993 0.01106 1003 993 0.01106 1003 992 0.01106 1004 990 0.01102 1004 990 0.011 1004 989 0.01097 1005 989 0.01098 1005 987 0.01097 1005 987 0.01095 1006 986 0.01092 1006 985 0.01091 1007 985 0.01089 1007 984 0.01087 1007 983 0.01089 1008 983 0.01081 1008 982 0.01082 1009 981 0.01079 1009 980 0.01081 1009 979 0.01077 1010 979 0.01077 1010 978 0.01075 1010 977 0.0107 1011 976 0.0107 1011 975 0.01071 1012 975 0.0107 1012 974 0.01068 1012 973 0.01065 1013 972 0.01063 1013 972 0.0106 1013 971 0.01058 1014 970 0.01054 1014 969 0.01055 1015 968 0.01053 1015 968 0.01053 1015 967 0.01051 1016 966 0.0105 1016 965 0.01048 1017 965 0.01043 1017 964 0.01042 1017 964 0.01044 1018 962 0.01042 1018 962 0.01035 1018 961 0.01035 1019 961 0.01037 1019 959 0.01033 1020 959 0.01032 1020 958 0.01032 1020 957 0.01033 1021 956 0.01028 1021 956 0.01027 1021 955 0.01024 1022 954 0.01023 1022 954 0.01019 1023 953 0.01019 1023 952 0.01017 1023 951 0.01016 1024 950 0.01013 1024 950 0.01012 1025 949 0.01009 1025 948 0.01009 1025 947 0.01006 1026 947 0.009995 1026 946 0.01002 1026 945 0.01001 1027 944 0.01002 1027 943 0.00997 1028 943 0.009945 1028 942 0.009957 1028 942 0.00992 1029 940 0.009895 1029 940 0.009895 1029 939 0.009871 1030 938 0.009858 1030 937 0.009834 1031 936 0.009809 1031 936 0.009772 1031 935 0.009784 1032 934 0.009796 1032 933 0.009796 1033 932 0.009772 1033 932 0.00971 1033 931 0.009722 1034 931 0.00971 1034 929 0.009673 1034 929 0.009648 1035 929 0.009636 1035 927 0.009636 1036 926 0.009636 1036 926 0.009598 1036 925 0.009586 1037 925 0.009574 1037 923 0.009598 1037 923 0.009611 1038 922 0.009574 1038 922 0.009537 1039 921 0.009512 1039 919 0.009462 1039 918 0.009438 1040 918 0.009425 1040 918 0.009376 1041 917 0.009363 1041 915 0.009314 1041 915 0.009277 1042 915 0.009252 1042 914 0.009252 1042 913 0.00924 1043 912 0.009227 1043 911 0.00924 1044 911 0.009227 1044 910 0.009227 1044 909 0.00924 1045 909 0.009202 1045 907 0.009202 1045 907 0.009178 1046 906 0.00914 1046 906 0.009116 1047 904 0.009091 1047 904 0.009079 1047 903 0.009091 1048 902 0.009066 1048 901 0.009004 1049 900 0.009004 1049 900 0.009004 1049 899 0.00898 1050 899 0.008955 1050 898 0.00893 1050 897 0.008918 1051 897 0.008918 1051 896 0.008905 1052 894 0.008856 1052 894 0.008831 1052 893 0.008806 1053 893 0.008782 1053 892 0.008782 1053 891 0.008757 1054 890 0.008732 1054 889 0.008683 1055 889 0.00867 1055 888 0.008658 1055 887 0.008683 1056 886 0.008683 1056 886 0.008645 1057 885 0.008658 1057 884 0.008658 1057 883 0.008608 1058 883 0.008621 1058 882 0.008596 1058 881 0.008571 1059 880 0.008584 1059 880 0.008559 1060 879 0.008522 1060 878 0.008509 1060 877 0.008497 1061 876 0.008509 1061 875 0.008485 1061 875 0.008423 1062 874 0.008324 1062 874 0.008324 1063 873 0.008373 1063 872 0.008385 1063 872 0.008385 1064 870 0.008361 1064 869 0.008336 1065 869 0.008311 1065 868 0.008286 1065 867 0.008262 1066 867 0.008249 1066 866 0.008212 1066 865 0.008187 1067 864 0.008175 1067 864 0.008138 1068 863 0.008113 1068 862 0.008126 1068 861 0.008113 1069 861 0.008039 1069 860 0.007965 1069 859 0.008002 1070 858 0.008039 1070 857 0.008027 1071 856 0.008002 1071 856 0.008002 1071 855 0.007989 1072 854 0.007977 1072 854 0.00794 1073 853 0.007928 1073 852 0.007915 1073 851 0.00789 1074 850 0.007866 1074 850 0.007853 1074 849 0.007853 1075 849 0.007816 1075 847 0.007804 1076 847 0.007791 1076 846 0.007791 1076 845 0.007767 1077 844 0.007754 1077 843 0.007742 1077 843 0.007717 1078 843 0.007705 1078 842 0.007655 1079 840 0.007643 1079 839 0.007618 1079 839 0.007618 1080 838 0.007606 1080 837 0.007618 1080 836 0.007581 1081 836 0.007544 1081 835 0.007507 1082 834 0.007482 1082 834 0.00747 1082 833 0.007482 1083 832 0.00747 1083 832 0.007457 1084 831 0.00742 1084 830 0.007383 1084 829 0.007358 1085 829 0.007358 1085 828 0.007346 1085 827 0.007383 1086 826 0.007333 1086 825 0.007296 1087 825 0.007234 1087 824 0.007185 1087 823 0.007148 1088 822 0.007098 1088 821 0.007135 1088 821 0.007197 1089 820 0.007185 1089 819 0.007185 1090 818 0.00716 1090 818 0.007135 1090 817 0.007049 1091 816 0.007049 1091 815 0.007024 1092 814 0.007049 1092 814 0.007024 1092 814 0.006999 1093 812 0.006999 1093 811 0.006999 1093 811 0.00695 1094 810 0.00695 1094 810 0.006925 1095 809 0.0069 1095 807 0.006888 1095 807 0.006863 1096 806 0.006838 1096 806 0.006838 1096 805 0.006826 1097 804 0.006801 1097 804 0.006789 1098 803 0.006764 1098 802 0.006752 1098 801 0.006715 1099 801 0.006702 1099 801 0.006665 1100 801 0.006628 1100 801 0.006653 1100 801 0.006616 1101 800 0.006591 1101 800 0.006578 1101 799 0.006554 1102 799 0.006529 1102 798 0.006517 1103 797 0.006479 1103 796 0.006492 1103 796 0.006479 1104 794 0.006467 1104 794 0.006455 1104 793 0.00643 1105 792 0.006455 1105 792 0.006418 1106 791 0.006356 1106 790 0.006306 1106 789 0.006306 1107 789 0.006331 1107 788 0.006306 1108 786 0.006269 1108 786 0.006269 1108 786 0.006257 1109 785 0.006232 1109 784 0.006219 1109 783 0.006182 1110 782 0.00617 1110 782 0.006133 1111 781 0.00612 1111 780 0.006108 1111 780 0.006108 1112 779 0.006108 1112 778 0.006083 1112 777 0.006059 1113 776 0.006083 1113 776 0.006059 1114 775 0.006009 1114 774 0.005972 1114 773 0.005972 1115 772 0.00596 1115 772 0.00591 1116 771 0.00591 1116 771 0.005885 1116 769 0.005848 1117 769 0.005823 1117 768 0.005786 1117 767 0.005811 1118 767 0.005811 1118 766 0.005786 1119 765 0.005762 1119 764 0.005724 1119 764 0.005712 1120 763 0.005675 1120 762 0.005675 1120 761 0.005675 1121 761 0.005638 1121 760 0.005625 1122 759 0.005613 1122 758 0.005588 1122 757 0.005576 1123 757 0.005539 1123 756 0.005526 1124 755 0.005514 1124 754 0.005514 1124 753 0.005477 1125 753 0.005464 1125 752 0.005427 1125 750 0.005427 1126 750 0.005378 1126 750 0.005328 1127 749 0.005365 1127 748 0.005353 1127 747 0.005328 1128 746 0.005328 1128 746 0.005279 1128 746 0.005291 1129 744 0.005254 1129 743 0.005242 1130 743 0.00518 1130 743 0.00518 1130 742 0.005167 1131 740 0.005143 1131 739 0.005167 1132 739 0.005143 1132 738 0.005118 1132 737 0.005106 1133 736 0.005093 1133 736 0.005068 1133 735 0.005068 1134 734 0.005044 1134 734 0.005031 1135 733 0.004994 1135 732 0.004969 1135 732 0.004945 1136 731 0.004895 1136 730 0.004883 1136 729 0.004908 1137 728 0.004883 1137 728 0.00487 1138 727 0.004833 1138 726 0.004821 1138 725 0.004833 1139 725 0.004809 1139 724 0.004747 1140 723 0.004734 1140 722 0.004734 1140 721 0.004697 1141 721 0.004672 1141 720 0.004672 1141 719 0.004623 1142 718 0.004635 1142 718 0.004635 1143 717 0.004586 1143 716 0.004573 1143 715 0.004549 1144 714 0.004549 1144 714 0.004511 1144 713 0.004499 1145 712 0.004499 1145 711 0.004499 1146 711 0.004474 1146 710 0.004425 1146 709 0.004412 1147 709 0.0044 1147 707 0.004363 1148 707 0.004351 1148 707 0.004313 1148 705 0.004301 1149 705 0.004264 1149 704 0.004252 1149 703 0.004252 1150 702 0.004239 1150 702 0.004227 1151 700 0.004177 1151 700 0.004153 1151 699 0.004153 1152 699 0.004165 1152 698 0.00419 1152 697 0.00414 1153 696 0.004103 1153 696 0.004091 1154 695 0.004054 1154 694 0.004029 1154 693 0.004016 1155 693 0.004004 1155 692 0.003992 1156 691 0.004004 1156 690 0.003979 1156 689 0.003942 1157 689 0.003893 1157 688 0.00388 1157 687 0.00388 1158 686 0.003855 1158 686 0.003831 1159 685 0.003818 1159 684 0.003781 1159 683 0.003769 1160 682 0.003756 1160 682 0.003769 1160 681 0.003744 1161 680 0.003719 1161 679 0.003732 1162 678 0.003682 1162 678 0.003657 1162 678 0.003645 1163 676 0.003633 1163 676 0.003596 1164 675 0.003596 1164 674 0.003583 1164 674 0.003558 1165 673 0.003534 1165 672 0.003534 1165 671 0.003509 1166 671 0.003472 1166 669 0.003472 1167 668 0.003447 1167 668 0.003422 1167 668 0.003422 1168 667 0.003385 1168 666 0.003373 1168 665 0.00336 1169 664 0.00336 1169 664 0.003336 1170 663 0.003286 1170 662 0.003274 1170 661 0.003261 1171 661 0.003261 1171 660 0.003212 1172 659 0.003199 1172 658 0.003199 1172 657 0.003162 1173 657 0.003175 1173 657 0.003138 1173 655 0.003138 1174 655 0.003125 1174 654 0.003088 1175 653 0.003026 1175 652 0.003076 1175 651 0.003076 1176 650 0.003026 1176 650 0.003001 1176 649 0.003014 1177 648 0.002989 1177 648 0.002964 1178 646 0.002915 1178 646 0.002915 1178 646 0.00294 1179 645 0.002927 1179 643 0.002865 1180 643 0.002841 1180 643 0.002841 1180 641 0.002803 1181 641 0.002779 1181 639 0.002742 1181 639 0.002742 1182 638 0.002742 1182 637 0.002717 1183 637 0.002692 1183 636 0.002667 1183 635 0.002667 1184 634 0.00263 1184 634 0.00263 1184 633 0.002605 1185 632 0.002543 1185 632 0.002556 1186 631 0.002568 1186 630 0.002506 1186 629 0.002506 1187 628 0.002482 1187 628 0.002457 1188 627 0.002457 1188 626 0.002432 1188 625 0.00242 1189 625 0.00237 1189 624 0.002358 1189 623 0.002333 1190 622 0.002296 1190 621 0.002271 1191 621 0.002259 1191 620 0.002284 1191 619 0.002296 1192 618 0.002271 1192 617 0.002259 1192 617 0.002246 1193 617 0.002222 1193 615 0.002197 1194 614 0.00216 1194 614 0.002135 1194 613 0.00211 1195 612 0.002086 1195 611 0.002061 1196 611 0.002073 1196 610 0.002061 1196 609 0.002036 1197 609 0.002036 1197 608 0.001999 1197 607 0.001962 1198 606 0.001962 1198 606 0.001949 1199 605 0.001925 1199 605 0.001875 1199 603 0.001888 1200 603 0.001888 1200 602 0.00185 1200 601 0.001813 1201 601 0.001764 1201 600 0.001714 1202 599 0.001702 1202 599 0.001665 1202 598 0.001702 1203 597 0.001689 1203 596 0.001665 1204 596 0.001615 1204 594 0.001615 1204 594 0.00164 1205 593 0.001615 1205 592 0.001615 1205 592 0.001578 1206 591 0.001553 1206 590 0.001541 1207 589 0.001504 1207 589 0.001479 1207 588 0.001491 1208 587 0.001454 1208 586 0.001454 1208 586 0.001417 1209 585 0.001405 1209 584 0.001392 1210 584 0.001368 1210 582 0.001331 1210 582 0.001306 1211 580 0.001318 1211 580 0.001281 1212 579 0.001269 1212 579 0.001269 1212 578 0.001244 1213 578 0.001219 1213 576 0.001219 1213 576 0.001182 1214 574 0.001182 1214 574 0.001133 1215 574 0.001108 1215 572 0.001108 1215 572 0.001083 1216 571 0.001058 1216 571 0.001058 1216 570 0.001046 1217 568 0.001021 1217 568 0.0009964 1218 567 0.000984 1218 566 0.0009592 1218 566 0.0009345 1219 565 0.0009221 1219 564 0.0008973 1220 564 0.0008973 1220 563 0.0008973 1220 562 0.0008478 1221 561 0.0008355 1221 560 0.0008107 1221 560 0.0007983 1222 559 0.0007612 1222 559 0.0007364 1223 557 0.0007241 1223 557 0.0007117 1223 556 0.0007117 1224 555 0.0006869 1224 554 0.0006869 1224 553 0.0006498 1225 553 0.0006374 1225 552 0.0006374 1226 551 0.0006127 1226 550 0.0005508 1226 549 0.0004518 1227 549 0.0004765 1227 549 0.0005136 1228 547 0.000526 1228 546 0.0004889 1228 546 0.000427 1229 545 0.000427 1229 544 0.000427 1229 543 0.000427 1230 543 0.0004146 1230 542 0.0003775 1231 542 0.0003404 1231 540 0.000328 1231 540 0.0003032 1232 539 0.0002785 1232 538 0.0002785 1232 538 0.0002661 1233 537 0.0002537 1233 536 0.000229 1234 535 0.0001918 1234 535 0.0001671 1234 534 0.00013 1235 533 0.0001176 1235 532 0.0001176 1236 531 0.0001176 1236 531 9.283e-05 1236 530 8.045e-05 1237 529 5.57e-05 1237 528 3.094e-05 1237 528 1.857e-05 1238 527 6.189e-06 1238 527 6.189e-06 1239 525 6.189e-06 1239 524 6.189e-06 1239 524 6.189e-06 1240 523 6.189e-06 1240 522 6.189e-06 1240 521 -5.57e-05 1241 521 -8.045e-05 1241 521 -3.094e-05 1242 519 -5.57e-05 1242 518 -0.0001176 1242 518 -0.0001671 1243 517 -0.0001423 1243 517 -0.0001052 1244 515 -0.0001176 1244 515 -0.0001795 1244 514 -0.0002166 1245 514 -0.0002537 1245 512 -0.0003156 1245 512 -0.0003651 1246 511 -0.0003899 1246 510 -0.0003775 1247 509 -0.0003775 1247 509 -0.0003651 1247 509 -0.0003527 1248 507 -0.0003156 1248 506 -0.000328 1248 506 -0.0003404 1249 505 -0.0003651 1249 505 -0.0004023 1250 504 -0.0004394 1250 503 -0.0004889 1250 503 -0.0005508 1251 502 -0.000625 1251 501 -0.0006374 1252 500 -0.0006003 1252 499 -0.0005136 1252 499 -0.000526 1253 499 -0.0005632 1253 498 -0.0005755 1253 499 -0.0006003 1254 499 -0.0006127 1254 499 -0.0006003 1255 500 -0.0005755 1255 499 -0.0005755 1255 499 -0.0005755 1256 498 -0.0005632 1256 496 -0.0006003 1256 496 -0.0006127 1257 494 -0.0006374 1257 492 -0.0006993 1258 489 -0.0007612 1258 487 -0.0008231 1258 486 -0.0008231 1259 485 -0.0007736 1259 485 -0.0007612 1260 484 -0.0008231 1260 484 -0.000885 1260 483 -0.0009221 1261 482 -0.0009221 1261 481 -0.0009592 1261 480 -0.0009345 1262 480 -0.0009345 1262 478 -0.0009592 1263 478 -0.0009716 1263 478 -0.001033 1263 477 -0.001033 1264 476 -0.001009 1264 475 -0.000984 1264 474 -0.000984 1265 474 -0.001021 1265 473 -0.001071 1266 472 -0.001058 1266 471 -0.001058 1266 471 -0.001095 1267 470 -0.00112 1267 469 -0.00112 1268 468 -0.001133 1268 467 -0.001133 1268 467 -0.001133 1269 466 -0.001157 1269 465 -0.00117 1269 464 -0.001182 1270 464 -0.001194 1270 464 -0.001219 1271 462 -0.001232 1271 461 -0.001232 1271 460 -0.001256 1272 460 -0.001281 1272 459 -0.001281 1272 459 -0.001306 1273 458 -0.001355 1273 456 -0.001392 1274 456 -0.00138 1274 455 -0.001355 1274 455 -0.001368 1275 454 -0.001405 1275 453 -0.001405 1276 452 -0.00138 1276 452 -0.001392 1276 450 -0.001368 1277 450 -0.001405 1277 449 -0.00143 1277 449 -0.001442 1278 447 -0.001454 1278 446 -0.001454 1279 445 -0.001454 1279 446 -0.001467 1279 446 -0.001479 1280 444 -0.001454 1280 444 -0.001491 1280 442 -0.001491 1281 441 -0.001491 1281 440 -0.001491 1282 440 -0.001491 1282 440 -0.001516 1282 438 -0.001504 1283 438 -0.001529 1283 436 -0.001529 1283 437 -0.001529 1284 435 -0.001541 1284 435 -0.001566 1285 434 -0.001615 1285 433 -0.001615 1285 432 -0.001603 1286 431 -0.001628 1286 431 -0.00164 1287 430 -0.00164 1287 430 -0.001615 1287 429 -0.001615 1288 428 -0.001665 1288 427 -0.001677 1288 426 -0.001689 1289 426 -0.001702 1289 424 -0.001702 1290 424 -0.001702 1290 423 -0.001727 1290 423 -0.001714 1291 421 -0.001689 1291 421 -0.001689 1291 421 -0.001739 1292 419 -0.001801 1292 419 -0.001826 1293 417 -0.001838 1293 417 -0.00185 1293 417 -0.001838 1294 416 -0.001838 1294 415 -0.001838 1295 414 -0.001863 1295 413 -0.0019 1295 413 -0.001925 1296 412 -0.001937 1296 411 -0.001925 1296 410 -0.001949 1297 410 -0.001949 1297 409 -0.001949 1298 408 -0.001962 1298 407 -0.001974 1298 406 -0.001987 1299 406 -0.002011 1299 405 -0.002036 1299 404 -0.002048 1300 403 -0.002048 1300 403 -0.002048 1301 402 -0.002024 1301 401 -0.002048 1301 401 -0.002098 1302 400 -0.002098 1302 400 -0.002098 1303 399 -0.002123 1303 399 -0.002123 1303 397 -0.00211 1304 396 -0.002123 1304 396 -0.002123 1304 395 -0.002147 1305 394 -0.002172 1305 394 -0.002197 1306 393 -0.002197 1306 392 -0.002197 1306 392 -0.002209 1307 391 -0.002234 1307 390 -0.002246 1307 389 -0.002246 1308 388 -0.002259 1308 388 -0.002259 1309 387 -0.002284 1309 386 -0.002308 1309 385 -0.002308 1310 384 -0.002308 1310 384 -0.002308 1311 383 -0.002308 1311 382 -0.002308 1311 381 -0.002333 1312 381 -0.002358 1312 380 -0.002358 1312 379 -0.002383 1313 378 -0.002395 1313 378 -0.002395 1314 377 -0.002432 1314 376 -0.002432 1314 375 -0.002407 1315 375 -0.002407 1315 374 -0.002457 1315 374 -0.002506 1316 371 -0.002531 1316 371 -0.002519 1317 370 -0.002506 1317 370 -0.002506 1317 369 -0.002531 1318 368 -0.002556 1318 367 -0.002556 1319 367 -0.002556 1319 367 -0.002568 1319 366 -0.002593 1320 365 -0.002605 1320 364 -0.002605 1320 363 -0.002605 1321 362 -0.00263 1321 361 -0.002655 1322 361 -0.002655 1322 360 -0.002667 1322 359 -0.002692 1323 359 -0.002704 1323 358 -0.002729 1323 358 -0.002729 1324 356 -0.002754 1324 355 -0.002742 1325 355 -0.002754 1325 354 -0.002742 1325 353 -0.002754 1326 353 -0.002766 1326 352 -0.002766 1327 351 -0.002779 1327 350 -0.002779 1327 349 -0.002779 1328 349 -0.002766 1328 348 -0.002803 1328 347 -0.002816 1329 346 -0.002803 1329 345 -0.002803 1330 345 -0.002803 1330 344 -0.002803 1330 343 -0.002791 1331 342 -0.002779 1331 342 -0.002779 1331 342 -0.002754 1332 340 -0.002729 1332 340 -0.002704 1333 338 -0.00268 1333 338 -0.002667 1333 337 -0.002643 1334 336 -0.002605 1334 336 -0.002593 1335 335 -0.002605 1335 335 -0.002543 1335 334 -0.002457 1336 333 -0.002395 1336 331 -0.002333 1336 331 -0.002296 1337 331 -0.002234 1337 330 -0.00216 1338 329 -0.00211 1338 328 -0.002011 1338 328 -0.001912 1339 327 -0.001838 1339 326 -0.001764 1339 324 -0.001714 1340 324 -0.001615 1340 323 -0.001541 1341 322 -0.001479 1341 322 -0.00138 1341 322 -0.001293 1342 320 -0.001207 1342 319 -0.001157 1343 318 -0.001083 1343 317 -0.001021 1343 317 -0.0009716 1344 317 -0.0008973 1344 315 -0.0008231 1344 315 -0.0007612 1345 314 -0.0006746 1345 314 -0.0006127 1346 312 -0.0005632 1346 313 -0.0005136 1346 311 -0.0004889 1347 310 -0.0004394 1347 310 -0.0004023 1347 309 -0.0003651 1348 309 -0.0003156 1348 307 -0.0002785 1349 306 -0.0002537 1349 306 -0.0002166 1349 305 -0.0001423 1350 305 -0.0001176 1350 304 -0.0001052 1351 302 -6.807e-05 1351 302 -5.57e-05 1351 301 -3.094e-05 1352 300 6.189e-06 1352 300 6.189e-06 1352 299 6.189e-06 1353 298 6.189e-06 1353 297 6.189e-06 1354 296 6.189e-06 1354 295 6.189e-06 1354 295 1.857e-05 1355 294 4.332e-05 1355 293 3.094e-05 1355 292 5.57e-05 1356 292 5.57e-05 1356 292 5.57e-05 1357 291 8.045e-05 1357 289 0.00013 1357 289 0.00013 1358 288 0.0001176 1358 288 0.00013 1359 287 0.0001671 1359 286 0.0001918 1359 285 0.0001795 1360 285 0.0001671 1360 284 0.0001052 1360 283 0.0001052 1361 281 0.0001176 1361 281 0.0001176 1362 281 0.0001423 1362 280 0.0001547 1362 279 0.0001795 1363 278 0.0001671 1363 277 0.0001671 1363 277 0.0001671 1364 276 0.0001671 1364 275 0.0001671 1365 274 0.0001671 1365 274 0.0001671 1365 273 0.0001671 1366 272 0.0001795 1366 271 0.0001671 1367 270 0.0001795 1367 270 0.0001671 1367 269 0.0001918 1368 268 0.0001918 1368 267 0.0002042 1368 267 0.0001918 1369 266 0.0002042 1369 265 0.0001918 1370 264 0.0002042 1370 263 0.0002042 1370 263 0.0002042 1371 262 0.0002166 1371 261 0.0002042 1371 260 0.0002166 1372 260 0.0001918 1372 259 0.0001795 1373 258 0.0001795 1373 257 0.0001795 1373 257 0.0001795 1374 256 0.0001671 1374 255 0.0001671 1375 255 0.0001671 1375 254 0.0001795 1375 253 0.000229 1376 252 0.000229 1376 252 0.0002166 1376 250 0.0002166 1377 249 0.0002042 1377 249 0.0001918 1378 248 0.0001547 1378 248 0.0001547 1378 246 0.0001547 1379 246 0.0001795 1379 245 0.0001671 1379 244 0.0001671 1380 243 0.00013 1380 243 5.57e-05 1381 242 9.283e-05 1381 242 0.00013 1381 241 0.0001423 1382 240 0.0001547 1382 239 0.0001671 1383 239 0.0001671 1383 238 0.0001547 1383 237 0.00013 1384 236 0.00013 1384 235 0.0001176 1384 234 0.0001052 1385 234 0.0001176 1385 233 0.0001176 1386 232 0.0001052 1386 231 8.045e-05 1386 231 8.045e-05 1387 230 9.283e-05 1387 230 8.045e-05 1387 229 8.045e-05 1388 227 6.807e-05 1388 227 6.807e-05 1389 227 5.57e-05 1389 226 5.57e-05 1389 224 5.57e-05 1390 224 3.094e-05 1390 223 1.857e-05 1391 222 6.189e-06 1391 221 1.857e-05 1391 221 1.857e-05 1392 220 1.857e-05 1392 220 1.857e-05 1392 219 6.189e-06 1393 217 6.189e-06 1393 217 6.189e-06 1394 217 6.189e-06 1394 216 6.189e-06 1394 214 6.189e-06 1395 214 -4.332e-05 1395 213 -1.857e-05 1395 213 6.189e-06 1396 212 6.189e-06 1396 211 6.189e-06 1397 210 6.189e-06 1397 209 6.189e-06 1397 209 6.189e-06 1398 207 6.189e-06 1398 207 6.189e-06 1399 206 6.189e-06 1399 206 6.189e-06 1399 205 -1.857e-05 1400 204 -3.094e-05 1400 204 -4.332e-05 1400 202 -5.57e-05 1401 202 -8.045e-05 1401 202 -8.045e-05 1402 201 -0.0001052 1402 200 -9.283e-05 1402 199 -0.0001052 1403 199 -0.0001176 1403 199 -0.00013 1403 198 -0.0001052 1404 197 -0.00013 1404 196 -0.0001423 1405 195 -0.0001423 1405 194 -0.00013 1405 193 -0.0001052 1406 193 -0.0001176 1406 191 -0.0001176 1407 191 -0.00013 1407 190 -0.0001423 1407 190 -0.00013 1408 189 -0.0001423 1408 188 -0.0001423 1408 188 -0.0001795 1409 187 -0.0002166 1409 185 -0.0002414 1410 185 -0.0002537 1410 184 -0.0002414 1410 184 -0.0002537 1411 183 -0.0002537 1411 182 -0.000229 1411 181 -0.0002537 1412 181 -0.0002909 1412 180 -0.000328 1413 179 -0.0003527 1413 178 -0.0003527 1413 177 -0.000328 1414 177 -0.0003032 1414 176 -0.0003032 1415 176 -0.0003032 1415 174 -0.0003156 1415 174 -0.0002785 1416 174 -0.0002661 1416 173 -0.0003032 1416 171 -0.0003156 1417 171 -0.0003404 1417 170 -0.0003775 1418 169 -0.0004023 1418 168 -0.0004146 1418 168 -0.0004146 1419 167 -0.0004146 1419 166 -0.0004146 1419 166 -0.000427 1420 165 -0.0004518 1420 164 -0.0004394 1421 163 -0.000427 1421 163 -0.000427 1421 162 -0.0004146 1422 162 -0.0004146 1422 160 -0.0004641 1423 159 -0.0004765 1423 159 -0.0004641 1423 158 -0.0004765 1424 156 -0.0005013 1424 156 -0.0005136 1424 155 -0.0005136 1425 155 -0.0005136 1425 154 -0.000526 1426 153 -0.000526 1426 152 -0.0005136 1426 152 -0.0005384 1427 151 -0.0005879 1427 150 -0.0006127 1427 149 -0.0006127 1428 149 -0.000625 1428 148 -0.000625 1429 148 -0.0006498 1429 146 -0.0006127 1429 146 -0.0005879 1430 145 -0.0006003 1430 144 -0.0006127 1431 143 -0.0006498 1431 142 -0.0006498 1431 141 -0.0006622 1432 141 -0.0006622 1432 140 -0.0006746 1432 140 -0.0006746 1433 139 -0.0006746 1433 138 -0.0006746 1434 137 -0.0006746 1434 136 -0.0006993 1434 136 -0.0006993 1435 134 -0.0007117 1435 134 -0.0007241 1435 134 -0.0007241 1436 133 -0.0007488 1436 132 -0.0007736 1437 131 -0.0007983 1437 131 -0.0007859 1437 130 -0.0007859 1438 129 -0.0007736 1438 129 -0.0007859 1439 127 -0.0008107 1439 127 -0.0008231 1439 126 -0.0008231 1440 125 -0.0008231 1440 124 -0.0008355 1440 123 -0.0008231 1441 123 -0.0008478 1441 122 -0.0008602 1442 121 -0.0008726 1442 121 -0.0008726 1442 120 -0.0008602 1443 119 -0.0008973 1443 118 -0.0008973 1443 117 -0.0009221 1444 116 -0.0009097 1444 116 -0.0009221 1445 116 -0.0009221 1445 114 -0.0009221 1445 114 -0.0009592 1446 113 -0.0009592 1446 112 -0.0009468 1447 112 -0.0009592 1447 111 -0.001009 1447 110 -0.001021 1448 109 -0.001021 1448 109 -0.001021 1448 108 -0.001033 1449 106 -0.001058 1449 106 -0.001058 1450 106 -0.001021 1450 105 -0.001058 1450 104 -0.001058 1451 103 -0.001033 1451 102 -0.001033 1451 102 -0.001058 1452 100 -0.001071 1452 100 -0.001083 1453 99 -0.00112 1453 98 -0.001108 1453 98 -0.00112 1454 98 -0.001157 1454 96 -0.001145 1455 95 -0.001145 1455 95 -0.001145 1455 94 -0.00117 1456 94 -0.001182 1456 92 -0.001182 1456 92 -0.001157 1457 91 -0.00117 1457 91 -0.001207 1458 89 -0.001219 1458 89 -0.001244 1458 88 -0.001244 1459 88 -0.001244 1459 87 -0.001256 1459 86 -0.001256 1460 85 -0.001244 1460 84 -0.001256 1461 84 -0.001306 1461 83 -0.001293 1461 82 -0.001318 1462 81 -0.001318 1462 81 -0.001306 1463 80 -0.001355 1463 79 -0.001392 1463 78 -0.001343 1464 77 -0.001331 1464 77 -0.001343 1464 77 -0.001368 1465 75 -0.00138 1465 74 -0.001392 1466 74 -0.001392 1466 73 -0.001405 1466 73 -0.001442 1467 72 -0.001417 1467 71 -0.001417 1467 70 -0.001454 1468 70 -0.001454 1468 69 -0.001454 1469 68 -0.001454 1469 68 -0.001467 1469 67 -0.001491 1470 67 -0.001467 1470 66 -0.001491 1471 66 -0.001491 1471 66 -0.001504 1471 65 -0.001504 1472 65 -0.001504 1472 64 -0.001516 1472 64 -0.001516 1473 62 -0.001529 1473 61 -0.001566 1474 59 -0.001578 1474 59 -0.00159 1474 56 -0.00159 1475 55 -0.001615 1475 55 -0.00164 1475 55 -0.00164 1476 53 -0.001665 1476 52 -0.001689 1477 52 -0.001677 1477 51 -0.001665 1477 50 -0.001689 1478 49 -0.001727 1478 49 -0.001714 1478 48 -0.001714 1479 48 -0.001702 1479 46 -0.001702 1480 46 -0.001702 1480 45 -0.001727 1480 45 -0.001739 1481 44 -0.001727 1481 44 -0.001714 1482 43 -0.001727 1482 42 -0.001764 1482 41 -0.001751 1483 41 -0.001751 1483 40 -0.001751 1483 39 -0.001751 1484 38 -0.001788 1484 38 -0.001788 1485 38 -0.001801 1485 37 -0.001801 1485 36 -0.001788 1486 35 -0.001813 1486 35 -0.001813 1486 34 -0.001838 1487 34 -0.001863 1487 34 -0.001888 1488 33 -0.001863 1488 33 -0.00185 1488 31 -0.00185 1489 31 -0.001875 1489 30 -0.001888 1490 30 -0.001888 1490 30 -0.0019 1490 30 -0.001925 1491 29 -0.001912 1491 28 -0.0019 1491 27 -0.001912 1492 27 -0.001962 1492 27 -0.001949 1493 26 -0.001949 1493 26 -0.001949 1493 26 -0.001949 1494 24 -0.001949 1494 24 -0.001949 1494 23 -0.001949 1495 23 -0.001949 1495 23 -0.001962 1496 23 -0.001987 1496 23 -0.001987 1496 22 -0.001987 1497 21 -0.001987 1497 21 -0.002011 1498 20 -0.001987 1498 21 -0.001962 1498 19 -0.001999 1499 20 -0.001999 1499 19 -0.002011 1499 19 -0.001999 1500 19 -0.002011 1500 19 -0.001999 1501 18 -0.001999 1501 18 -0.002011 1501 18 -0.001999 1502 17 -0.001999 1502 17 -0.001987 1502 17 -0.001999 1503 17 -0.002036 1503 17 -0.001999 1504 17 -0.002024 1504 16 -0.002036 1504 16 -0.002036 1505 16 -0.002048 1505 16 -0.002036 1506 16 -0.002048 1506 16 -0.002048 1506 16 -0.002048 1507 15 -0.002024 1507 15 -0.002036 1507 15 -0.002024 1508 15 -0.002073 1508 15 -0.002073 1509 15 -0.002024 1509 15 -0.002011 1509 15 -0.002036 1510 14 -0.002061 1510 14 -0.002098 1510 15 -0.002098 1511 14 -0.00211 1511 14 -0.002098 1512 14 -0.002061 1512 14 -0.002061 1512 14 -0.002061 1513 13 -0.002061 1513 13 -0.002048 1514 13 -0.002048 1514 13 -0.002061 1514 13 -0.002061 1515 13 -0.002061 1515 13 -0.002073 1515 13 -0.002073 1516 13 -0.002086 1516 13 -0.002098 1517 13 -0.002086 1517 13 -0.002061 1517 13 -0.002061 1518 13 -0.002086 1518 13 -0.00211 1518 13 -0.00211 1519 13 -0.00211 1519 13 -0.002086 1520 13 -0.002061 1520 13 -0.002061 1520 13 -0.002061 1521 12 -0.002061 1521 12 -0.002073 1522 13 -0.002086 1522 12 -0.002098 1522 12 -0.002098 1523 12 -0.002073 1523 13 -0.002086 1523 12 -0.002086 1524 12 -0.002061 1524 12 -0.002061 1525 12 -0.002048 1525 12 -0.002048 1525 12 -0.002073 1526 12 -0.002048 1526 12 -0.002061 1526 12 -0.002086 1527 12 -0.002073 1527 12 -0.002061 1528 11 -0.002061 1528 12 -0.002061 1528 12 -0.002073 1529 11 -0.002098 1529 11 -0.002098 1530 11 -0.002073 1530 11 -0.002061 1530 12 -0.002086 1531 11 -0.002086 1531 12 -0.002098 1531 11 -0.00211 1532 11 -0.002098 1532 11 -0.002061 1533 11 -0.002061 1533 11 -0.002048 1533 11 -0.002048 1534 11 -0.002061 1534 11 -0.002048 1534 11 -0.002048 1535 11 -0.002048 1535 11 -0.002024 1536 11 -0.002036 1536 11 -0.002048 1536 11 -0.002073 1537 11 -0.002061 1537 11 -0.002061 1538 11 -0.002048 1538 10 -0.002061 1538 11 -0.002086 1539 11 -0.002098 1539 10 -0.002098 1539 11 -0.002073 1540 11 -0.002073 1540 10 -0.002061 1541 11 -0.002061 1541 11 -0.002048 1541 11 -0.002048 1542 10 -0.002061 1542 11 -0.002048 1542 11 -0.002061 1543 10 -0.002086 1543 10 -0.002086 1544 10 -0.00211 1544 10 -0.002123 1544 11 -0.00211 1545 10 -0.002098 1545 10 -0.002086 1546 10 -0.002086 1546 10 -0.002086 1546 10 -0.002098 1547 10 -0.002098 1547 10 -0.002086 1547 10 -0.002048 1548 10 -0.002073 1548 10 -0.002073 1549 10 -0.002061 1549 10 -0.002061 1549 9 -0.002048 1550 10 -0.002048 1550 10 -0.002061 1550 10 -0.002061 1551 10 -0.002048 1551 10 -0.002048 1552 10 -0.002061 1552 10 -0.002061 1552 10 -0.002123 1553 10 -0.002073 1553 10 -0.002036 1554 9 -0.002048 1554 10 -0.002048 1554 10 -0.002036 1555 11 -0.002011 1555 9 -0.002011 1555 10 -0.002011 1556 10 -0.002036 1556 10 -0.002073 1557 10 -0.002086 1557 9 -0.002123 1557 10 -0.00211 1558 10 -0.002048 1558 10 -0.002024 1558 9 -0.002048 1559 4 0.29 0.09 0.74 0.002 0.007 0.66 1.3 1.02 0.292 0 0 0.001 0.0041 0 5 -0.0001423 0 6 -0.0001547 0.2344 5 -0.0001423 0.4688 6 -0.00013 0.7031 6 -0.00013 0.9375 6 -0.00013 1.172 6 -0.0001052 1.406 6 -8.045e-05 1.641 6 -8.045e-05 1.875 6 -8.045e-05 2.109 6 -6.807e-05 2.344 6 -8.045e-05 2.578 6 -6.807e-05 2.813 5 -6.807e-05 3.047 6 -6.807e-05 3.281 6 -6.807e-05 3.516 6 -6.807e-05 3.75 6 -6.807e-05 3.984 6 -6.807e-05 4.219 7 -6.807e-05 4.453 8 -6.807e-05 4.688 9 -6.807e-05 4.922 10 -6.807e-05 5.156 11 -5.57e-05 5.391 13 -3.094e-05 5.625 14 -3.094e-05 5.859 16 -1.857e-05 6.094 17 6.189e-06 6.328 19 6.189e-06 6.563 20 6.189e-06 6.797 22 6.189e-06 7.031 23 6.189e-06 7.266 25 6.189e-06 7.5 27 1.857e-05 7.734 28 5.57e-05 7.969 29 9.283e-05 8.203 30 0.00013 8.438 31 0.00013 8.672 33 0.00013 8.906 34 0.0001795 9.141 35 0.0002042 9.375 36 0.000229 9.609 37 0.000229 9.844 38 0.0002414 10.08 38 0.0002661 10.31 40 0.0002785 10.55 41 0.0002909 10.78 41 0.0002909 11.02 42 0.0002909 11.25 43 0.0002909 11.48 44 0.0003032 11.72 45 0.000328 11.95 45 0.0003404 12.19 46 0.0003404 12.42 48 0.0003651 12.66 48 0.0003775 12.89 49 0.0003899 13.13 50 0.0003899 13.36 52 0.0004023 13.59 52 0.000427 13.83 52 0.0004394 14.06 54 0.0004518 14.3 55 0.0004518 14.53 55 0.0004765 14.77 56 0.0004765 15 58 0.0005013 15.23 59 0.0005013 15.47 60 0.000526 15.7 61 0.0005384 15.94 62 0.0005508 16.17 63 0.0005508 16.41 63 0.0005632 16.64 64 0.0005632 16.88 65 0.0005632 17.11 66 0.0005879 17.34 67 0.0005879 17.58 68 0.0005879 17.81 69 0.0006127 18.05 70 0.000625 18.28 71 0.0006498 18.52 72 0.0006498 18.75 73 0.0006622 18.98 73 0.0006869 19.22 74 0.0006993 19.45 76 0.0006993 19.69 77 0.0007117 19.92 77 0.0007241 20.16 79 0.0007364 20.39 80 0.0007488 20.63 81 0.0007612 20.86 81 0.0007612 21.09 83 0.0007736 21.33 84 0.0007859 21.56 84 0.0007983 21.8 85 0.0008231 22.03 86 0.0008478 22.27 87 0.0008478 22.5 88 0.0008478 22.73 89 0.0008602 22.97 90 0.0008726 23.2 91 0.000885 23.44 92 0.0008973 23.67 93 0.0009097 23.91 94 0.0009097 24.14 95 0.0009221 24.38 95 0.0009345 24.61 97 0.0009468 24.84 98 0.0009592 25.08 98 0.0009716 25.31 99 0.000984 25.55 101 0.0009964 25.78 102 0.0009964 26.02 102 0.001021 26.25 103 0.001033 26.48 104 0.001058 26.72 105 0.001058 26.95 106 0.001083 27.19 106 0.001095 27.42 108 0.001108 27.66 109 0.001108 27.89 109 0.00112 28.13 111 0.001157 28.36 112 0.001157 28.59 113 0.00117 28.83 113 0.00117 29.06 114 0.001194 29.3 115 0.001194 29.53 116 0.001207 29.77 117 0.001219 30 118 0.001232 30.23 119 0.001219 30.47 120 0.001219 30.7 121 0.001219 30.94 122 0.001219 31.17 123 0.001219 31.41 124 0.001219 31.64 124 0.001256 31.88 126 0.001256 32.11 127 0.001293 32.34 127 0.001306 32.58 129 0.001306 32.81 129 0.001343 33.05 131 0.001343 33.28 131 0.001355 33.52 132 0.001368 33.75 134 0.00138 33.98 134 0.00138 34.22 135 0.001392 34.45 136 0.001392 34.69 137 0.001405 34.92 138 0.001417 35.16 138 0.001417 35.39 140 0.001454 35.63 141 0.001454 35.86 142 0.001467 36.09 143 0.001491 36.33 144 0.001504 36.56 145 0.001516 36.8 145 0.001516 37.03 146 0.001541 37.27 148 0.001553 37.5 149 0.001566 37.73 149 0.001566 37.97 150 0.00159 38.2 152 0.001603 38.44 152 0.001603 38.67 153 0.001615 38.91 154 0.001615 39.14 155 0.00164 39.38 156 0.001652 39.61 156 0.001665 39.84 158 0.001665 40.08 159 0.001677 40.31 159 0.001702 40.55 160 0.001714 40.78 162 0.001714 41.02 163 0.001714 41.25 163 0.001714 41.48 165 0.001727 41.72 165 0.001727 41.95 166 0.001751 42.19 167 0.001764 42.42 168 0.001764 42.66 169 0.001776 42.89 170 0.001801 43.13 171 0.001801 43.36 172 0.001813 43.59 173 0.001813 43.83 174 0.001826 44.06 175 0.00185 44.3 176 0.001863 44.53 177 0.001888 44.77 177 0.0019 45 179 0.001912 45.23 180 0.001937 45.47 181 0.001962 45.7 181 0.001962 45.94 183 0.001974 46.17 184 0.001974 46.41 184 0.001974 46.64 185 0.001974 46.88 186 0.001987 47.11 188 0.002011 47.34 188 0.002011 47.58 189 0.002036 47.81 190 0.002061 48.05 191 0.002061 48.28 192 0.002073 48.52 193 0.002073 48.75 194 0.002073 48.98 195 0.00211 49.22 195 0.00211 49.45 196 0.002123 49.69 198 0.002147 49.92 199 0.00216 50.16 200 0.002172 50.39 201 0.002172 50.63 201 0.002209 50.86 202 0.002222 51.09 202 0.002234 51.33 204 0.002234 51.56 204 0.002246 51.8 206 0.002259 52.03 206 0.002271 52.27 207 0.002296 52.5 209 0.002308 52.73 209 0.002321 52.97 210 0.002345 53.2 211 0.002358 53.44 212 0.00237 53.67 213 0.00237 53.91 214 0.00237 54.14 215 0.002395 54.38 217 0.002407 54.61 217 0.00242 54.84 218 0.002432 55.08 219 0.002444 55.31 220 0.002457 55.55 220 0.002482 55.78 221 0.002506 56.02 223 0.002519 56.25 224 0.002531 56.48 224 0.002531 56.72 225 0.002556 56.95 227 0.002568 57.19 227 0.002581 57.42 228 0.002605 57.66 229 0.002605 57.89 230 0.00263 58.13 231 0.00263 58.36 231 0.002655 58.59 233 0.00268 58.83 234 0.002667 59.06 234 0.002692 59.3 236 0.002692 59.53 237 0.002704 59.77 238 0.002729 60 238 0.002742 60.23 239 0.002742 60.47 241 0.002766 60.7 242 0.002791 60.94 242 0.002803 61.17 243 0.002828 61.41 244 0.002841 61.64 245 0.002865 61.88 246 0.002878 62.11 247 0.00289 62.34 249 0.00289 62.58 249 0.002902 62.81 249 0.002902 63.05 251 0.002927 63.28 252 0.00294 63.52 253 0.00294 63.75 254 0.002952 63.98 255 0.002964 64.22 256 0.002989 64.45 256 0.003014 64.69 258 0.003026 64.92 259 0.003039 65.16 259 0.003051 65.39 260 0.003051 65.63 261 0.003063 65.86 262 0.003076 66.09 263 0.003088 66.33 264 0.003113 66.56 265 0.003125 66.8 267 0.003138 67.03 267 0.003162 67.27 268 0.003175 67.5 269 0.003175 67.73 270 0.003187 67.97 270 0.003187 68.2 271 0.003224 68.44 273 0.003224 68.67 274 0.003237 68.91 274 0.003237 69.14 275 0.003249 69.38 277 0.003261 69.61 277 0.003286 69.84 278 0.003286 70.08 280 0.003311 70.31 280 0.003336 70.55 281 0.003336 70.78 282 0.003336 71.02 283 0.00336 71.25 284 0.003373 71.48 285 0.00341 71.72 286 0.003422 71.95 287 0.003435 72.19 288 0.003459 72.42 289 0.003472 72.66 290 0.003484 72.89 292 0.003497 73.13 292 0.003497 73.36 292 0.003497 73.59 293 0.003534 73.83 294 0.003534 74.06 295 0.003546 74.3 296 0.003546 74.53 298 0.003571 74.77 298 0.003558 75 299 0.003583 75.23 299 0.003596 75.47 301 0.003596 75.7 302 0.00362 75.94 302 0.003633 76.17 304 0.003657 76.41 305 0.003682 76.64 306 0.003695 76.88 306 0.003695 77.11 308 0.003707 77.34 309 0.003719 77.58 310 0.003744 77.81 310 0.003744 78.05 311 0.003756 78.28 312 0.003781 78.52 313 0.003794 78.75 314 0.003818 78.98 315 0.003831 79.22 317 0.003843 79.45 317 0.003855 79.69 318 0.00388 79.92 319 0.003905 80.16 320 0.00393 80.39 321 0.003954 80.63 322 0.003979 80.86 323 0.003992 81.09 324 0.003992 81.33 324 0.004004 81.56 326 0.004029 81.8 327 0.004066 82.03 328 0.004091 82.27 329 0.004115 82.5 330 0.00414 82.73 331 0.004153 82.97 331 0.004177 83.2 332 0.00419 83.44 334 0.004214 83.67 334 0.004214 83.91 335 0.004227 84.14 336 0.004214 84.38 337 0.004227 84.61 338 0.004239 84.84 338 0.004239 85.08 339 0.004239 85.31 340 0.004239 85.55 342 0.004252 85.78 342 0.004264 86.02 343 0.004264 86.25 345 0.004276 86.48 345 0.004289 86.72 346 0.004301 86.95 347 0.004338 87.19 348 0.004351 87.42 349 0.004388 87.66 350 0.0044 87.89 351 0.004412 88.13 353 0.004425 88.36 353 0.004437 88.59 354 0.00445 88.83 355 0.004462 89.06 356 0.004474 89.3 356 0.004487 89.53 358 0.004511 89.77 359 0.004511 90 360 0.004536 90.23 361 0.004549 90.47 361 0.004561 90.7 363 0.004573 90.94 363 0.004586 91.17 365 0.00461 91.41 365 0.004623 91.64 367 0.004623 91.88 367 0.004623 92.11 368 0.004635 92.34 369 0.004648 92.58 370 0.00466 92.81 371 0.004672 93.05 371 0.004697 93.28 373 0.004709 93.52 374 0.004722 93.75 374 0.004722 93.98 376 0.004734 94.22 378 0.004759 94.45 378 0.004759 94.69 379 0.004771 94.92 380 0.004784 95.16 380 0.004809 95.39 381 0.004809 95.63 382 0.004833 95.86 384 0.004846 96.09 384 0.004858 96.33 385 0.00487 96.56 386 0.004883 96.8 387 0.004908 97.03 388 0.00492 97.27 388 0.00492 97.5 389 0.00492 97.73 390 0.004945 97.97 392 0.004957 98.2 392 0.004969 98.44 393 0.005007 98.67 394 0.005019 98.91 396 0.005044 99.14 396 0.005056 99.38 397 0.005093 99.61 399 0.005118 99.84 399 0.005118 100.1 400 0.005155 100.3 401 0.005143 100.5 402 0.005155 100.8 403 0.005167 101 403 0.00518 101.3 405 0.005205 101.5 406 0.005217 101.7 406 0.005217 102 407 0.005242 102.2 408 0.005266 102.4 409 0.005279 102.7 410 0.005279 102.9 411 0.005279 103.1 411 0.005291 103.4 413 0.005316 103.6 413 0.005316 103.8 414 0.005328 104.1 415 0.005341 104.3 417 0.005353 104.5 417 0.005378 104.8 418 0.005378 105 419 0.005378 105.2 421 0.00539 105.5 421 0.005415 105.7 423 0.005452 105.9 424 0.005464 106.2 424 0.005502 106.4 425 0.005514 106.6 426 0.005526 106.9 427 0.005526 107.1 428 0.005564 107.3 429 0.005576 107.6 430 0.005576 107.8 431 0.005613 108 431 0.005613 108.3 433 0.005613 108.5 433 0.005613 108.8 435 0.005638 109 435 0.00565 109.2 436 0.005675 109.5 438 0.005675 109.7 438 0.005687 109.9 439 0.005724 110.2 440 0.005724 110.4 442 0.005737 110.6 442 0.005749 110.9 443 0.005774 111.1 444 0.005774 111.3 444 0.005811 111.6 446 0.005823 111.8 446 0.005836 112 448 0.005848 112.3 449 0.005873 112.5 449 0.005885 112.7 450 0.00591 113 452 0.005935 113.2 453 0.005947 113.4 454 0.005972 113.7 455 0.005984 113.9 455 0.005997 114.1 456 0.005997 114.4 457 0.005997 114.6 458 0.005997 114.8 459 0.005972 115.1 460 0.005997 115.3 461 0.006021 115.5 462 0.006071 115.8 463 0.006108 116 464 0.006133 116.3 464 0.006158 116.5 467 0.006158 116.7 467 0.006158 117 467 0.006195 117.2 468 0.006195 117.4 469 0.006232 117.7 471 0.006244 117.9 471 0.006257 118.1 472 0.006269 118.4 474 0.006281 118.6 474 0.006306 118.8 475 0.006306 119.1 476 0.006306 119.3 477 0.006319 119.5 478 0.006331 119.8 479 0.006343 120 480 0.006356 120.2 481 0.00638 120.5 481 0.006405 120.7 483 0.006418 120.9 484 0.00643 121.2 485 0.006442 121.4 485 0.006455 121.6 486 0.006455 121.9 488 0.006467 122.1 489 0.006479 122.3 489 0.006504 122.6 490 0.006504 122.8 492 0.006529 123 492 0.006541 123.3 493 0.006566 123.5 494 0.006578 123.8 495 0.006591 124 496 0.006603 124.2 497 0.006616 124.5 498 0.00664 124.7 499 0.006665 124.9 499 0.006677 125.2 500 0.00669 125.4 501 0.006702 125.6 503 0.006715 125.9 503 0.006739 126.1 505 0.006752 126.3 505 0.006764 126.6 506 0.006789 126.8 507 0.006789 127 508 0.006814 127.3 509 0.006826 127.5 510 0.006851 127.7 511 0.006863 128 512 0.006875 128.2 513 0.006888 128.4 514 0.0069 128.7 515 0.006925 128.9 515 0.00695 129.1 517 0.00695 129.4 517 0.006962 129.6 518 0.006962 129.8 519 0.006987 130.1 521 0.006999 130.3 521 0.006999 130.5 521 0.007024 130.8 523 0.007049 131 524 0.007049 131.3 525 0.007074 131.5 527 0.007098 131.7 527 0.007123 132 528 0.007148 132.2 529 0.007148 132.4 530 0.00716 132.7 531 0.007173 132.9 532 0.007197 133.1 532 0.007197 133.4 534 0.007222 133.6 535 0.007234 133.8 535 0.007259 134.1 536 0.007259 134.3 537 0.007272 134.5 538 0.007296 134.8 539 0.007296 135 540 0.007309 135.2 542 0.007321 135.5 542 0.007346 135.7 542 0.007358 135.9 544 0.007358 136.2 545 0.007383 136.4 546 0.007395 136.6 546 0.007408 136.9 547 0.007432 137.1 549 0.007445 137.3 549 0.007457 137.6 550 0.007494 137.8 552 0.007507 138 553 0.007507 138.3 553 0.007531 138.5 554 0.007556 138.8 555 0.007556 139 556 0.007581 139.2 557 0.007606 139.5 558 0.007606 139.7 559 0.007618 139.9 560 0.007618 140.2 561 0.00763 140.4 562 0.007655 140.6 563 0.007668 140.9 564 0.00768 141.1 565 0.007692 141.3 565 0.007717 141.6 567 0.007717 141.8 567 0.007754 142 568 0.007754 142.3 569 0.007767 142.5 571 0.007791 142.7 571 0.007816 143 572 0.007829 143.2 574 0.007841 143.4 574 0.007866 143.7 575 0.007866 143.9 576 0.00789 144.1 577 0.007903 144.4 578 0.007928 144.6 579 0.007952 144.8 580 0.007965 145.1 581 0.007977 145.3 582 0.008002 145.5 583 0.008014 145.8 584 0.008027 146 585 0.008027 146.3 585 0.008051 146.5 587 0.008064 146.7 588 0.008076 147 589 0.008076 147.2 589 0.008076 147.4 590 0.008101 147.7 592 0.008113 147.9 592 0.008138 148.1 593 0.00815 148.4 594 0.008163 148.6 595 0.008175 148.8 596 0.0082 149.1 596 0.008212 149.3 598 0.008212 149.5 599 0.008249 149.8 600 0.008249 150 601 0.008274 150.2 601 0.008274 150.5 602 0.008299 150.7 603 0.008311 150.9 604 0.008336 151.2 604 0.008361 151.4 606 0.008385 151.6 607 0.00841 151.9 607 0.008423 152.1 609 0.008435 152.3 610 0.008435 152.6 610 0.008435 152.8 611 0.00846 153 613 0.008485 153.3 613 0.008509 153.5 614 0.008522 153.8 615 0.008534 154 617 0.008559 154.2 617 0.008584 154.5 618 0.008584 154.7 619 0.008608 154.9 620 0.008621 155.2 621 0.008633 155.4 621 0.008633 155.6 623 0.008658 155.9 624 0.008683 156.1 625 0.008683 156.3 626 0.008707 156.6 627 0.008707 156.8 628 0.008695 157 628 0.008695 157.3 629 0.008695 157.5 630 0.00872 157.7 631 0.008757 158 632 0.008782 158.2 633 0.008794 158.4 634 0.008806 158.7 635 0.008831 158.9 636 0.008843 159.1 637 0.008868 159.4 638 0.008881 159.6 639 0.008918 159.8 639 0.008942 160.1 640 0.008942 160.3 643 0.008967 160.5 643 0.00898 160.8 644 0.008992 161 645 0.008992 161.3 646 0.008992 161.5 646 0.009004 161.7 647 0.009029 162 649 0.009041 162.2 650 0.009041 162.4 650 0.009066 162.7 651 0.009079 162.9 653 0.009103 163.1 653 0.009128 163.4 654 0.00914 163.6 655 0.009153 163.8 657 0.009153 164.1 657 0.009165 164.3 658 0.009178 164.5 659 0.009202 164.8 660 0.009202 165 660 0.009227 165.2 662 0.00924 165.5 663 0.009252 165.7 664 0.009264 165.9 664 0.009277 166.2 665 0.009301 166.4 667 0.009326 166.6 668 0.009339 166.9 668 0.009351 167.1 669 0.009363 167.3 670 0.009376 167.6 671 0.009388 167.8 671 0.009425 168 673 0.009438 168.3 674 0.00945 168.5 675 0.009475 168.8 676 0.009475 169 678 0.009499 169.2 678 0.009512 169.5 679 0.009512 169.7 680 0.009537 169.9 680 0.009549 170.2 682 0.009549 170.4 683 0.009549 170.6 683 0.009574 170.9 685 0.009586 171.1 685 0.009598 171.3 686 0.009598 171.6 687 0.009611 171.8 688 0.009636 172 689 0.009648 172.3 689 0.009648 172.5 691 0.009685 172.7 692 0.009697 173 693 0.009697 173.2 694 0.00971 173.4 695 0.009722 173.7 696 0.009735 173.9 696 0.009747 174.1 697 0.009772 174.4 699 0.009784 174.6 699 0.009796 174.8 700 0.009821 175.1 701 0.009834 175.3 702 0.009846 175.5 703 0.009846 175.8 703 0.009871 176 705 0.009895 176.3 706 0.009908 176.5 707 0.00992 176.7 708 0.009945 177 709 0.009957 177.2 710 0.009957 177.4 711 0.00997 177.7 711 0.009982 177.9 712 0.009995 178.1 714 0.01001 178.4 714 0.01002 178.6 715 0.01003 178.8 717 0.01004 179.1 718 0.01006 179.3 718 0.01008 179.5 719 0.01009 179.8 720 0.01011 180 721 0.01013 180.2 721 0.01014 180.5 723 0.01016 180.7 724 0.01017 180.9 725 0.01018 181.2 726 0.01018 181.4 727 0.0102 181.6 728 0.01022 181.9 729 0.01022 182.1 730 0.01023 182.3 731 0.01025 182.6 732 0.01027 182.8 732 0.01027 183 733 0.0103 183.3 734 0.01032 183.5 735 0.01034 183.8 736 0.01037 184 736 0.01037 184.2 737 0.01037 184.5 738 0.0104 184.7 738 0.01042 184.9 739 0.01042 185.2 739 0.01042 185.4 740 0.01044 185.6 742 0.01046 185.9 743 0.01046 186.1 743 0.01046 186.3 744 0.01049 186.6 745 0.01051 186.8 746 0.01051 187 746 0.01053 187.3 748 0.01053 187.5 748 0.01053 187.7 750 0.01053 188 750 0.01053 188.2 752 0.01054 188.4 752 0.01056 188.7 753 0.01056 188.9 754 0.01056 189.1 755 0.01059 189.4 756 0.01061 189.6 757 0.01061 189.8 757 0.01063 190.1 758 0.01066 190.3 759 0.01066 190.5 759 0.01068 190.8 760 0.01068 191 761 0.01069 191.3 762 0.01071 191.5 763 0.01074 191.7 764 0.01074 192 765 0.01076 192.2 766 0.01079 192.4 767 0.01081 192.7 768 0.01082 192.9 769 0.01085 193.1 771 0.01086 193.4 771 0.01089 193.6 772 0.01091 193.8 774 0.0109 194.1 775 0.0109 194.3 775 0.01089 194.5 777 0.01089 194.8 778 0.01089 195 779 0.01086 195.2 780 0.01084 195.5 782 0.0108 195.7 782 0.01076 195.9 783 0.01072 196.2 785 0.01071 196.4 786 0.01066 196.6 786 0.01063 196.9 787 0.01056 197.1 788 0.0105 197.3 789 0.01045 197.6 790 0.01038 197.8 792 0.01032 198 793 0.01024 198.3 793 0.01016 198.5 794 0.01008 198.8 796 0.009982 199 796 0.009895 199.2 799 0.009809 199.5 799 0.009722 199.7 800 0.009636 199.9 800 0.009537 200.2 801 0.00945 200.4 801 0.009351 200.6 801 0.009264 200.9 801 0.009178 201.1 802 0.009091 201.3 803 0.009004 201.6 804 0.008942 201.8 805 0.008881 202 807 0.008806 202.3 807 0.008757 202.5 809 0.008707 202.7 811 0.008658 203 811 0.008633 203.2 813 0.008596 203.4 814 0.008584 203.7 815 0.008584 203.9 817 0.008571 204.1 818 0.008584 204.4 818 0.008584 204.6 819 0.008608 204.8 821 0.008608 205.1 821 0.008621 205.3 823 0.008633 205.5 824 0.008645 205.8 824 0.008645 206 825 0.008658 206.3 826 0.008683 206.5 826 0.008695 206.7 827 0.008732 207 828 0.008744 207.2 829 0.008757 207.4 829 0.008757 207.7 830 0.008782 207.9 830 0.008794 208.1 831 0.008794 208.4 832 0.008794 208.6 832 0.008831 208.8 833 0.008831 209.1 834 0.008843 209.3 834 0.008881 209.5 836 0.008881 209.8 836 0.008905 210 837 0.00893 210.2 838 0.008967 210.5 839 0.00898 210.7 840 0.009004 210.9 840 0.009041 211.2 842 0.009054 211.4 843 0.009079 211.6 843 0.009116 211.9 844 0.009128 212.1 846 0.009165 212.3 847 0.009178 212.6 848 0.009202 212.8 849 0.00924 213 850 0.009264 213.3 851 0.009277 213.5 852 0.009301 213.8 853 0.009339 214 854 0.009351 214.2 855 0.009388 214.5 856 0.009425 214.7 857 0.00945 214.9 858 0.009475 215.2 859 0.009499 215.4 860 0.009524 215.6 861 0.009537 215.9 861 0.009549 216.1 862 0.009574 216.3 864 0.009586 216.6 864 0.009611 216.8 865 0.009648 217 866 0.00966 217.3 868 0.009685 217.5 868 0.009697 217.7 869 0.009722 218 870 0.009759 218.2 872 0.009759 218.4 872 0.009772 218.7 874 0.009809 218.9 874 0.009834 219.1 875 0.009846 219.4 876 0.009871 219.6 877 0.009895 219.8 878 0.009933 220.1 879 0.009945 220.3 879 0.00997 220.5 880 0.009995 220.8 882 0.01003 221 882 0.01004 221.3 883 0.01006 221.5 884 0.01009 221.7 885 0.01011 222 886 0.01013 222.2 887 0.01012 222.4 889 0.01017 222.7 889 0.01019 222.9 889 0.0102 223.1 890 0.01023 223.4 892 0.01025 223.6 893 0.01028 223.8 894 0.0103 224.1 894 0.01033 224.3 895 0.01035 224.5 897 0.01038 224.8 897 0.0104 225 898 0.01043 225.2 899 0.01045 225.5 900 0.01048 225.7 900 0.0105 225.9 902 0.01051 226.2 903 0.01053 226.4 904 0.01055 226.6 905 0.01059 226.9 906 0.01061 227.1 907 0.01063 227.3 907 0.01065 227.6 909 0.01066 227.8 910 0.0107 228 911 0.01074 228.3 911 0.01077 228.5 912 0.01079 228.8 913 0.01081 229 914 0.01084 229.2 915 0.01086 229.5 917 0.0109 229.7 917 0.01091 229.9 918 0.01095 230.2 918 0.01096 230.4 919 0.011 230.6 921 0.01102 230.9 922 0.01103 231.1 923 0.01106 231.3 924 0.0111 231.6 925 0.01112 231.8 925 0.01112 232 926 0.01115 232.3 928 0.01117 232.5 928 0.01118 232.7 929 0.01121 233 930 0.01122 233.2 931 0.01126 233.4 932 0.01129 233.7 933 0.01132 233.9 934 0.01134 234.1 935 0.01136 234.4 936 0.01141 234.6 936 0.01142 234.8 938 0.01146 235.1 939 0.01147 235.3 940 0.0115 235.5 940 0.01152 235.8 942 0.01155 236 943 0.01158 236.3 943 0.0116 236.5 944 0.01162 236.7 945 0.01165 237 947 0.01168 237.2 947 0.0117 237.4 948 0.01171 237.7 949 0.01174 237.9 950 0.01175 238.1 950 0.01178 238.4 950 0.01179 238.6 952 0.01183 238.8 953 0.01185 239.1 954 0.01186 239.3 954 0.01189 239.5 955 0.01193 239.8 956 0.01195 240 956 0.01195 240.2 957 0.01197 240.5 957 0.012 240.7 957 0.01201 240.9 957 0.01201 241.2 958 0.01202 241.4 959 0.01205 241.6 960 0.01207 241.9 961 0.01209 242.1 962 0.0121 242.3 964 0.01212 242.6 965 0.01215 242.8 967 0.01219 243 968 0.01221 243.3 969 0.01225 243.5 971 0.0123 243.8 972 0.01233 244 973 0.01236 244.2 975 0.0124 244.5 976 0.01243 244.7 977 0.01246 244.9 979 0.01249 245.2 980 0.01253 245.4 981 0.01256 245.6 982 0.01259 245.9 983 0.01261 246.1 984 0.01264 246.3 985 0.01268 246.6 986 0.01268 246.8 986 0.01268 247 987 0.01268 247.3 989 0.01271 247.5 990 0.01272 247.7 990 0.01275 248 991 0.01279 248.2 992 0.0128 248.4 993 0.01282 248.7 994 0.01284 248.9 994 0.01287 249.1 996 0.01289 249.4 997 0.01293 249.6 997 0.01294 249.8 998 0.01295 250.1 999 0.01299 250.3 1000 0.01301 250.5 1001 0.01304 250.8 1001 0.01305 251 1003 0.01306 251.3 1004 0.01306 251.5 1004 0.01306 251.7 1005 0.0131 252 1006 0.0131 252.2 1007 0.01314 252.4 1008 0.01318 252.7 1009 0.0132 252.9 1009 0.01321 253.1 1011 0.01324 253.4 1011 0.01327 253.6 1013 0.01332 253.8 1014 0.01334 254.1 1015 0.01334 254.3 1015 0.01336 254.5 1017 0.01337 254.8 1018 0.01337 255 1018 0.01337 255.2 1019 0.01339 255.5 1021 0.01339 255.7 1022 0.01342 255.9 1022 0.01346 256.2 1023 0.0135 256.4 1024 0.01355 256.6 1025 0.01358 256.9 1026 0.01361 257.1 1027 0.01365 257.3 1028 0.01368 257.6 1029 0.01372 257.8 1030 0.01372 258 1031 0.01373 258.3 1032 0.01376 258.5 1033 0.01377 258.8 1033 0.01379 259 1035 0.01384 259.2 1036 0.01386 259.5 1036 0.01387 259.7 1038 0.01388 259.9 1038 0.01388 260.2 1040 0.01391 260.4 1040 0.01393 260.6 1042 0.01394 260.9 1042 0.01398 261.1 1043 0.01402 261.3 1043 0.01404 261.6 1044 0.01407 261.8 1046 0.01409 262 1047 0.01412 262.3 1049 0.01414 262.5 1049 0.01417 262.7 1050 0.01418 263 1051 0.01419 263.2 1051 0.01419 263.4 1053 0.01422 263.7 1054 0.01424 263.9 1054 0.01424 264.1 1055 0.01425 264.4 1057 0.01428 264.6 1057 0.0143 264.8 1058 0.01433 265.1 1059 0.01434 265.3 1060 0.01433 265.5 1061 0.01434 265.8 1062 0.01436 266 1063 0.01438 266.3 1065 0.01439 266.5 1065 0.01439 266.7 1066 0.0144 267 1067 0.01444 267.2 1068 0.01446 267.4 1068 0.01448 267.7 1069 0.0145 267.9 1070 0.01454 268.1 1072 0.01455 268.4 1073 0.01457 268.6 1074 0.0146 268.8 1075 0.01462 269.1 1076 0.01466 269.3 1076 0.01466 269.5 1077 0.01469 269.8 1079 0.01471 270 1079 0.01472 270.2 1080 0.01475 270.5 1081 0.01477 270.7 1082 0.01481 270.9 1083 0.01483 271.2 1084 0.0148 271.4 1085 0.01478 271.6 1086 0.01481 271.9 1086 0.01485 272.1 1088 0.01491 272.3 1089 0.01497 272.6 1090 0.01498 272.8 1090 0.01501 273 1091 0.01502 273.3 1093 0.01503 273.5 1094 0.01504 273.8 1094 0.01508 274 1094 0.01511 274.2 1096 0.01513 274.5 1097 0.01514 274.7 1098 0.01518 274.9 1099 0.01519 275.2 1100 0.01521 275.4 1101 0.01527 275.6 1101 0.01527 275.9 1102 0.0153 276.1 1104 0.01532 276.3 1104 0.01535 276.6 1105 0.01538 276.8 1106 0.01543 277 1107 0.01544 277.3 1108 0.01545 277.5 1109 0.01551 277.7 1110 0.01551 278 1111 0.01555 278.2 1112 0.01559 278.4 1112 0.0156 278.7 1114 0.01564 278.9 1115 0.01568 279.1 1115 0.0157 279.4 1117 0.01573 279.6 1118 0.01575 279.8 1119 0.01576 280.1 1120 0.01579 280.3 1122 0.01582 280.5 1122 0.01585 280.8 1123 0.01586 281 1124 0.01589 281.3 1125 0.0159 281.5 1126 0.01591 281.7 1126 0.01596 282 1128 0.01597 282.2 1128 0.016 282.4 1129 0.01603 282.7 1130 0.01603 282.9 1131 0.01607 283.1 1132 0.01611 283.4 1133 0.01613 283.6 1134 0.01615 283.8 1134 0.01617 284.1 1135 0.01618 284.3 1136 0.01622 284.5 1136 0.01624 284.8 1138 0.01626 285 1138 0.01628 285.2 1140 0.01631 285.5 1141 0.01632 285.7 1142 0.01637 285.9 1143 0.01639 286.2 1144 0.01642 286.4 1145 0.01646 286.6 1147 0.01648 286.9 1148 0.01649 287.1 1149 0.01652 287.3 1150 0.01653 287.6 1151 0.01655 287.8 1151 0.01659 288 1152 0.01662 288.3 1154 0.0166 288.5 1154 0.01662 288.8 1155 0.01665 289 1156 0.01669 289.2 1157 0.01672 289.5 1158 0.01673 289.7 1158 0.01673 289.9 1159 0.01675 290.2 1161 0.01679 290.4 1162 0.01681 290.6 1162 0.01683 290.9 1164 0.01684 291.1 1165 0.01686 291.3 1165 0.01688 291.6 1166 0.01689 291.8 1167 0.0169 292 1168 0.01693 292.3 1169 0.01694 292.5 1170 0.01698 292.7 1172 0.017 293 1172 0.01702 293.2 1173 0.01704 293.4 1174 0.01706 293.7 1175 0.01709 293.9 1176 0.01709 294.1 1177 0.01711 294.4 1178 0.01712 294.6 1178 0.01715 294.8 1179 0.01717 295.1 1180 0.0172 295.3 1181 0.01722 295.5 1183 0.01726 295.8 1183 0.01728 296 1184 0.01731 296.3 1185 0.01732 296.5 1187 0.01735 296.7 1187 0.01735 297 1188 0.01737 297.2 1189 0.0174 297.4 1190 0.01741 297.7 1190 0.01742 297.9 1192 0.01746 298.1 1193 0.01748 298.4 1194 0.0175 298.6 1194 0.01752 298.8 1195 0.01756 299.1 1197 0.01758 299.3 1197 0.01759 299.5 1199 0.01763 299.8 1200 0.01763 300 1201 0.01767 300.2 1201 0.01768 300.5 1201 0.01771 300.7 1201 0.01769 300.9 1201 0.01771 301.2 1201 0.01771 301.4 1201 0.01769 301.6 1201 0.01769 301.9 1201 0.01771 302.1 1201 0.01769 302.3 1200 0.01768 302.6 1200 0.01767 302.8 1200 0.01768 303 1200 0.01766 303.3 1200 0.01764 303.5 1199 0.01762 303.8 1199 0.01763 304 1199 0.01761 304.2 1199 0.01762 304.5 1199 0.01761 304.7 1199 0.01761 304.9 1199 0.01756 305.2 1199 0.01759 305.4 1199 0.01758 305.6 1199 0.01759 305.9 1199 0.01757 306.1 1199 0.01758 306.3 1199 0.01756 306.6 1199 0.01756 306.8 1199 0.01754 307 1199 0.01754 307.3 1199 0.01753 307.5 1199 0.01754 307.7 1199 0.01753 308 1199 0.01753 308.2 1199 0.01754 308.4 1199 0.01752 308.7 1199 0.01752 308.9 1199 0.01752 309.1 1199 0.01751 309.4 1199 0.01751 309.6 1199 0.01752 309.8 1199 0.01753 310.1 1199 0.01752 310.3 1199 0.01753 310.5 1199 0.01751 310.8 1199 0.01751 311 1199 0.01751 311.3 1199 0.0175 311.5 1199 0.0175 311.7 1199 0.01748 312 1199 0.0175 312.2 1199 0.01751 312.4 1199 0.01748 312.7 1199 0.0175 312.9 1199 0.0175 313.1 1199 0.0175 313.4 1199 0.0175 313.6 1199 0.01751 313.8 1199 0.0175 314.1 1199 0.01748 314.3 1199 0.01747 314.5 1199 0.01746 314.8 1199 0.01745 315 1199 0.01746 315.2 1199 0.01746 315.5 1199 0.01743 315.7 1199 0.01745 315.9 1199 0.01746 316.2 1199 0.01745 316.4 1199 0.01743 316.6 1199 0.01742 316.9 1199 0.01743 317.1 1199 0.01745 317.3 1199 0.01743 317.6 1199 0.01742 317.8 1199 0.01743 318 1199 0.01745 318.3 1199 0.01743 318.5 1199 0.01742 318.8 1199 0.01742 319 1199 0.01742 319.2 1199 0.01741 319.5 1199 0.01741 319.7 1199 0.01741 319.9 1199 0.01741 320.2 1199 0.01741 320.4 1199 0.01741 320.6 1199 0.01742 320.9 1199 0.01741 321.1 1199 0.0174 321.3 1199 0.0174 321.6 1199 0.0174 321.8 1199 0.0174 322 1199 0.01741 322.3 1199 0.01741 322.5 1199 0.01741 322.7 1199 0.01738 323 1199 0.01738 323.2 1199 0.01737 323.4 1199 0.01736 323.7 1199 0.01737 323.9 1199 0.01736 324.1 1199 0.01736 324.4 1199 0.01737 324.6 1199 0.01736 324.8 1199 0.01736 325.1 1199 0.01736 325.3 1199 0.01736 325.5 1199 0.01736 325.8 1199 0.01736 326 1199 0.01736 326.3 1199 0.01736 326.5 1199 0.01736 326.7 1199 0.01736 327 1199 0.01733 327.2 1199 0.01732 327.4 1199 0.01731 327.7 1199 0.01732 327.9 1200 0.01731 328.1 1199 0.0173 328.4 1199 0.01731 328.6 1199 0.01731 328.8 1199 0.0173 329.1 1199 0.01731 329.3 1199 0.01731 329.5 1199 0.01731 329.8 1199 0.01731 330 1199 0.0173 330.2 1199 0.0173 330.5 1199 0.0173 330.7 1199 0.01731 330.9 1199 0.0173 331.2 1199 0.01731 331.4 1199 0.0173 331.6 1199 0.0173 331.9 1199 0.01728 332.1 1199 0.01727 332.3 1199 0.01727 332.6 1199 0.01728 332.8 1199 0.01728 333 1199 0.01726 333.3 1199 0.01727 333.5 1199 0.01726 333.8 1199 0.01726 334 1199 0.01726 334.2 1199 0.01726 334.5 1199 0.01726 334.7 1199 0.01726 334.9 1199 0.01726 335.2 1199 0.01724 335.4 1199 0.01725 335.6 1199 0.01725 335.9 1199 0.01726 336.1 1199 0.01724 336.3 1199 0.01724 336.6 1199 0.01725 336.8 1199 0.01724 337 1199 0.01724 337.3 1199 0.01725 337.5 1199 0.01724 337.7 1199 0.01724 338 1199 0.01725 338.2 1199 0.01724 338.4 1199 0.01722 338.7 1199 0.01721 338.9 1199 0.01721 339.1 1199 0.0172 339.4 1199 0.01722 339.6 1199 0.0172 339.8 1199 0.0172 340.1 1199 0.0172 340.3 1199 0.01719 340.5 1199 0.01719 340.8 1199 0.01717 341 1199 0.0172 341.3 1199 0.01717 341.5 1199 0.01716 341.7 1199 0.01716 342 1199 0.01716 342.2 1199 0.01717 342.4 1199 0.01716 342.7 1199 0.01716 342.9 1199 0.01716 343.1 1199 0.01715 343.4 1199 0.01715 343.6 1199 0.01716 343.8 1199 0.01715 344.1 1199 0.01715 344.3 1199 0.01715 344.5 1199 0.01715 344.8 1199 0.01714 345 1199 0.01715 345.2 1199 0.01715 345.5 1199 0.01715 345.7 1199 0.01715 345.9 1199 0.01715 346.2 1199 0.01715 346.4 1199 0.01712 346.6 1199 0.01714 346.9 1199 0.01712 347.1 1199 0.01715 347.3 1199 0.01714 347.6 1199 0.01712 347.8 1199 0.01714 348 1199 0.01715 348.3 1199 0.01712 348.5 1199 0.01711 348.8 1199 0.01712 349 1199 0.01711 349.2 1199 0.01711 349.5 1199 0.0171 349.7 1199 0.01712 349.9 1199 0.01712 350.2 1199 0.01711 350.4 1199 0.0171 350.6 1199 0.01712 350.9 1199 0.01712 351.1 1199 0.01711 351.3 1199 0.0171 351.6 1199 0.01711 351.8 1199 0.01712 352 1199 0.01711 352.3 1199 0.0171 352.5 1199 0.01709 352.7 1199 0.0171 353 1199 0.0171 353.2 1199 0.0171 353.4 1199 0.01709 353.7 1199 0.01706 353.9 1199 0.01706 354.1 1199 0.01706 354.4 1199 0.01705 354.6 1199 0.01706 354.8 1199 0.01709 355.1 1199 0.0171 355.3 1199 0.0171 355.5 1199 0.0171 355.8 1199 0.0171 356 1199 0.01711 356.3 1199 0.0171 356.5 1199 0.0171 356.7 1199 0.0171 357 1199 0.01711 357.2 1199 0.0171 357.4 1199 0.0171 357.7 1199 0.0171 357.9 1199 0.01707 358.1 1199 0.01706 358.4 1199 0.01705 358.6 1199 0.01706 358.8 1199 0.01705 359.1 1199 0.01705 359.3 1199 0.01707 359.5 1199 0.01706 359.8 1199 0.01709 360 1199 0.01709 360.2 1199 0.0171 360.5 1199 0.0171 360.7 1199 0.0171 360.9 1199 0.0171 361.2 1199 0.01709 361.4 1199 0.01707 361.6 1199 0.01707 361.9 1199 0.01709 362.1 1199 0.01709 362.3 1199 0.01706 362.6 1199 0.01706 362.8 1199 0.01705 363 1199 0.01706 363.3 1199 0.01706 363.5 1199 0.01707 363.8 1199 0.01706 364 1199 0.01706 364.2 1199 0.01705 364.5 1199 0.01705 364.7 1199 0.01705 364.9 1199 0.01705 365.2 1199 0.01705 365.4 1199 0.01705 365.6 1199 0.01705 365.9 1199 0.01706 366.1 1199 0.01705 366.3 1199 0.01705 366.6 1199 0.01705 366.8 1199 0.01704 367 1199 0.01704 367.3 1199 0.01705 367.5 1199 0.01705 367.7 1199 0.01705 368 1199 0.01702 368.2 1199 0.01704 368.4 1199 0.01704 368.7 1199 0.01705 368.9 1199 0.01705 369.1 1199 0.01705 369.4 1199 0.01705 369.6 1199 0.01705 369.8 1199 0.01705 370.1 1199 0.01705 370.3 1199 0.01705 370.5 1199 0.01705 370.8 1199 0.01702 371 1199 0.01702 371.3 1199 0.01704 371.5 1199 0.01701 371.7 1199 0.01701 372 1199 0.01701 372.2 1199 0.017 372.4 1199 0.01702 372.7 1199 0.01702 372.9 1199 0.01705 373.1 1199 0.01705 373.4 1199 0.01702 373.6 1199 0.01704 373.8 1199 0.01705 374.1 1199 0.01705 374.3 1199 0.01705 374.5 1199 0.01704 374.8 1199 0.01702 375 1199 0.01702 375.2 1199 0.01701 375.5 1199 0.01702 375.7 1199 0.01702 375.9 1199 0.01701 376.2 1199 0.017 376.4 1199 0.01701 376.6 1199 0.01701 376.9 1199 0.01701 377.1 1199 0.01702 377.3 1199 0.01701 377.6 1199 0.017 377.8 1199 0.017 378 1199 0.01701 378.3 1199 0.017 378.5 1199 0.017 378.8 1199 0.017 379 1199 0.01699 379.2 1199 0.01699 379.5 1199 0.017 379.7 1199 0.017 379.9 1199 0.017 380.2 1199 0.01698 380.4 1199 0.01698 380.6 1199 0.017 380.9 1199 0.01699 381.1 1199 0.01698 381.3 1199 0.01699 381.6 1199 0.017 381.8 1199 0.017 382 1199 0.017 382.3 1199 0.017 382.5 1199 0.017 382.7 1199 0.017 383 1199 0.01701 383.2 1199 0.01699 383.4 1199 0.017 383.7 1199 0.017 383.9 1199 0.017 384.1 1199 0.017 384.4 1199 0.01699 384.6 1199 0.017 384.8 1199 0.01696 385.1 1199 0.01694 385.3 1199 0.01695 385.5 1199 0.01696 385.8 1199 0.01698 386 1199 0.01699 386.3 1199 0.017 386.5 1199 0.017 386.7 1199 0.017 387 1199 0.017 387.2 1199 0.017 387.4 1199 0.017 387.7 1199 0.01696 387.9 1199 0.01698 388.1 1199 0.01699 388.4 1199 0.01699 388.6 1199 0.017 388.8 1199 0.017 389.1 1199 0.017 389.3 1199 0.017 389.5 1199 0.017 389.8 1199 0.017 390 1199 0.01698 390.2 1199 0.01696 390.5 1199 0.01696 390.7 1199 0.01695 390.9 1199 0.01695 391.2 1199 0.01695 391.4 1199 0.01695 391.6 1199 0.01695 391.9 1199 0.01695 392.1 1199 0.01695 392.3 1199 0.01695 392.6 1199 0.01696 392.8 1199 0.01696 393 1199 0.01696 393.3 1199 0.01695 393.5 1199 0.01695 393.8 1199 0.01695 394 1199 0.01696 394.2 1199 0.01695 394.5 1199 0.01695 394.7 1199 0.01695 394.9 1199 0.01695 395.2 1199 0.01695 395.4 1199 0.01695 395.6 1199 0.01695 395.9 1199 0.01695 396.1 1199 0.01695 396.3 1199 0.01695 396.6 1199 0.01695 396.8 1199 0.01695 397 1199 0.01695 397.3 1199 0.01695 397.5 1199 0.01695 397.7 1199 0.01695 398 1199 0.01693 398.2 1199 0.01693 398.4 1199 0.01694 398.7 1199 0.01694 398.9 1199 0.01695 399.1 1199 0.01694 399.4 1199 0.01693 399.6 1199 0.01694 399.8 1199 0.01695 400.1 1199 0.01695 400.3 1199 0.01693 400.5 1199 0.01693 400.8 1199 0.01694 401 1199 0.01694 401.3 1199 0.01695 401.5 1199 0.01695 401.7 1199 0.01695 402 1199 0.01695 402.2 1199 0.01693 402.4 1199 0.01694 402.7 1199 0.01695 402.9 1199 0.01693 403.1 1199 0.01691 403.4 1199 0.01693 403.6 1199 0.01693 403.8 1199 0.01693 404.1 1199 0.01693 404.3 1199 0.01693 404.5 1199 0.01691 404.8 1199 0.01691 405 1199 0.01691 405.2 1199 0.01693 405.5 1199 0.01693 405.7 1199 0.01694 405.9 1199 0.01696 406.2 1199 0.01696 406.4 1199 0.01694 406.6 1199 0.01693 406.9 1199 0.01693 407.1 1199 0.01691 407.3 1199 0.01693 407.6 1199 0.01691 407.8 1199 0.01693 408 1199 0.01691 408.3 1199 0.01693 408.5 1200 0.01691 408.8 1199 0.01693 409 1199 0.01694 409.2 1199 0.01694 409.5 1200 0.01693 409.7 1199 0.01693 409.9 1199 0.01693 410.2 1199 0.01693 410.4 1199 0.01691 410.6 1199 0.01693 410.9 1199 0.01691 411.1 1199 0.01693 411.3 1199 0.01693 411.6 1199 0.01693 411.8 1199 0.01693 412 1199 0.01691 412.3 1199 0.01691 412.5 1199 0.0169 412.7 1199 0.0169 413 1199 0.01693 413.2 1199 0.01691 413.4 1199 0.01693 413.7 1199 0.01691 413.9 1199 0.01691 414.1 1199 0.01693 414.4 1199 0.01691 414.6 1199 0.01693 414.8 1199 0.01693 415.1 1199 0.0169 415.3 1199 0.01693 415.5 1199 0.01691 415.8 1199 0.01691 416 1199 0.01693 416.3 1199 0.01691 416.5 1199 0.0169 416.7 1199 0.01693 417 1199 0.01691 417.2 1199 0.0169 417.4 1199 0.0169 417.7 1199 0.0169 417.9 1199 0.01689 418.1 1199 0.01689 418.4 1199 0.0169 418.6 1199 0.01691 418.8 1199 0.01691 419.1 1199 0.0169 419.3 1199 0.0169 419.5 1199 0.01691 419.8 1199 0.0169 420 1199 0.0169 420.2 1199 0.0169 420.5 1199 0.0169 420.7 1199 0.0169 420.9 1199 0.0169 421.2 1200 0.0169 421.4 1199 0.0169 421.6 1199 0.01691 421.9 1199 0.01693 422.1 1199 0.01693 422.3 1199 0.01691 422.6 1199 0.01689 422.8 1199 0.01686 423 1199 0.01686 423.3 1199 0.01685 423.5 1199 0.01685 423.8 1199 0.01685 424 1199 0.01685 424.2 1199 0.01686 424.5 1199 0.01688 424.7 1199 0.01688 424.9 1199 0.01686 425.2 1200 0.01686 425.4 1199 0.01686 425.6 1199 0.01686 425.9 1199 0.01688 426.1 1199 0.01689 426.3 1199 0.01686 426.6 1199 0.01686 426.8 1199 0.01686 427 1199 0.01689 427.3 1199 0.01689 427.5 1199 0.0169 427.7 1199 0.01688 428 1199 0.01686 428.2 1199 0.01686 428.4 1199 0.01685 428.7 1199 0.01684 428.9 1199 0.01684 429.1 1199 0.01683 429.4 1199 0.01681 429.6 1199 0.0168 429.8 1199 0.0168 430.1 1199 0.01681 430.3 1199 0.01683 430.5 1199 0.01684 430.8 1199 0.01684 431 1199 0.01685 431.3 1199 0.01685 431.5 1199 0.01685 431.7 1199 0.01685 432 1199 0.01685 432.2 1199 0.01685 432.4 1199 0.01686 432.7 1199 0.01686 432.9 1199 0.01686 433.1 1199 0.01685 433.4 1199 0.01685 433.6 1199 0.01685 433.8 1199 0.01685 434.1 1199 0.01685 434.3 1199 0.01685 434.5 1199 0.01685 434.8 1199 0.01685 435 1199 0.01685 435.2 1199 0.01685 435.5 1199 0.01685 435.7 1199 0.01685 435.9 1199 0.01684 436.2 1199 0.01685 436.4 1199 0.01685 436.6 1199 0.01685 436.9 1199 0.01685 437.1 1199 0.01684 437.3 1199 0.01685 437.6 1199 0.01685 437.8 1199 0.01688 438 1199 0.01686 438.3 1199 0.01686 438.5 1199 0.01685 438.8 1199 0.01685 439 1199 0.01683 439.2 1199 0.01684 439.5 1199 0.01684 439.7 1199 0.01684 439.9 1199 0.01685 440.2 1199 0.01683 440.4 1199 0.01683 440.6 1199 0.01686 440.9 1199 0.01686 441.1 1199 0.01686 441.3 1199 0.01686 441.6 1199 0.01686 441.8 1199 0.01686 442 1199 0.01685 442.3 1199 0.01684 442.5 1199 0.01683 442.7 1199 0.0168 443 1199 0.01679 443.2 1199 0.01678 443.4 1199 0.01679 443.7 1199 0.01679 443.9 1199 0.01681 444.1 1199 0.01681 444.4 1199 0.01683 444.6 1199 0.01683 444.8 1199 0.01684 445.1 1199 0.01685 445.3 1199 0.01685 445.5 1199 0.01684 445.8 1199 0.01686 446 1199 0.01686 446.3 1199 0.01685 446.5 1199 0.01684 446.7 1199 0.01684 447 1199 0.01684 447.2 1199 0.01683 447.4 1199 0.01681 447.7 1199 0.01683 447.9 1199 0.01684 448.1 1199 0.01684 448.4 1199 0.01681 448.6 1199 0.01684 448.8 1199 0.01684 449.1 1199 0.01684 449.3 1199 0.01684 449.5 1199 0.01683 449.8 1199 0.01683 450 1199 0.01681 450.2 1199 0.01681 450.5 1199 0.01683 450.7 1199 0.01681 450.9 1199 0.0168 451.2 1199 0.01684 451.4 1199 0.01681 451.6 1199 0.0168 451.9 1199 0.01681 452.1 1199 0.01681 452.3 1199 0.0168 452.6 1199 0.0168 452.8 1199 0.0168 453 1199 0.01679 453.3 1199 0.01676 453.5 1199 0.01678 453.8 1199 0.01678 454 1199 0.0168 454.2 1199 0.01679 454.5 1199 0.0168 454.7 1199 0.01683 454.9 1199 0.0168 455.2 1199 0.0168 455.4 1199 0.0168 455.6 1199 0.01683 455.9 1199 0.01683 456.1 1199 0.01681 456.3 1199 0.01681 456.6 1199 0.0168 456.8 1199 0.01683 457 1199 0.01684 457.3 1199 0.01683 457.5 1199 0.0168 457.7 1199 0.0168 458 1199 0.0168 458.2 1199 0.0168 458.4 1199 0.0168 458.7 1199 0.0168 458.9 1199 0.0168 459.1 1199 0.0168 459.4 1199 0.0168 459.6 1199 0.0168 459.8 1199 0.0168 460.1 1199 0.0168 460.3 1199 0.0168 460.5 1199 0.01683 460.8 1199 0.01683 461 1199 0.01684 461.3 1199 0.01684 461.5 1199 0.01685 461.7 1199 0.01684 462 1199 0.01685 462.2 1199 0.01681 462.4 1199 0.01681 462.7 1199 0.01678 462.9 1199 0.01676 463.1 1199 0.01678 463.4 1199 0.01676 463.6 1199 0.01678 463.8 1199 0.01678 464.1 1199 0.0168 464.3 1199 0.0168 464.5 1199 0.0168 464.8 1199 0.0168 465 1199 0.0168 465.2 1199 0.0168 465.5 1199 0.0168 465.7 1199 0.01679 465.9 1199 0.0168 466.2 1199 0.0168 466.4 1199 0.0168 466.6 1199 0.0168 466.9 1199 0.0168 467.1 1199 0.0168 467.3 1199 0.0168 467.6 1199 0.0168 467.8 1199 0.0168 468 1199 0.0168 468.3 1199 0.01679 468.5 1199 0.0168 468.8 1199 0.0168 469 1199 0.0168 469.2 1199 0.0168 469.5 1199 0.0168 469.7 1199 0.0168 469.9 1199 0.0168 470.2 1199 0.01678 470.4 1199 0.01678 470.6 1199 0.01679 470.9 1199 0.0168 471.1 1199 0.0168 471.3 1199 0.0168 471.6 1199 0.0168 471.8 1199 0.0168 472 1199 0.0168 472.3 1199 0.0168 472.5 1199 0.0168 472.7 1199 0.0168 473 1199 0.0168 473.2 1199 0.0168 473.4 1199 0.01678 473.7 1199 0.01678 473.9 1199 0.0168 474.1 1199 0.01679 474.4 1199 0.01678 474.6 1199 0.01678 474.8 1199 0.01679 475.1 1199 0.01676 475.3 1199 0.01675 475.5 1199 0.01678 475.8 1199 0.01679 476 1199 0.01676 476.3 1199 0.01678 476.5 1199 0.01679 476.7 1199 0.01676 477 1199 0.01678 477.2 1199 0.01678 477.4 1199 0.0168 477.7 1199 0.01679 477.9 1199 0.01678 478.1 1199 0.01678 478.4 1199 0.01679 478.6 1199 0.01679 478.8 1199 0.0168 479.1 1199 0.0168 479.3 1199 0.01679 479.5 1199 0.01678 479.8 1199 0.01678 480 1199 0.01679 480.2 1199 0.0168 480.5 1199 0.0168 480.7 1199 0.0168 480.9 1199 0.01678 481.2 1199 0.01678 481.4 1199 0.01676 481.6 1199 0.01678 481.9 1199 0.01676 482.1 1199 0.01678 482.3 1199 0.01676 482.6 1199 0.01678 482.8 1199 0.01678 483 1199 0.01678 483.3 1200 0.01676 483.5 1199 0.0168 483.8 1199 0.01678 484 1199 0.01679 484.2 1199 0.0168 484.5 1199 0.0168 484.7 1199 0.0168 484.9 1199 0.0168 485.2 1199 0.01679 485.4 1199 0.0168 485.6 1199 0.01678 485.9 1199 0.01678 486.1 1199 0.01676 486.3 1199 0.01679 486.6 1199 0.01679 486.8 1199 0.01678 487 1199 0.01678 487.3 1199 0.01676 487.5 1199 0.01675 487.7 1199 0.01676 488 1199 0.01676 488.2 1199 0.01678 488.4 1199 0.01678 488.7 1199 0.01678 488.9 1199 0.01678 489.1 1199 0.01679 489.4 1199 0.0168 489.6 1199 0.0168 489.8 1199 0.0168 490.1 1199 0.0168 490.3 1199 0.01679 490.5 1199 0.01676 490.8 1200 0.01676 491 1199 0.01675 491.3 1199 0.01675 491.5 1199 0.01675 491.7 1199 0.01676 492 1199 0.01676 492.2 1199 0.01675 492.4 1199 0.01675 492.7 1199 0.01678 492.9 1199 0.01678 493.1 1199 0.01676 493.4 1199 0.01675 493.6 1199 0.01678 493.8 1199 0.01678 494.1 1199 0.01676 494.3 1199 0.01676 494.5 1199 0.01675 494.8 1199 0.01675 495 1199 0.01676 495.2 1199 0.01679 495.5 1199 0.0168 495.7 1199 0.01678 495.9 1199 0.01674 496.2 1199 0.0167 496.4 1199 0.0167 496.6 1199 0.01673 496.9 1199 0.01675 497.1 1199 0.01676 497.3 1199 0.01676 497.6 1199 0.01675 497.8 1199 0.01674 498 1199 0.01675 498.3 1199 0.01675 498.5 1199 0.01674 498.8 1199 0.01674 499 1199 0.01675 499.2 1199 0.01676 499.5 1199 0.01678 499.7 1199 0.01679 499.9 1199 0.0168 500.2 1199 0.0168 500.4 1199 0.0168 500.6 1199 0.01678 500.9 1199 0.01676 501.1 1199 0.01675 501.3 1199 0.01675 501.6 1199 0.01674 501.8 1199 0.01676 502 1199 0.01676 502.3 1199 0.01675 502.5 1199 0.01675 502.7 1199 0.01675 503 1199 0.01675 503.2 1199 0.01676 503.4 1199 0.01678 503.7 1199 0.01679 503.9 1199 0.01676 504.1 1199 0.01676 504.4 1199 0.01675 504.6 1199 0.01675 504.8 1199 0.01675 505.1 1199 0.01675 505.3 1199 0.01674 505.5 1199 0.01674 505.8 1199 0.01676 506 1199 0.01675 506.3 1199 0.01675 506.5 1199 0.01675 506.7 1199 0.01676 507 1199 0.01678 507.2 1199 0.01679 507.4 1199 0.0168 507.7 1199 0.01679 507.9 1199 0.01678 508.1 1199 0.01676 508.4 1199 0.01675 508.6 1199 0.01676 508.8 1199 0.01678 509.1 1199 0.01678 509.3 1199 0.01676 509.5 1199 0.01675 509.8 1199 0.01676 510 1199 0.01678 510.2 1199 0.01678 510.5 1199 0.01676 510.7 1199 0.01675 510.9 1199 0.01675 511.2 1199 0.01678 511.4 1199 0.01678 511.6 1199 0.01679 511.9 1199 0.01678 512.1 1199 0.01674 512.3 1199 0.01674 512.6 1199 0.01672 512.8 1199 0.01672 513 1199 0.01672 513.3 1199 0.01675 513.5 1199 0.01676 513.8 1199 0.01675 514 1199 0.01675 514.2 1199 0.01673 514.5 1199 0.0167 514.7 1199 0.0167 514.9 1199 0.0167 515.2 1199 0.0167 515.4 1199 0.0167 515.6 1199 0.01673 515.9 1199 0.01673 516.1 1199 0.01674 516.3 1199 0.01676 516.6 1199 0.01676 516.8 1199 0.01675 517 1199 0.01674 517.3 1199 0.01673 517.5 1199 0.01672 517.7 1199 0.0167 518 1199 0.0167 518.2 1199 0.01674 518.4 1199 0.01674 518.7 1199 0.01676 518.9 1199 0.01675 519.1 1199 0.01676 519.4 1199 0.01676 519.6 1199 0.01674 519.8 1199 0.01675 520.1 1199 0.01676 520.3 1199 0.01676 520.5 1199 0.01676 520.8 1199 0.01675 521 1199 0.01676 521.3 1199 0.01675 521.5 1199 0.01675 521.7 1199 0.01674 522 1199 0.01675 522.2 1199 0.01676 522.4 1199 0.01675 522.7 1199 0.01675 522.9 1199 0.01674 523.1 1199 0.01675 523.4 1199 0.01675 523.6 1199 0.01675 523.8 1199 0.01676 524.1 1199 0.01675 524.3 1199 0.01678 524.5 1199 0.01676 524.8 1199 0.01678 525 1199 0.01676 525.2 1199 0.01678 525.5 1199 0.01676 525.7 1199 0.01675 525.9 1199 0.01676 526.2 1199 0.01676 526.4 1199 0.01676 526.6 1199 0.01676 526.9 1199 0.01676 527.1 1199 0.01676 527.3 1199 0.01678 527.6 1199 0.01676 527.8 1199 0.01678 528 1199 0.01676 528.3 1199 0.01675 528.5 1199 0.01676 528.8 1199 0.01675 529 1199 0.01673 529.2 1199 0.01676 529.5 1199 0.01675 529.7 1199 0.01675 529.9 1199 0.01676 530.2 1199 0.01678 530.4 1199 0.01676 530.6 1199 0.01678 530.9 1199 0.01678 531.1 1199 0.01678 531.3 1199 0.01676 531.6 1199 0.01678 531.8 1199 0.01678 532 1199 0.01678 532.3 1199 0.01678 532.5 1199 0.01679 532.7 1199 0.01679 533 1199 0.0168 533.2 1199 0.01679 533.4 1199 0.01676 533.7 1199 0.01675 533.9 1199 0.01675 534.1 1199 0.01675 534.4 1199 0.01673 534.6 1199 0.0167 534.8 1199 0.01669 535.1 1199 0.01669 535.3 1199 0.01669 535.5 1199 0.01672 535.8 1199 0.01673 536 1199 0.01674 536.3 1199 0.01672 536.5 1199 0.0167 536.7 1199 0.0167 537 1199 0.01672 537.2 1199 0.01673 537.4 1199 0.01675 537.7 1199 0.01676 537.9 1199 0.01679 538.1 1199 0.01676 538.4 1199 0.01676 538.6 1199 0.01676 538.8 1199 0.01676 539.1 1199 0.01675 539.3 1199 0.01675 539.5 1199 0.01675 539.8 1199 0.01675 540 1199 0.01675 540.2 1199 0.01674 540.5 1199 0.01674 540.7 1199 0.01675 540.9 1199 0.01675 541.2 1199 0.01675 541.4 1199 0.01675 541.6 1199 0.01675 541.9 1199 0.01675 542.1 1199 0.01675 542.3 1199 0.01675 542.6 1199 0.01674 542.8 1199 0.01675 543 1199 0.01675 543.3 1199 0.01675 543.5 1199 0.01675 543.8 1199 0.01674 544 1199 0.01675 544.2 1199 0.01675 544.5 1199 0.01675 544.7 1200 0.01675 544.9 1199 0.01675 545.2 1199 0.01678 545.4 1199 0.01678 545.6 1199 0.01679 545.9 1199 0.01678 546.1 1199 0.01678 546.3 1199 0.01678 546.6 1199 0.01676 546.8 1199 0.01678 547 1199 0.01679 547.3 1199 0.01679 547.5 1199 0.0168 547.7 1199 0.01679 548 1199 0.01678 548.2 1199 0.01676 548.4 1199 0.01675 548.7 1199 0.01675 548.9 1199 0.01675 549.1 1199 0.01675 549.4 1199 0.01676 549.6 1199 0.01678 549.8 1199 0.01678 550.1 1199 0.01676 550.3 1199 0.01676 550.5 1199 0.01679 550.8 1199 0.01678 551 1199 0.01676 551.3 1199 0.01676 551.5 1199 0.01678 551.7 1199 0.01678 552 1199 0.01675 552.2 1199 0.01675 552.4 1199 0.01676 552.7 1199 0.01678 552.9 1199 0.01675 553.1 1199 0.01675 553.4 1199 0.01678 553.6 1199 0.01678 553.8 1199 0.01676 554.1 1199 0.01675 554.3 1199 0.01678 554.5 1199 0.01675 554.8 1199 0.01672 555 1199 0.01673 555.2 1199 0.01674 555.5 1199 0.01672 555.7 1199 0.01674 555.9 1199 0.01676 556.2 1199 0.01676 556.4 1199 0.01676 556.6 1199 0.01676 556.9 1199 0.01676 557.1 1199 0.01676 557.3 1199 0.01676 557.6 1199 0.01676 557.8 1199 0.01679 558 1199 0.01678 558.3 1199 0.01678 558.5 1199 0.01678 558.8 1199 0.01676 559 1199 0.01678 559.2 1199 0.01678 559.5 1199 0.01676 559.7 1199 0.01678 559.9 1199 0.01676 560.2 1199 0.01678 560.4 1199 0.01676 560.6 1199 0.01678 560.9 1199 0.01679 561.1 1199 0.0168 561.3 1199 0.01679 561.6 1199 0.01678 561.8 1199 0.01678 562 1199 0.01675 562.3 1199 0.01674 562.5 1199 0.01672 562.7 1199 0.0167 563 1199 0.01667 563.2 1199 0.01665 563.4 1199 0.01667 563.7 1199 0.01668 563.9 1199 0.01669 564.1 1199 0.0167 564.4 1199 0.01673 564.6 1199 0.01673 564.8 1199 0.01673 565.1 1199 0.01673 565.3 1199 0.01673 565.5 1199 0.01675 565.8 1199 0.01675 566 1199 0.01676 566.3 1199 0.01676 566.5 1199 0.01675 566.7 1199 0.01676 567 1199 0.01676 567.2 1199 0.01679 567.4 1199 0.0168 567.7 1199 0.0168 567.9 1199 0.0168 568.1 1199 0.01676 568.4 1199 0.01675 568.6 1199 0.01675 568.8 1199 0.01674 569.1 1199 0.01675 569.3 1199 0.01676 569.5 1199 0.01674 569.8 1199 0.01674 570 1199 0.01675 570.2 1199 0.01675 570.5 1199 0.01675 570.7 1199 0.01676 570.9 1199 0.01678 571.2 1199 0.01675 571.4 1199 0.01675 571.6 1199 0.01676 571.9 1199 0.01676 572.1 1199 0.01675 572.3 1199 0.01678 572.6 1199 0.01679 572.8 1199 0.01679 573 1199 0.0168 573.3 1199 0.01681 573.5 1199 0.01681 573.8 1199 0.01678 574 1199 0.01678 574.2 1199 0.01679 574.5 1199 0.01678 574.7 1199 0.01675 574.9 1199 0.01673 575.2 1199 0.01674 575.4 1199 0.01673 575.6 1199 0.01673 575.9 1199 0.01673 576.1 1199 0.01672 576.3 1199 0.0167 576.6 1199 0.0167 576.8 1199 0.01673 577 1199 0.01675 577.3 1199 0.01676 577.5 1199 0.01674 577.7 1199 0.01674 578 1199 0.01675 578.2 1199 0.01676 578.4 1199 0.01678 578.7 1199 0.01679 578.9 1199 0.01679 579.1 1199 0.0168 579.4 1199 0.0168 579.6 1199 0.0168 579.8 1199 0.0168 580.1 1199 0.0168 580.3 1199 0.0168 580.5 1199 0.0168 580.8 1199 0.0168 581 1199 0.01679 581.3 1199 0.01678 581.5 1199 0.01678 581.7 1199 0.01676 582 1199 0.01675 582.2 1199 0.01676 582.4 1199 0.01678 582.7 1199 0.01679 582.9 1199 0.0168 583.1 1199 0.0168 583.4 1199 0.0168 583.6 1199 0.01679 583.8 1199 0.01676 584.1 1199 0.01676 584.3 1199 0.01673 584.5 1199 0.01669 584.8 1199 0.01667 585 1199 0.01665 585.2 1199 0.01668 585.5 1199 0.0167 585.7 1199 0.01674 585.9 1199 0.01676 586.2 1199 0.01678 586.4 1199 0.01676 586.6 1199 0.01676 586.9 1199 0.01675 587.1 1199 0.01675 587.3 1199 0.01675 587.6 1199 0.01673 587.8 1199 0.01673 588 1199 0.01673 588.3 1199 0.01672 588.5 1199 0.01669 588.8 1199 0.01668 589 1199 0.01668 589.2 1199 0.0167 589.5 1199 0.01672 589.7 1199 0.01673 589.9 1199 0.01673 590.2 1199 0.01676 590.4 1199 0.0168 590.6 1199 0.01681 590.9 1199 0.0168 591.1 1199 0.0168 591.3 1199 0.01678 591.6 1199 0.01675 591.8 1199 0.01674 592 1199 0.01675 592.3 1199 0.01676 592.5 1199 0.01676 592.7 1199 0.01673 593 1200 0.01673 593.2 1199 0.01675 593.4 1199 0.01679 593.7 1199 0.0168 593.9 1199 0.01679 594.1 1199 0.01676 594.4 1199 0.01678 594.6 1199 0.01678 594.8 1199 0.01678 595.1 1199 0.01676 595.3 1199 0.01678 595.5 1199 0.0168 595.8 1199 0.01679 596 1199 0.01678 596.3 1199 0.01679 596.5 1199 0.01681 596.7 1199 0.01678 597 1199 0.01676 597.2 1199 0.01678 597.4 1199 0.01679 597.7 1199 0.01676 597.9 1199 0.01678 598.1 1199 0.01679 598.4 1199 0.01676 598.6 1199 0.01676 598.8 1199 0.01678 599.1 1199 0.01675 599.3 1199 0.01676 599.5 1198 0.01678 599.8 1198 0.01676 600 1198 0.01678 600.2 1187 0.01676 600.5 1188 0.01678 600.7 1190 0.01676 600.9 1190 0.01678 601.2 1190 0.01679 601.4 1190 0.01679 601.6 1189 0.0168 601.9 1188 0.0168 602.1 1188 0.0168 602.3 1187 0.01678 602.6 1187 0.01675 602.8 1186 0.01675 603 1185 0.01674 603.3 1183 0.01672 603.5 1182 0.0167 603.8 1182 0.01668 604 1180 0.01665 604.2 1180 0.01664 604.5 1179 0.0166 604.7 1178 0.01655 604.9 1177 0.01652 605.2 1176 0.01647 605.4 1174 0.01644 605.6 1174 0.01641 605.9 1172 0.01641 606.1 1172 0.01637 606.3 1171 0.01637 606.6 1169 0.01632 606.8 1169 0.01634 607 1168 0.01629 607.3 1167 0.01633 607.5 1165 0.01628 607.7 1165 0.01629 608 1164 0.01626 608.2 1163 0.01626 608.4 1162 0.01623 608.7 1161 0.01622 608.9 1160 0.0162 609.1 1159 0.01616 609.4 1158 0.01616 609.6 1157 0.01616 609.8 1156 0.01615 610.1 1155 0.01613 610.3 1154 0.01611 610.5 1153 0.01606 610.8 1152 0.01605 611 1151 0.016 611.3 1151 0.01596 611.5 1150 0.01596 611.7 1149 0.01594 612 1148 0.01591 612.2 1147 0.01591 612.4 1146 0.0159 612.7 1144 0.01585 612.9 1144 0.01585 613.1 1143 0.01585 613.4 1142 0.0158 613.6 1140 0.01577 613.8 1140 0.01577 614.1 1139 0.01574 614.3 1138 0.01568 614.5 1137 0.01565 614.8 1136 0.01566 615 1136 0.01566 615.2 1134 0.01563 615.5 1134 0.01559 615.7 1133 0.01558 615.9 1131 0.01559 616.2 1131 0.01555 616.4 1129 0.01551 616.6 1129 0.01547 616.9 1128 0.01543 617.1 1127 0.01542 617.3 1126 0.01539 617.6 1125 0.01534 617.8 1124 0.01532 618 1123 0.0153 618.3 1122 0.01528 618.5 1122 0.01525 618.8 1120 0.01524 619 1119 0.01523 619.2 1119 0.01522 619.5 1118 0.01522 619.7 1117 0.01519 619.9 1115 0.01518 620.2 1115 0.01517 620.4 1114 0.01514 620.6 1112 0.01513 620.9 1111 0.01511 621.1 1111 0.01508 621.3 1110 0.01504 621.6 1109 0.01502 621.8 1108 0.01499 622 1107 0.01498 622.3 1106 0.01497 622.5 1105 0.01495 622.7 1104 0.01492 623 1103 0.0149 623.2 1103 0.01487 623.4 1101 0.01485 623.7 1101 0.0148 623.9 1099 0.01476 624.1 1099 0.01473 624.4 1098 0.01472 624.6 1097 0.01472 624.8 1096 0.01469 625.1 1095 0.01466 625.3 1094 0.01464 625.5 1093 0.01462 625.8 1092 0.01461 626 1091 0.01457 626.3 1090 0.01452 626.5 1089 0.0145 626.7 1088 0.01451 627 1086 0.01449 627.2 1086 0.01444 627.4 1085 0.01444 627.7 1084 0.01445 627.9 1083 0.0144 628.1 1083 0.01439 628.4 1082 0.01439 628.6 1080 0.01436 628.8 1080 0.01434 629.1 1079 0.01434 629.3 1078 0.01429 629.5 1077 0.01426 629.8 1076 0.01425 630 1075 0.0142 630.2 1074 0.01419 630.5 1073 0.01417 630.7 1072 0.01413 630.9 1072 0.01413 631.2 1070 0.01405 631.4 1069 0.01408 631.6 1068 0.01399 631.9 1068 0.014 632.1 1067 0.01393 632.3 1065 0.01396 632.6 1065 0.01388 632.8 1064 0.01389 633 1063 0.01383 633.3 1062 0.01383 633.5 1061 0.01379 633.8 1060 0.01377 634 1059 0.01378 634.2 1058 0.01373 634.5 1057 0.01373 634.7 1056 0.01372 634.9 1055 0.01368 635.2 1054 0.01368 635.4 1054 0.01366 635.6 1052 0.01361 635.9 1051 0.01363 636.1 1051 0.0136 636.3 1049 0.01353 636.6 1048 0.01358 636.8 1047 0.01357 637 1047 0.01347 637.3 1046 0.01345 637.5 1044 0.0135 637.7 1043 0.01348 638 1043 0.0134 638.2 1042 0.0134 638.4 1041 0.01345 638.7 1040 0.01345 638.9 1039 0.01336 639.1 1038 0.01329 639.4 1037 0.01322 639.6 1036 0.0132 639.8 1035 0.01319 640.1 1034 0.01318 640.3 1033 0.01315 640.5 1032 0.0131 640.8 1031 0.01309 641 1030 0.0131 641.3 1029 0.01314 641.5 1029 0.01318 641.7 1028 0.01319 642 1027 0.01318 642.2 1026 0.01315 642.4 1025 0.0131 642.7 1024 0.01304 642.9 1023 0.01297 643.1 1022 0.0129 643.4 1021 0.01285 643.6 1019 0.0128 643.8 1019 0.01278 644.1 1018 0.01275 644.3 1017 0.01274 644.5 1016 0.01274 644.8 1015 0.01274 645 1015 0.01275 645.2 1014 0.01277 645.5 1013 0.01277 645.7 1011 0.01278 645.9 1011 0.01275 646.2 1010 0.01274 646.4 1008 0.01268 646.6 1008 0.01267 646.9 1007 0.01262 647.1 1006 0.01259 647.3 1005 0.01263 647.6 1004 0.01264 647.8 1003 0.01263 648 1002 0.01254 648.3 1001 0.01249 648.5 1001 0.01249 648.8 1000 0.01251 649 999 0.01247 649.2 998 0.0124 649.5 997 0.01237 649.7 996 0.0124 649.9 995 0.01237 650.2 994 0.0123 650.4 993 0.0123 650.6 993 0.0123 650.9 992 0.01223 651.1 990 0.01222 651.3 990 0.01222 651.6 988 0.01217 651.8 987 0.01216 652 986 0.01215 652.3 986 0.01211 652.5 985 0.01211 652.7 984 0.01207 653 983 0.01206 653.2 982 0.01204 653.4 981 0.01201 653.7 980 0.012 653.9 979 0.01197 654.1 978 0.01196 654.4 977 0.01193 654.6 976 0.01191 654.8 975 0.01188 655.1 974 0.01188 655.3 974 0.01183 655.5 973 0.01183 655.8 972 0.01178 656 971 0.01178 656.3 969 0.01174 656.5 968 0.0117 656.7 968 0.0117 657 967 0.01167 657.2 965 0.01165 657.4 965 0.01164 657.7 964 0.01162 657.9 963 0.01159 658.1 962 0.01158 658.4 961 0.01155 658.6 961 0.01154 658.8 959 0.01152 659.1 958 0.01149 659.3 957 0.01144 659.5 956 0.01142 659.8 955 0.01138 660 954 0.01137 660.2 954 0.01134 660.5 953 0.01133 660.7 951 0.01132 660.9 950 0.01129 661.2 950 0.01127 661.4 949 0.01123 661.6 948 0.01123 661.9 947 0.01122 662.1 946 0.0112 662.3 945 0.01116 662.6 944 0.01113 662.8 943 0.01112 663 942 0.01112 663.3 941 0.0111 663.5 940 0.01108 663.8 940 0.01106 664 939 0.01103 664.2 937 0.01102 664.5 936 0.01101 664.7 936 0.01101 664.9 935 0.01097 665.2 934 0.01094 665.4 932 0.01089 665.6 932 0.01086 665.9 931 0.01082 666.1 930 0.01079 666.3 929 0.01075 666.6 928 0.01072 666.8 927 0.01069 667 926 0.01066 667.3 925 0.01066 667.5 924 0.01063 667.7 923 0.01059 668 922 0.01055 668.2 922 0.0105 668.4 921 0.01048 668.7 919 0.01046 668.9 918 0.01045 669.1 918 0.01046 669.4 917 0.01049 669.6 915 0.01049 669.8 915 0.01046 670.1 914 0.01044 670.3 913 0.01042 670.5 912 0.01039 670.8 911 0.01035 671 910 0.01033 671.3 909 0.0103 671.5 908 0.01028 671.7 907 0.01025 672 906 0.01022 672.2 905 0.0102 672.4 904 0.01018 672.7 903 0.01017 672.9 903 0.01016 673.1 902 0.01012 673.4 901 0.01008 673.6 900 0.01007 673.8 899 0.01004 674.1 898 0.01002 674.3 897 0.009995 674.5 896 0.009995 674.8 895 0.00997 675 894 0.009957 675.2 893 0.00992 675.5 893 0.009908 675.7 891 0.009883 675.9 890 0.009871 676.2 889 0.009834 676.4 889 0.009821 676.6 888 0.009784 676.9 886 0.009772 677.1 886 0.009759 677.3 885 0.009735 677.6 883 0.009722 677.8 883 0.009685 678 882 0.00966 678.3 881 0.009648 678.5 880 0.009636 678.8 879 0.009598 679 878 0.009574 679.2 877 0.009549 679.5 876 0.009537 679.7 875 0.009512 679.9 875 0.009512 680.2 874 0.009475 680.4 872 0.009438 680.6 872 0.0094 680.9 871 0.009376 681.1 869 0.009351 681.3 868 0.009339 681.6 868 0.009326 681.8 867 0.009301 682 865 0.009277 682.3 865 0.009252 682.5 864 0.009227 682.7 863 0.009202 683 861 0.00919 683.2 861 0.009178 683.4 860 0.009153 683.7 859 0.009128 683.9 858 0.009091 684.1 857 0.009066 684.4 856 0.009029 684.6 855 0.009004 684.8 854 0.00898 685.1 854 0.00898 685.3 853 0.008955 685.5 852 0.00893 685.8 850 0.008893 686 850 0.008881 686.3 849 0.008856 686.5 848 0.008843 686.7 847 0.008806 687 846 0.008782 687.2 845 0.008782 687.4 844 0.008757 687.7 843 0.00872 687.9 843 0.008683 688.1 841 0.008683 688.4 840 0.008645 688.6 839 0.008633 688.8 838 0.008608 689.1 837 0.008584 689.3 836 0.008571 689.5 836 0.008559 689.8 834 0.008534 690 834 0.008497 690.2 832 0.008485 690.5 832 0.00846 690.7 831 0.008435 690.9 830 0.008423 691.2 829 0.008385 691.4 828 0.008373 691.6 827 0.008336 691.9 826 0.008324 692.1 825 0.008311 692.3 824 0.008286 692.6 823 0.008262 692.8 822 0.008237 693 821 0.008225 693.3 820 0.0082 693.5 819 0.00815 693.8 818 0.008126 694 818 0.008113 694.2 816 0.008088 694.5 816 0.008051 694.7 814 0.008039 694.9 814 0.008002 695.2 813 0.007977 695.4 812 0.007952 695.6 811 0.00794 695.9 810 0.007915 696.1 809 0.00789 696.3 808 0.007866 696.6 807 0.007841 696.8 806 0.007816 697 805 0.007791 697.3 804 0.007767 697.5 803 0.007742 697.7 803 0.007692 698 801 0.007692 698.2 801 0.007692 698.4 801 0.007692 698.7 801 0.00768 698.9 801 0.007655 699.1 800 0.00763 699.4 800 0.007618 699.6 799 0.007593 699.8 799 0.007569 700.1 797 0.007531 700.3 796 0.007519 700.5 795 0.007494 700.8 794 0.00747 701 793 0.007445 701.3 793 0.007408 701.5 792 0.007395 701.7 790 0.007371 702 789 0.007346 702.2 789 0.007321 702.4 788 0.007296 702.7 787 0.007272 702.9 786 0.007247 703.1 785 0.007222 703.4 784 0.007197 703.6 783 0.007173 703.8 782 0.00716 704.1 781 0.007123 704.3 780 0.007098 704.5 779 0.007074 704.8 778 0.007024 705 778 0.006999 705.2 776 0.00695 705.5 775 0.006913 705.7 775 0.0069 705.9 774 0.006875 706.2 773 0.006851 706.4 771 0.006863 706.6 771 0.006863 706.9 770 0.006863 707.1 768 0.006826 707.3 768 0.006789 707.6 767 0.006764 707.8 766 0.006739 708 765 0.006752 708.3 764 0.006752 708.5 763 0.006727 708.8 762 0.006702 709 761 0.006677 709.2 761 0.006653 709.5 759 0.006616 709.7 758 0.006566 709.9 757 0.006541 710.2 757 0.006517 710.4 756 0.006467 710.6 755 0.006455 710.9 754 0.00643 711.1 753 0.006405 711.3 752 0.006405 711.6 750 0.006368 711.8 750 0.006343 712 749 0.006356 712.3 748 0.006343 712.5 747 0.006331 712.7 746 0.006306 713 745 0.006281 713.2 744 0.006257 713.4 743 0.006232 713.7 743 0.006207 713.9 742 0.006195 714.1 740 0.006158 714.4 740 0.006133 714.6 739 0.006108 714.8 739 0.006096 715.1 738 0.006083 715.3 739 0.006083 715.5 740 0.006083 715.8 740 0.006071 716 740 0.006071 716.3 739 0.006071 716.5 738 0.006046 716.7 737 0.006059 717 736 0.006021 717.2 734 0.005997 717.4 733 0.00596 717.7 732 0.005947 717.9 730 0.00591 718.1 728 0.005898 718.4 725 0.005885 718.6 722 0.005861 718.8 721 0.005823 719.1 721 0.005786 719.3 721 0.005737 719.5 718 0.005687 719.8 717 0.005663 720 717 0.005638 720.2 716 0.005625 720.5 715 0.005613 720.7 714 0.005613 720.9 712 0.005576 721.2 711 0.005526 721.4 711 0.005489 721.6 711 0.005464 721.9 710 0.00544 722.1 708 0.005427 722.3 707 0.005403 722.6 707 0.005365 722.8 706 0.005341 723 705 0.005328 723.3 703 0.005304 723.5 702 0.005279 723.8 702 0.005242 724 701 0.005229 724.2 700 0.005205 724.5 699 0.005192 724.7 698 0.005167 724.9 696 0.005155 725.2 696 0.005118 725.4 695 0.005106 725.6 694 0.005081 725.9 693 0.005068 726.1 692 0.005044 726.3 691 0.005019 726.6 690 0.005007 726.8 689 0.004969 727 688 0.004945 727.3 687 0.004883 727.5 686 0.004821 727.7 685 0.004784 728 685 0.004747 728.2 684 0.004722 728.4 683 0.004722 728.7 682 0.004697 728.9 681 0.004697 729.1 680 0.004697 729.4 678 0.004685 729.6 678 0.004672 729.8 678 0.004648 730.1 677 0.00466 730.3 675 0.004648 730.5 674 0.004623 730.8 674 0.004598 731 672 0.004573 731.3 671 0.004524 731.5 671 0.004474 731.7 669 0.004412 732 668 0.004363 732.2 668 0.004313 732.4 667 0.004289 732.7 666 0.004276 732.9 664 0.004239 733.1 664 0.004214 733.4 663 0.00419 733.6 662 0.00419 733.8 661 0.00419 734.1 660 0.004214 734.3 659 0.00419 734.5 658 0.00419 734.8 657 0.004177 735 656 0.004165 735.2 655 0.00414 735.5 654 0.004128 735.7 653 0.004103 735.9 653 0.004078 736.2 651 0.004054 736.4 650 0.004029 736.6 650 0.004016 736.9 649 0.004004 737.1 648 0.003967 737.3 646 0.00393 737.6 646 0.003893 737.8 645 0.003855 738.1 644 0.003818 738.3 643 0.003794 738.5 643 0.003756 738.8 641 0.003732 739 640 0.003719 739.2 639 0.003707 739.5 638 0.003707 739.7 637 0.003682 739.9 636 0.003657 740.2 635 0.003608 740.4 635 0.003596 740.6 633 0.003571 740.9 633 0.003534 741.1 632 0.003509 741.3 632 0.003497 741.6 630 0.003484 741.8 628 0.003459 742 628 0.003435 742.3 627 0.003435 742.5 626 0.003398 742.7 625 0.00341 743 624 0.003373 743.2 623 0.00336 743.4 622 0.003348 743.7 621 0.003298 743.9 621 0.003274 744.1 619 0.003249 744.4 618 0.003224 744.6 617 0.003212 744.8 617 0.003175 745.1 615 0.003162 745.3 614 0.003138 745.6 614 0.003088 745.8 613 0.003063 746 612 0.003039 746.3 610 0.003014 746.5 610 0.003026 746.7 609 0.003039 747 608 0.003014 747.2 607 0.002952 747.4 606 0.002902 747.7 605 0.002853 747.9 604 0.002853 748.1 603 0.002878 748.4 603 0.002853 748.6 602 0.002841 748.8 601 0.002841 749.1 600 0.002816 749.3 600 0.002791 749.5 599 0.002754 749.8 597 0.002704 750 596 0.002667 750.2 596 0.002643 750.5 594 0.002643 750.7 594 0.00263 750.9 592 0.002581 751.2 592 0.002556 751.4 590 0.002543 751.6 589 0.002494 751.9 589 0.002469 752.1 588 0.002432 752.3 587 0.002407 752.6 586 0.002407 752.8 585 0.002407 753.1 584 0.002383 753.3 583 0.00237 753.5 582 0.002345 753.8 582 0.002321 754 580 0.002308 754.2 580 0.002259 754.5 578 0.002259 754.7 578 0.002234 754.9 576 0.002234 755.2 576 0.002197 755.4 574 0.00216 755.6 574 0.002147 755.9 572 0.002123 756.1 571 0.002073 756.3 571 0.002048 756.6 570 0.002024 756.8 568 0.002011 757 568 0.002011 757.3 567 0.001987 757.5 566 0.001949 757.7 565 0.001925 758 564 0.001912 758.2 563 0.001875 758.4 563 0.001838 758.7 561 0.001813 758.9 561 0.001801 759.1 560 0.001776 759.4 559 0.001764 759.6 558 0.001714 759.8 557 0.001714 760.1 556 0.001727 760.3 555 0.001714 760.6 553 0.001652 760.8 553 0.001566 761 552 0.001529 761.3 550 0.001529 761.5 549 0.001529 761.7 549 0.001516 762 549 0.001504 762.2 547 0.001504 762.4 546 0.001479 762.7 546 0.001454 762.9 544 0.001442 763.1 543 0.001417 763.4 542 0.001368 763.6 542 0.001355 763.8 540 0.001331 764.1 539 0.001318 764.3 538 0.001281 764.5 538 0.001219 764.8 537 0.001194 765 535 0.001182 765.2 535 0.001157 765.5 534 0.001133 765.7 533 0.001083 765.9 532 0.001071 766.2 531 0.001058 766.4 530 0.001021 766.6 529 0.001021 766.9 528 0.001021 767.1 527 0.001009 767.3 526 0.000984 767.6 526 0.0009345 767.8 524 0.0009221 768.1 524 0.0008973 768.3 522 0.0008726 768.5 521 0.0008478 768.8 521 0.0008231 769 520 0.0007859 769.2 519 0.0007612 769.5 518 0.0007241 769.7 517 0.0006993 769.9 516 0.0006869 770.2 515 0.0006622 770.4 514 0.0006622 770.6 514 0.000625 770.9 512 0.0005632 771.1 511 0.0005384 771.3 510 0.0005755 771.6 510 0.0005508 771.8 509 0.0005013 772 507 0.0004889 772.3 506 0.0004641 772.5 506 0.0004394 772.7 505 0.0004146 773 504 0.0003775 773.2 503 0.0003527 773.4 502 0.000328 773.7 501 0.0002909 773.9 500 0.0002909 774.1 499 0.0002661 774.4 499 0.000229 774.6 497 0.0001918 774.8 496 0.0001671 775.1 495 0.0001795 775.3 494 0.0001918 775.6 493 0.0001918 775.8 492 0.0001671 776 492 0.0001176 776.3 490 6.807e-05 776.5 489 1.857e-05 776.7 489 6.189e-06 777 488 6.189e-06 777.2 487 6.189e-06 777.4 486 6.189e-06 777.7 485 -6.189e-06 777.9 484 -3.094e-05 778.1 483 -5.57e-05 778.4 482 -6.807e-05 778.6 481 -8.045e-05 778.8 480 -0.0001176 779.1 480 -0.0001547 779.3 478 -0.0001795 779.5 478 -0.0002042 779.8 477 -0.000229 780 476 -0.0002661 780.2 474 -0.0003032 780.5 474 -0.0003156 780.7 473 -0.0003032 780.9 472 -0.000328 781.2 471 -0.0003404 781.4 470 -0.0003775 781.6 469 -0.0003899 781.9 468 -0.0004023 782.1 467 -0.000427 782.3 466 -0.0004394 782.6 465 -0.0004518 782.8 464 -0.0004765 783.1 463 -0.0005013 783.3 463 -0.000526 783.5 461 -0.0005384 783.8 461 -0.0005508 784 460 -0.0005755 784.2 459 -0.0006003 784.5 458 -0.000625 784.7 456 -0.0006622 784.9 456 -0.0006869 785.2 455 -0.0007241 785.4 454 -0.0007241 785.6 453 -0.0007736 785.9 452 -0.0007983 786.1 451 -0.0008107 786.3 450 -0.0008231 786.6 449 -0.0008602 786.8 449 -0.0008726 787 447 -0.000885 787.3 446 -0.0009097 787.5 446 -0.0009345 787.7 444 -0.0009592 788 443 -0.0009964 788.2 442 -0.001009 788.4 442 -0.001021 788.7 441 -0.001046 788.9 440 -0.001058 789.1 439 -0.001095 789.4 438 -0.001133 789.6 437 -0.001157 789.8 435 -0.001182 790.1 435 -0.001207 790.3 435 -0.001219 790.6 433 -0.001232 790.8 432 -0.001256 791 431 -0.001318 791.3 430 -0.001355 791.5 430 -0.001368 791.7 428 -0.00138 792 428 -0.00138 792.2 427 -0.00138 792.4 426 -0.001392 792.7 424 -0.001417 792.9 424 -0.001417 793.1 423 -0.001417 793.4 422 -0.00143 793.6 421 -0.001454 793.8 419 -0.001479 794.1 419 -0.001516 794.3 418 -0.001578 794.5 417 -0.001603 794.8 417 -0.00159 795 415 -0.00159 795.2 414 -0.001615 795.5 413 -0.001652 795.7 413 -0.001665 795.9 411 -0.001689 796.2 411 -0.001689 796.4 410 -0.001714 796.6 409 -0.001714 796.9 408 -0.001739 797.1 406 -0.001764 797.3 406 -0.001788 797.6 405 -0.001826 797.8 404 -0.00185 798.1 403 -0.001863 798.3 402 -0.001863 798.5 401 -0.0019 798.8 401 -0.001925 799 401 -0.001962 799.2 399 -0.001974 799.5 399 -0.002011 799.7 397 -0.002036 799.9 396 -0.002048 800.2 396 -0.002061 800.4 394 -0.002061 800.6 394 -0.002073 800.9 392 -0.002061 801.1 392 -0.002061 801.3 390 -0.002086 801.6 390 -0.002086 801.8 388 -0.002098 802 388 -0.002098 802.3 387 -0.00211 802.5 386 -0.002123 802.7 385 -0.002135 803 385 -0.002147 803.2 383 -0.00216 803.4 382 -0.002185 803.7 381 -0.002197 803.9 380 -0.002234 804.1 380 -0.002234 804.4 379 -0.002246 804.6 378 -0.002259 804.8 377 -0.002284 805.1 376 -0.002308 805.3 374 -0.002308 805.6 374 -0.002321 805.8 372 -0.002345 806 371 -0.00237 806.3 371 -0.002383 806.5 370 -0.002395 806.7 369 -0.002407 807 368 -0.002432 807.2 367 -0.002444 807.4 367 -0.002457 807.7 366 -0.002457 807.9 364 -0.002457 808.1 363 -0.002482 808.4 363 -0.002494 808.6 362 -0.002506 808.8 360 -0.002519 809.1 360 -0.002543 809.3 359 -0.002543 809.5 358 -0.002568 809.8 356 -0.002593 810 356 -0.002605 810.2 355 -0.002605 810.5 354 -0.00263 810.7 353 -0.002643 810.9 352 -0.002655 811.2 350 -0.002655 811.4 350 -0.002643 811.6 349 -0.002643 811.9 349 -0.002643 812.1 348 -0.002643 812.3 346 -0.002643 812.6 346 -0.00263 812.8 345 -0.002643 813.1 345 -0.002655 813.3 343 -0.002655 813.5 342 -0.002667 813.8 342 -0.002655 814 340 -0.002667 814.2 340 -0.002643 814.5 338 -0.00263 814.7 338 -0.00263 814.9 337 -0.002618 815.2 336 -0.00263 815.4 335 -0.002618 815.6 334 -0.002605 815.9 333 -0.002581 816.1 332 -0.002543 816.3 331 -0.002519 816.6 330 -0.002482 816.8 329 -0.002444 817 328 -0.002432 817.3 327 -0.002383 817.5 326 -0.002345 817.7 324 -0.002296 818 324 -0.002259 818.2 323 -0.002234 818.4 322 -0.002197 818.7 320 -0.002147 818.9 320 -0.002086 819.1 319 -0.002011 819.4 318 -0.001949 819.6 317 -0.001863 819.8 316 -0.001788 820.1 315 -0.001727 820.3 314 -0.001665 820.6 313 -0.001578 820.8 312 -0.001504 821 311 -0.001417 821.3 310 -0.001331 821.5 309 -0.001244 821.7 309 -0.001157 822 307 -0.001071 822.2 306 -0.000984 822.4 306 -0.0009097 822.7 305 -0.0008231 822.9 303 -0.0007488 823.1 302 -0.0006746 823.4 301 -0.0006003 823.6 301 -0.000526 823.8 299 -0.0004641 824.1 299 -0.0004023 824.3 298 -0.000328 824.5 297 -0.0002661 824.8 295 -0.0002042 825 295 -0.00013 825.2 294 -8.045e-05 825.5 292 -1.857e-05 825.7 292 6.189e-06 825.9 291 6.189e-06 826.2 290 6.189e-06 826.4 289 1.857e-05 826.6 288 3.094e-05 826.9 287 6.807e-05 827.1 286 9.283e-05 827.3 285 0.0001423 827.6 285 0.0001671 827.8 284 0.0001918 828.1 282 0.000229 828.3 281 0.0002661 828.5 281 0.0002785 828.8 280 0.0002909 829 279 0.0003156 829.2 277 0.000328 829.5 277 0.0003527 829.7 276 0.0003527 829.9 276 0.0003651 830.2 274 0.0003651 830.4 274 0.0003899 830.6 272 0.0004023 830.9 271 0.000427 831.1 270 0.0004518 831.3 269 0.0004518 831.6 268 0.0004641 831.8 267 0.0004765 832 267 0.0004889 832.3 265 0.0005136 832.5 264 0.0004889 832.7 263 0.0004889 833 263 0.0004765 833.2 262 0.0004889 833.4 260 0.0004889 833.7 260 0.000526 833.9 259 0.0005384 834.1 258 0.0005632 834.4 256 0.0005632 834.6 256 0.0005632 834.8 255 0.0005632 835.1 254 0.0005632 835.3 253 0.0005632 835.6 252 0.0005632 835.8 252 0.0005632 836 250 0.0005632 836.3 249 0.0005755 836.5 249 0.0005755 836.7 248 0.0006003 837 247 0.0006127 837.2 246 0.0006127 837.4 245 0.0006127 837.7 244 0.0006127 837.9 242 0.000625 838.1 242 0.000625 838.4 242 0.000625 838.6 240 0.000625 838.8 239 0.0006127 839.1 238 0.0006127 839.3 237 0.000625 839.5 236 0.0006127 839.8 235 0.000625 840 234 0.000625 840.2 234 0.000625 840.5 232 0.0006127 840.7 231 0.0006127 840.9 231 0.0006003 841.2 230 0.0005879 841.4 229 0.0005879 841.6 228 0.0005879 841.9 227 0.0005879 842.1 226 0.0005755 842.3 225 0.0005755 842.6 224 0.0005632 842.8 224 0.0005755 843.1 222 0.0005632 843.3 221 0.0005632 843.5 220 0.0005632 843.8 219 0.0005632 844 218 0.0005384 844.2 217 0.000526 844.5 217 0.0005013 844.7 215 0.0004889 844.9 214 0.0004765 845.2 213 0.0004641 845.4 213 0.0004765 845.6 212 0.0004641 845.9 210 0.0004641 846.1 209 0.0004641 846.3 209 0.0004641 846.6 208 0.0004641 846.8 207 0.0004641 847 206 0.0004641 847.3 205 0.0004641 847.5 204 0.0004641 847.7 203 0.0004641 848 202 0.0004394 848.2 202 0.000427 848.4 201 0.0004023 848.7 200 0.0003899 848.9 199 0.0003775 849.1 199 0.0003651 849.4 197 0.0003404 849.6 196 0.000328 849.8 195 0.000328 850.1 194 0.0003156 850.3 193 0.0003156 850.6 192 0.0003404 850.8 191 0.000328 851 191 0.0003156 851.3 189 0.0003156 851.5 188 0.0003156 851.7 188 0.000328 852 187 0.0002909 852.2 186 0.0002785 852.4 184 0.0002785 852.7 184 0.0002537 852.9 183 0.0002414 853.1 182 0.000229 853.4 181 0.0002166 853.6 181 0.0001918 853.8 180 0.0002042 854.1 178 0.0002042 854.3 177 0.0001795 854.5 177 0.0001671 854.8 175 0.0001671 855 174 0.0001671 855.2 174 0.0001671 855.5 173 0.0001671 855.7 171 0.0001547 855.9 170 0.00013 856.2 170 0.00013 856.4 169 0.0001176 856.6 168 0.0001176 856.9 167 0.0001176 857.1 166 9.283e-05 857.3 165 8.045e-05 857.6 164 6.807e-05 857.8 163 6.807e-05 858.1 163 6.807e-05 858.3 162 5.57e-05 858.5 160 5.57e-05 858.8 159 5.57e-05 859 159 4.332e-05 859.2 157 3.094e-05 859.5 156 1.857e-05 859.7 156 6.189e-06 859.9 155 6.189e-06 860.2 154 6.189e-06 860.4 152 6.189e-06 860.6 152 6.189e-06 860.9 150 6.189e-06 861.1 150 6.189e-06 861.3 149 6.189e-06 861.6 149 6.189e-06 861.8 147 6.189e-06 862 147 -1.857e-05 862.3 145 -6.189e-06 862.5 144 6.189e-06 862.7 144 6.189e-06 863 142 6.189e-06 863.2 141 -1.857e-05 863.4 141 -3.094e-05 863.7 139 -3.094e-05 863.9 139 -4.332e-05 864.1 138 -3.094e-05 864.4 137 -4.332e-05 864.6 136 -5.57e-05 864.8 135 -8.045e-05 865.1 134 -0.0001052 865.3 133 -0.0001423 865.6 132 -0.0001795 865.8 131 -0.0002042 866 131 -0.0002537 866.3 129 -0.0003032 866.5 128 -0.0002785 866.7 127 -0.0002166 867 127 -0.0001671 867.2 126 -0.0001423 867.4 124 -0.0001547 867.7 123 -0.0001795 867.9 123 -0.0002042 868.1 122 -0.0002042 868.4 121 -0.0002166 868.6 120 -0.0002042 868.8 119 -0.0002042 869.1 118 -0.0002042 869.3 117 -0.000229 869.5 116 -0.0002785 869.8 115 -0.0003404 870 114 -0.0004023 870.2 113 -0.000427 870.5 112 -0.000427 870.7 111 -0.000427 870.9 110 -0.0004023 871.2 109 -0.0003775 871.4 109 -0.0003775 871.6 108 -0.0003651 871.9 106 -0.0003775 872.1 106 -0.0003899 872.3 105 -0.0004023 872.6 104 -0.0004146 872.8 102 -0.0004146 873.1 102 -0.000427 873.3 102 -0.0004518 873.5 100 -0.0004641 873.8 100 -0.0004765 874 98 -0.0005013 874.2 98 -0.000526 874.5 97 -0.0005384 874.7 96 -0.0005755 874.9 95 -0.0005879 875.2 94 -0.0005755 875.4 93 -0.0005632 875.6 92 -0.0005632 875.9 91 -0.0005384 876.1 90 -0.0005508 876.3 89 -0.0005632 876.6 88 -0.0005632 876.8 88 -0.0005755 877 86 -0.0005879 877.3 86 -0.0005755 877.5 84 -0.0005879 877.7 84 -0.0006127 878 83 -0.0006127 878.2 82 -0.000625 878.4 81 -0.0006498 878.7 80 -0.0006622 878.9 80 -0.0006746 879.1 78 -0.0006993 879.4 77 -0.0007117 879.6 77 -0.0007364 879.8 76 -0.0007488 880.1 75 -0.0007612 880.3 73 -0.0007736 880.6 73 -0.0007736 880.8 72 -0.0007983 881 71 -0.0008107 881.3 70 -0.0008231 881.5 69 -0.0008107 881.7 68 -0.0007736 882 67 -0.0007612 882.2 66 -0.0007612 882.4 66 -0.0007736 882.7 65 -0.0007983 882.9 64 -0.0008231 883.1 63 -0.0008478 883.4 62 -0.0008602 883.6 62 -0.0008726 883.8 61 -0.0008726 884.1 60 -0.0008726 884.3 59 -0.0008726 884.5 59 -0.0008726 884.8 58 -0.0008726 885 58 -0.000885 885.2 56 -0.0008726 885.5 55 -0.0008726 885.7 55 -0.0008726 885.9 55 -0.0008726 886.2 54 -0.0008726 886.4 52 -0.0008726 886.6 52 -0.0008973 886.9 52 -0.0009097 887.1 50 -0.0009221 887.3 50 -0.0009221 887.6 49 -0.0009468 887.8 48 -0.0009592 888.1 48 -0.0009964 888.3 47 -0.001021 888.5 46 -0.001033 888.8 45 -0.001033 889 45 -0.001033 889.2 44 -0.001046 889.5 44 -0.001033 889.7 43 -0.001033 889.9 42 -0.001046 890.2 42 -0.001058 890.4 41 -0.001058 890.6 40 -0.001071 890.9 40 -0.001071 891.1 39 -0.001083 891.3 38 -0.001083 891.6 38 -0.001095 891.8 38 -0.001083 892 37 -0.001083 892.3 36 -0.001071 892.5 36 -0.001083 892.7 35 -0.001083 893 34 -0.001083 893.2 34 -0.001108 893.4 34 -0.00112 893.7 33 -0.00112 893.9 32 -0.001133 894.1 31 -0.001133 894.4 31 -0.001133 894.6 31 -0.001157 894.8 30 -0.00117 895.1 30 -0.001182 895.3 30 -0.001194 895.6 30 -0.001219 895.8 29 -0.001219 896 29 -0.001232 896.3 28 -0.001244 896.5 28 -0.001256 896.7 27 -0.001244 897 27 -0.001244 897.2 27 -0.001244 897.4 27 -0.001244 897.7 27 -0.001232 897.9 27 -0.001244 898.1 26 -0.001244 898.4 27 -0.001244 898.6 26 -0.001244 898.8 26 -0.001244 899.1 24 -0.001244 899.3 24 -0.001244 899.5 24 -0.001244 899.8 23 -0.001256 900 23 -0.001256 900.2 23 -0.001244 900.5 23 -0.001244 900.7 23 -0.001244 900.9 23 -0.001244 901.2 23 -0.001244 901.4 22 -0.001244 901.6 22 -0.001244 901.9 22 -0.001244 902.1 22 -0.001244 902.3 22 -0.001244 902.6 22 -0.001244 902.8 21 -0.001244 903.1 21 -0.001244 903.3 21 -0.001244 903.5 21 -0.001244 903.8 21 -0.001256 904 20 -0.001281 904.2 20 -0.001281 904.5 20 -0.001293 904.7 20 -0.001293 904.9 20 -0.001293 905.2 20 -0.001293 905.4 20 -0.001293 905.6 20 -0.001293 905.9 20 -0.001293 906.1 19 -0.001293 906.3 19 -0.001293 906.6 19 -0.001293 906.8 19 -0.001293 907 19 -0.001293 907.3 18 -0.001293 907.5 19 -0.001293 907.7 18 -0.001293 908 19 -0.001293 908.2 18 -0.001293 908.4 18 -0.001293 908.7 18 -0.001293 908.9 18 -0.001293 909.1 17 -0.001293 909.4 17 -0.001293 909.6 17 -0.001293 909.8 17 -0.001293 910.1 17 -0.001293 910.3 17 -0.001293 910.6 17 -0.001306 910.8 17 -0.001318 911 17 -0.001343 911.3 17 -0.00138 911.5 17 -0.001405 911.7 16 -0.001392 912 17 -0.001392 912.2 17 -0.00138 912.4 16 -0.001368 912.7 16 -0.001355 912.9 16 -0.001318 913.1 16 -0.001306 913.4 16 -0.001293 913.6 16 -0.001293 913.8 16 -0.001293 914.1 16 -0.001293 914.3 16 -0.001293 914.5 16 -0.001293 914.8 16 -0.001293 915 16 -0.001318 915.2 16 -0.001318 915.5 16 -0.001355 915.7 16 -0.001368 915.9 15 -0.00138 916.2 15 -0.00138 916.4 15 -0.001368 916.6 15 -0.001355 916.9 15 -0.001355 917.1 15 -0.001343 917.3 15 -0.001343 917.6 15 -0.001355 917.8 15 -0.001355 918.1 15 -0.001343 918.3 15 -0.001331 918.5 15 -0.001318 918.8 15 -0.001293 919 15 -0.001293 919.2 15 -0.001306 919.5 15 -0.001318 919.7 15 -0.001331 919.9 15 -0.001331 920.2 15 -0.001343 920.4 15 -0.001355 920.6 14 -0.001355 920.9 14 -0.001355 921.1 15 -0.001318 921.3 14 -0.001331 921.6 14 -0.001331 921.8 14 -0.001318 922 14 -0.001306 922.3 14 -0.001306 922.5 14 -0.001293 922.7 14 -0.001293 923 14 -0.001293 923.2 14 -0.001293 923.4 14 -0.001318 923.7 14 -0.001318 923.9 14 -0.001331 924.1 14 -0.001331 924.4 13 -0.001331 924.6 13 -0.001331 924.8 13 -0.001343 925.1 13 -0.001331 925.3 13 -0.001343 925.6 13 -0.001331 925.8 14 -0.001318 926 13 -0.001331 926.3 13 -0.001331 926.5 13 -0.001331 926.7 13 -0.001343 927 13 -0.001331 927.2 13 -0.001343 927.4 13 -0.001343 927.7 13 -0.001331 927.9 13 -0.001343 928.1 13 -0.001355 928.4 13 -0.001355 928.6 13 -0.001343 928.8 13 -0.001355 929.1 13 -0.001343 929.3 13 -0.001355 929.5 13 -0.001343 929.8 13 -0.001343 930 13 -0.001343 930.2 13 -0.001331 930.5 13 -0.001343 930.7 12 -0.001343 930.9 13 -0.001343 931.2 13 -0.001343 931.4 13 -0.001343 931.6 12 -0.001331 931.9 13 -0.001318 932.1 12 -0.001318 932.3 13 -0.001331 932.6 12 -0.001331 932.8 13 -0.001343 933.1 13 -0.001343 933.3 13 -0.001343 933.5 13 -0.001331 933.8 12 -0.001331 934 13 -0.001331 934.2 12 -0.001331 934.5 12 -0.001343 934.7 12 -0.001343 934.9 13 -0.001343 935.2 12 -0.001343 935.4 12 -0.001343 935.6 12 -0.001343 935.9 12 -0.001343 936.1 12 -0.001331 936.3 12 -0.001343 936.6 12 -0.001343 936.8 12 -0.001343 937 12 -0.001343 937.3 12 -0.001343 937.5 12 -0.001343 937.7 12 -0.001343 938 12 -0.001343 938.2 12 -0.001343 938.4 12 -0.001343 938.7 12 -0.001343 938.9 12 -0.001343 939.1 12 -0.001331 939.4 12 -0.001318 939.6 12 -0.001331 939.8 12 -0.001331 940.1 12 -0.001331 940.3 12 -0.001318 940.6 12 -0.001306 940.8 12 -0.001318 941 12 -0.001318 941.3 11 -0.001306 941.5 11 -0.001318 941.7 11 -0.001318 942 12 -0.001318 942.2 11 -0.001318 942.4 11 -0.001331 942.7 11 -0.001331 942.9 11 -0.001318 943.1 11 -0.001331 943.4 11 -0.001331 943.6 11 -0.001331 943.8 11 -0.001343 944.1 11 -0.001343 944.3 12 -0.001331 944.5 11 -0.001318 944.8 11 -0.001306 945 11 -0.001293 945.2 11 -0.001306 945.5 11 -0.001318 945.7 11 -0.001306 945.9 11 -0.001306 946.2 11 -0.001318 946.4 11 -0.001343 946.6 11 -0.00138 946.9 11 -0.001392 947.1 11 -0.001392 947.3 12 -0.001392 947.6 11 -0.001392 947.8 10 -0.00138 948.1 11 -0.00138 948.3 10 -0.00138 948.5 11 -0.00138 948.8 11 -0.001355 949 10 -0.001355 949.2 11 -0.001355 949.5 11 -0.001343 949.7 11 -0.001343 949.9 11 -0.001331 950.2 11 -0.001331 950.4 11 -0.001331 950.6 11 -0.001368 950.9 11 -0.00138 951.1 11 -0.00138 951.3 11 -0.001392 951.6 10 -0.001368 951.8 11 -0.001368 952 11 -0.001355 952.3 11 -0.001355 952.5 10 -0.001343 952.7 11 -0.001343 953 11 -0.001343 953.2 11 -0.001331 953.4 11 -0.001318 953.7 11 -0.001306 953.9 11 -0.001293 954.1 11 -0.001293 954.4 11 -0.001306 954.6 10 -0.001293 954.8 11 -0.001306 955.1 10 -0.001318 955.3 11 -0.001318 955.6 10 -0.001331 955.8 10 -0.001343 956 10 -0.001368 956.3 10 -0.00138 956.5 10 -0.001392 956.7 10 -0.001392 957 10 -0.001392 957.2 11 -0.001392 957.4 10 -0.001392 957.7 10 -0.001368 957.9 10 -0.001355 958.1 10 -0.001355 958.4 10 -0.001343 958.6 10 -0.001343 958.8 8 0.29 0.09 0.74 0.002 0.007 0.66 1.3 1.02 0.292 0 0 0.001 0.0041 0 6 -0.0003393 0 8 -0.0003393 0.1611 8 -0.0003639 0.3223 8 -0.0003639 0.4834 8 -0.0003639 0.6445 8 -0.0003639 0.8057 8 -0.0003763 0.9668 8 -0.0003763 1.128 8 -0.0003763 1.289 8 -0.0003763 1.45 8 -0.0003763 1.611 8 -0.0003763 1.772 8 -0.0003763 1.934 8 -0.0003763 2.095 8 -0.0003763 2.256 8 -0.0003763 2.417 9 -0.0003763 2.578 9 -0.0003639 2.739 10 -0.0003639 2.9 11 -0.0003639 3.062 12 -0.0003886 3.223 14 -0.0003639 3.384 15 -0.0003516 3.545 17 -0.0003393 3.706 20 -0.0003269 3.867 21 -0.0003146 4.028 23 -0.0003022 4.189 25 -0.0002652 4.351 27 -0.0002282 4.512 29 -0.0002159 4.673 31 -0.0001665 4.834 33 -0.0001419 4.995 34 -9.252e-05 5.156 37 -6.785e-05 5.317 38 -4.318e-05 5.479 40 -1.85e-05 5.64 41 6.168e-06 5.801 43 6.168e-06 5.962 45 6.168e-06 6.123 46 6.168e-06 6.284 48 1.85e-05 6.445 49 4.318e-05 6.606 51 6.785e-05 6.768 52 6.785e-05 6.929 54 0.0001049 7.09 55 0.0001172 7.251 56 0.0001295 7.412 58 0.0001665 7.573 59 0.0001912 7.734 60 0.0002159 7.896 62 0.0002282 8.057 63 0.0002529 8.218 64 0.0002652 8.379 66 0.0002776 8.54 67 0.0002899 8.701 68 0.0003146 8.862 69 0.0003269 9.024 71 0.0003393 9.185 71 0.0003639 9.346 73 0.0003886 9.507 75 0.0004256 9.668 76 0.0004503 9.829 77 0.0004626 9.99 78 0.0004873 10.15 80 0.000512 10.31 81 0.0005243 10.47 82 0.0005366 10.63 84 0.0005243 10.8 84 0.0005243 10.96 86 0.0005243 11.12 87 0.0005366 11.28 88 0.0005613 11.44 90 0.0005736 11.6 91 0.000586 11.76 92 0.0005983 11.92 93 0.0005983 12.09 94 0.0005983 12.25 96 0.0006107 12.41 98 0.000623 12.57 98 0.0006723 12.73 100 0.0007217 12.89 102 0.0007587 13.05 102 0.0007834 13.21 105 0.000771 13.37 106 0.0007587 13.54 106 0.0007464 13.7 108 0.0007587 13.86 109 0.0007834 14.02 110 0.0008204 14.18 112 0.0008204 14.34 113 0.0008327 14.5 114 0.0008574 14.66 116 0.0008821 14.82 117 0.0009191 14.99 118 0.0009191 15.15 120 0.0009191 15.31 121 0.0009437 15.47 123 0.0009437 15.63 123 0.0009684 15.79 125 0.0009807 15.95 127 0.0009931 16.11 127 0.001005 16.27 129 0.001018 16.44 130 0.00103 16.6 131 0.001042 16.76 133 0.001055 16.92 134 0.001092 17.08 135 0.001129 17.24 137 0.001153 17.4 138 0.001178 17.56 140 0.00119 17.72 141 0.001178 17.89 142 0.001203 18.05 143 0.001215 18.21 144 0.00124 18.37 146 0.001252 18.53 147 0.001264 18.69 149 0.001289 18.85 149 0.001301 19.01 151 0.001301 19.17 152 0.001326 19.34 154 0.001326 19.5 155 0.001363 19.66 156 0.001388 19.82 157 0.0014 19.98 159 0.0014 20.14 159 0.001425 20.3 161 0.00145 20.46 162 0.001487 20.63 163 0.001511 20.79 165 0.001536 20.95 166 0.001548 21.11 168 0.001585 21.27 169 0.00161 21.43 170 0.00161 21.59 171 0.001635 21.75 173 0.001635 21.91 174 0.001635 22.08 175 0.001647 22.24 177 0.001659 22.4 178 0.001684 22.56 179 0.001696 22.72 181 0.001709 22.88 181 0.001709 23.04 184 0.001733 23.2 184 0.001758 23.36 185 0.001783 23.53 187 0.001807 23.69 188 0.001844 23.85 190 0.001881 24.01 191 0.001906 24.17 192 0.001943 24.33 194 0.001968 24.49 195 0.001968 24.65 196 0.00198 24.81 197 0.00198 24.98 199 0.002005 25.14 200 0.002029 25.3 201 0.002042 25.46 202 0.002066 25.62 203 0.002103 25.78 205 0.002128 25.94 206 0.002165 26.1 207 0.002202 26.26 209 0.002227 26.43 209 0.002264 26.59 211 0.002288 26.75 212 0.002301 26.91 213 0.002313 27.07 215 0.002325 27.23 217 0.002325 27.39 217 0.002338 27.55 219 0.002362 27.72 220 0.002387 27.88 221 0.002387 28.04 223 0.002399 28.2 224 0.002399 28.36 226 0.002436 28.52 227 0.002461 28.68 228 0.002498 28.84 230 0.002547 29 231 0.002572 29.17 232 0.002584 29.33 233 0.002597 29.49 234 0.002621 29.65 236 0.002646 29.81 237 0.002659 29.97 238 0.002671 30.13 240 0.002696 30.29 242 0.002696 30.45 242 0.002708 30.62 244 0.00272 30.78 245 0.002745 30.94 246 0.002757 31.1 248 0.00277 31.26 249 0.002794 31.42 250 0.002807 31.58 252 0.002807 31.74 252 0.002819 31.9 254 0.002819 32.07 256 0.002819 32.23 256 0.002807 32.39 258 0.002819 32.55 260 0.002819 32.71 261 0.002831 32.87 263 0.002844 33.03 263 0.002893 33.19 265 0.00293 33.35 267 0.002979 33.52 267 0.003004 33.68 268 0.003029 33.84 270 0.003053 34 271 0.003078 34.16 273 0.003127 34.32 274 0.00314 34.48 274 0.003164 34.64 277 0.003164 34.8 277 0.003177 34.97 279 0.003177 35.13 281 0.003189 35.29 281 0.003189 35.45 283 0.003214 35.61 284 0.003201 35.77 285 0.003177 35.93 287 0.003201 36.09 288 0.003226 36.26 289 0.003238 36.42 291 0.003275 36.58 292 0.0033 36.74 293 0.003337 36.9 294 0.003374 37.06 295 0.003411 37.22 297 0.003436 37.38 299 0.00346 37.54 299 0.003485 37.71 301 0.003522 37.87 302 0.003522 38.03 303 0.003547 38.19 305 0.003584 38.35 306 0.003608 38.51 307 0.003621 38.67 309 0.003633 38.83 311 0.003645 38.99 311 0.00367 39.16 313 0.003695 39.32 314 0.003719 39.48 315 0.003719 39.64 317 0.003744 39.8 317 0.003781 39.96 319 0.003806 40.12 320 0.003818 40.28 322 0.003843 40.44 323 0.003867 40.61 324 0.00388 40.77 326 0.003904 40.93 327 0.003917 41.09 328 0.003966 41.25 329 0.004003 41.41 331 0.004016 41.57 332 0.004028 41.73 334 0.004053 41.89 335 0.004077 42.06 336 0.004102 42.22 337 0.004127 42.38 338 0.004164 42.54 340 0.004188 42.7 342 0.004213 42.86 342 0.004225 43.02 344 0.004225 43.18 345 0.004238 43.35 346 0.004262 43.51 348 0.004299 43.67 349 0.004324 43.83 349 0.004324 43.99 352 0.004324 44.15 353 0.004324 44.31 354 0.004324 44.47 356 0.004324 44.63 356 0.004324 44.8 358 0.004336 44.96 360 0.004373 45.12 361 0.004373 45.28 362 0.004398 45.44 363 0.00441 45.6 365 0.00441 45.76 367 0.004423 45.92 367 0.00446 46.08 368 0.004472 46.25 370 0.004484 46.41 371 0.004497 46.57 373 0.004509 46.73 374 0.004534 46.89 374 0.004546 47.05 377 0.004558 47.21 378 0.004558 47.37 379 0.004595 47.53 381 0.004608 47.7 381 0.004632 47.86 383 0.004632 48.02 384 0.004645 48.18 385 0.004645 48.34 387 0.004669 48.5 388 0.004706 48.66 389 0.004706 48.82 390 0.004706 48.98 392 0.004706 49.15 393 0.004731 49.31 394 0.004768 49.47 396 0.00478 49.63 397 0.004793 49.79 399 0.004805 49.95 400 0.00483 50.11 401 0.00483 50.27 401 0.004854 50.43 403 0.004879 50.6 404 0.004891 50.76 406 0.004916 50.92 406 0.004928 51.08 408 0.004941 51.24 410 0.004965 51.4 410 0.004978 51.56 412 0.005002 51.72 413 0.005039 51.89 414 0.005052 52.05 415 0.005052 52.21 417 0.005052 52.37 418 0.005064 52.53 420 0.005064 52.69 421 0.005076 52.85 422 0.005101 53.01 423 0.005113 53.17 424 0.00515 53.34 426 0.005175 53.5 428 0.005212 53.66 429 0.005249 53.82 430 0.005274 53.98 431 0.005311 54.14 433 0.005336 54.3 434 0.005373 54.46 435 0.005397 54.62 437 0.005397 54.79 438 0.00541 54.95 439 0.005434 55.11 441 0.005447 55.27 442 0.005459 55.43 443 0.005484 55.59 444 0.005508 55.75 446 0.005521 55.91 446 0.005533 56.07 449 0.005545 56.24 449 0.00557 56.4 451 0.005607 56.56 453 0.005632 56.72 453 0.005656 56.88 455 0.005669 57.04 456 0.005693 57.2 457 0.005718 57.36 459 0.00573 57.52 460 0.00573 57.69 461 0.00573 57.85 462 0.005755 58.01 464 0.005792 58.17 465 0.005841 58.33 467 0.005878 58.49 467 0.005891 58.65 468 0.005903 58.81 470 0.00594 58.98 471 0.005952 59.14 473 0.005965 59.3 474 0.005977 59.46 475 0.005989 59.62 477 0.006026 59.78 478 0.006051 59.94 479 0.006063 60.1 481 0.006088 60.26 482 0.006113 60.43 484 0.00615 60.59 485 0.006174 60.75 486 0.006187 60.91 487 0.006199 61.07 489 0.006224 61.23 490 0.006248 61.39 492 0.006261 61.55 492 0.006273 61.71 494 0.006285 61.88 495 0.00631 62.04 496 0.006335 62.2 497 0.006347 62.36 499 0.006372 62.52 500 0.006396 62.68 502 0.006433 62.84 503 0.006458 63 504 0.00647 63.16 505 0.006483 63.33 506 0.006495 63.49 508 0.00647 63.65 509 0.00647 63.81 510 0.006495 63.97 512 0.006544 64.13 513 0.006594 64.29 514 0.006631 64.45 516 0.006631 64.61 517 0.006656 64.78 518 0.00668 64.94 519 0.006693 65.1 521 0.006717 65.26 522 0.006717 65.42 523 0.006952 65.58 524 0.007038 65.74 526 0.006952 65.9 528 0.006915 66.06 528 0.006902 66.23 530 0.006902 66.39 532 0.006902 66.55 532 0.006927 66.71 534 0.006952 66.87 535 0.006964 67.03 537 0.006989 67.19 537 0.007026 67.35 539 0.00705 67.52 540 0.007075 67.68 542 0.007087 67.84 542 0.007112 68 544 0.007137 68.16 546 0.007174 68.32 546 0.007198 68.48 548 0.007198 68.64 549 0.007161 68.8 550 0.007174 68.97 553 0.007174 69.13 553 0.007211 69.29 554 0.007235 69.45 556 0.007248 69.61 557 0.007272 69.77 559 0.007285 69.93 560 0.007309 70.09 561 0.007346 70.25 562 0.007371 70.42 564 0.007408 70.58 565 0.00742 70.74 567 0.007433 70.9 568 0.00747 71.06 569 0.007494 71.22 571 0.007519 71.38 571 0.007531 71.54 573 0.007556 71.7 574 0.007568 71.87 575 0.007581 72.03 577 0.007593 72.19 578 0.007605 72.35 580 0.007593 72.51 581 0.007618 72.67 582 0.00763 72.83 584 0.007642 72.99 584 0.007667 73.15 586 0.007679 73.32 587 0.007704 73.48 589 0.007729 73.64 590 0.007741 73.8 591 0.007778 73.96 592 0.00779 74.12 594 0.007827 74.28 595 0.007864 74.44 596 0.007889 74.61 598 0.007914 74.77 599 0.007926 74.93 600 0.007951 75.09 601 0.007976 75.25 603 0.008 75.41 603 0.008025 75.57 604 0.008037 75.73 607 0.008062 75.89 607 0.008074 76.06 609 0.008087 76.22 610 0.008099 76.38 611 0.008124 76.54 613 0.008124 76.7 614 0.008161 76.86 615 0.008185 77.02 617 0.00821 77.18 617 0.008235 77.34 619 0.008259 77.51 621 0.008272 77.67 621 0.008284 77.83 623 0.008309 77.99 625 0.008321 78.15 625 0.008346 78.31 627 0.008358 78.47 628 0.00837 78.63 629 0.008358 78.79 631 0.008358 78.96 632 0.008358 79.12 634 0.008321 79.28 635 0.008296 79.44 636 0.008296 79.6 637 0.008296 79.76 639 0.008321 79.92 640 0.008333 80.08 642 0.008358 80.24 643 0.008395 80.41 644 0.008432 80.57 646 0.008494 80.73 646 0.008518 80.89 649 0.008543 81.05 649 0.008531 81.21 650 0.00858 81.37 652 0.008642 81.53 653 0.008679 81.69 654 0.008716 81.86 656 0.008753 82.02 657 0.008765 82.18 658 0.008765 82.34 660 0.00879 82.5 661 0.008814 82.66 662 0.008851 82.82 664 0.008888 82.98 665 0.008913 83.15 665 0.008938 83.31 668 0.00895 83.47 668 0.008962 83.63 669 0.008962 83.79 671 0.008962 83.95 672 0.008962 84.11 674 0.008975 84.27 675 0.008987 84.43 676 0.009024 84.6 678 0.009049 84.76 679 0.009049 84.92 680 0.009073 85.08 682 0.00911 85.24 683 0.009123 85.4 684 0.009172 85.56 685 0.009222 85.72 687 0.009246 85.88 689 0.009271 86.05 690 0.009283 86.21 691 0.009296 86.37 692 0.009333 86.53 693 0.009345 86.69 694 0.009357 86.85 696 0.00937 87.01 697 0.009382 87.17 699 0.009394 87.33 700 0.009419 87.5 701 0.009456 87.66 703 0.009481 87.82 703 0.009481 87.98 705 0.009505 88.14 706 0.009505 88.3 707 0.00953 88.46 709 0.009542 88.62 710 0.009555 88.78 711 0.009579 88.95 713 0.009604 89.11 714 0.009616 89.27 715 0.009641 89.43 717 0.009666 89.59 718 0.009653 89.75 719 0.009678 89.91 720 0.009703 90.07 721 0.009727 90.24 723 0.00974 90.4 724 0.009752 90.56 725 0.009777 90.72 727 0.009801 90.88 728 0.009814 91.04 730 0.009838 91.2 731 0.009863 91.36 732 0.009888 91.52 734 0.0099 91.69 735 0.009925 91.85 736 0.009937 92.01 738 0.009974 92.17 739 0.009999 92.33 740 0.01001 92.49 742 0.01002 92.65 743 0.01002 92.81 744 0.01004 92.97 745 0.01005 93.14 746 0.01006 93.3 747 0.0101 93.46 749 0.01011 93.62 750 0.0101 93.78 750 0.01009 93.94 751 0.01007 94.1 753 0.01006 94.26 753 0.01007 94.42 754 0.01011 94.59 755 0.01013 94.75 755 0.01017 94.91 756 0.01021 95.07 756 0.01023 95.23 757 0.01026 95.39 757 0.01029 95.55 757 0.01031 95.71 759 0.01034 95.87 759 0.01039 96.04 761 0.01044 96.2 761 0.0105 96.36 762 0.01055 96.52 764 0.0106 96.68 764 0.01064 96.84 766 0.01068 97 767 0.0107 97.16 768 0.01071 97.32 769 0.01076 97.49 771 0.01079 97.65 772 0.01084 97.81 774 0.01086 97.97 775 0.0109 98.13 778 0.01091 98.29 779 0.01097 98.45 780 0.01102 98.61 782 0.01106 98.78 784 0.01111 98.94 785 0.01117 99.1 787 0.0112 99.26 789 0.01123 99.42 790 0.01128 99.58 792 0.01131 99.74 793 0.01133 99.9 794 0.01136 100.1 796 0.01137 100.2 796 0.01136 100.4 797 0.01134 100.5 799 0.01133 100.7 800 0.01132 100.9 801 0.01131 101 801 0.01128 101.2 801 0.01126 101.4 801 0.01124 101.5 801 0.01122 101.7 803 0.01117 101.8 804 0.01115 102 806 0.01111 102.2 807 0.01105 102.3 809 0.01097 102.5 811 0.01085 102.6 812 0.01076 102.8 814 0.01071 103 815 0.01066 103.1 818 0.01059 103.3 819 0.01053 103.4 821 0.01043 103.6 823 0.01033 103.8 825 0.01025 103.9 828 0.01016 104.1 829 0.01009 104.3 832 0.009986 104.4 834 0.009937 104.6 836 0.009875 104.7 839 0.009777 104.9 841 0.009703 105.1 843 0.009653 105.2 844 0.009604 105.4 847 0.009555 105.5 848 0.009518 105.7 850 0.009481 105.9 851 0.009456 106 853 0.009444 106.2 854 0.009456 106.3 856 0.009456 106.5 857 0.009444 106.7 859 0.009444 106.8 861 0.009444 107 864 0.009481 107.2 865 0.009505 107.3 867 0.009518 107.5 868 0.00953 107.6 870 0.009567 107.8 872 0.009604 108 873 0.009641 108.1 874 0.009666 108.3 875 0.00969 108.4 876 0.009715 108.6 877 0.00974 108.8 878 0.009752 108.9 879 0.009777 109.1 879 0.009789 109.2 880 0.009801 109.4 881 0.009814 109.6 881 0.009851 109.7 882 0.009851 109.9 883 0.009875 110.1 883 0.009888 110.2 884 0.009888 110.4 885 0.009912 110.5 886 0.009937 110.7 886 0.009949 110.9 887 0.009986 111 887 0.01001 111.2 889 0.01004 111.3 889 0.01005 111.5 890 0.01009 111.7 891 0.01011 111.8 892 0.01013 112 893 0.01016 112.1 893 0.01017 112.3 895 0.0102 112.5 897 0.01023 112.6 897 0.01027 112.8 899 0.01029 113 900 0.01033 113.1 901 0.01036 113.3 902 0.01039 113.4 903 0.01041 113.6 905 0.01044 113.8 906 0.01049 113.9 907 0.01053 114.1 909 0.01057 114.2 911 0.01059 114.4 911 0.01063 114.6 913 0.01066 114.7 915 0.01071 114.9 915 0.01078 115 917 0.01083 115.2 918 0.01087 115.4 919 0.01091 115.5 921 0.01092 115.7 922 0.0109 115.9 924 0.0109 116 925 0.01092 116.2 926 0.01099 116.3 928 0.01107 116.5 929 0.01112 116.7 931 0.01112 116.8 932 0.01113 117 934 0.01117 117.1 935 0.01121 117.3 936 0.01123 117.5 937 0.01126 117.6 939 0.01126 117.8 940 0.01129 118 942 0.01131 118.1 943 0.01133 118.3 944 0.01136 118.4 946 0.01139 118.6 947 0.01143 118.8 948 0.01148 118.9 950 0.01153 119.1 950 0.01157 119.2 952 0.01159 119.4 953 0.01164 119.6 955 0.0117 119.7 956 0.01174 119.9 957 0.01176 120 958 0.01182 120.2 960 0.01186 120.4 961 0.01189 120.5 962 0.01192 120.7 963 0.01194 120.9 964 0.01192 121 965 0.01191 121.2 965 0.01192 121.3 968 0.01196 121.5 968 0.01201 121.7 968 0.01205 121.8 968 0.01208 122 969 0.01212 122.1 972 0.01213 122.3 972 0.01216 122.5 973 0.01217 122.6 974 0.01221 122.8 975 0.01226 122.9 977 0.01228 123.1 978 0.01232 123.3 980 0.01235 123.4 981 0.0124 123.6 983 0.01243 123.8 984 0.01248 123.9 986 0.01252 124.1 987 0.01258 124.2 989 0.01264 124.4 990 0.01264 124.6 993 0.01266 124.7 994 0.0127 124.9 996 0.01274 125 997 0.01277 125.2 998 0.01281 125.4 1000 0.01285 125.5 1001 0.01289 125.7 1003 0.01291 125.8 1004 0.01296 126 1006 0.01301 126.2 1007 0.01306 126.3 1009 0.01308 126.5 1010 0.01312 126.7 1011 0.01316 126.8 1012 0.01321 127 1013 0.01322 127.1 1014 0.01327 127.3 1015 0.01332 127.5 1016 0.01335 127.6 1017 0.0134 127.8 1018 0.01345 127.9 1019 0.0135 128.1 1022 0.01356 128.3 1023 0.01363 128.4 1025 0.01366 128.6 1026 0.01371 128.7 1028 0.01376 128.9 1029 0.01379 129.1 1031 0.01385 129.2 1033 0.01388 129.4 1034 0.01393 129.6 1036 0.01396 129.7 1037 0.01401 129.9 1039 0.01405 130 1040 0.01406 130.2 1041 0.01408 130.4 1043 0.01411 130.5 1043 0.01414 130.7 1045 0.01417 130.8 1047 0.01421 131 1048 0.01422 131.2 1049 0.01424 131.3 1050 0.01428 131.5 1051 0.0143 131.6 1053 0.01433 131.8 1054 0.01433 132 1055 0.01438 132.1 1056 0.0144 132.3 1057 0.01444 132.5 1059 0.01448 132.6 1059 0.0145 132.8 1061 0.01454 132.9 1062 0.01458 133.1 1064 0.01461 133.3 1065 0.01464 133.4 1067 0.01467 133.6 1068 0.01469 133.7 1068 0.01472 133.9 1069 0.01476 134.1 1072 0.01479 134.2 1073 0.01483 134.4 1074 0.01486 134.5 1076 0.01488 134.7 1077 0.01492 134.9 1078 0.01497 135 1079 0.01501 135.2 1081 0.01506 135.4 1082 0.01511 135.5 1083 0.01512 135.7 1084 0.01516 135.8 1086 0.01519 136 1087 0.0152 136.2 1088 0.01525 136.3 1090 0.01528 136.5 1091 0.01532 136.6 1092 0.01534 136.8 1094 0.01533 137 1095 0.01533 137.1 1097 0.01534 137.3 1098 0.01538 137.4 1099 0.0154 137.6 1101 0.01544 137.8 1101 0.01545 137.9 1103 0.01549 138.1 1104 0.01553 138.3 1106 0.01557 138.4 1107 0.01561 138.6 1108 0.01565 138.7 1109 0.01569 138.9 1111 0.01572 139.1 1112 0.01574 139.2 1114 0.01576 139.4 1115 0.01578 139.5 1115 0.01582 139.7 1117 0.01585 139.9 1119 0.01587 140 1119 0.01591 140.2 1121 0.01593 140.3 1122 0.01597 140.5 1124 0.01599 140.7 1125 0.01604 140.8 1126 0.01606 141 1128 0.01611 141.2 1129 0.01613 141.3 1130 0.01615 141.5 1132 0.0162 141.6 1133 0.01622 141.8 1134 0.01625 142 1136 0.01627 142.1 1136 0.0163 142.3 1137 0.01635 142.4 1139 0.01638 142.6 1140 0.01641 142.8 1142 0.01644 142.9 1144 0.01646 143.1 1144 0.0165 143.2 1146 0.01651 143.4 1147 0.01656 143.6 1148 0.01659 143.7 1150 0.01662 143.9 1151 0.01666 144.1 1152 0.01671 144.2 1154 0.01676 144.4 1155 0.01678 144.5 1156 0.01681 144.7 1157 0.01683 144.9 1159 0.01687 145 1160 0.01689 145.2 1162 0.01692 145.3 1162 0.01696 145.5 1164 0.01699 145.7 1165 0.01703 145.8 1166 0.01707 146 1168 0.01712 146.1 1169 0.01714 146.3 1170 0.01717 146.5 1172 0.0172 146.6 1173 0.01722 146.8 1174 0.01724 147 1175 0.01728 147.1 1177 0.0173 147.3 1178 0.01735 147.4 1179 0.01738 147.6 1180 0.01743 147.8 1182 0.01745 147.9 1183 0.01746 148.1 1184 0.01751 148.2 1186 0.01755 148.4 1187 0.01759 148.6 1188 0.01762 148.7 1190 0.01767 148.9 1191 0.01773 149 1193 0.01777 149.2 1194 0.01782 149.4 1194 0.01784 149.5 1197 0.01789 149.7 1198 0.01796 149.9 1200 0.01796 150 1201 0.01796 150.2 1201 0.01794 150.3 1201 0.01793 150.5 1201 0.01792 150.7 1202 0.01793 150.8 1202 0.01794 151 1202 0.01793 151.1 1202 0.01794 151.3 1203 0.01793 151.5 1203 0.01791 151.6 1202 0.01789 151.8 1202 0.01788 151.9 1202 0.01787 152.1 1201 0.01788 152.3 1201 0.01789 152.4 1201 0.01789 152.6 1201 0.01791 152.8 1201 0.01792 152.9 1201 0.01793 153.1 1201 0.01793 153.2 1201 0.01792 153.4 1200 0.01791 153.6 1200 0.01791 153.7 1200 0.01789 153.9 1199 0.01789 154 1199 0.01788 154.2 1199 0.01788 154.4 1199 0.01789 154.5 1199 0.01788 154.7 1199 0.01788 154.8 1199 0.01789 155 1199 0.01788 155.2 1198 0.01787 155.3 1198 0.01787 155.5 1198 0.01786 155.7 1199 0.01786 155.8 1198 0.01786 156 1198 0.01784 156.1 1198 0.01784 156.3 1198 0.01784 156.5 1198 0.01784 156.6 1198 0.01784 156.8 1198 0.01784 156.9 1199 0.01786 157.1 1198 0.01784 157.3 1199 0.01786 157.4 1199 0.01786 157.6 1199 0.01786 157.8 1199 0.01786 157.9 1199 0.01787 158.1 1199 0.01788 158.2 1199 0.01788 158.4 1199 0.01788 158.6 1199 0.01788 158.7 1199 0.01788 158.9 1199 0.01787 159 1199 0.01787 159.2 1199 0.01788 159.4 1199 0.01789 159.5 1199 0.01788 159.7 1199 0.01789 159.8 1199 0.01789 160 1199 0.01791 160.2 1199 0.01791 160.3 1199 0.01791 160.5 1199 0.01791 160.7 1199 0.01791 160.8 1199 0.01791 161 1199 0.01791 161.1 1199 0.01791 161.3 1199 0.01791 161.5 1199 0.01791 161.6 1199 0.01791 161.8 1199 0.01791 161.9 1199 0.01791 162.1 1199 0.01791 162.3 1199 0.01792 162.4 1199 0.01791 162.6 1199 0.01789 162.7 1199 0.01788 162.9 1199 0.01787 163.1 1199 0.01784 163.2 1199 0.01783 163.4 1199 0.01784 163.6 1199 0.01786 163.7 1199 0.01787 163.9 1199 0.01787 164 1199 0.01787 164.2 1199 0.01788 164.4 1199 0.01787 164.5 1199 0.01787 164.7 1199 0.01787 164.8 1199 0.01787 165 1199 0.01787 165.2 1199 0.01788 165.3 1199 0.01787 165.5 1199 0.01786 165.6 1199 0.01788 165.8 1199 0.01788 166 1199 0.01789 166.1 1199 0.01787 166.3 1199 0.01787 166.5 1199 0.01787 166.6 1199 0.01789 166.8 1198 0.01789 166.9 1199 0.01789 167.1 1199 0.01789 167.3 1199 0.01789 167.4 1199 0.01789 167.6 1199 0.01788 167.7 1199 0.01789 167.9 1198 0.01789 168.1 1199 0.01789 168.2 1199 0.01791 168.4 1199 0.01789 168.5 1199 0.01788 168.7 1199 0.01788 168.9 1199 0.01787 169 1199 0.01787 169.2 1199 0.01788 169.4 1199 0.01789 169.5 1199 0.01789 169.7 1199 0.01789 169.8 1199 0.01789 170 1199 0.01791 170.2 1199 0.01791 170.3 1199 0.01791 170.5 1199 0.01791 170.6 1199 0.01791 170.8 1199 0.01789 171 1199 0.01791 171.1 1199 0.01791 171.3 1200 0.01791 171.4 1199 0.01791 171.6 1199 0.01789 171.8 1199 0.01789 171.9 1199 0.01789 172.1 1199 0.01789 172.3 1199 0.01788 172.4 1199 0.01789 172.6 1199 0.01788 172.7 1199 0.01788 172.9 1199 0.01787 173.1 1199 0.01787 173.2 1199 0.01787 173.4 1199 0.01786 173.5 1199 0.01787 173.7 1199 0.01788 173.9 1199 0.01787 174 1199 0.01787 174.2 1199 0.01786 174.3 1199 0.01787 174.5 1199 0.01786 174.7 1199 0.01787 174.8 1199 0.01788 175 1199 0.01789 175.2 1199 0.01789 175.3 1199 0.01788 175.5 1199 0.01788 175.6 1199 0.01787 175.8 1199 0.01786 176 1199 0.01787 176.1 1199 0.01786 176.3 1199 0.01784 176.4 1199 0.01784 176.6 1199 0.01788 176.8 1199 0.01788 176.9 1199 0.01789 177.1 1199 0.01789 177.2 1199 0.01788 177.4 1199 0.01789 177.6 1199 0.01792 177.7 1199 0.01789 177.9 1199 0.01789 178.1 1199 0.01789 178.2 1199 0.01789 178.4 1199 0.01787 178.5 1199 0.01784 178.7 1199 0.01786 178.9 1199 0.01787 179 1199 0.01787 179.2 1199 0.01789 179.3 1199 0.01789 179.5 1199 0.01788 179.7 1199 0.01789 179.8 1199 0.01789 180 1199 0.01789 180.1 1199 0.01789 180.3 1199 0.01791 180.5 1199 0.01793 180.6 1199 0.01793 180.8 1199 0.01792 181 1199 0.01789 181.1 1199 0.01792 181.3 1199 0.01793 181.4 1199 0.01794 181.6 1199 0.01793 181.8 1199 0.01792 181.9 1199 0.01789 182.1 1199 0.01789 182.2 1199 0.01788 182.4 1199 0.01789 182.6 1199 0.01792 182.7 1199 0.01793 182.9 1199 0.01794 183 1199 0.01793 183.2 1199 0.01793 183.4 1199 0.01792 183.5 1199 0.01792 183.7 1199 0.01792 183.9 1199 0.01792 184 1199 0.01791 184.2 1199 0.01792 184.3 1199 0.01793 184.5 1199 0.01793 184.7 1199 0.01793 184.8 1199 0.01792 185 1199 0.01793 185.1 1199 0.01793 185.3 1199 0.01794 185.5 1199 0.01796 185.6 1199 0.01796 185.8 1199 0.01796 185.9 1199 0.01796 186.1 1199 0.01799 186.3 1199 0.01796 186.4 1199 0.01794 186.6 1199 0.01793 186.8 1199 0.01792 186.9 1199 0.01792 187.1 1199 0.01789 187.2 1199 0.01789 187.4 1199 0.01789 187.6 1199 0.01791 187.7 1199 0.01791 187.9 1199 0.01793 188 1199 0.01796 188.2 1199 0.01796 188.4 1199 0.01797 188.5 1199 0.01796 188.7 1199 0.01794 188.8 1199 0.01792 189 1199 0.01789 189.2 1199 0.01789 189.3 1199 0.01789 189.5 1199 0.01789 189.7 1199 0.01791 189.8 1199 0.01791 190 1199 0.01791 190.1 1199 0.01791 190.3 1199 0.01793 190.5 1199 0.01793 190.6 1199 0.01794 190.8 1199 0.01794 190.9 1199 0.01794 191.1 1199 0.01796 191.3 1199 0.01796 191.4 1199 0.01796 191.6 1199 0.01796 191.7 1199 0.01796 191.9 1199 0.01796 192.1 1199 0.01798 192.2 1199 0.01799 192.4 1199 0.01798 192.6 1199 0.01796 192.7 1199 0.01794 192.9 1199 0.01793 193 1199 0.01793 193.2 1199 0.01792 193.4 1199 0.01792 193.5 1199 0.01792 193.7 1199 0.01792 193.8 1199 0.01792 194 1199 0.01792 194.2 1199 0.01794 194.3 1199 0.01793 194.5 1199 0.01793 194.6 1199 0.01794 194.8 1199 0.01796 195 1199 0.01797 195.1 1199 0.01798 195.3 1199 0.01796 195.5 1199 0.01792 195.6 1199 0.01788 195.8 1199 0.01788 195.9 1199 0.01789 196.1 1199 0.01792 196.3 1199 0.01793 196.4 1199 0.01794 196.6 1199 0.01794 196.7 1198 0.01794 196.9 1199 0.01793 197.1 1199 0.01792 197.2 1199 0.01792 197.4 1199 0.01792 197.6 1199 0.01791 197.7 1199 0.01792 197.9 1199 0.01792 198 1199 0.01794 198.2 1199 0.01794 198.4 1199 0.01793 198.5 1199 0.01793 198.7 1199 0.01793 198.8 1199 0.01793 199 1199 0.01793 199.2 1199 0.01794 199.3 1199 0.01796 199.5 1199 0.01796 199.6 1199 0.01796 199.8 1199 0.01794 200 1199 0.01793 200.1 1199 0.01794 200.3 1199 0.01794 200.5 1199 0.01793 200.6 1199 0.01792 200.8 1199 0.01792 200.9 1199 0.01793 201.1 1199 0.01793 201.3 1199 0.01794 201.4 1199 0.01794 201.6 1199 0.01797 201.7 1199 0.01799 201.9 1199 0.01799 202.1 1199 0.01799 202.2 1199 0.01797 202.4 1199 0.01794 202.5 1199 0.01794 202.7 1199 0.01793 202.9 1199 0.01793 203 1199 0.01791 203.2 1199 0.01789 203.4 1199 0.01789 203.5 1199 0.01789 203.7 1199 0.01789 203.8 1199 0.01792 204 1199 0.01791 204.2 1199 0.01791 204.3 1199 0.01789 204.5 1199 0.01791 204.6 1199 0.01793 204.8 1199 0.01792 205 1199 0.01793 205.1 1199 0.01792 205.3 1199 0.01792 205.4 1199 0.01792 205.6 1199 0.01791 205.8 1199 0.01792 205.9 1199 0.01793 206.1 1199 0.01793 206.3 1199 0.01794 206.4 1199 0.01794 206.6 1199 0.01796 206.7 1199 0.01797 206.9 1199 0.01798 207.1 1199 0.01799 207.2 1199 0.01799 207.4 1199 0.01798 207.5 1199 0.01797 207.7 1199 0.01797 207.9 1199 0.01796 208 1199 0.01794 208.2 1199 0.01794 208.3 1199 0.01794 208.5 1199 0.01796 208.7 1199 0.01798 208.8 1199 0.01798 209 1199 0.01797 209.2 1199 0.01796 209.3 1199 0.01794 209.5 1199 0.01793 209.6 1199 0.01793 209.8 1199 0.01794 210 1199 0.01793 210.1 1199 0.01794 210.3 1199 0.01796 210.4 1199 0.01796 210.6 1199 0.01794 210.8 1199 0.01796 210.9 1199 0.01796 211.1 1199 0.01796 211.2 1199 0.01796 211.4 1199 0.01796 211.6 1199 0.01797 211.7 1199 0.01796 211.9 1199 0.01794 212.1 1199 0.01793 212.2 1199 0.01792 212.4 1199 0.01792 212.5 1199 0.01792 212.7 1199 0.01792 212.9 1199 0.01794 213 1199 0.01793 213.2 1199 0.01793 213.3 1199 0.01792 213.5 1199 0.01792 213.7 1199 0.01792 213.8 1199 0.01793 214 1199 0.01794 214.1 1199 0.01794 214.3 1199 0.01794 214.5 1199 0.01796 214.6 1199 0.01796 214.8 1199 0.01796 215 1199 0.01797 215.1 1199 0.01796 215.3 1199 0.01794 215.4 1199 0.01794 215.6 1199 0.01794 215.8 1199 0.01797 215.9 1199 0.01796 216.1 1199 0.01796 216.2 1199 0.01796 216.4 1199 0.01796 216.6 1199 0.01797 216.7 1199 0.01798 216.9 1199 0.01798 217 1199 0.01798 217.2 1199 0.01797 217.4 1199 0.01797 217.5 1199 0.01796 217.7 1199 0.01796 217.9 1199 0.01797 218 1199 0.01796 218.2 1199 0.01797 218.3 1199 0.01797 218.5 1199 0.01796 218.7 1199 0.01796 218.8 1199 0.01797 219 1199 0.01798 219.1 1199 0.01798 219.3 1199 0.01798 219.5 1199 0.01797 219.6 1199 0.01798 219.8 1199 0.01799 219.9 1199 0.01801 220.1 1200 0.01801 220.3 1199 0.01802 220.4 1199 0.01802 220.6 1199 0.01799 220.8 1199 0.01799 220.9 1199 0.01798 221.1 1199 0.01799 221.2 1199 0.01801 221.4 1199 0.01799 221.6 1199 0.01801 221.7 1199 0.01802 221.9 1199 0.01799 222 1199 0.01798 222.2 1199 0.01794 222.4 1199 0.01793 222.5 1199 0.01793 222.7 1199 0.01793 222.8 1199 0.01796 223 1199 0.01798 223.2 1199 0.01799 223.3 1199 0.01801 223.5 1199 0.01799 223.7 1199 0.01799 223.8 1199 0.01802 224 1199 0.01802 224.1 1199 0.01802 224.3 1199 0.01799 224.5 1199 0.01799 224.6 1199 0.01798 224.8 1199 0.01797 224.9 1199 0.01799 225.1 1199 0.01802 225.3 1199 0.01803 225.4 1199 0.01804 225.6 1199 0.01803 225.7 1199 0.01799 225.9 1199 0.01798 226.1 1199 0.01798 226.2 1199 0.01802 226.4 1199 0.01802 226.6 1199 0.01798 226.7 1199 0.01798 226.9 1199 0.01798 227 1199 0.01797 227.2 1199 0.01799 227.4 1199 0.01797 227.5 1199 0.01796 227.7 1199 0.01796 227.8 1199 0.01796 228 1199 0.01796 228.2 1199 0.01798 228.3 1199 0.01799 228.5 1199 0.01799 228.6 1199 0.01802 228.8 1199 0.01802 229 1199 0.01802 229.1 1199 0.01799 229.3 1199 0.01799 229.5 1199 0.01799 229.6 1199 0.01799 229.8 1199 0.01799 229.9 1199 0.01802 230.1 1199 0.01802 230.3 1199 0.01802 230.4 1199 0.01802 230.6 1199 0.01802 230.7 1199 0.01802 230.9 1199 0.01802 231.1 1199 0.01802 231.2 1199 0.01802 231.4 1199 0.01802 231.5 1199 0.01802 231.7 1199 0.01802 231.9 1199 0.01804 232 1199 0.01803 232.2 1199 0.01803 232.4 1199 0.01804 232.5 1199 0.01804 232.7 1199 0.01804 232.8 1199 0.01804 233 1199 0.01804 233.2 1199 0.01804 233.3 1199 0.01804 233.5 1199 0.01802 233.6 1199 0.01799 233.8 1199 0.01802 234 1199 0.01802 234.1 1199 0.01804 234.3 1199 0.01804 234.4 1199 0.01805 234.6 1199 0.01808 234.8 1199 0.01808 234.9 1199 0.01805 235.1 1199 0.01804 235.3 1199 0.01804 235.4 1199 0.01803 235.6 1199 0.01803 235.7 1199 0.01802 235.9 1199 0.01803 236.1 1199 0.01802 236.2 1199 0.01804 236.4 1199 0.01803 236.5 1199 0.01803 236.7 1199 0.01803 236.9 1199 0.01802 237 1199 0.01801 237.2 1199 0.01801 237.4 1199 0.01801 237.5 1199 0.01802 237.7 1199 0.01802 237.8 1199 0.01802 238 1199 0.01802 238.2 1199 0.01803 238.3 1199 0.01804 238.5 1199 0.01804 238.6 1199 0.01807 238.8 1199 0.01809 239 1199 0.01809 239.1 1199 0.01809 239.3 1199 0.01808 239.4 1199 0.01808 239.6 1199 0.01808 239.8 1199 0.01807 239.9 1199 0.01809 240.1 1199 0.0181 240.3 1199 0.01812 240.4 1199 0.01812 240.6 1199 0.0181 240.7 1199 0.01812 240.9 1199 0.01809 241.1 1199 0.01809 241.2 1199 0.01808 241.4 1199 0.01809 241.5 1199 0.01809 241.7 1199 0.01808 241.9 1199 0.01808 242 1199 0.01805 242.2 1199 0.01805 242.3 1199 0.01808 242.5 1200 0.01809 242.7 1199 0.01809 242.8 1199 0.01809 243 1199 0.01807 243.2 1199 0.01804 243.3 1199 0.01804 243.5 1199 0.01804 243.6 1199 0.01804 243.8 1199 0.01805 244 1199 0.01808 244.1 1199 0.01809 244.3 1199 0.01809 244.4 1199 0.01809 244.6 1199 0.01808 244.8 1199 0.01808 244.9 1199 0.01808 245.1 1199 0.01808 245.2 1199 0.01807 245.4 1199 0.01807 245.6 1199 0.01807 245.7 1199 0.01803 245.9 1199 0.01803 246.1 1199 0.01802 246.2 1199 0.01802 246.4 1199 0.01803 246.5 1199 0.01804 246.7 1199 0.01804 246.9 1199 0.01805 247 1199 0.01805 247.2 1199 0.01807 247.3 1199 0.01805 247.5 1199 0.01804 247.7 1199 0.01804 247.8 1199 0.01804 248 1199 0.01804 248.1 1199 0.01804 248.3 1199 0.01805 248.5 1199 0.01805 248.6 1199 0.01803 248.8 1199 0.01802 249 1199 0.01799 249.1 1199 0.01799 249.3 1199 0.01798 249.4 1199 0.01799 249.6 1199 0.01802 249.8 1199 0.01803 249.9 1199 0.01807 250.1 1199 0.01808 250.2 1199 0.01809 250.4 1199 0.01809 250.6 1199 0.01809 250.7 1199 0.01809 250.9 1199 0.01808 251 1199 0.01808 251.2 1199 0.01808 251.4 1199 0.0181 251.5 1199 0.01813 251.7 1199 0.01812 251.9 1199 0.01813 252 1199 0.01813 252.2 1199 0.01813 252.3 1199 0.01813 252.5 1199 0.01813 252.7 1199 0.01813 252.8 1199 0.01812 253 1199 0.01812 253.1 1199 0.01813 253.3 1199 0.01812 253.5 1199 0.01813 253.6 1199 0.01813 253.8 1199 0.01813 253.9 1199 0.01812 254.1 1199 0.01812 254.3 1199 0.01814 254.4 1199 0.01813 254.6 1199 0.01813 254.8 1199 0.01812 254.9 1199 0.01809 255.1 1199 0.01809 255.2 1199 0.01809 255.4 1199 0.01812 255.6 1199 0.01813 255.7 1199 0.01813 255.9 1199 0.01813 256 1199 0.01812 256.2 1199 0.01814 256.4 1199 0.01813 256.5 1199 0.01813 256.7 1199 0.01813 256.8 1199 0.01812 257 1199 0.0181 257.2 1199 0.0181 257.3 1199 0.01812 257.5 1199 0.01813 257.7 1199 0.01814 257.8 1199 0.01815 258 1199 0.01815 258.1 1199 0.01815 258.3 1199 0.01815 258.5 1199 0.01815 258.6 1199 0.01815 258.8 1199 0.01815 258.9 1199 0.01815 259.1 1199 0.01813 259.3 1199 0.01813 259.4 1199 0.01814 259.6 1199 0.01815 259.7 1199 0.01814 259.9 1199 0.01813 260.1 1199 0.01813 260.2 1199 0.01814 260.4 1199 0.01813 260.6 1199 0.01813 260.7 1199 0.0181 260.9 1199 0.0181 261 1199 0.01809 261.2 1199 0.01807 261.4 1199 0.01808 261.5 1199 0.01808 261.7 1199 0.01809 261.8 1199 0.01808 262 1199 0.01809 262.2 1199 0.01813 262.3 1199 0.01812 262.5 1199 0.01813 262.6 1199 0.01814 262.8 1199 0.01815 263 1199 0.01815 263.1 1199 0.01814 263.3 1199 0.01815 263.5 1199 0.01814 263.6 1199 0.01813 263.8 1199 0.01817 263.9 1199 0.01815 264.1 1199 0.01815 264.3 1199 0.01815 264.4 1199 0.01817 264.6 1199 0.01819 264.7 1199 0.01819 264.9 1199 0.01818 265.1 1199 0.01818 265.2 1199 0.01813 265.4 1200 0.01813 265.5 1199 0.01818 265.7 1199 0.01815 265.9 1199 0.01813 266 1199 0.01813 266.2 1199 0.01812 266.4 1199 0.01813 266.5 1199 0.01818 266.7 1199 0.01815 266.8 1199 0.01815 267 1199 0.01818 267.2 1199 0.01815 267.3 1199 0.01815 267.5 1199 0.01815 267.6 1199 0.01817 267.8 1199 0.01817 268 1199 0.01817 268.1 1199 0.01818 268.3 1199 0.01817 268.4 1199 0.01818 268.6 1199 0.01819 268.8 1199 0.0182 268.9 1199 0.01817 269.1 1199 0.01814 269.3 1200 0.01813 269.4 1199 0.01809 269.6 1199 0.0181 269.7 1199 0.01813 269.9 1199 0.01813 270.1 1199 0.01815 270.2 1199 0.01815 270.4 1199 0.01815 270.5 1199 0.01812 270.7 1199 0.01808 270.9 1199 0.01809 271 1199 0.01813 271.2 1199 0.01815 271.3 1199 0.01815 271.5 1199 0.01818 271.7 1199 0.0182 271.8 1199 0.01818 272 1199 0.01814 272.2 1199 0.0181 272.3 1199 0.01813 272.5 1199 0.01814 272.6 1199 0.01814 272.8 1199 0.01814 273 1199 0.01815 273.1 1199 0.01818 273.3 1199 0.01817 273.4 1199 0.01815 273.6 1199 0.01815 273.8 1199 0.01819 273.9 1199 0.01821 274.1 1199 0.01821 274.3 1199 0.01817 274.4 1199 0.01814 274.6 1199 0.01812 274.7 1199 0.01813 274.9 1199 0.0181 275.1 1199 0.01809 275.2 1199 0.01809 275.4 1199 0.01809 275.5 1199 0.01814 275.7 1199 0.01814 275.9 1199 0.01813 276 1199 0.01808 276.2 1199 0.01807 276.3 1199 0.01809 276.5 1199 0.01815 276.7 1199 0.01817 276.8 1200 0.01815 277 1199 0.01817 277.2 1199 0.01814 277.3 1199 0.01813 277.5 1199 0.01814 277.6 1199 0.01817 277.8 1199 0.01818 278 1199 0.01818 278.1 1199 0.01814 278.3 1199 0.01814 278.4 1199 0.01814 278.6 1199 0.01817 278.8 1199 0.01819 278.9 1199 0.01819 279.1 1199 0.01819 279.2 1199 0.01818 279.4 1199 0.01814 279.6 1199 0.01812 279.7 1199 0.0181 279.9 1199 0.01814 280.1 1199 0.01818 280.2 1199 0.01821 280.4 1199 0.01819 280.5 1199 0.01818 280.7 1199 0.01817 280.9 1199 0.01814 281 1199 0.01815 281.2 1199 0.01815 281.3 1199 0.01818 281.5 1199 0.01819 281.7 1199 0.0182 281.8 1199 0.01819 282 1199 0.01815 282.1 1199 0.0181 282.3 1199 0.01807 282.5 1199 0.01804 282.6 1199 0.01804 282.8 1199 0.01805 283 1199 0.0181 283.1 1199 0.01817 283.3 1199 0.01819 283.4 1199 0.01821 283.6 1199 0.01821 283.8 1199 0.01819 283.9 1199 0.0182 284.1 1199 0.01821 284.2 1199 0.01819 284.4 1199 0.01817 284.6 1199 0.01813 284.7 1199 0.01812 284.9 1199 0.01809 285 1199 0.01808 285.2 1199 0.01808 285.4 1199 0.01809 285.5 1199 0.01808 285.7 1199 0.01808 285.9 1199 0.01808 286 1199 0.01807 286.2 1199 0.01809 286.3 1199 0.01809 286.5 1199 0.01808 286.7 1199 0.01809 286.8 1199 0.01809 287 1199 0.0181 287.1 1199 0.0181 287.3 1199 0.0181 287.5 1199 0.01809 287.6 1199 0.01808 287.8 1199 0.01808 287.9 1199 0.01809 288.1 1199 0.01812 288.3 1200 0.01813 288.4 1199 0.01813 288.6 1199 0.01812 288.8 1199 0.0181 288.9 1199 0.0181 289.1 1199 0.01808 289.2 1199 0.01807 289.4 1200 0.0181 289.6 1199 0.01812 289.7 1199 0.01812 289.9 1199 0.01812 290 1199 0.01813 290.2 1199 0.01814 290.4 1199 0.01817 290.5 1199 0.01819 290.7 1199 0.01819 290.8 1199 0.0182 291 1199 0.0182 291.2 1200 0.01819 291.3 1199 0.01815 291.5 1199 0.01813 291.7 1199 0.0181 291.8 1199 0.01812 292 1199 0.01812 292.1 1199 0.01812 292.3 1199 0.01813 292.5 1200 0.01817 292.6 1199 0.01819 292.8 1199 0.01819 292.9 1199 0.01819 293.1 1199 0.01817 293.3 1199 0.01813 293.4 1199 0.01812 293.6 1199 0.01812 293.7 1199 0.01814 293.9 1199 0.01815 294.1 1199 0.01819 294.2 1199 0.0182 294.4 1199 0.01819 294.6 1199 0.01818 294.7 1199 0.01813 294.9 1199 0.01809 295 1199 0.01809 295.2 1199 0.0181 295.4 1199 0.01813 295.5 1199 0.01812 295.7 1199 0.01809 295.8 1199 0.01807 296 1199 0.01808 296.2 1199 0.01809 296.3 1199 0.01812 296.5 1199 0.01814 296.6 1199 0.01813 296.8 1199 0.01814 297 1199 0.01817 297.1 1199 0.0182 297.3 1199 0.01824 297.5 1199 0.01821 297.6 1199 0.01814 297.8 1199 0.0181 297.9 1199 0.01809 298.1 1199 0.01813 298.3 1199 0.01814 298.4 1199 0.01814 298.6 1199 0.01813 298.7 1199 0.01812 298.9 1199 0.01815 299.1 1200 0.01818 299.2 1199 0.01818 299.4 1199 0.01818 299.5 1199 0.01819 299.7 1200 0.01819 299.9 1199 0.01817 300 1199 0.01815 300.2 1199 0.01814 300.4 1199 0.01814 300.5 1199 0.01814 300.7 1199 0.01812 300.8 1199 0.01812 301 1199 0.01813 301.2 1199 0.01813 301.3 1199 0.01813 301.5 1199 0.0181 301.6 1199 0.01812 301.8 1199 0.01812 302 1199 0.01812 302.1 1199 0.01812 302.3 1199 0.01813 302.4 1199 0.01815 302.6 1200 0.01817 302.8 1199 0.01814 302.9 1199 0.01814 303.1 1199 0.01817 303.3 1199 0.01815 303.4 1199 0.01815 303.6 1200 0.01815 303.7 1199 0.01814 303.9 1199 0.01813 304.1 1199 0.01814 304.2 1199 0.01814 304.4 1199 0.01817 304.5 1199 0.01813 304.7 1199 0.01813 304.9 1199 0.01814 305 1199 0.01813 305.2 1199 0.01814 305.3 1199 0.01814 305.5 1199 0.01814 305.7 1199 0.01814 305.8 1199 0.01814 306 1199 0.01815 306.2 1199 0.01813 306.3 1199 0.01813 306.5 1199 0.01814 306.6 1199 0.01814 306.8 1199 0.01814 307 1199 0.01814 307.1 1199 0.01814 307.3 1199 0.01814 307.4 1199 0.01815 307.6 1199 0.01814 307.8 1199 0.01813 307.9 1199 0.01813 308.1 1199 0.01813 308.2 1199 0.01813 308.4 1199 0.01813 308.6 1199 0.01813 308.7 1199 0.01813 308.9 1199 0.01812 309.1 1199 0.01813 309.2 1199 0.01814 309.4 1199 0.01813 309.5 1199 0.01815 309.7 1199 0.01817 309.9 1199 0.01815 310 1199 0.01817 310.2 1199 0.01818 310.3 1199 0.01817 310.5 1199 0.01815 310.7 1199 0.01813 310.8 1199 0.01813 311 1199 0.01813 311.1 1199 0.01813 311.3 1199 0.01813 311.5 1199 0.01814 311.6 1200 0.01813 311.8 1199 0.01814 312 1199 0.01815 312.1 1199 0.01815 312.3 1199 0.01815 312.4 1199 0.01814 312.6 1199 0.01815 312.8 1199 0.01814 312.9 1199 0.01814 313.1 1199 0.01815 313.2 1199 0.01815 313.4 1199 0.01815 313.6 1199 0.01814 313.7 1199 0.01814 313.9 1199 0.01817 314.1 1200 0.01815 314.2 1199 0.01814 314.4 1199 0.01814 314.5 1199 0.01815 314.7 1199 0.01817 314.9 1199 0.01815 315 1199 0.01817 315.2 1199 0.01815 315.3 1199 0.01814 315.5 1199 0.01815 315.7 1199 0.01814 315.8 1199 0.01813 316 1199 0.01815 316.1 1199 0.01815 316.3 1199 0.01817 316.5 1199 0.01817 316.6 1199 0.01815 316.8 1199 0.01817 317 1199 0.01817 317.1 1199 0.01818 317.3 1199 0.01817 317.4 1199 0.01815 317.6 1199 0.01815 317.8 1199 0.01815 317.9 1199 0.01817 318.1 1199 0.01815 318.2 1199 0.01814 318.4 1199 0.01814 318.6 1199 0.01814 318.7 1199 0.01814 318.9 1199 0.01813 319 1199 0.01813 319.2 1199 0.01813 319.4 1199 0.01813 319.5 1199 0.01814 319.7 1199 0.01814 319.9 1199 0.01815 320 1199 0.01815 320.2 1199 0.01814 320.3 1199 0.01813 320.5 1199 0.01812 320.7 1199 0.01813 320.8 1199 0.01813 321 1199 0.01812 321.1 1199 0.01813 321.3 1199 0.01812 321.5 1199 0.01813 321.6 1199 0.01812 321.8 1199 0.01812 321.9 1199 0.01813 322.1 1199 0.01813 322.3 1199 0.01813 322.4 1200 0.01814 322.6 1199 0.01813 322.8 1199 0.01813 322.9 1199 0.01813 323.1 1200 0.01812 323.2 1199 0.01812 323.4 1199 0.01812 323.6 1199 0.01813 323.7 1199 0.01812 323.9 1199 0.01812 324 1199 0.01812 324.2 1199 0.01812 324.4 1199 0.01813 324.5 1199 0.01812 324.7 1199 0.01813 324.8 1199 0.01814 325 1199 0.01813 325.2 1199 0.01813 325.3 1199 0.01813 325.5 1199 0.01813 325.7 1199 0.01813 325.8 1199 0.01813 326 1199 0.01812 326.1 1199 0.01813 326.3 1199 0.01814 326.5 1199 0.01813 326.6 1199 0.01813 326.8 1199 0.01813 326.9 1199 0.01813 327.1 1199 0.01812 327.3 1199 0.01813 327.4 1199 0.01812 327.6 1199 0.01813 327.7 1199 0.01812 327.9 1199 0.01814 328.1 1199 0.01815 328.2 1199 0.01818 328.4 1199 0.01818 328.6 1199 0.01817 328.7 1199 0.01814 328.9 1199 0.01813 329 1199 0.01812 329.2 1199 0.0181 329.4 1199 0.01809 329.5 1199 0.01809 329.7 1199 0.0181 329.8 1199 0.0181 330 1199 0.01812 330.2 1199 0.01812 330.3 1199 0.01812 330.5 1199 0.01812 330.6 1199 0.01812 330.8 1199 0.0181 331 1199 0.01809 331.1 1199 0.0181 331.3 1199 0.01812 331.5 1199 0.0181 331.6 1199 0.01809 331.8 1199 0.01809 331.9 1199 0.01808 332.1 1199 0.01808 332.3 1199 0.01808 332.4 1199 0.01808 332.6 1199 0.01807 332.7 1199 0.01807 332.9 1199 0.01808 333.1 1199 0.01807 333.2 1199 0.01808 333.4 1199 0.01807 333.5 1199 0.01808 333.7 1199 0.01812 333.9 1199 0.01813 334 1199 0.01813 334.2 1199 0.01813 334.4 1199 0.01812 334.5 1200 0.01813 334.7 1199 0.01812 334.8 1199 0.01813 335 1199 0.01812 335.2 1199 0.01812 335.3 1199 0.01813 335.5 1199 0.01812 335.6 1199 0.01812 335.8 1199 0.01813 336 1199 0.01813 336.1 1199 0.01815 336.3 1199 0.01815 336.4 1199 0.01815 336.6 1199 0.01817 336.8 1199 0.01817 336.9 1199 0.01818 337.1 1199 0.01814 337.3 1199 0.01812 337.4 1199 0.01804 337.6 1199 0.01803 337.7 1199 0.01803 337.9 1199 0.01805 338.1 1199 0.01807 338.2 1199 0.01809 338.4 1199 0.01808 338.5 1199 0.01809 338.7 1199 0.01809 338.9 1199 0.01809 339 1199 0.01813 339.2 1199 0.01812 339.3 1199 0.01809 339.5 1199 0.01809 339.7 1199 0.01809 339.8 1199 0.01809 340 1199 0.01809 340.2 1199 0.01809 340.3 1199 0.01809 340.5 1199 0.01808 340.6 1199 0.01807 340.8 1199 0.01808 341 1199 0.01808 341.1 1199 0.01808 341.3 1199 0.01807 341.4 1199 0.01808 341.6 1199 0.01809 341.8 1199 0.01809 341.9 1199 0.01809 342.1 1199 0.01812 342.2 1199 0.0181 342.4 1199 0.01812 342.6 1199 0.01812 342.7 1199 0.01809 342.9 1199 0.01809 343.1 1199 0.0181 343.2 1199 0.0181 343.4 1199 0.01812 343.5 1199 0.01812 343.7 1199 0.01812 343.9 1200 0.01812 344 1199 0.01812 344.2 1199 0.01813 344.3 1199 0.0181 344.5 1199 0.01809 344.7 1199 0.0181 344.8 1199 0.01809 345 1199 0.01813 345.1 1199 0.01809 345.3 1200 0.01809 345.5 1199 0.01809 345.6 1199 0.01808 345.8 1199 0.01808 346 1199 0.01805 346.1 1199 0.01804 346.3 1199 0.01805 346.4 1199 0.01807 346.6 1199 0.01807 346.8 1199 0.01807 346.9 1199 0.01807 347.1 1199 0.01805 347.2 1199 0.01804 347.4 1199 0.01802 347.6 1199 0.01802 347.7 1199 0.01799 347.9 1199 0.01799 348 1199 0.01802 348.2 1199 0.01802 348.4 1199 0.01804 348.5 1199 0.01805 348.7 1199 0.01805 348.9 1199 0.01807 349 1199 0.01805 349.2 1199 0.01807 349.3 1199 0.01807 349.5 1199 0.01807 349.7 1199 0.01807 349.8 1199 0.01807 350 1199 0.01808 350.1 1199 0.01812 350.3 1199 0.01812 350.5 1199 0.0181 350.6 1199 0.0181 350.8 1199 0.01809 350.9 1199 0.01808 351.1 1199 0.01803 351.3 1199 0.01804 351.4 1199 0.01807 351.6 1199 0.01809 351.8 1199 0.01809 351.9 1199 0.01809 352.1 1199 0.01809 352.2 1199 0.0181 352.4 1199 0.0181 352.6 1199 0.01812 352.7 1199 0.01809 352.9 1199 0.01809 353 1199 0.01809 353.2 1199 0.01808 353.4 1199 0.01808 353.5 1199 0.01809 353.7 1199 0.01809 353.9 1199 0.01812 354 1199 0.0181 354.2 1199 0.01809 354.3 1199 0.01809 354.5 1199 0.0181 354.7 1199 0.01807 354.8 1199 0.01804 355 1199 0.01804 355.1 1199 0.01807 355.3 1199 0.01808 355.5 1199 0.01809 355.6 1199 0.0181 355.8 1199 0.01809 355.9 1199 0.01808 356.1 1199 0.01807 356.3 1199 0.01805 356.4 1199 0.01808 356.6 1199 0.01807 356.8 1200 0.01807 356.9 1199 0.01809 357.1 1199 0.01808 357.2 1199 0.01805 357.4 1199 0.01804 357.6 1199 0.01804 357.7 1199 0.01808 357.9 1199 0.01809 358 1199 0.01809 358.2 1199 0.01808 358.4 1199 0.01807 358.5 1199 0.01808 358.7 1199 0.01807 358.8 1199 0.01802 359 1199 0.01799 359.2 1199 0.01799 359.3 1199 0.01798 359.5 1199 0.01798 359.7 1199 0.01799 359.8 1200 0.01803 360 1199 0.01803 360.1 1199 0.01803 360.3 1199 0.01803 360.5 1199 0.01804 360.6 1199 0.01803 360.8 1199 0.01802 360.9 1199 0.01801 361.1 1199 0.01802 361.3 1199 0.01802 361.4 1199 0.01804 361.6 1199 0.01808 361.7 1199 0.0181 361.9 1199 0.01813 362.1 1199 0.01815 362.2 1199 0.01817 362.4 1199 0.01817 362.6 1199 0.01817 362.7 1199 0.01815 362.9 1199 0.01814 363 1199 0.01809 363.2 1199 0.01809 363.4 1199 0.01807 363.5 1199 0.01805 363.7 1199 0.01803 363.8 1199 0.01802 364 1199 0.01802 364.2 1199 0.01803 364.3 1199 0.01804 364.5 1199 0.01802 364.6 1199 0.01799 364.8 1199 0.01796 365 1199 0.01793 365.1 1199 0.01794 365.3 1199 0.01797 365.5 1199 0.01799 365.6 1199 0.01803 365.8 1199 0.01805 365.9 1199 0.01809 366.1 1199 0.01808 366.3 1199 0.01807 366.4 1199 0.01807 366.6 1199 0.01808 366.7 1199 0.01808 366.9 1199 0.01808 367.1 1199 0.01808 367.2 1199 0.01808 367.4 1199 0.01808 367.5 1199 0.01808 367.7 1199 0.01807 367.9 1199 0.01808 368 1199 0.01807 368.2 1200 0.01807 368.4 1199 0.01808 368.5 1199 0.01808 368.7 1199 0.01809 368.8 1200 0.01808 369 1199 0.01809 369.2 1199 0.01809 369.3 1199 0.01807 369.5 1199 0.01805 369.6 1199 0.01807 369.8 1199 0.01807 370 1199 0.01807 370.1 1199 0.01807 370.3 1199 0.01807 370.4 1199 0.01808 370.6 1199 0.01809 370.8 1199 0.0181 370.9 1199 0.01809 371.1 1199 0.01809 371.3 1199 0.01807 371.4 1199 0.01805 371.6 1199 0.01804 371.7 1199 0.01803 371.9 1199 0.01803 372.1 1199 0.01804 372.2 1199 0.01805 372.4 1199 0.01808 372.5 1199 0.01808 372.7 1199 0.01805 372.9 1199 0.01804 373 1199 0.01808 373.2 1199 0.01808 373.3 1199 0.01807 373.5 1199 0.01809 373.7 1199 0.01808 373.8 1199 0.01805 374 1199 0.01809 374.2 1199 0.01809 374.3 1199 0.01809 374.5 1199 0.01809 374.6 1199 0.01809 374.8 1199 0.01809 375 1199 0.01807 375.1 1199 0.01807 375.3 1199 0.01805 375.4 1199 0.01807 375.6 1199 0.01807 375.8 1199 0.01807 375.9 1199 0.01807 376.1 1199 0.01807 376.2 1199 0.01809 376.4 1199 0.01807 376.6 1199 0.01805 376.7 1199 0.01807 376.9 1199 0.01807 377.1 1199 0.01807 377.2 1199 0.01807 377.4 1199 0.01807 377.5 1199 0.01808 377.7 1199 0.01809 377.9 1199 0.01809 378 1199 0.01808 378.2 1199 0.01804 378.3 1199 0.01805 378.5 1199 0.01805 378.7 1199 0.01805 378.8 1199 0.01807 379 1199 0.01805 379.1 1199 0.01807 379.3 1199 0.01805 379.5 1199 0.01804 379.6 1200 0.01803 379.8 1199 0.01804 380 1199 0.01805 380.1 1199 0.01808 380.3 1199 0.01809 380.4 1199 0.01809 380.6 1199 0.01807 380.8 1199 0.01807 380.9 1199 0.01807 381.1 1199 0.01807 381.2 1199 0.01805 381.4 1199 0.01804 381.6 1199 0.01805 381.7 1199 0.01807 381.9 1199 0.01808 382 1199 0.01808 382.2 1199 0.01808 382.4 1199 0.01808 382.5 1199 0.01804 382.7 1199 0.01805 382.9 1199 0.01805 383 1199 0.01805 383.2 1199 0.01807 383.3 1199 0.01807 383.5 1199 0.01808 383.7 1199 0.01809 383.8 1199 0.01809 384 1199 0.01809 384.1 1199 0.01808 384.3 1199 0.01808 384.5 1199 0.01808 384.6 1199 0.01807 384.8 1199 0.01808 384.9 1199 0.01808 385.1 1199 0.01807 385.3 1199 0.01808 385.4 1199 0.01809 385.6 1199 0.0181 385.8 1199 0.01812 385.9 1199 0.01813 386.1 1199 0.01813 386.2 1199 0.01812 386.4 1199 0.01809 386.6 1199 0.01803 386.7 1200 0.01798 386.9 1199 0.01794 387 1199 0.01793 387.2 1199 0.01793 387.4 1199 0.01794 387.5 1199 0.01797 387.7 1199 0.01799 387.8 1199 0.01798 388 1199 0.01798 388.2 1199 0.01797 388.3 1199 0.01796 388.5 1199 0.01796 388.7 1199 0.01796 388.8 1199 0.01799 389 1199 0.01802 389.1 1199 0.01803 389.3 1199 0.01804 389.5 1199 0.01804 389.6 1199 0.01803 389.8 1199 0.01803 389.9 1199 0.01803 390.1 1199 0.01803 390.3 1199 0.01802 390.4 1199 0.01802 390.6 1199 0.01802 390.7 1199 0.01802 390.9 1199 0.01802 391.1 1200 0.01799 391.2 1199 0.01802 391.4 1199 0.01803 391.6 1199 0.01803 391.7 1199 0.01801 391.9 1199 0.01799 392 1199 0.01798 392.2 1199 0.01799 392.4 1199 0.01799 392.5 1199 0.01802 392.7 1199 0.01802 392.8 1199 0.01802 393 1199 0.01802 393.2 1199 0.01803 393.3 1199 0.01803 393.5 1199 0.01805 393.7 1199 0.01804 393.8 1199 0.01805 394 1199 0.01805 394.1 1199 0.01807 394.3 1199 0.01809 394.5 1199 0.01812 394.6 1199 0.01812 394.8 1199 0.01812 394.9 1199 0.0181 395.1 1199 0.01809 395.3 1199 0.01805 395.4 1199 0.01804 395.6 1199 0.01804 395.7 1199 0.01805 395.9 1199 0.01805 396.1 1199 0.01805 396.2 1199 0.01805 396.4 1199 0.01805 396.6 1199 0.01803 396.7 1199 0.01803 396.9 1199 0.01803 397 1199 0.01803 397.2 1199 0.01804 397.4 1199 0.01803 397.5 1199 0.01803 397.7 1199 0.01802 397.8 1199 0.01802 398 1199 0.01802 398.2 1200 0.01802 398.3 1199 0.01804 398.5 1199 0.01804 398.6 1199 0.01805 398.8 1199 0.01804 399 1199 0.01803 399.1 1199 0.01802 399.3 1199 0.01799 399.5 1200 0.01799 399.6 1199 0.01803 399.8 1199 0.01803 399.9 1199 0.01804 400.1 1199 0.01803 400.3 1199 0.01804 400.4 1199 0.01805 400.6 1199 0.01805 400.7 1199 0.01805 400.9 1199 0.01805 401.1 1199 0.01805 401.2 1199 0.01808 401.4 1199 0.01807 401.5 1199 0.01807 401.7 1199 0.01807 401.9 1199 0.01807 402 1199 0.01807 402.2 1199 0.01807 402.4 1199 0.01807 402.5 1200 0.01807 402.7 1199 0.01807 402.8 1199 0.01808 403 1199 0.0181 403.2 1199 0.0181 403.3 1199 0.01809 403.5 1199 0.01809 403.6 1199 0.01812 403.8 1199 0.0181 404 1199 0.01808 404.1 1199 0.01807 404.3 1199 0.01807 404.4 1199 0.01809 404.6 1199 0.01809 404.8 1199 0.01807 404.9 1199 0.01804 405.1 1199 0.01802 405.3 1199 0.01801 405.4 1199 0.01801 405.6 1199 0.01802 405.7 1199 0.01803 405.9 1199 0.01804 406.1 1199 0.01803 406.2 1199 0.01799 406.4 1199 0.01802 406.5 1199 0.01804 406.7 1199 0.01809 406.9 1199 0.01809 407 1199 0.01809 407.2 1199 0.01807 407.3 1199 0.01802 407.5 1199 0.01802 407.7 1199 0.01807 407.8 1199 0.01809 408 1199 0.01812 408.2 1199 0.01813 408.3 1199 0.01812 408.5 1199 0.01812 408.6 1199 0.01809 408.8 1199 0.01812 409 1199 0.01813 409.1 1199 0.01812 409.3 1199 0.01813 409.4 1199 0.01812 409.6 1199 0.01813 409.8 1199 0.01812 409.9 1199 0.01812 410.1 1199 0.01813 410.2 1199 0.01809 410.4 1199 0.01809 410.6 1199 0.01809 410.7 1199 0.01808 410.9 1199 0.01808 411.1 1199 0.01809 411.2 1199 0.01809 411.4 1199 0.01809 411.5 1199 0.01809 411.7 1199 0.01809 411.9 1199 0.01809 412 1199 0.01809 412.2 1199 0.01809 412.3 1199 0.01809 412.5 1199 0.0181 412.7 1199 0.01808 412.8 1199 0.01807 413 1199 0.01809 413.1 1199 0.01808 413.3 1199 0.01809 413.5 1199 0.0181 413.6 1199 0.01812 413.8 1199 0.01809 414 1199 0.01809 414.1 1199 0.0181 414.3 1199 0.01812 414.4 1199 0.01812 414.6 1199 0.01812 414.8 1199 0.01812 414.9 1199 0.0181 415.1 1199 0.01809 415.2 1199 0.01809 415.4 1199 0.01809 415.6 1199 0.0181 415.7 1199 0.0181 415.9 1199 0.0181 416 1199 0.01812 416.2 1199 0.01809 416.4 1199 0.01812 416.5 1199 0.01813 416.7 1199 0.01813 416.9 1199 0.01813 417 1199 0.01812 417.2 1199 0.01812 417.3 1199 0.01813 417.5 1199 0.01812 417.7 1199 0.01814 417.8 1199 0.01813 418 1199 0.01813 418.1 1199 0.01813 418.3 1199 0.01813 418.5 1199 0.01813 418.6 1199 0.01812 418.8 1199 0.01813 418.9 1199 0.01812 419.1 1199 0.01812 419.3 1199 0.0181 419.4 1199 0.01809 419.6 1199 0.0181 419.8 1199 0.0181 419.9 1199 0.0181 420.1 1199 0.01809 420.2 1199 0.01809 420.4 1199 0.01809 420.6 1199 0.01809 420.7 1199 0.01805 420.9 1199 0.01804 421 1199 0.01805 421.2 1199 0.01807 421.4 1199 0.01809 421.5 1199 0.01813 421.7 1199 0.01817 421.8 1199 0.01818 422 1199 0.01815 422.2 1199 0.01814 422.3 1199 0.01814 422.5 1199 0.01813 422.7 1199 0.01813 422.8 1199 0.01813 423 1199 0.01813 423.1 1199 0.01812 423.3 1199 0.01808 423.5 1199 0.01805 423.6 1199 0.01805 423.8 1199 0.01808 423.9 1199 0.01812 424.1 1199 0.01813 424.3 1199 0.01813 424.4 1199 0.01812 424.6 1199 0.01812 424.7 1199 0.01813 424.9 1199 0.01812 425.1 1199 0.01813 425.2 1199 0.01812 425.4 1199 0.01814 425.6 1199 0.01814 425.7 1199 0.01815 425.9 1199 0.01815 426 1199 0.01814 426.2 1199 0.01815 426.4 1199 0.01814 426.5 1199 0.01814 426.7 1199 0.01815 426.8 1199 0.01814 427 1199 0.01814 427.2 1199 0.01813 427.3 1199 0.01814 427.5 1199 0.01814 427.6 1199 0.01815 427.8 1199 0.01815 428 1199 0.01814 428.1 1199 0.01815 428.3 1199 0.01814 428.5 1199 0.01813 428.6 1199 0.01813 428.8 1199 0.01812 428.9 1199 0.01814 429.1 1199 0.01814 429.3 1199 0.01813 429.4 1199 0.01813 429.6 1199 0.01814 429.7 1199 0.01813 429.9 1199 0.0181 430.1 1199 0.01809 430.2 1199 0.01812 430.4 1199 0.01813 430.6 1199 0.01814 430.7 1199 0.01815 430.9 1199 0.01817 431 1199 0.01815 431.2 1199 0.01818 431.4 1199 0.01819 431.5 1199 0.01819 431.7 1199 0.01823 431.8 1199 0.01824 432 1199 0.01824 432.2 1199 0.01825 432.3 1199 0.01825 432.5 1199 0.01825 432.6 1199 0.01821 432.8 1199 0.01819 433 1199 0.01815 433.1 1199 0.01814 433.3 1199 0.01815 433.5 1199 0.01819 433.6 1199 0.0182 433.8 1199 0.01819 433.9 1199 0.01817 434.1 1199 0.01817 434.3 1199 0.01817 434.4 1199 0.01818 434.6 1199 0.01817 434.7 1199 0.01817 434.9 1199 0.01817 435.1 1199 0.01817 435.2 1199 0.01818 435.4 1199 0.01817 435.5 1199 0.01817 435.7 1199 0.01818 435.9 1199 0.01817 436 1199 0.01818 436.2 1199 0.01818 436.4 1199 0.01818 436.5 1199 0.01817 436.7 1199 0.01814 436.8 1199 0.01815 437 1199 0.01815 437.2 1199 0.01817 437.3 1199 0.01818 437.5 1199 0.01819 437.6 1199 0.0182 437.8 1199 0.01818 438 1199 0.01817 438.1 1199 0.01817 438.3 1199 0.01817 438.4 1199 0.01815 438.6 1199 0.01814 438.8 1199 0.01813 438.9 1199 0.01812 439.1 1199 0.01813 439.3 1199 0.01814 439.4 1199 0.01815 439.6 1199 0.01817 439.7 1199 0.01815 439.9 1199 0.01817 440.1 1199 0.01819 440.2 1199 0.01819 440.4 1199 0.0182 440.5 1199 0.01821 440.7 1199 0.01821 440.9 1199 0.01821 441 1199 0.01819 441.2 1199 0.01819 441.3 1199 0.01818 441.5 1199 0.01818 441.7 1199 0.01819 441.8 1199 0.01819 442 1199 0.0182 442.2 1199 0.0182 442.3 1199 0.01819 442.5 1199 0.0182 442.6 1199 0.0182 442.8 1199 0.01819 443 1199 0.01819 443.1 1199 0.01821 443.3 1199 0.01821 443.4 1199 0.0182 443.6 1199 0.01823 443.8 1199 0.01821 443.9 1199 0.0182 444.1 1199 0.01819 444.2 1199 0.0182 444.4 1199 0.01821 444.6 1199 0.01821 444.7 1199 0.01821 444.9 1199 0.01821 445.1 1199 0.01821 445.2 1199 0.01823 445.4 1199 0.01823 445.5 1199 0.01823 445.7 1199 0.01821 445.9 1199 0.01821 446 1199 0.0182 446.2 1199 0.0182 446.3 1199 0.0182 446.5 1199 0.01819 446.7 1199 0.01819 446.8 1199 0.0182 447 1199 0.01823 447.1 1199 0.01823 447.3 1199 0.01821 447.5 1199 0.01823 447.6 1199 0.01824 447.8 1199 0.01824 448 1199 0.01824 448.1 1199 0.01823 448.3 1199 0.01824 448.4 1199 0.01825 448.6 1199 0.01825 448.8 1199 0.01826 448.9 1199 0.01826 449.1 1199 0.01829 449.2 1199 0.01828 449.4 1199 0.01825 449.6 1199 0.01823 449.7 1199 0.01823 449.9 1198 0.01823 450 1198 0.01821 450.2 1197 0.01818 450.4 1197 0.01817 450.5 1151 0.01817 450.7 1160 0.01834 450.9 1172 0.01852 451 1176 0.0187 451.2 1179 0.01876 451.3 1180 0.01875 451.5 1181 0.01873 451.7 1182 0.01873 451.8 1182 0.01873 452 1182 0.01873 452.1 1181 0.01871 452.3 1181 0.01871 452.5 1180 0.01868 452.6 1179 0.01866 452.8 1179 0.01865 452.9 1178 0.01861 453.1 1176 0.01857 453.3 1175 0.01854 453.4 1173 0.01852 453.6 1172 0.01847 453.8 1169 0.01841 453.9 1169 0.01838 454.1 1167 0.01831 454.2 1165 0.01825 454.4 1164 0.01821 454.6 1162 0.01818 454.7 1161 0.01813 454.9 1159 0.01808 455 1158 0.01803 455.2 1156 0.01798 455.4 1154 0.01793 455.5 1153 0.01788 455.7 1151 0.01783 455.8 1149 0.0178 456 1148 0.01777 456.2 1147 0.01775 456.3 1144 0.01772 456.5 1144 0.01766 456.7 1142 0.01762 456.8 1140 0.01759 457 1139 0.01756 457.1 1137 0.01755 457.3 1136 0.0175 457.5 1135 0.01747 457.6 1134 0.01745 457.8 1133 0.0174 457.9 1131 0.01736 458.1 1129 0.01733 458.3 1129 0.01729 458.4 1128 0.01724 458.6 1126 0.0172 458.7 1125 0.01717 458.9 1124 0.01714 459.1 1122 0.01714 459.2 1122 0.01709 459.4 1119 0.01703 459.6 1119 0.01696 459.7 1117 0.01687 459.9 1115 0.01685 460 1115 0.01683 460.2 1114 0.01686 460.4 1112 0.01685 460.5 1111 0.0168 460.7 1109 0.01676 460.8 1108 0.01672 461 1107 0.0167 461.2 1106 0.01664 461.3 1104 0.01661 461.5 1103 0.0166 461.6 1102 0.01654 461.8 1101 0.01649 462 1100 0.01644 462.1 1099 0.01641 462.3 1097 0.01638 462.5 1096 0.01635 462.6 1094 0.01634 462.8 1093 0.0163 462.9 1092 0.01625 463.1 1090 0.0162 463.3 1090 0.01617 463.4 1088 0.01613 463.6 1086 0.01607 463.7 1086 0.01603 463.9 1084 0.01601 464.1 1083 0.01597 464.2 1082 0.01594 464.4 1080 0.01591 464.5 1079 0.01586 464.7 1078 0.01582 464.9 1076 0.01578 465 1075 0.01575 465.2 1074 0.0157 465.4 1072 0.01567 465.5 1072 0.01562 465.7 1069 0.01559 465.8 1068 0.01555 466 1068 0.0155 466.2 1065 0.01549 466.3 1065 0.01546 466.5 1063 0.01546 466.6 1062 0.01546 466.8 1061 0.01541 467 1059 0.01538 467.1 1058 0.01534 467.3 1057 0.01528 467.4 1056 0.01522 467.6 1054 0.01516 467.8 1054 0.01514 467.9 1052 0.01512 468.1 1051 0.01508 468.3 1051 0.01506 468.4 1050 0.01501 468.6 1048 0.01497 468.7 1047 0.01496 468.9 1047 0.01497 469.1 1046 0.01498 469.2 1044 0.01492 469.4 1044 0.01486 469.5 1043 0.01481 469.7 1043 0.01482 469.9 1042 0.01479 470 1041 0.01475 470.2 1040 0.01471 470.4 1039 0.01467 470.5 1037 0.01464 470.7 1036 0.0146 470.8 1035 0.01456 471 1033 0.01451 471.2 1031 0.01449 471.3 1030 0.01446 471.5 1028 0.01439 471.6 1027 0.01434 471.8 1025 0.01429 472 1024 0.01424 472.1 1021 0.01418 472.3 1018 0.01414 472.4 1017 0.01412 472.6 1011 0.01411 472.8 1013 0.01408 472.9 1009 0.01407 473.1 1009 0.01401 473.3 1008 0.01395 473.4 1006 0.01388 473.6 1007 0.01387 473.7 1003 0.01386 473.9 1004 0.01381 474.1 1000 0.01376 474.2 1001 0.01372 474.4 998 0.01371 474.5 998 0.01365 474.7 997 0.0136 474.9 994 0.01361 475 997 0.01361 475.2 990 0.0136 475.3 993 0.0136 475.5 988 0.01359 475.7 990 0.01354 475.8 988 0.01348 476 986 0.01342 476.2 987 0.01338 476.3 981 0.01333 476.5 984 0.0133 476.6 979 0.01329 476.8 981 0.01323 477 978 0.01318 477.1 976 0.01316 477.3 978 0.01313 477.4 972 0.0131 477.6 976 0.01305 477.8 968 0.01301 477.9 973 0.01298 478.1 965 0.01295 478.2 968 0.0129 478.4 967 0.01285 478.6 965 0.01281 478.7 967 0.0128 478.9 960 0.0128 479.1 965 0.0128 479.2 956 0.01277 479.4 961 0.01273 479.5 954 0.01269 479.7 957 0.01264 479.9 953 0.01264 480 953 0.01264 480.2 956 0.01264 480.3 948 0.01264 480.5 955 0.01259 480.7 943 0.01254 480.8 950 0.0125 481 941 0.01245 481.1 947 0.0124 481.3 942 0.01237 481.5 940 0.01233 481.6 945 0.01229 481.8 936 0.01226 482 943 0.01222 482.1 931 0.01217 482.3 940 0.01213 482.4 929 0.01211 482.6 934 0.01206 482.8 931 0.01203 482.9 929 0.01198 483.1 933 0.012 483.2 924 0.01201 483.4 932 0.01196 483.6 919 0.0119 483.7 929 0.01185 483.9 916 0.01185 484 924 0.01184 484.2 915 0.0118 484.4 918 0.0117 484.5 918 0.01164 484.7 914 0.01163 484.9 921 0.01159 485 909 0.01158 485.2 918 0.01155 485.3 904 0.01153 485.5 915 0.0115 485.7 900 0.01148 485.8 911 0.01144 486 901 0.01142 486.1 906 0.01138 486.3 903 0.01134 486.5 900 0.01132 486.6 906 0.01128 486.8 896 0.01123 486.9 905 0.01122 487.1 889 0.01122 487.3 902 0.0112 487.4 886 0.01113 487.6 899 0.01107 487.8 883 0.01103 487.9 894 0.011 488.1 882 0.01096 488.2 889 0.0109 488.4 886 0.01087 488.6 884 0.01085 488.7 888 0.01084 488.9 879 0.01084 489 889 0.01081 489.2 874 0.01074 489.4 887 0.01071 489.5 868 0.0107 489.7 884 0.01068 489.8 865 0.01063 490 880 0.01055 490.2 861 0.01054 490.3 876 0.01053 490.5 860 0.01053 490.7 872 0.01047 490.8 861 0.01041 491 868 0.01034 491.1 861 0.01034 491.3 863 0.01034 491.5 862 0.01033 491.6 858 0.01028 491.8 864 0.01025 491.9 854 0.0102 492.1 865 0.01018 492.3 849 0.01017 492.4 864 0.01017 492.6 844 0.01009 492.7 862 0.01002 492.9 840 0.01004 493.1 860 0.01002 493.2 837 0.009999 493.4 857 0.009962 493.6 833 0.009912 493.7 854 0.009863 493.9 830 0.009888 494 851 0.009863 494.2 827 0.009838 494.4 849 0.009777 494.5 824 0.009715 494.7 846 0.009666 494.8 821 0.009666 495 843 0.009641 495.2 818 0.009629 495.3 841 0.009567 495.5 816 0.00953 495.6 839 0.009481 495.8 814 0.009493 496 836 0.009493 496.1 811 0.009493 496.3 834 0.009456 496.5 807 0.00937 496.6 832 0.009296 496.8 805 0.009296 496.9 830 0.009283 497.1 802 0.009271 497.3 828 0.009246 497.4 801 0.009209 497.6 826 0.00916 497.7 801 0.009147 497.9 824 0.00916 498.1 801 0.00916 498.2 820 0.009135 498.4 800 0.009086 498.5 817 0.008999 498.7 800 0.00895 498.9 811 0.008913 499 799 0.008913 499.2 806 0.008913 499.4 799 0.008888 499.5 801 0.008839 499.7 799 0.008777 499.8 796 0.00874 500 800 0.008703 500.2 790 0.008716 500.3 800 0.008716 500.5 784 0.008716 500.6 800 0.008654 500.8 777 0.008617 501 800 0.008568 501.1 774 0.008531 501.3 800 0.008494 501.4 773 0.008481 501.6 797 0.008457 501.8 773 0.00842 501.9 790 0.008358 502.1 775 0.008284 502.3 782 0.008259 502.4 777 0.008259 502.6 774 0.008247 502.7 780 0.008247 502.9 765 0.008222 503.1 782 0.008185 503.2 758 0.008124 503.4 782 0.008037 503.5 756 0.008013 503.7 780 0.008013 503.9 756 0.008 504 773 0.007963 504.2 759 0.007914 504.3 763 0.007852 504.5 762 0.007815 504.7 753 0.00779 504.8 765 0.007729 505 745 0.007716 505.2 768 0.007692 505.3 741 0.007642 505.5 765 0.00763 505.6 742 0.007618 505.8 757 0.007581 506 746 0.007519 506.1 746 0.007445 506.3 750 0.007371 506.4 735 0.007334 506.6 754 0.007322 506.8 728 0.007297 506.9 754 0.007272 507.1 730 0.00726 507.2 746 0.007235 507.4 734 0.007186 507.6 733 0.007137 507.7 740 0.007063 507.9 722 0.007038 508.1 744 0.007001 508.2 718 0.006989 508.4 742 0.006976 508.5 721 0.006952 508.7 729 0.006927 508.9 727 0.006902 509 716 0.00689 509.2 732 0.006828 509.3 708 0.006767 509.5 734 0.00673 509.7 709 0.006693 509.8 723 0.006668 510 716 0.006643 510.2 709 0.006619 510.3 722 0.006594 510.5 699 0.006594 510.6 725 0.006544 510.8 700 0.006507 511 714 0.006446 511.1 706 0.006384 511.3 700 0.006347 511.4 714 0.00631 511.6 689 0.006273 511.8 715 0.006236 511.9 693 0.006211 512.1 703 0.006211 512.2 700 0.006199 512.4 687 0.006199 512.6 707 0.006174 512.7 681 0.006137 512.9 704 0.006063 513.1 686 0.006014 513.2 689 0.005952 513.4 694 0.005903 513.5 675 0.005891 513.7 700 0.005866 513.9 675 0.005854 514 690 0.005817 514.2 682 0.005792 514.3 674 0.005767 514.5 691 0.005743 514.7 666 0.005706 514.8 688 0.005669 515 672 0.005607 515.1 671 0.005545 515.3 681 0.005496 515.5 659 0.005459 515.6 683 0.005447 515.8 663 0.005422 516 668 0.00541 516.1 671 0.005385 516.3 655 0.005348 516.4 677 0.005286 516.6 655 0.005224 516.8 664 0.0052 516.9 664 0.0052 517.1 649 0.005187 517.2 671 0.005163 517.4 649 0.005163 517.6 659 0.005138 517.7 657 0.005076 517.9 642 0.005039 518 664 0.005015 518.2 643 0.004978 518.4 651 0.004941 518.5 651 0.004867 518.7 635 0.004805 518.9 657 0.004743 519 636 0.004719 519.2 643 0.004694 519.3 646 0.004669 519.5 628 0.004669 519.7 650 0.00462 519.8 632 0.004595 520 633 0.004558 520.1 642 0.004509 520.3 622 0.004472 520.5 640 0.004423 520.6 630 0.004398 520.8 623 0.004373 520.9 639 0.004361 521.1 617 0.004336 521.3 629 0.004312 521.4 627 0.004238 521.6 614 0.004188 521.8 632 0.004127 521.9 615 0.004065 522.1 615 0.004016 522.2 626 0.003991 522.4 606 0.003991 522.6 621 0.003966 522.7 614 0.003954 522.9 604 0.003929 523 621 0.003904 523.2 604 0.003892 523.4 607 0.003855 523.5 614 0.003806 523.7 596 0.003744 523.8 610 0.003719 524 604 0.003682 524.2 593 0.003645 524.3 611 0.003621 524.5 595 0.003596 524.7 596 0.003571 524.8 605 0.003497 525 588 0.00346 525.1 599 0.003436 525.3 596 0.003411 525.5 582 0.003386 525.6 600 0.003362 525.8 588 0.003325 525.9 582 0.0033 526.1 596 0.003251 526.3 580 0.003226 526.4 583 0.003189 526.6 591 0.003164 526.7 573 0.00314 526.9 584 0.003115 527.1 582 0.003078 527.2 568 0.003016 527.4 584 0.002955 527.6 575 0.002918 527.7 566 0.002893 527.9 582 0.002881 528 567 0.002844 528.2 565 0.002807 528.4 578 0.00277 528.5 560 0.002733 528.7 565 0.002696 528.8 571 0.002671 529 555 0.002646 529.2 564 0.002634 529.3 566 0.002609 529.5 550 0.00256 529.6 564 0.00251 529.8 560 0.002473 530 548 0.002436 530.1 562 0.002424 530.3 553 0.002399 530.5 543 0.00235 530.6 559 0.002301 530.8 548 0.002276 530.9 540 0.002239 531.1 556 0.002227 531.3 542 0.002202 531.4 538 0.002153 531.6 552 0.002128 531.7 536 0.002116 531.9 535 0.002079 532.1 547 0.002054 532.2 532 0.002029 532.4 534 0.002029 532.5 542 0.001992 532.7 528 0.001955 532.9 531 0.001894 533 539 0.001844 533.2 523 0.001832 533.4 528 0.001783 533.5 535 0.001758 533.7 518 0.001733 533.8 524 0.001709 534 531 0.001684 534.2 514 0.001635 534.3 521 0.001598 534.5 527 0.001548 534.6 510 0.001511 534.8 517 0.001462 535 522 0.001413 535.1 507 0.001376 535.3 512 0.001326 535.4 518 0.001301 535.6 504 0.001289 535.8 506 0.001264 535.9 515 0.001227 536.1 501 0.001178 536.3 502 0.001178 536.4 512 0.001153 536.6 498 0.001153 536.7 497 0.001129 536.9 508 0.001116 537.1 496 0.001067 537.2 492 0.001042 537.4 504 0.001005 537.5 493 0.0009561 537.7 487 0.0009191 537.9 499 0.0008944 538 492 0.0008821 538.2 481 0.000845 538.3 494 0.000808 538.5 489 0.0007464 538.7 478 0.000734 538.8 488 0.0007217 539 489 0.00066 539.2 475 0.0005983 539.3 480 0.0005736 539.5 486 0.0005736 539.6 472 0.0005366 539.8 473 0.0004996 540 484 0.0004379 540.1 471 0.0004009 540.3 466 0.0003516 540.4 478 0.0003146 540.6 472 0.0003146 540.8 461 0.0003269 540.9 471 0.0003269 541.1 471 0.0002776 541.2 459 0.0002529 541.4 461 0.0002282 541.6 470 0.0002036 541.7 458 0.0001912 541.9 454 0.0002036 542.1 465 0.0001665 542.2 459 0.0001049 542.4 449 6.168e-06 542.5 457 6.168e-06 542.7 460 6.168e-06 542.9 446 -1.85e-05 543 446 -5.551e-05 543.2 457 -8.019e-05 543.3 446 -0.0001049 543.5 439 -0.0001419 543.7 450 -0.0001912 543.8 449 -0.0002159 544 436 -0.0002282 544.1 441 -0.0002652 544.3 448 -0.0003146 544.5 435 -0.0003516 544.6 431 -0.0003763 544.8 442 -0.0004133 545 438 -0.0004379 545.1 427 -0.000475 545.3 431 -0.000512 545.4 438 -0.0005366 545.6 427 -0.0005736 545.8 422 -0.000586 545.9 433 -0.0006107 546.1 431 -0.0006107 546.2 418 -0.0006353 546.4 421 -0.0006847 546.6 430 -0.0007217 546.7 419 -0.0007587 546.9 412 -0.0007834 547 421 -0.0007957 547.2 424 -0.000845 547.4 411 -0.0008821 547.5 409 -0.0009067 547.7 419 -0.0009191 547.9 414 -0.0009191 548 404 -0.0009561 548.2 408 -0.0009684 548.3 415 -0.001005 548.5 406 -0.001042 548.7 399 -0.001141 548.8 406 -0.001215 549 409 -0.00124 549.1 399 -0.001227 549.3 394 -0.001215 549.5 403 -0.00124 549.6 403 -0.001277 549.8 392 -0.001314 550 391 -0.001351 550.1 401 -0.001413 550.3 396 -0.00145 550.4 385 -0.001499 550.6 388 -0.001474 550.8 396 -0.00145 550.9 388 -0.00145 551.1 380 -0.001487 551.2 385 -0.001548 551.4 392 -0.001573 551.6 381 -0.001585 551.7 374 -0.001598 551.9 381 -0.00161 552 386 -0.001647 552.2 374 -0.001672 552.4 370 -0.001721 552.5 378 -0.001746 552.7 381 -0.001758 552.9 369 -0.001807 553 364 -0.001844 553.2 373 -0.001881 553.3 375 -0.001906 553.5 364 -0.001931 553.7 359 -0.001943 553.8 367 -0.001955 554 370 -0.00198 554.1 359 -0.002005 554.3 354 -0.002066 554.5 362 -0.002091 554.6 365 -0.002091 554.8 353 -0.002116 554.9 349 -0.002153 555.1 356 -0.002202 555.3 360 -0.002214 555.4 349 -0.002227 555.6 344 -0.002227 555.8 349 -0.002239 555.9 355 -0.002239 556.1 346 -0.002276 556.2 338 -0.002325 556.4 342 -0.002362 556.6 349 -0.002387 556.7 344 -0.002387 556.9 334 -0.002399 557 336 -0.002387 557.2 343 -0.002449 557.4 342 -0.002486 557.5 330 -0.002486 557.7 329 -0.002523 557.8 336 -0.002572 558 337 -0.002621 558.2 328 -0.002634 558.3 322 -0.002646 558.5 328 -0.002646 558.7 332 -0.002646 558.8 326 -0.002659 559 317 -0.002671 559.1 320 -0.002671 559.3 326 -0.002696 559.5 324 -0.002708 559.6 313 -0.00272 559.8 313 -0.002733 559.9 317 -0.002745 560.1 318 -0.002745 560.3 311 -0.002745 560.4 307 -0.002733 560.6 310 -0.002733 560.7 311 -0.002757 560.9 306 -0.002794 561.1 304 -0.002794 561.2 306 -0.002794 561.4 304 -0.002794 561.6 302 -0.00277 561.7 301 -0.002733 561.9 300 -0.002696 562 300 -0.002683 562.2 298 -0.002696 562.4 297 -0.002696 562.5 295 -0.002696 562.7 294 -0.002683 562.8 293 -0.002671 563 292 -0.002659 563.2 292 -0.002634 563.3 290 -0.002621 563.5 289 -0.002609 563.6 288 -0.002584 563.8 288 -0.00256 564 286 -0.002535 564.1 285 -0.002535 564.3 283 -0.00251 564.5 281 -0.002473 564.6 280 -0.002449 564.8 279 -0.002412 564.9 277 -0.00235 565.1 276 -0.002288 565.3 274 -0.002227 565.4 274 -0.002177 565.6 272 -0.002153 565.7 271 -0.002091 565.9 269 -0.002029 566.1 268 -0.001992 566.2 267 -0.001906 566.4 267 -0.001832 566.5 266 -0.001795 566.7 264 -0.001733 566.9 263 -0.001672 567 262 -0.00161 567.2 261 -0.001536 567.4 259 -0.001462 567.5 258 -0.001363 567.7 256 -0.001289 567.8 256 -0.001203 568 254 -0.001116 568.2 252 -0.001055 568.3 251 -0.0009807 568.5 249 -0.0008944 568.6 249 -0.0008204 568.8 246 -0.0007587 569 245 -0.0006723 569.1 243 -0.0005983 569.3 242 -0.0005366 569.4 241 -0.0004503 569.6 239 -0.0003639 569.8 238 -0.0003022 569.9 236 -0.0002282 570.1 234 -0.0001665 570.3 233 -0.0001172 570.4 231 -9.252e-05 570.6 230 -5.551e-05 570.7 227 -1.85e-05 570.9 226 6.168e-06 571.1 224 6.168e-06 571.2 223 6.168e-06 571.4 221 5.551e-05 571.5 220 0.0001172 571.7 219 0.0001665 571.9 217 0.0001789 572 216 0.0001789 572.2 214 0.0001542 572.3 213 0.0001172 572.5 211 0.0001049 572.7 210 0.0001295 572.8 209 0.0001665 573 208 0.0001912 573.2 206 0.0001912 573.3 205 0.0002159 573.5 204 0.0002282 573.6 202 0.0002159 573.8 202 0.0001912 574 200 0.0001789 574.1 199 0.0001789 574.3 199 0.0001542 574.4 197 0.0001542 574.6 195 0.0001542 574.8 194 0.0001789 574.9 194 0.0001789 575.1 192 0.0001789 575.2 191 0.0001542 575.4 189 0.0001172 575.6 188 0.0001295 575.7 188 0.0001419 575.9 186 0.0001665 576.1 184 0.0001912 576.2 184 0.0001542 576.4 181 0.0001295 576.5 181 6.785e-05 576.7 180 6.785e-05 576.9 179 6.785e-05 577 177 8.019e-05 577.2 176 8.019e-05 577.3 174 6.785e-05 577.5 174 5.551e-05 577.7 172 3.084e-05 577.8 171 6.168e-06 578 169 6.168e-06 578.1 168 6.168e-06 578.3 167 6.168e-06 578.5 166 6.168e-06 578.6 165 6.168e-06 578.8 163 6.168e-06 579 162 6.168e-06 579.1 161 -1.85e-05 579.3 159 -1.85e-05 579.4 159 -3.084e-05 579.6 156 -1.85e-05 579.8 156 -3.084e-05 579.9 155 -5.551e-05 580.1 154 -8.019e-05 580.2 152 -0.0001049 580.4 151 -0.0001049 580.6 149 -0.0001172 580.7 149 -0.0001419 580.9 147 -0.0001542 581 146 -0.0001665 581.2 144 -0.0001789 581.4 143 -0.0002036 581.5 141 -0.0002159 581.7 141 -0.0002282 581.9 139 -0.0002282 582 138 -0.0002406 582.2 137 -0.0002406 582.3 135 -0.0002529 582.5 134 -0.0002652 582.7 133 -0.0002652 582.8 131 -0.0003146 583 131 -0.0003393 583.1 129 -0.0003639 583.3 127 -0.0003763 583.5 127 -0.0003763 583.6 125 -0.0003516 583.8 123 -0.0003269 583.9 123 -0.0003393 584.1 121 -0.0003639 584.3 119 -0.0004133 584.4 119 -0.0004379 584.6 117 -0.0004626 584.8 115 -0.000475 584.9 114 -0.0004996 585.1 113 -0.000512 585.2 113 -0.000512 585.4 111 -0.000512 585.6 109 -0.000512 585.7 109 -0.0005366 585.9 106 -0.0005613 586 106 -0.0005983 586.2 104 -0.000623 586.4 103 -0.0006477 586.5 102 -0.00066 586.7 101 -0.000697 586.9 99 -0.0007093 587 98 -0.0007217 587.2 98 -0.0007217 587.3 96 -0.0007217 587.5 95 -0.0007217 587.7 94 -0.0007217 587.8 94 -0.0007217 588 92 -0.000734 588.1 91 -0.0007464 588.3 90 -0.0007587 588.5 89 -0.0007587 588.6 88 -0.000771 588.8 87 -0.0007834 588.9 86 -0.0007957 589.1 84 -0.000808 589.3 84 -0.000808 589.4 82 -0.0008327 589.6 81 -0.0008574 589.8 80 -0.0008697 589.9 79 -0.0008944 590.1 77 -0.0008944 590.2 77 -0.0008821 590.4 76 -0.0008944 590.6 75 -0.0009067 590.7 74 -0.0009191 590.9 73 -0.0009067 591 72 -0.0009437 591.2 71 -0.0009684 591.4 70 -0.0009807 591.5 69 -0.001005 591.7 69 -0.00103 591.8 67 -0.001042 592 67 -0.001055 592.2 66 -0.001055 592.3 65 -0.001055 592.5 64 -0.001055 592.7 63 -0.001055 592.8 63 -0.001067 593 62 -0.001092 593.1 61 -0.001104 593.3 60 -0.001116 593.5 59 -0.001116 593.6 59 -0.001141 593.8 58 -0.001141 593.9 57 -0.001141 594.1 56 -0.001153 594.3 55 -0.001178 594.4 55 -0.001203 594.6 55 -0.001215 594.7 54 -0.001264 594.9 53 -0.001301 595.1 52 -0.001314 595.2 52 -0.001289 595.4 52 -0.001277 595.6 51 -0.001289 595.7 50 -0.001277 595.9 50 -0.001252 596 49 -0.001264 596.2 48 -0.001289 596.4 48 -0.001301 596.5 48 -0.001314 596.7 47 -0.001326 596.8 47 -0.001351 597 46 -0.001351 597.2 46 -0.001363 597.3 45 -0.001376 597.5 45 -0.001388 597.6 44 -0.001376 597.8 44 -0.001388 598 43 -0.001388 598.1 44 -0.001388 598.3 42 -0.001413 598.5 42 -0.0014 598.6 42 -0.0014 598.8 41 -0.0014 598.9 41 -0.001388 599.1 41 -0.0014 599.3 41 -0.001413 599.4 40 -0.001437 599.6 39 -0.001437 599.7 39 -0.00145 599.9 38 -0.00145 600.1 38 -0.001462 600.2 38 -0.001474 600.4 38 -0.001487 600.5 38 -0.001487 600.7 37 -0.001487 600.9 37 -0.001487 601 37 -0.001487 601.2 36 -0.001499 601.4 36 -0.001511 601.5 36 -0.001536 601.7 36 -0.001573 601.8 35 -0.00161 602 35 -0.001635 602.2 34 -0.00161 602.3 34 -0.001598 602.5 34 -0.001561 602.6 34 -0.001548 602.8 34 -0.001548 603 34 -0.001561 603.1 34 -0.001561 603.3 33 -0.001548 603.4 33 -0.001548 603.6 33 -0.001548 603.8 33 -0.001561 603.9 32 -0.001561 604.1 32 -0.001548 604.3 31 -0.001561 604.4 31 -0.001548 604.6 31 -0.001548 604.7 31 -0.001548 604.9 30 -0.001561 605.1 30 -0.001573 605.2 30 -0.001573 605.4 30 -0.001598 605.5 30 -0.001598 605.7 30 -0.001598 605.9 30 -0.00161 606 30 -0.00161 606.2 30 -0.001622 606.3 30 -0.001635 606.5 30 -0.001635 606.7 30 -0.001635 606.8 29 -0.00161 607 29 -0.00161 607.2 29 -0.00161 607.3 29 -0.00161 607.5 28 -0.001622 607.6 28 -0.001635 607.8 28 -0.001635 608 28 -0.001622 608.1 27 -0.00161 608.3 27 -0.001622 608.4 27 -0.001622 608.6 27 -0.001622 608.8 27 -0.001635 608.9 27 -0.001635 609.1 27 -0.001635 609.2 27 -0.001647 609.4 27 -0.001659 609.6 27 -0.001647 609.7 27 -0.001647 609.9 27 -0.001647 610.1 26 -0.001647 610.2 27 -0.001647 610.4 26 -0.001647 610.5 26 -0.001659 610.7 26 -0.001659 610.9 26 -0.001647 611 26 -0.001635 611.2 25 -0.001647 611.3 25 -0.001647 611.5 25 -0.001647 611.7 26 -0.001647 611.8 25 -0.001647 612 24 -0.001659 612.1 24 -0.001672 612.3 24 -0.001696 612.5 24 -0.001696 612.6 24 -0.001696 612.8 24 -0.001696 613 24 -0.001696 613.1 23 -0.001684 613.3 23 -0.001696 613.4 23 -0.001696 613.6 23 -0.001684 613.8 23 -0.001672 613.9 23 -0.001672 614.1 23 -0.001684 614.2 23 -0.001684 614.4 23 -0.001696 614.6 23 -0.001709 614.7 23 -0.001696 614.9 23 -0.001696 615 23 -0.001696 615.2 23 -0.001696 615.4 23 -0.001709 615.5 23 -0.001721 615.7 23 -0.001709 615.9 23 -0.001709 616 22 -0.001696 616.2 23 -0.001684 616.3 23 -0.001696 616.5 23 -0.001721 616.7 21 -0.001758 616.8 22 -0.00177 617 22 -0.001758 617.1 23 -0.001758 617.3 21 -0.001733 617.5 22 -0.001721 617.6 22 -0.001709 617.8 22 -0.001709 617.9 21 -0.001709 618.1 21 -0.001696 618.3 21 -0.001709 618.4 21 -0.001709 618.6 21 -0.001721 618.8 21 -0.001721 618.9 21 -0.001733 619.1 21 -0.001733 619.2 21 -0.001733 619.4 21 -0.001733 619.6 21 -0.001746 619.7 21 -0.001721 619.9 20 -0.001709 620 21 -0.001721 620.2 20 -0.001721 620.4 20 -0.001733 620.5 20 -0.001733 620.7 20 -0.001733 620.8 20 -0.001733 621 20 -0.001746 621.2 20 -0.001746 621.3 20 -0.001733 621.5 20 -0.001721 621.7 20 -0.001721 621.8 20 -0.001721 622 20 -0.001721 622.1 20 -0.001733 622.3 19 -0.001733 622.5 20 -0.001746 622.6 19 -0.001746 622.8 19 -0.001746 622.9 20 -0.001746 623.1 19 -0.001746 623.3 19 -0.001746 623.4 19 -0.001746 623.6 19 -0.001746 623.7 19 -0.001746 623.9 19 -0.001733 624.1 19 -0.001733 624.2 19 -0.001733 624.4 19 -0.001746 624.6 19 -0.001746 624.7 19 -0.001733 624.9 19 -0.001746 625 19 -0.001746 625.2 19 -0.001758 625.4 19 -0.001758 625.5 19 -0.00177 625.7 19 -0.001758 625.8 18 -0.001746 626 18 -0.001758 626.2 18 -0.001758 626.3 18 -0.001758 626.5 18 -0.00177 626.7 18 -0.001758 626.8 18 -0.001746 627 18 -0.001746 627.1 18 -0.001758 627.3 18 -0.00177 627.5 18 -0.00177 627.6 18 -0.001783 627.8 18 -0.001758 627.9 18 -0.001758 628.1 18 -0.00177 628.3 18 -0.001758 628.4 18 -0.001758 628.6 18 -0.001758 628.7 18 -0.001758 628.9 18 -0.001758 629.1 17 -0.001758 629.2 17 -0.00177 629.4 17 -0.00177 629.6 18 -0.001758 629.7 17 -0.001758 629.9 17 -0.00177 630 17 -0.00177 630.2 17 -0.001783 630.4 17 -0.001783 630.5 17 -0.001783 630.7 17 -0.001783 630.8 17 -0.001783 631 17 -0.00177 631.2 16 -0.001252 631.3 17 -0.0005983 631.5 16 -0.0009561 631.6 17 -0.001215 631.8 16 -0.001388 632 17 -0.001511 632.1 17 -0.001598 632.3 16 -0.001659 632.5 16 -0.001696 632.6 17 -0.001721 632.8 16 -0.001733 632.9 16 -0.001758 633.1 17 -0.001758 633.3 17 -0.001746 633.4 16 -0.001783 633.6 16 -0.001795 633.7 16 -0.001807 633.9 16 -0.001795 634.1 16 -0.001795 634.2 16 -0.00177 634.4 16 -0.001758 634.5 16 -0.001746 634.7 16 -0.001721 634.9 16 -0.001733 635 16 -0.001733 635.2 16 -0.001746 635.4 16 -0.001733 635.5 16 -0.001746 635.7 16 -0.001758 635.8 16 -0.001783 636 16 -0.001795 636.2 16 -0.001783 636.3 16 -0.001783 636.5 16 -0.001783 636.6 16 -0.001783 636.8 16 -0.001783 637 16 -0.001783 637.1 16 -0.001807 637.3 16 -0.001807 637.4 16 -0.001795 637.6 16 -0.001807 637.8 16 -0.001807 637.9 16 -0.001795 638.1 16 -0.001783 638.3 16 -0.00177 638.4 15 -0.001783 638.6 16 -0.001795 638.7 15 -0.001795 638.9 15 -0.001795 639.1 15 -0.001795 639.2 16 -0.001783 639.4 16 -0.001783 639.5 15 -0.001807 639.7 16 -0.00182 639.9 16 -0.001832 640 15 -0.001807 640.2 15 -0.001807 640.3 16 -0.001807 640.5 15 -0.001832 640.7 16 -0.001832 640.8 15 -0.001807 641 15 -0.001795 641.2 15 -0.001783 641.3 15 -0.001783 641.5 15 -0.001783 641.6 15 -0.001783 641.8 15 -0.001783 642 15 -0.001783 642.1 15 -0.001783 642.3 15 -0.001783 642.4 15 -0.001783 642.6 15 -0.001783 642.8 15 -0.001783 642.9 15 -0.001807 643.1 15 -0.001807 643.2 15 -0.001807 643.4 15 -0.001807 643.6 15 -0.001795 643.7 15 -0.001795 643.9 15 -0.001795 644.1 15 -0.001795 644.2 15 -0.001807 644.4 15 -0.001807 644.5 15 -0.00182 644.7 15 -0.001832 644.9 15 -0.001832 645 15 -0.00182 645.2 15 -0.001807 645.3 15 -0.001807 645.5 15 -0.001795 645.7 15 -0.001783 645.8 14 -0.001795 646 14 -0.001783 646.1 14 -0.001807 646.3 15 -0.001807 646.5 14 -0.001795 646.6 14 -0.001795 646.8 14 -0.001783 647 14 -0.001783 647.1 15 -0.001783 647.3 14 -0.001783 647.4 14 -0.001783 647.6 14 -0.001783 647.8 15 -0.001795 647.9 14 -0.001807 648.1 14 -0.001795 648.2 14 -0.001795 648.4 14 -0.001795 648.6 14 -0.001783 648.7 14 -0.001783 648.9 15 -0.001783 649 14 -0.001783 649.2 14 -0.001783 649.4 14 -0.001783 649.5 14 -0.001783 649.7 14 -0.001783 649.9 14 -0.001783 650 14 -0.001783 650.2 14 -0.001795 650.3 14 -0.001807 650.5 14 -0.001795 650.7 14 -0.001795 650.8 14 -0.001807 651 13 -0.00182 651.1 14 -0.001807 651.3 14 -0.001807 651.5 13 -0.001783 651.6 14 -0.00177 651.8 14 -0.001758 651.9 14 -0.001758 652.1 14 -0.00177 652.3 14 -0.001783 652.4 14 -0.001758 652.6 14 -0.00177 652.8 14 -0.00177 652.9 13 -0.00177 653.1 14 -0.001783 653.2 13 -0.001783 653.4 13 -0.001783 653.6 14 -0.001783 653.7 14 -0.001783 653.9 13 -0.001783 654 13 -0.001783 654.2 13 -0.001783 654.4 13 -0.001783 654.5 13 -0.001783 654.7 13 -0.001783 654.8 13 -0.001783 655 14 -0.001783 655.2 13 -0.001783 655.3 13 -0.001783 655.5 13 -0.001783 655.7 14 -0.001783 655.8 13 -0.001783 656 13 -0.001783 656.1 13 -0.001783 656.3 13 -0.001795 656.5 13 -0.001795 656.6 13 -0.001795 656.8 13 -0.001795 656.9 13 -0.001795 657.1 13 -0.001783 657.3 13 -0.001783 657.4 13 -0.001783 657.6 13 -0.001795 657.7 13 -0.001807 657.9 13 -0.001832 658.1 13 -0.001844 658.2 13 -0.001857 658.4 13 -0.001857 658.6 13 -0.001857 658.7 13 -0.001832 658.9 13 -0.00182 659 13 -0.001807 659.2 13 -0.001795 659.4 16 0.29 0.09 0.74 0.002 0.007 0.66 1.3 1.02 0.292 0 0 0.001 0.0041 0 5 -0.0001302 0 7 -0.0001302 0.1245 7 -0.0001302 0.249 7 -0.0001302 0.3735 7 -0.0001302 0.4981 7 -0.0001302 0.6226 7 -0.0001178 0.7471 6 -0.0001302 0.8716 7 -0.0001302 0.9961 7 -0.0001178 1.121 7 -0.0001178 1.245 8 -0.0001054 1.37 9 -9.299e-05 1.494 9 -9.299e-05 1.619 10 -6.82e-05 1.743 12 -6.82e-05 1.868 13 -3.1e-05 1.992 15 6.2e-06 2.117 18 6.2e-06 2.241 20 6.2e-06 2.366 22 6.2e-06 2.49 24 3.1e-05 2.615 27 6.82e-05 2.739 29 0.0001054 2.864 32 0.000155 2.988 35 0.0001798 3.113 39 0.0002418 3.237 42 0.000279 3.362 45 0.0003286 3.486 48 0.0003782 3.611 52 0.0004278 3.735 54 0.0004526 3.86 57 0.0005022 3.984 60 0.0005518 4.109 63 0.0005766 4.233 65 0.0006262 4.358 68 0.0006758 4.482 71 0.0007005 4.607 73 0.0007625 4.731 76 0.0007997 4.856 77 0.0008369 4.981 81 0.0008741 5.105 82 0.0008989 5.23 84 0.0009237 5.354 87 0.0009485 5.479 88 0.0009609 5.603 91 0.001011 5.728 93 0.001048 5.852 95 0.001073 5.977 96 0.001097 6.101 98 0.001122 6.226 100 0.001159 6.35 102 0.001184 6.475 104 0.001197 6.599 106 0.001221 6.724 109 0.001246 6.848 110 0.001271 6.973 112 0.001296 7.097 113 0.001333 7.222 115 0.001358 7.346 116 0.00137 7.471 118 0.001382 7.595 121 0.001395 7.72 123 0.001407 7.844 125 0.00142 7.969 126 0.001457 8.093 128 0.001482 8.218 131 0.001531 8.342 132 0.001568 8.467 134 0.001606 8.591 137 0.00163 8.716 138 0.001643 8.84 140 0.001643 8.965 143 0.001668 9.089 145 0.00168 9.214 147 0.001705 9.338 149 0.001717 9.463 152 0.001754 9.588 152 0.001767 9.712 156 0.001792 9.837 157 0.001816 9.961 159 0.001841 10.09 162 0.001878 10.21 163 0.001916 10.33 166 0.00194 10.46 168 0.001965 10.58 170 0.001978 10.71 172 0.00199 10.83 174 0.002015 10.96 176 0.00204 11.08 177 0.002064 11.21 180 0.002077 11.33 182 0.002102 11.46 184 0.002126 11.58 186 0.002139 11.7 187 0.002151 11.83 190 0.002164 11.95 191 0.002201 12.08 193 0.002238 12.2 195 0.002263 12.33 197 0.002288 12.45 199 0.002312 12.58 201 0.002337 12.7 202 0.002362 12.82 204 0.002387 12.95 206 0.002412 13.07 208 0.002436 13.2 209 0.002461 13.32 212 0.002511 13.45 214 0.002523 13.57 217 0.002536 13.7 218 0.002548 13.82 220 0.002585 13.95 223 0.00261 14.07 224 0.002647 14.19 227 0.002672 14.32 229 0.002709 14.44 231 0.002722 14.57 233 0.002759 14.69 235 0.002784 14.82 237 0.002808 14.94 239 0.002821 15.07 242 0.002846 15.19 243 0.002883 15.32 245 0.002908 15.44 247 0.002945 15.56 249 0.002957 15.69 252 0.00297 15.81 253 0.003007 15.94 256 0.003032 16.06 257 0.003056 16.19 260 0.003106 16.31 262 0.003143 16.44 263 0.003168 16.56 265 0.003205 16.68 267 0.00323 16.81 269 0.003242 16.93 271 0.003267 17.06 274 0.003304 17.18 276 0.003329 17.31 277 0.003354 17.43 279 0.003391 17.56 281 0.003428 17.68 284 0.003453 17.81 286 0.003478 17.93 288 0.003503 18.05 289 0.003552 18.18 292 0.003577 18.3 293 0.003614 18.43 295 0.003652 18.55 297 0.003689 18.68 299 0.003701 18.8 301 0.003738 18.93 302 0.003751 19.05 306 0.003763 19.18 307 0.003813 19.3 310 0.00385 19.42 311 0.003887 19.55 313 0.003924 19.67 315 0.003962 19.8 317 0.003986 19.92 320 0.004024 20.05 321 0.004048 20.17 323 0.004073 20.3 326 0.004098 20.42 328 0.004147 20.54 329 0.004172 20.67 331 0.004222 20.79 334 0.004271 20.92 335 0.004296 21.04 337 0.004309 21.17 339 0.004358 21.29 342 0.004395 21.42 343 0.00442 21.54 345 0.004433 21.67 348 0.004482 21.79 349 0.004495 21.91 351 0.004544 22.04 353 0.004581 22.16 356 0.004606 22.29 357 0.004631 22.41 359 0.004631 22.54 362 0.004656 22.66 363 0.004668 22.79 365 0.004705 22.91 368 0.00473 23.03 369 0.004755 23.16 371 0.00478 23.28 374 0.004805 23.41 375 0.004829 23.53 378 0.004867 23.66 380 0.004891 23.78 381 0.004929 23.91 384 0.004966 24.03 385 0.005015 24.16 387 0.00504 24.28 389 0.005065 24.4 392 0.005102 24.53 394 0.005139 24.65 396 0.005164 24.78 398 0.005189 24.9 399 0.005214 25.03 401 0.005239 25.15 403 0.005276 25.28 404 0.005301 25.4 406 0.005325 25.53 409 0.005363 25.65 410 0.005387 25.77 412 0.005425 25.9 415 0.005462 26.02 417 0.005474 26.15 418 0.005499 26.27 421 0.005524 26.4 423 0.005536 26.52 424 0.005561 26.65 427 0.005586 26.77 428 0.005635 26.89 431 0.00566 27.02 432 0.005685 27.14 435 0.00571 27.27 437 0.005747 27.39 438 0.005784 27.52 440 0.005809 27.64 442 0.005846 27.77 445 0.005883 27.89 446 0.005921 28.02 449 0.005945 28.14 451 0.005983 28.26 453 0.006007 28.39 455 0.006032 28.51 456 0.006069 28.64 459 0.006082 28.76 460 0.006094 28.89 463 0.006131 29.01 465 0.006144 29.14 467 0.006181 29.26 468 0.006218 29.39 471 0.006255 29.51 473 0.00628 29.63 474 0.006317 29.76 478 0.006355 29.88 479 0.006379 30.01 481 0.006417 30.13 484 0.006454 30.26 485 0.006479 30.38 487 0.006503 30.51 489 0.006528 30.63 491 0.006565 30.75 493 0.006578 30.88 495 0.006627 31 497 0.006665 31.13 499 0.006702 31.25 501 0.006751 31.38 503 0.006801 31.5 506 0.006826 31.63 507 0.006863 31.75 509 0.006888 31.88 512 0.006937 32 513 0.006974 32.12 515 0.006999 32.25 517 0.007024 32.37 519 0.007061 32.5 521 0.007086 32.62 523 0.007123 32.75 526 0.00716 32.87 528 0.007198 33 529 0.007235 33.12 531 0.007284 33.24 534 0.007322 33.37 535 0.007371 33.49 537 0.007396 33.62 540 0.007433 33.74 542 0.00747 33.87 543 0.007495 33.99 545 0.00752 34.12 547 0.00757 34.24 549 0.007619 34.37 551 0.007632 34.49 553 0.007681 34.61 556 0.007718 34.74 557 0.007756 34.86 559 0.007793 34.99 562 0.00783 35.11 564 0.007855 35.24 565 0.007892 35.36 568 0.007917 35.49 569 0.007942 35.61 571 0.007991 35.74 574 0.008016 35.86 575 0.008053 35.98 578 0.008078 36.11 579 0.008115 36.23 582 0.008165 36.36 584 0.00819 36.48 585 0.008239 36.61 587 0.008276 36.73 590 0.008314 36.86 592 0.008351 36.98 593 0.008388 37.1 595 0.008413 37.23 597 0.008462 37.35 600 0.0085 37.48 601 0.008524 37.6 603 0.008549 37.73 604 0.008599 37.85 607 0.008636 37.98 609 0.008686 38.1 610 0.008723 38.23 613 0.00876 38.35 615 0.00881 38.47 617 0.008834 38.6 618 0.008859 38.72 621 0.008859 38.85 623 0.008872 38.97 625 0.008896 39.1 627 0.008934 39.22 628 0.008996 39.35 631 0.009033 39.47 632 0.00907 39.6 634 0.009095 39.72 636 0.009132 39.84 638 0.009169 39.97 640 0.009206 40.09 643 0.009244 40.22 645 0.009281 40.34 646 0.009318 40.47 649 0.00938 40.59 650 0.009417 40.72 653 0.009467 40.84 655 0.009516 40.96 657 0.009541 41.09 659 0.009591 41.21 661 0.009628 41.34 663 0.009665 41.46 665 0.009702 41.59 667 0.009739 41.71 668 0.009764 41.84 671 0.009789 41.96 673 0.009814 42.09 675 0.009851 42.21 677 0.009888 42.33 679 0.009913 42.46 681 0.00995 42.58 683 0.01 42.71 685 0.01002 42.83 687 0.01006 42.96 689 0.0101 43.08 691 0.01016 43.21 693 0.0102 43.33 694 0.01025 43.46 696 0.01027 43.58 699 0.0103 43.7 700 0.01035 43.83 703 0.01038 43.95 704 0.01041 44.08 706 0.01045 44.2 708 0.01046 44.33 710 0.01047 44.45 712 0.01048 44.58 714 0.01051 44.7 715 0.01053 44.82 718 0.01057 44.95 718 0.0106 45.07 721 0.01062 45.2 723 0.01066 45.32 725 0.01069 45.45 726 0.01072 45.57 728 0.01076 45.7 729 0.01079 45.82 731 0.01082 45.95 732 0.01084 46.07 734 0.01088 46.19 736 0.01091 46.32 739 0.01092 46.44 742 0.01097 46.57 743 0.011 46.69 745 0.01104 46.82 745 0.01107 46.94 746 0.01109 47.07 746 0.0111 47.19 748 0.01113 47.31 750 0.01117 47.44 750 0.01119 47.56 751 0.0112 47.69 753 0.01125 47.81 755 0.01129 47.94 756 0.01131 48.06 758 0.01134 48.19 760 0.01143 48.31 762 0.01149 48.44 763 0.01151 48.56 765 0.01154 48.68 767 0.01156 48.81 768 0.01159 48.93 771 0.01161 49.06 772 0.01164 49.18 775 0.01169 49.31 776 0.0117 49.43 779 0.01174 49.56 781 0.01177 49.68 784 0.01182 49.81 786 0.01186 49.93 788 0.01191 50.05 790 0.01195 50.18 793 0.01198 50.3 794 0.01202 50.43 796 0.01205 50.55 800 0.01207 50.68 801 0.01207 50.8 801 0.01207 50.93 801 0.01207 51.05 803 0.01205 51.17 806 0.01202 51.3 807 0.01198 51.42 809 0.01193 51.55 812 0.01186 51.67 815 0.01177 51.8 817 0.01166 51.92 819 0.01156 52.05 821 0.01141 52.17 825 0.01128 52.3 828 0.0111 52.42 831 0.01095 52.54 834 0.01082 52.67 837 0.01069 52.79 840 0.01057 52.92 843 0.01045 53.04 847 0.01032 53.17 850 0.01022 53.29 853 0.01017 53.42 856 0.01011 53.54 859 0.01011 53.67 862 0.01012 53.79 865 0.01015 53.91 868 0.01017 54.04 872 0.01022 54.16 874 0.01025 54.29 876 0.0103 54.41 879 0.01035 54.54 881 0.0104 54.66 883 0.01045 54.79 886 0.01051 54.91 887 0.01056 55.03 889 0.01062 55.16 890 0.01064 55.28 893 0.01071 55.41 894 0.01074 55.53 897 0.01081 55.66 898 0.01086 55.78 900 0.01089 55.91 901 0.01093 56.03 903 0.01097 56.16 904 0.011 56.28 906 0.01104 56.4 907 0.01108 56.53 909 0.01112 56.65 911 0.01114 56.78 912 0.01118 56.9 914 0.01121 57.03 915 0.01124 57.15 917 0.0113 57.28 918 0.01134 57.4 920 0.01139 57.53 922 0.01144 57.65 923 0.01148 57.77 925 0.01151 57.9 926 0.01156 58.02 928 0.0116 58.15 929 0.01165 58.27 931 0.01169 58.4 934 0.01174 58.52 935 0.01179 58.65 937 0.01182 58.77 938 0.01187 58.89 940 0.01193 59.02 942 0.01196 59.14 943 0.01202 59.27 947 0.01206 59.39 947 0.0121 59.52 950 0.01214 59.64 950 0.01219 59.77 953 0.01224 59.89 955 0.01232 60.02 957 0.01237 60.14 959 0.01243 60.26 962 0.01248 60.39 963 0.01252 60.51 965 0.01257 60.64 967 0.01263 60.76 969 0.01268 60.89 972 0.0127 61.01 973 0.01273 61.14 975 0.01278 61.26 978 0.01283 61.38 979 0.01288 61.51 982 0.01293 61.63 984 0.01298 61.76 986 0.013 61.88 988 0.01305 62.01 990 0.01311 62.13 992 0.01315 62.26 993 0.0132 62.38 997 0.01325 62.51 998 0.01329 62.63 1001 0.01336 62.75 1001 0.01341 62.88 1004 0.01345 63 1006 0.01352 63.13 1009 0.01356 63.25 1010 0.01362 63.38 1012 0.01367 63.5 1015 0.01372 63.63 1017 0.01377 63.75 1018 0.01382 63.88 1020 0.01387 64 1022 0.01393 64.12 1025 0.01397 64.25 1026 0.01404 64.37 1029 0.01409 64.5 1031 0.01414 64.62 1033 0.01418 64.75 1035 0.01424 64.87 1037 0.01427 65 1039 0.01433 65.12 1040 0.01439 65.24 1043 0.01444 65.37 1044 0.01449 65.49 1047 0.01455 65.62 1050 0.01459 65.74 1051 0.01462 65.87 1053 0.01465 65.99 1054 0.01471 66.12 1057 0.01476 66.24 1059 0.01479 66.37 1061 0.01481 66.49 1063 0.01486 66.61 1065 0.0149 66.74 1067 0.01496 66.86 1068 0.01501 66.99 1072 0.01506 67.11 1073 0.01512 67.24 1075 0.01518 67.36 1077 0.01526 67.49 1079 0.01531 67.61 1081 0.01538 67.74 1083 0.01544 67.86 1085 0.01551 67.98 1087 0.01555 68.11 1089 0.0156 68.23 1091 0.01565 68.36 1094 0.0157 68.48 1095 0.01575 68.61 1097 0.0158 68.73 1100 0.01586 68.86 1101 0.0159 68.98 1103 0.01594 69.1 1106 0.016 69.23 1108 0.01605 69.35 1109 0.0161 69.48 1112 0.01615 69.6 1113 0.01622 69.73 1115 0.01627 69.85 1117 0.01631 69.98 1119 0.01635 70.1 1122 0.01641 70.23 1123 0.01646 70.35 1126 0.01651 70.47 1128 0.01655 70.6 1129 0.0166 70.72 1131 0.01665 70.85 1134 0.01672 70.97 1136 0.01677 71.1 1137 0.01683 71.22 1140 0.01688 71.35 1142 0.01694 71.47 1144 0.01699 71.59 1145 0.01705 71.72 1147 0.01709 71.84 1150 0.01715 71.97 1151 0.01722 72.09 1153 0.01725 72.22 1156 0.01729 72.34 1158 0.01736 72.47 1159 0.0174 72.59 1162 0.01746 72.72 1164 0.01751 72.84 1165 0.01759 72.96 1167 0.01763 73.09 1169 0.01765 73.21 1172 0.01771 73.34 1173 0.01777 73.46 1175 0.01782 73.59 1178 0.01789 73.71 1179 0.01794 73.84 1182 0.01798 73.96 1184 0.01803 74.09 1186 0.0181 74.21 1187 0.01816 74.33 1190 0.01822 74.46 1192 0.01828 74.58 1194 0.01836 74.71 1195 0.01842 74.83 1198 0.01848 74.96 1200 0.01854 75.08 1201 0.0186 75.21 1201 0.01863 75.33 1201 0.01865 75.45 1203 0.01867 75.58 1203 0.0187 75.7 1203 0.01873 75.83 1204 0.01875 75.95 1204 0.01878 76.08 1204 0.01882 76.2 1204 0.01882 76.33 1204 0.01883 76.45 1204 0.01879 76.58 1204 0.01878 76.7 1204 0.01882 76.82 1204 0.01883 76.95 1204 0.01882 77.07 1204 0.01883 77.2 1203 0.0188 77.32 1203 0.01879 77.45 1203 0.01879 77.57 1203 0.01878 77.7 1203 0.01878 77.82 1202 0.01878 77.95 1201 0.01878 78.07 1201 0.01878 78.19 1201 0.01877 78.32 1201 0.01877 78.44 1201 0.01878 78.57 1201 0.01877 78.69 1200 0.01875 78.82 1200 0.01874 78.94 1200 0.01873 79.07 1200 0.01874 79.19 1200 0.01874 79.31 1200 0.01875 79.44 1200 0.01875 79.56 1200 0.01874 79.69 1199 0.01873 79.81 1199 0.01873 79.94 1198 0.01873 80.06 1199 0.01872 80.19 1198 0.0187 80.31 1198 0.0187 80.44 1198 0.0187 80.56 1198 0.0187 80.68 1198 0.01868 80.81 1198 0.01869 80.93 1198 0.01868 81.06 1198 0.01868 81.18 1198 0.01868 81.31 1198 0.01868 81.43 1198 0.0187 81.56 1198 0.01868 81.68 1198 0.01868 81.81 1198 0.01869 81.93 1198 0.01869 82.05 1198 0.01868 82.18 1198 0.01868 82.3 1198 0.01869 82.43 1198 0.01869 82.55 1198 0.01868 82.68 1198 0.01868 82.8 1198 0.01869 82.93 1199 0.01869 83.05 1199 0.01868 83.17 1199 0.01869 83.3 1199 0.01869 83.42 1199 0.0187 83.55 1199 0.0187 83.67 1199 0.0187 83.8 1199 0.0187 83.92 1199 0.01869 84.05 1199 0.01868 84.17 1200 0.01867 84.3 1199 0.01865 84.42 1200 0.01865 84.54 1200 0.01868 84.67 1199 0.01868 84.79 1200 0.01868 84.92 1199 0.01868 85.04 1200 0.01867 85.17 1200 0.01867 85.29 1200 0.01867 85.42 1200 0.01867 85.54 1200 0.01867 85.66 1200 0.01867 85.79 1200 0.01867 85.91 1200 0.01865 86.04 1200 0.01864 86.16 1200 0.01864 86.29 1200 0.01863 86.41 1200 0.01862 86.54 1200 0.01863 86.66 1200 0.01862 86.79 1200 0.01862 86.91 1200 0.01863 87.03 1200 0.01862 87.16 1200 0.0186 87.28 1200 0.01862 87.41 1200 0.01862 87.53 1200 0.01862 87.66 1200 0.01862 87.78 1200 0.01862 87.91 1200 0.01862 88.03 1200 0.01862 88.16 1200 0.0186 88.28 1200 0.01863 88.4 1200 0.01862 88.53 1200 0.0186 88.65 1200 0.01862 88.78 1200 0.0186 88.9 1200 0.01862 89.03 1200 0.01862 89.15 1200 0.0186 89.28 1200 0.01862 89.4 1200 0.0186 89.52 1200 0.0186 89.65 1200 0.01863 89.77 1200 0.01862 89.9 1200 0.01863 90.02 1200 0.01863 90.15 1200 0.01863 90.27 1200 0.01863 90.4 1200 0.01863 90.52 1200 0.01862 90.65 1200 0.01862 90.77 1199 0.01863 90.89 1200 0.01863 91.02 1199 0.01863 91.14 1200 0.01863 91.27 1200 0.01863 91.39 1200 0.01865 91.52 1200 0.01864 91.64 1200 0.01865 91.77 1200 0.01865 91.89 1200 0.01863 92.02 1200 0.01864 92.14 1200 0.01865 92.26 1200 0.01864 92.39 1200 0.01864 92.51 1200 0.01863 92.64 1200 0.01863 92.76 1200 0.01864 92.89 1199 0.01864 93.01 1200 0.01865 93.14 1200 0.01868 93.26 1200 0.01868 93.38 1200 0.01868 93.51 1200 0.01868 93.63 1200 0.01867 93.76 1200 0.01867 93.88 1199 0.01865 94.01 1200 0.01865 94.13 1200 0.01864 94.26 1199 0.01865 94.38 1199 0.01865 94.51 1200 0.01865 94.63 1200 0.01863 94.75 1199 0.01863 94.88 1200 0.01863 95 1200 0.01863 95.13 1200 0.01863 95.25 1200 0.01863 95.38 1200 0.01863 95.5 1200 0.01864 95.63 1200 0.01863 95.75 1199 0.01863 95.88 1200 0.01864 96 1200 0.01864 96.12 1200 0.01865 96.25 1200 0.01865 96.37 1200 0.01865 96.5 1200 0.01865 96.62 1200 0.01865 96.75 1200 0.01863 96.87 1200 0.01865 97 1200 0.01865 97.12 1200 0.01864 97.24 1200 0.01863 97.37 1200 0.01863 97.49 1199 0.01865 97.62 1200 0.01863 97.74 1199 0.01863 97.87 1200 0.01864 97.99 1200 0.01865 98.12 1200 0.01863 98.24 1200 0.01863 98.37 1200 0.01863 98.49 1200 0.01863 98.61 1200 0.01863 98.74 1200 0.01862 98.86 1200 0.01862 98.99 1200 0.01862 99.11 1200 0.01862 99.24 1200 0.01862 99.36 1199 0.0186 99.49 1200 0.01858 99.61 1200 0.01859 99.73 1200 0.01858 99.86 1200 0.01858 99.98 1200 0.01858 100.1 1200 0.01856 100.2 1200 0.01856 100.4 1200 0.01856 100.5 1200 0.01856 100.6 1200 0.01858 100.7 1200 0.01858 100.9 1199 0.01857 101 1199 0.01858 101.1 1200 0.01858 101.2 1200 0.01858 101.4 1200 0.01858 101.5 1200 0.01858 101.6 1200 0.0186 101.7 1200 0.01859 101.9 1199 0.01858 102 1200 0.01858 102.1 1200 0.01858 102.2 1200 0.01858 102.3 1200 0.01857 102.5 1200 0.01857 102.6 1200 0.01858 102.7 1200 0.01857 102.8 1200 0.01857 103 1200 0.01856 103.1 1200 0.01854 103.2 1200 0.01853 103.3 1200 0.01853 103.5 1200 0.01853 103.6 1200 0.01856 103.7 1199 0.01853 103.8 1200 0.01853 104 1200 0.01853 104.1 1200 0.01853 104.2 1200 0.01853 104.3 1200 0.01854 104.5 1200 0.01853 104.6 1200 0.01853 104.7 1200 0.01853 104.8 1200 0.01852 105 1200 0.01853 105.1 1200 0.01852 105.2 1200 0.01853 105.3 1200 0.01854 105.5 1200 0.01854 105.6 1200 0.01856 105.7 1200 0.01854 105.8 1200 0.01853 106 1200 0.01853 106.1 1200 0.01853 106.2 1200 0.01853 106.3 1200 0.01854 106.5 1200 0.01854 106.6 1200 0.01856 106.7 1200 0.01856 106.8 1200 0.01854 107 1200 0.01854 107.1 1200 0.01853 107.2 1199 0.01853 107.3 1200 0.01853 107.5 1200 0.01853 107.6 1200 0.01853 107.7 1200 0.01853 107.8 1200 0.01853 108 1200 0.01856 108.1 1200 0.01856 108.2 1200 0.01856 108.3 1200 0.01857 108.5 1200 0.01858 108.6 1200 0.01859 108.7 1200 0.01859 108.8 1200 0.01858 108.9 1200 0.01858 109.1 1200 0.01858 109.2 1200 0.01859 109.3 1200 0.01859 109.4 1200 0.0186 109.6 1200 0.01862 109.7 1200 0.0186 109.8 1200 0.0186 109.9 1200 0.01862 110.1 1200 0.01863 110.2 1200 0.01863 110.3 1200 0.01863 110.4 1200 0.01863 110.6 1200 0.01864 110.7 1200 0.01865 110.8 1200 0.01865 110.9 1200 0.01865 111.1 1200 0.01868 111.2 1200 0.01868 111.3 1200 0.01868 111.4 1200 0.01868 111.6 1200 0.01868 111.7 1200 0.01868 111.8 1200 0.01867 111.9 1200 0.01868 112.1 1200 0.01867 112.2 1200 0.01868 112.3 1200 0.01868 112.4 1200 0.01868 112.6 1200 0.0187 112.7 1200 0.0187 112.8 1200 0.0187 112.9 1200 0.01873 113.1 1200 0.01873 113.2 1200 0.01873 113.3 1200 0.01875 113.4 1200 0.01875 113.6 1200 0.01875 113.7 1200 0.01877 113.8 1200 0.01877 113.9 1200 0.01875 114.1 1200 0.01874 114.2 1200 0.01875 114.3 1200 0.01878 114.4 1200 0.01878 114.6 1200 0.01878 114.7 1200 0.01878 114.8 1200 0.01878 114.9 1200 0.01878 115.1 1200 0.01879 115.2 1200 0.0188 115.3 1200 0.01882 115.4 1200 0.01882 115.5 1200 0.0188 115.7 1200 0.01882 115.8 1200 0.01882 115.9 1199 0.01883 116 1200 0.01884 116.2 1200 0.01882 116.3 1200 0.0188 116.4 1200 0.01879 116.5 1200 0.01879 116.7 1200 0.0188 116.8 1200 0.01882 116.9 1200 0.0188 117 1200 0.01882 117.2 1200 0.01882 117.3 1200 0.01882 117.4 1199 0.01882 117.5 1200 0.01882 117.7 1200 0.0188 117.8 1200 0.01879 117.9 1200 0.0188 118 1200 0.0188 118.2 1200 0.01879 118.3 1200 0.01878 118.4 1200 0.0188 118.5 1200 0.01879 118.7 1200 0.01878 118.8 1200 0.01878 118.9 1200 0.01878 119 1200 0.01878 119.2 1200 0.0188 119.3 1200 0.01879 119.4 1200 0.01878 119.5 1200 0.01878 119.7 1200 0.01878 119.8 1200 0.01878 119.9 1200 0.01878 120 1200 0.01878 120.2 1200 0.01878 120.3 1200 0.01875 120.4 1200 0.01875 120.5 1200 0.01875 120.7 1200 0.01875 120.8 1200 0.01875 120.9 1200 0.01877 121 1199 0.01878 121.2 1200 0.01875 121.3 1200 0.01875 121.4 1200 0.01874 121.5 1200 0.01873 121.6 1200 0.01873 121.8 1200 0.01873 121.9 1200 0.01873 122 1200 0.01872 122.1 1200 0.01872 122.3 1200 0.01873 122.4 1200 0.01872 122.5 1200 0.01872 122.6 1200 0.01872 122.8 1200 0.0187 122.9 1200 0.0187 123 1200 0.0187 123.1 1200 0.0187 123.3 1200 0.0187 123.4 1200 0.01872 123.5 1200 0.01872 123.6 1200 0.0187 123.8 1200 0.0187 123.9 1200 0.01869 124 1200 0.0187 124.1 1200 0.0187 124.3 1200 0.0187 124.4 1200 0.0187 124.5 1200 0.01869 124.6 1200 0.01868 124.8 1200 0.01868 124.9 1200 0.01868 125 1200 0.01868 125.1 1200 0.01868 125.3 1200 0.01868 125.4 1200 0.0187 125.5 1200 0.0187 125.6 1200 0.01868 125.8 1200 0.01867 125.9 1200 0.01868 126 1200 0.01865 126.1 1200 0.01868 126.3 1200 0.01868 126.4 1200 0.01868 126.5 1200 0.01868 126.6 1200 0.01867 126.8 1200 0.01865 126.9 1200 0.01865 127 1200 0.01867 127.1 1200 0.01867 127.3 1200 0.01867 127.4 1200 0.01867 127.5 1200 0.01867 127.6 1200 0.01867 127.8 1200 0.01865 127.9 1200 0.01867 128 1200 0.01868 128.1 1200 0.01865 128.2 1200 0.01867 128.4 1200 0.01868 128.5 1200 0.01867 128.6 1199 0.01867 128.7 1200 0.01868 128.9 1200 0.01867 129 1200 0.01867 129.1 1200 0.01868 129.2 1200 0.01867 129.4 1200 0.01867 129.5 1200 0.01867 129.6 1200 0.01867 129.7 1200 0.01868 129.9 1200 0.01868 130 1200 0.01869 130.1 1200 0.01872 130.2 1200 0.0187 130.4 1200 0.0187 130.5 1200 0.01872 130.6 1200 0.01872 130.7 1200 0.01872 130.9 1200 0.01872 131 1200 0.0187 131.1 1200 0.01869 131.2 1200 0.01869 131.4 1200 0.01868 131.5 1200 0.01869 131.6 1200 0.0187 131.7 1200 0.0187 131.9 1200 0.0187 132 1200 0.0187 132.1 1200 0.0187 132.2 1200 0.01872 132.4 1200 0.01872 132.5 1200 0.01872 132.6 1200 0.01872 132.7 1200 0.01872 132.9 1200 0.01872 133 1200 0.01872 133.1 1200 0.01872 133.2 1200 0.0187 133.4 1200 0.01869 133.5 1200 0.0187 133.6 1200 0.0187 133.7 1200 0.01872 133.9 1200 0.01872 134 1200 0.01872 134.1 1200 0.0187 134.2 1200 0.0187 134.3 1200 0.0187 134.5 1200 0.0187 134.6 1200 0.0187 134.7 1200 0.01869 134.8 1200 0.01868 135 1200 0.0187 135.1 1200 0.0187 135.2 1200 0.0187 135.3 1200 0.01872 135.5 1200 0.0187 135.6 1200 0.0187 135.7 1200 0.0187 135.8 1200 0.01868 136 1200 0.01867 136.1 1200 0.01867 136.2 1200 0.01865 136.3 1200 0.01867 136.5 1200 0.01868 136.6 1200 0.01869 136.7 1200 0.0187 136.8 1200 0.0187 137 1200 0.01868 137.1 1200 0.01868 137.2 1200 0.01868 137.3 1200 0.01868 137.5 1200 0.01868 137.6 1200 0.01868 137.7 1200 0.01869 137.8 1200 0.01869 138 1200 0.01868 138.1 1200 0.01868 138.2 1200 0.01868 138.3 1200 0.01868 138.5 1200 0.01869 138.6 1200 0.01868 138.7 1200 0.01868 138.8 1200 0.01867 139 1200 0.01865 139.1 1200 0.01865 139.2 1200 0.01865 139.3 1200 0.01865 139.5 1200 0.01865 139.6 1200 0.01867 139.7 1200 0.01865 139.8 1200 0.01867 140 1200 0.01868 140.1 1200 0.01865 140.2 1199 0.01865 140.3 1200 0.01865 140.5 1200 0.01864 140.6 1200 0.01865 140.7 1200 0.01865 140.8 1200 0.01864 140.9 1200 0.01863 141.1 1200 0.01863 141.2 1200 0.01862 141.3 1200 0.0186 141.4 1200 0.01859 141.6 1200 0.01858 141.7 1200 0.01859 141.8 1200 0.01859 141.9 1200 0.0186 142.1 1200 0.0186 142.2 1200 0.0186 142.3 1200 0.01862 142.4 1200 0.01862 142.6 1200 0.01862 142.7 1200 0.0186 142.8 1200 0.01862 142.9 1200 0.0186 143.1 1200 0.01862 143.2 1200 0.01862 143.3 1200 0.0186 143.4 1200 0.0186 143.6 1200 0.01859 143.7 1200 0.0186 143.8 1200 0.0186 143.9 1200 0.01859 144.1 1200 0.01858 144.2 1200 0.01858 144.3 1200 0.01858 144.4 1200 0.01858 144.6 1200 0.01858 144.7 1200 0.01858 144.8 1200 0.01857 144.9 1200 0.01858 145.1 1200 0.01858 145.2 1200 0.01858 145.3 1200 0.01858 145.4 1200 0.01859 145.6 1200 0.01859 145.7 1200 0.01859 145.8 1200 0.01858 145.9 1200 0.01859 146.1 1200 0.01859 146.2 1200 0.01858 146.3 1200 0.01858 146.4 1200 0.0186 146.6 1200 0.01859 146.7 1200 0.01858 146.8 1200 0.01858 146.9 1200 0.01859 147 1200 0.0186 147.2 1200 0.0186 147.3 1200 0.0186 147.4 1200 0.01862 147.5 1200 0.0186 147.7 1200 0.01862 147.8 1200 0.01862 147.9 1200 0.01862 148 1200 0.01863 148.2 1200 0.01863 148.3 1200 0.01863 148.4 1200 0.01863 148.5 1200 0.01863 148.7 1200 0.01863 148.8 1200 0.01864 148.9 1200 0.01865 149 1200 0.01865 149.2 1200 0.01865 149.3 1200 0.01867 149.4 1200 0.01867 149.5 1200 0.01868 149.7 1200 0.01868 149.8 1200 0.01869 149.9 1200 0.0187 150 1200 0.0187 150.2 1200 0.0187 150.3 1200 0.01872 150.4 1200 0.0187 150.5 1200 0.01872 150.7 1200 0.01872 150.8 1200 0.01872 150.9 1200 0.01872 151 1200 0.01873 151.2 1200 0.01873 151.3 1200 0.01873 151.4 1200 0.01873 151.5 1200 0.01874 151.7 1200 0.01875 151.8 1200 0.01875 151.9 1200 0.01875 152 1200 0.01877 152.2 1200 0.01878 152.3 1200 0.01878 152.4 1200 0.01879 152.5 1200 0.0188 152.7 1200 0.0188 152.8 1200 0.01882 152.9 1200 0.01882 153 1200 0.01882 153.2 1200 0.01882 153.3 1200 0.01882 153.4 1200 0.01882 153.5 1200 0.01883 153.6 1200 0.0188 153.8 1200 0.01879 153.9 1200 0.0188 154 1200 0.0188 154.1 1200 0.01883 154.3 1200 0.01884 154.4 1200 0.01883 154.5 1200 0.01883 154.6 1200 0.01883 154.8 1200 0.01883 154.9 1200 0.01883 155 1200 0.01884 155.1 1200 0.01884 155.3 1200 0.01884 155.4 1200 0.01884 155.5 1200 0.01885 155.6 1200 0.01887 155.8 1200 0.01888 155.9 1200 0.01887 156 1200 0.01888 156.1 1200 0.01887 156.3 1200 0.01887 156.4 1200 0.0189 156.5 1200 0.0189 156.6 1200 0.01888 156.8 1200 0.01889 156.9 1200 0.01888 157 1200 0.01888 157.1 1200 0.01888 157.3 1200 0.01888 157.4 1200 0.0189 157.5 1200 0.0189 157.6 1200 0.01889 157.8 1200 0.01889 157.9 1200 0.01888 158 1200 0.01888 158.1 1200 0.0189 158.3 1200 0.0189 158.4 1200 0.01888 158.5 1200 0.01888 158.6 1200 0.01888 158.8 1200 0.01888 158.9 1200 0.01888 159 1200 0.01888 159.1 1200 0.01888 159.3 1200 0.01887 159.4 1200 0.01885 159.5 1200 0.01884 159.6 1200 0.01884 159.8 1200 0.01883 159.9 1200 0.01883 160 1200 0.01884 160.1 1200 0.01884 160.2 1200 0.01884 160.4 1200 0.01883 160.5 1200 0.01883 160.6 1200 0.01883 160.7 1200 0.01883 160.9 1200 0.01883 161 1200 0.01883 161.1 1200 0.01883 161.2 1200 0.01883 161.4 1200 0.01883 161.5 1200 0.01882 161.6 1200 0.01882 161.7 1200 0.0188 161.9 1200 0.01879 162 1200 0.01882 162.1 1200 0.0188 162.2 1200 0.01879 162.4 1200 0.01879 162.5 1200 0.01878 162.6 1200 0.01878 162.7 1200 0.01878 162.9 1200 0.01878 163 1200 0.01878 163.1 1200 0.01878 163.2 1200 0.01875 163.4 1200 0.01875 163.5 1200 0.01873 163.6 1200 0.01873 163.7 1200 0.01873 163.9 1200 0.01873 164 1200 0.01873 164.1 1200 0.01873 164.2 1200 0.01872 164.4 1200 0.01872 164.5 1200 0.01872 164.6 1200 0.01872 164.7 1200 0.01873 164.9 1200 0.01872 165 1200 0.01872 165.1 1200 0.01873 165.2 1200 0.01872 165.4 1200 0.01873 165.5 1200 0.01874 165.6 1200 0.01873 165.7 1200 0.01873 165.9 1200 0.01873 166 1200 0.01873 166.1 1200 0.01873 166.2 1200 0.01872 166.3 1200 0.01872 166.5 1200 0.01873 166.6 1200 0.0187 166.7 1200 0.01869 166.8 1200 0.0187 167 1200 0.0187 167.1 1200 0.0187 167.2 1200 0.01872 167.3 1200 0.0187 167.5 1200 0.01872 167.6 1200 0.01872 167.7 1200 0.01872 167.8 1200 0.01872 168 1200 0.01872 168.1 1200 0.01872 168.2 1200 0.01872 168.3 1200 0.01872 168.5 1200 0.01872 168.6 1200 0.01872 168.7 1200 0.01872 168.8 1200 0.01872 169 1200 0.0187 169.1 1200 0.0187 169.2 1200 0.0187 169.3 1200 0.0187 169.5 1200 0.01869 169.6 1200 0.01869 169.7 1200 0.01869 169.8 1200 0.0187 170 1200 0.0187 170.1 1200 0.0187 170.2 1200 0.0187 170.3 1200 0.01872 170.5 1200 0.01872 170.6 1200 0.01872 170.7 1200 0.01872 170.8 1200 0.01872 171 1200 0.0187 171.1 1200 0.01872 171.2 1200 0.01873 171.3 1200 0.01873 171.5 1200 0.01873 171.6 1200 0.01873 171.7 1200 0.01873 171.8 1200 0.01873 172 1200 0.01872 172.1 1200 0.01873 172.2 1200 0.01873 172.3 1200 0.01873 172.5 1200 0.01874 172.6 1200 0.01873 172.7 1200 0.01873 172.8 1200 0.01873 172.9 1200 0.01873 173.1 1200 0.01873 173.2 1200 0.01873 173.3 1200 0.01874 173.4 1200 0.01875 173.6 1200 0.01875 173.7 1200 0.01873 173.8 1200 0.01875 173.9 1200 0.01875 174.1 1200 0.01875 174.2 1200 0.01877 174.3 1200 0.01875 174.4 1200 0.01875 174.6 1200 0.01874 174.7 1200 0.01873 174.8 1200 0.01873 174.9 1200 0.01875 175.1 1200 0.01874 175.2 1200 0.01873 175.3 1200 0.01873 175.4 1200 0.01873 175.6 1200 0.01873 175.7 1200 0.01872 175.8 1200 0.01872 175.9 1200 0.01873 176.1 1200 0.01872 176.2 1200 0.0187 176.3 1200 0.0187 176.4 1200 0.0187 176.6 1200 0.0187 176.7 1200 0.01872 176.8 1200 0.01872 176.9 1200 0.01872 177.1 1200 0.0187 177.2 1200 0.01869 177.3 1200 0.0187 177.4 1200 0.0187 177.6 1200 0.0187 177.7 1200 0.01872 177.8 1200 0.0187 177.9 1200 0.0187 178.1 1200 0.01872 178.2 1200 0.01872 178.3 1200 0.0187 178.4 1200 0.0187 178.6 1200 0.01868 178.7 1200 0.01868 178.8 1200 0.0187 178.9 1200 0.0187 179 1200 0.01868 179.2 1200 0.01868 179.3 1200 0.01868 179.4 1200 0.01868 179.5 1200 0.01868 179.7 1200 0.01868 179.8 1200 0.01868 179.9 1200 0.01869 180 1200 0.01868 180.2 1200 0.01869 180.3 1200 0.01869 180.4 1200 0.01869 180.5 1200 0.01869 180.7 1200 0.01868 180.8 1200 0.01868 180.9 1200 0.01868 181 1200 0.01868 181.2 1200 0.01865 181.3 1200 0.01865 181.4 1200 0.01863 181.5 1200 0.01863 181.7 1200 0.01863 181.8 1200 0.01863 181.9 1200 0.01864 182 1200 0.01864 182.2 1200 0.01863 182.3 1200 0.01863 182.4 1200 0.01863 182.5 1200 0.01863 182.7 1200 0.01863 182.8 1200 0.01862 182.9 1200 0.01863 183 1200 0.01864 183.2 1200 0.01863 183.3 1200 0.01863 183.4 1200 0.01863 183.5 1200 0.01862 183.7 1200 0.01862 183.8 1200 0.01863 183.9 1200 0.01862 184 1200 0.01862 184.2 1200 0.01863 184.3 1200 0.01862 184.4 1200 0.01862 184.5 1200 0.01862 184.7 1200 0.01862 184.8 1200 0.01862 184.9 1200 0.0186 185 1200 0.01858 185.2 1200 0.0186 185.3 1200 0.0186 185.4 1200 0.0186 185.5 1200 0.01862 185.6 1200 0.0186 185.8 1200 0.0186 185.9 1200 0.0186 186 1200 0.01859 186.1 1200 0.0186 186.3 1200 0.0186 186.4 1200 0.0186 186.5 1200 0.01859 186.6 1200 0.01859 186.8 1200 0.01858 186.9 1200 0.01859 187 1200 0.0186 187.1 1200 0.01858 187.3 1200 0.01858 187.4 1200 0.0186 187.5 1200 0.0186 187.6 1200 0.01863 187.8 1200 0.01863 187.9 1200 0.01862 188 1200 0.01863 188.1 1200 0.01864 188.3 1200 0.01864 188.4 1200 0.01865 188.5 1200 0.01865 188.6 1200 0.01865 188.8 1200 0.01865 188.9 1200 0.01863 189 1200 0.01864 189.1 1200 0.01865 189.3 1200 0.01864 189.4 1199 0.01863 189.5 1200 0.01863 189.6 1200 0.01863 189.8 1200 0.01865 189.9 1200 0.01867 190 1200 0.01867 190.1 1200 0.01868 190.3 1200 0.01868 190.4 1200 0.0187 190.5 1200 0.0187 190.6 1200 0.01873 190.8 1200 0.01872 190.9 1200 0.01872 191 1200 0.01873 191.1 1200 0.01873 191.3 1200 0.01873 191.4 1200 0.01873 191.5 1200 0.01873 191.6 1200 0.01873 191.8 1200 0.01872 191.9 1200 0.01873 192 1200 0.01874 192.1 1200 0.01875 192.2 1200 0.01875 192.4 1200 0.01875 192.5 1200 0.01875 192.6 1200 0.01878 192.7 1200 0.01878 192.9 1200 0.01878 193 1200 0.01878 193.1 1200 0.01878 193.2 1200 0.01878 193.4 1200 0.01878 193.5 1200 0.01879 193.6 1200 0.0188 193.7 1200 0.01883 193.9 1200 0.01883 194 1200 0.01883 194.1 1200 0.01884 194.2 1200 0.01884 194.4 1200 0.01884 194.5 1200 0.01884 194.6 1200 0.01884 194.7 1200 0.01884 194.9 1200 0.01887 195 1200 0.01887 195.1 1200 0.01887 195.2 1200 0.01887 195.4 1200 0.01887 195.5 1200 0.01888 195.6 1200 0.01888 195.7 1200 0.01888 195.9 1200 0.01888 196 1200 0.01888 196.1 1200 0.01888 196.2 1200 0.01888 196.4 1200 0.01888 196.5 1200 0.01888 196.6 1200 0.01888 196.7 1200 0.01888 196.9 1200 0.01889 197 1200 0.0189 197.1 1199 0.0189 197.2 1200 0.01891 197.4 1200 0.01891 197.5 1200 0.01891 197.6 1200 0.01891 197.7 1200 0.01893 197.9 1200 0.01893 198 1200 0.01893 198.1 1200 0.01893 198.2 1200 0.01893 198.3 1200 0.01893 198.5 1200 0.01893 198.6 1200 0.01894 198.7 1200 0.01895 198.8 1200 0.01893 199 1200 0.01894 199.1 1200 0.01895 199.2 1200 0.01896 199.3 1200 0.01896 199.5 1199 0.01898 199.6 1200 0.01898 199.7 1200 0.01895 199.8 1200 0.01895 200 1200 0.01895 200.1 1200 0.01895 200.2 1200 0.01896 200.3 1200 0.01898 200.5 1200 0.01896 200.6 1200 0.01895 200.7 1200 0.01895 200.8 1200 0.01896 201 1200 0.01895 201.1 1200 0.01894 201.2 1200 0.01895 201.3 1200 0.01893 201.5 1200 0.01893 201.6 1200 0.01894 201.7 1200 0.01893 201.8 1200 0.01893 202 1200 0.01893 202.1 1200 0.01893 202.2 1200 0.01893 202.3 1200 0.01893 202.5 1200 0.01893 202.6 1200 0.01893 202.7 1200 0.01893 202.8 1200 0.01893 203 1200 0.01893 203.1 1200 0.01891 203.2 1200 0.01888 203.3 1200 0.01887 203.5 1200 0.01884 203.6 1200 0.01882 203.7 1200 0.01882 203.8 1200 0.0188 204 1200 0.01882 204.1 1200 0.01883 204.2 1200 0.01883 204.3 1200 0.01885 204.5 1200 0.01888 204.6 1200 0.01888 204.7 1200 0.01888 204.8 1200 0.01888 204.9 1200 0.01888 205.1 1200 0.01887 205.2 1200 0.01885 205.3 1200 0.01885 205.4 1200 0.01887 205.6 1200 0.01885 205.7 1200 0.01883 205.8 1200 0.01884 205.9 1200 0.01884 206.1 1200 0.01887 206.2 1200 0.01888 206.3 1200 0.01884 206.4 1200 0.01884 206.6 1200 0.01884 206.7 1200 0.01883 206.8 1200 0.01883 206.9 1200 0.01883 207.1 1200 0.01883 207.2 1200 0.01883 207.3 1200 0.01883 207.4 1200 0.01882 207.6 1200 0.01883 207.7 1200 0.01882 207.8 1200 0.0188 207.9 1200 0.01879 208.1 1200 0.01875 208.2 1200 0.01874 208.3 1200 0.01875 208.4 1200 0.01875 208.6 1200 0.01875 208.7 1200 0.01878 208.8 1200 0.01878 208.9 1200 0.01878 209.1 1200 0.01878 209.2 1200 0.01878 209.3 1200 0.01878 209.4 1200 0.01878 209.6 1200 0.01878 209.7 1200 0.01878 209.8 1200 0.01878 209.9 1200 0.01878 210.1 1200 0.01879 210.2 1200 0.01878 210.3 1200 0.01878 210.4 1200 0.01878 210.6 1200 0.01878 210.7 1200 0.01877 210.8 1200 0.01875 210.9 1200 0.01874 211 1200 0.01873 211.2 1200 0.01875 211.3 1200 0.01875 211.4 1200 0.01875 211.5 1200 0.01877 211.7 1200 0.01877 211.8 1200 0.01877 211.9 1200 0.01878 212 1200 0.01877 212.2 1200 0.01878 212.3 1200 0.01879 212.4 1200 0.01878 212.5 1200 0.01878 212.7 1200 0.01879 212.8 1200 0.01879 212.9 1200 0.0188 213 1200 0.01878 213.2 1200 0.01878 213.3 1200 0.01879 213.4 1200 0.01879 213.5 1200 0.01879 213.7 1200 0.01879 213.8 1200 0.01878 213.9 1200 0.01879 214 1200 0.0188 214.2 1200 0.0188 214.3 1200 0.0188 214.4 1200 0.01879 214.5 1200 0.01878 214.7 1200 0.01878 214.8 1200 0.01878 214.9 1200 0.01878 215 1200 0.01878 215.2 1200 0.01879 215.3 1200 0.0188 215.4 1200 0.01882 215.5 1200 0.01882 215.7 1200 0.01882 215.8 1200 0.01882 215.9 1200 0.01882 216 1200 0.01882 216.2 1200 0.01883 216.3 1200 0.01883 216.4 1200 0.01883 216.5 1200 0.01884 216.7 1200 0.01883 216.8 1200 0.01883 216.9 1200 0.01883 217 1200 0.01884 217.2 1200 0.01884 217.3 1200 0.01885 217.4 1200 0.01885 217.5 1200 0.01884 217.6 1200 0.01882 217.8 1200 0.01879 217.9 1200 0.01878 218 1200 0.01878 218.1 1200 0.01878 218.3 1200 0.01879 218.4 1200 0.01879 218.5 1200 0.0188 218.6 1200 0.0188 218.8 1200 0.01882 218.9 1200 0.01882 219 1199 0.01883 219.1 1200 0.01882 219.3 1200 0.01882 219.4 1200 0.01882 219.5 1200 0.01882 219.6 1200 0.01882 219.8 1200 0.0188 219.9 1200 0.01878 220 1200 0.01878 220.1 1200 0.01875 220.3 1200 0.01874 220.4 1200 0.01875 220.5 1200 0.01877 220.6 1200 0.01877 220.8 1200 0.01878 220.9 1200 0.01878 221 1200 0.01878 221.1 1200 0.01879 221.3 1200 0.01878 221.4 1200 0.01878 221.5 1200 0.01878 221.6 1200 0.01877 221.8 1200 0.01875 221.9 1200 0.01875 222 1200 0.01875 222.1 1200 0.01877 222.3 1200 0.01877 222.4 1200 0.01877 222.5 1200 0.01878 222.6 1200 0.01877 222.8 1200 0.01877 222.9 1200 0.01878 223 1200 0.01878 223.1 1200 0.01875 223.3 1200 0.01875 223.4 1200 0.01874 223.5 1200 0.01873 223.6 1200 0.01873 223.7 1200 0.01873 223.9 1200 0.0187 224 1200 0.0187 224.1 1200 0.01872 224.2 1200 0.01873 224.4 1200 0.01873 224.5 1200 0.01872 224.6 1200 0.01872 224.7 1200 0.0187 224.9 1200 0.0187 225 1200 0.01872 225.1 1200 0.01872 225.2 1200 0.0187 225.4 1200 0.01872 225.5 1200 0.0187 225.6 1200 0.0187 225.7 1200 0.0187 225.9 1200 0.01868 226 1200 0.01868 226.1 1200 0.0187 226.2 1200 0.01869 226.4 1200 0.01868 226.5 1200 0.01868 226.6 1200 0.01868 226.7 1200 0.01868 226.9 1200 0.01868 227 1200 0.01868 227.1 1200 0.01868 227.2 1200 0.01867 227.4 1200 0.01867 227.5 1200 0.01868 227.6 1200 0.01868 227.7 1200 0.01868 227.9 1200 0.01868 228 1200 0.01868 228.1 1200 0.01868 228.2 1200 0.01868 228.4 1200 0.01867 228.5 1200 0.01867 228.6 1200 0.01867 228.7 1200 0.01868 228.9 1200 0.01869 229 1200 0.01868 229.1 1200 0.01868 229.2 1200 0.01868 229.4 1200 0.01868 229.5 1200 0.01867 229.6 1200 0.01868 229.7 1200 0.01867 229.9 1200 0.01868 230 1200 0.01868 230.1 1200 0.01867 230.2 1200 0.01867 230.3 1200 0.01868 230.5 1200 0.01868 230.6 1200 0.01868 230.7 1200 0.0187 230.8 1200 0.0187 231 1200 0.0187 231.1 1200 0.01872 231.2 1200 0.0187 231.3 1200 0.01872 231.5 1200 0.0187 231.6 1200 0.0187 231.7 1200 0.01868 231.8 1200 0.01867 232 1200 0.01868 232.1 1200 0.01868 232.2 1200 0.01868 232.3 1200 0.01867 232.5 1200 0.01868 232.6 1200 0.01868 232.7 1200 0.01868 232.8 1200 0.0187 233 1200 0.0187 233.1 1200 0.0187 233.2 1200 0.01872 233.3 1200 0.0187 233.5 1200 0.01872 233.6 1200 0.01872 233.7 1200 0.01872 233.8 1200 0.01872 234 1200 0.01872 234.1 1200 0.01872 234.2 1200 0.01872 234.3 1200 0.01872 234.5 1200 0.01872 234.6 1200 0.01872 234.7 1200 0.01872 234.8 1200 0.01873 235 1200 0.01875 235.1 1200 0.01875 235.2 1200 0.01875 235.3 1200 0.01877 235.5 1200 0.01877 235.6 1200 0.01878 235.7 1200 0.01879 235.8 1200 0.01878 236 1200 0.01878 236.1 1200 0.01878 236.2 1200 0.01878 236.3 1200 0.01878 236.5 1200 0.0188 236.6 1200 0.0188 236.7 1200 0.0188 236.8 1200 0.01882 236.9 1200 0.01882 237.1 1200 0.01882 237.2 1200 0.01882 237.3 1200 0.01882 237.4 1200 0.01882 237.6 1200 0.01882 237.7 1200 0.01883 237.8 1200 0.01884 237.9 1200 0.01884 238.1 1200 0.01885 238.2 1200 0.01887 238.3 1200 0.01887 238.4 1200 0.01885 238.6 1200 0.01888 238.7 1200 0.01887 238.8 1200 0.01888 238.9 1200 0.01888 239.1 1200 0.01888 239.2 1200 0.01888 239.3 1200 0.01888 239.4 1200 0.01888 239.6 1200 0.01888 239.7 1200 0.01889 239.8 1200 0.0189 239.9 1200 0.01889 240.1 1200 0.01889 240.2 1200 0.0189 240.3 1200 0.0189 240.4 1200 0.01891 240.6 1200 0.01891 240.7 1200 0.01893 240.8 1200 0.01893 240.9 1200 0.01891 241.1 1199 0.01893 241.2 1200 0.01893 241.3 1200 0.01895 241.4 1200 0.01896 241.6 1200 0.01895 241.7 1200 0.01895 241.8 1200 0.01895 241.9 1200 0.01894 242.1 1200 0.01893 242.2 1200 0.01893 242.3 1200 0.01894 242.4 1200 0.01894 242.6 1200 0.01896 242.7 1200 0.01896 242.8 1200 0.01898 242.9 1200 0.01898 243 1200 0.01898 243.2 1200 0.01898 243.3 1200 0.01898 243.4 1200 0.01898 243.5 1200 0.01898 243.7 1200 0.01898 243.8 1200 0.01898 243.9 1200 0.01898 244 1200 0.01898 244.2 1200 0.01898 244.3 1200 0.01898 244.4 1200 0.01898 244.5 1200 0.01896 244.7 1200 0.01896 244.8 1200 0.01894 244.9 1200 0.01894 245 1200 0.01894 245.2 1200 0.01893 245.3 1200 0.01893 245.4 1200 0.01893 245.5 1200 0.01893 245.7 1200 0.01893 245.8 1200 0.01894 245.9 1200 0.01893 246 1200 0.01893 246.2 1200 0.01893 246.3 1200 0.01891 246.4 1200 0.0189 246.5 1200 0.01891 246.7 1200 0.01891 246.8 1200 0.0189 246.9 1200 0.0189 247 1200 0.01888 247.2 1200 0.01888 247.3 1200 0.0189 247.4 1200 0.0189 247.5 1200 0.0189 247.7 1200 0.0189 247.8 1200 0.01888 247.9 1200 0.01888 248 1200 0.01888 248.2 1200 0.01888 248.3 1200 0.01887 248.4 1200 0.01887 248.5 1200 0.01888 248.7 1200 0.01888 248.8 1200 0.01887 248.9 1200 0.01885 249 1200 0.01888 249.2 1200 0.01888 249.3 1200 0.01887 249.4 1200 0.01888 249.5 1200 0.01888 249.6 1200 0.01888 249.8 1200 0.01888 249.9 1200 0.01888 250 1200 0.01888 250.1 1200 0.01887 250.3 1200 0.01885 250.4 1200 0.01885 250.5 1200 0.01887 250.6 1200 0.01884 250.8 1200 0.01884 250.9 1200 0.01884 251 1200 0.01883 251.1 1200 0.01882 251.3 1200 0.0188 251.4 1200 0.01879 251.5 1200 0.01879 251.6 1200 0.01878 251.8 1200 0.01878 251.9 1200 0.01878 252 1200 0.01878 252.1 1200 0.01878 252.3 1200 0.01878 252.4 1200 0.01878 252.5 1200 0.01877 252.6 1200 0.01878 252.8 1200 0.01878 252.9 1200 0.01878 253 1200 0.01878 253.1 1200 0.01879 253.3 1200 0.01878 253.4 1200 0.01879 253.5 1200 0.01879 253.6 1200 0.01879 253.8 1200 0.0188 253.9 1200 0.01878 254 1200 0.01878 254.1 1200 0.01878 254.3 1200 0.01878 254.4 1200 0.01878 254.5 1200 0.01878 254.6 1200 0.01875 254.8 1200 0.01875 254.9 1200 0.01877 255 1200 0.01875 255.1 1200 0.01874 255.3 1200 0.01874 255.4 1200 0.01875 255.5 1200 0.01878 255.6 1200 0.01878 255.7 1200 0.01879 255.9 1200 0.0188 256 1200 0.01879 256.1 1200 0.01878 256.2 1200 0.0188 256.4 1200 0.0188 256.5 1200 0.01879 256.6 1200 0.01879 256.7 1200 0.01878 256.9 1200 0.01878 257 1200 0.01882 257.1 1200 0.01882 257.2 1200 0.01882 257.4 1200 0.01883 257.5 1200 0.01882 257.6 1200 0.01882 257.7 1200 0.01882 257.9 1200 0.01879 258 1200 0.0188 258.1 1200 0.0188 258.2 1200 0.01879 258.4 1200 0.01879 258.5 1200 0.01878 258.6 1200 0.01878 258.7 1200 0.01878 258.9 1200 0.01878 259 1200 0.01879 259.1 1200 0.0188 259.2 1200 0.01878 259.4 1200 0.01878 259.5 1200 0.01878 259.6 1200 0.01878 259.7 1200 0.01879 259.9 1200 0.01879 260 1200 0.01878 260.1 1200 0.01879 260.2 1200 0.01879 260.4 1200 0.0188 260.5 1200 0.01882 260.6 1200 0.01882 260.7 1200 0.01882 260.9 1200 0.01882 261 1200 0.01882 261.1 1200 0.01882 261.2 1200 0.01883 261.4 1200 0.01882 261.5 1200 0.01883 261.6 1200 0.01883 261.7 1200 0.01882 261.9 1200 0.01884 262 1200 0.01884 262.1 1200 0.01884 262.2 1200 0.01884 262.3 1200 0.01883 262.5 1200 0.01883 262.6 1200 0.01884 262.7 1200 0.01884 262.8 1200 0.01884 263 1200 0.01883 263.1 1200 0.01884 263.2 1200 0.01885 263.3 1200 0.01884 263.5 1200 0.01884 263.6 1200 0.01884 263.7 1200 0.01883 263.8 1200 0.01883 264 1200 0.01883 264.1 1200 0.01882 264.2 1200 0.01883 264.3 1200 0.0188 264.5 1200 0.0188 264.6 1199 0.01882 264.7 1200 0.0188 264.8 1200 0.01879 265 1200 0.01879 265.1 1200 0.01879 265.2 1200 0.0188 265.3 1200 0.01882 265.5 1200 0.0188 265.6 1200 0.0188 265.7 1200 0.01879 265.8 1200 0.01878 266 1200 0.01878 266.1 1200 0.01875 266.2 1200 0.01878 266.3 1200 0.01878 266.5 1200 0.01878 266.6 1200 0.01877 266.7 1200 0.01878 266.8 1200 0.01878 267 1200 0.01878 267.1 1200 0.01878 267.2 1200 0.01878 267.3 1200 0.01878 267.5 1200 0.01878 267.6 1200 0.01878 267.7 1200 0.01878 267.8 1200 0.01877 268 1200 0.01877 268.1 1200 0.01874 268.2 1200 0.01874 268.3 1200 0.01874 268.5 1200 0.01873 268.6 1200 0.01873 268.7 1200 0.01873 268.8 1200 0.01873 268.9 1200 0.01873 269.1 1200 0.01872 269.2 1200 0.01872 269.3 1200 0.01873 269.4 1200 0.01872 269.6 1200 0.01872 269.7 1200 0.01872 269.8 1200 0.01872 269.9 1200 0.01872 270.1 1200 0.0187 270.2 1200 0.01872 270.3 1200 0.01873 270.4 1200 0.01872 270.6 1200 0.01872 270.7 1200 0.01873 270.8 1200 0.01872 270.9 1200 0.0187 271.1 1200 0.0187 271.2 1200 0.01872 271.3 1200 0.01874 271.4 1200 0.01872 271.6 1200 0.01872 271.7 1200 0.01873 271.8 1200 0.01873 271.9 1200 0.01873 272.1 1200 0.01873 272.2 1200 0.01872 272.3 1200 0.0187 272.4 1200 0.01869 272.6 1200 0.0187 272.7 1200 0.0187 272.8 1200 0.01869 272.9 1200 0.01868 273.1 1200 0.01868 273.2 1200 0.01868 273.3 1200 0.01869 273.4 1200 0.01869 273.6 1200 0.01868 273.7 1200 0.01868 273.8 1200 0.01868 273.9 1200 0.01868 274.1 1200 0.01869 274.2 1200 0.01869 274.3 1200 0.01869 274.4 1200 0.01872 274.6 1200 0.0187 274.7 1200 0.0187 274.8 1200 0.0187 274.9 1200 0.01868 275 1200 0.01868 275.2 1200 0.01868 275.3 1200 0.0187 275.4 1200 0.0187 275.5 1200 0.01868 275.7 1200 0.01868 275.8 1200 0.01868 275.9 1200 0.01865 276 1200 0.01868 276.2 1200 0.01869 276.3 1200 0.01869 276.4 1200 0.0187 276.5 1200 0.0187 276.7 1200 0.0187 276.8 1200 0.01872 276.9 1200 0.0187 277 1200 0.01869 277.2 1200 0.01869 277.3 1200 0.01868 277.4 1200 0.01868 277.5 1200 0.0187 277.7 1200 0.0187 277.8 1200 0.01873 277.9 1200 0.01873 278 1200 0.01874 278.2 1200 0.01874 278.3 1200 0.01873 278.4 1200 0.01873 278.5 1200 0.01873 278.7 1200 0.0187 278.8 1200 0.01868 278.9 1200 0.01868 279 1200 0.0187 279.2 1200 0.0187 279.3 1200 0.0187 279.4 1200 0.01872 279.5 1200 0.01873 279.7 1200 0.01874 279.8 1200 0.01875 279.9 1200 0.01874 280 1200 0.01873 280.2 1200 0.01874 280.3 1200 0.01875 280.4 1200 0.01875 280.5 1200 0.01875 280.7 1200 0.01875 280.8 1200 0.01874 280.9 1200 0.01875 281 1200 0.01875 281.2 1200 0.01873 281.3 1200 0.01873 281.4 1200 0.01873 281.5 1200 0.01875 281.6 1200 0.01877 281.8 1200 0.01878 281.9 1200 0.0188 282 1200 0.01883 282.1 1200 0.01883 282.3 1200 0.01884 282.4 1200 0.01884 282.5 1200 0.01883 282.6 1200 0.01882 282.8 1200 0.0188 282.9 1200 0.01882 283 1200 0.01882 283.1 1200 0.01882 283.3 1200 0.01882 283.4 1200 0.01883 283.5 1200 0.01883 283.6 1200 0.01884 283.8 1200 0.01885 283.9 1200 0.01885 284 1200 0.01885 284.1 1200 0.01888 284.3 1200 0.01888 284.4 1199 0.01888 284.5 1200 0.0189 284.6 1200 0.0189 284.8 1200 0.01891 284.9 1200 0.01894 285 1200 0.01893 285.1 1200 0.01893 285.3 1200 0.01894 285.4 1200 0.01895 285.5 1200 0.01895 285.6 1200 0.01896 285.8 1200 0.01898 285.9 1200 0.01898 286 1200 0.01895 286.1 1200 0.01895 286.3 1200 0.01895 286.4 1200 0.01894 286.5 1200 0.01894 286.6 1200 0.01893 286.8 1200 0.01893 286.9 1199 0.01894 287 1200 0.01894 287.1 1200 0.01895 287.3 1200 0.01896 287.4 1200 0.01898 287.5 1200 0.01898 287.6 1200 0.019 287.7 1200 0.01899 287.9 1200 0.01898 288 1200 0.01899 288.1 1200 0.01898 288.2 1200 0.01898 288.4 1200 0.01898 288.5 1200 0.01896 288.6 1200 0.01895 288.7 1200 0.01894 288.9 1200 0.01895 289 1200 0.01898 289.1 1200 0.01898 289.2 1200 0.01898 289.4 1200 0.01898 289.5 1200 0.01896 289.6 1200 0.01895 289.7 1200 0.01898 289.9 1200 0.01898 290 1200 0.01898 290.1 1200 0.01901 290.2 1200 0.01903 290.4 1200 0.01905 290.5 1200 0.01905 290.6 1200 0.01904 290.7 1200 0.01903 290.9 1200 0.01901 291 1200 0.019 291.1 1200 0.01901 291.2 1200 0.01901 291.4 1200 0.01903 291.5 1200 0.01904 291.6 1200 0.01903 291.7 1200 0.01901 291.9 1200 0.01899 292 1200 0.01898 292.1 1200 0.01899 292.2 1200 0.019 292.4 1200 0.019 292.5 1200 0.01901 292.6 1200 0.019 292.7 1200 0.019 292.9 1200 0.01901 293 1200 0.01901 293.1 1200 0.019 293.2 1200 0.01898 293.4 1200 0.01895 293.5 1200 0.01895 293.6 1200 0.01898 293.7 1200 0.01898 293.9 1200 0.01898 294 1200 0.01898 294.1 1200 0.01895 294.2 1200 0.01895 294.3 1200 0.01894 294.5 1200 0.01893 294.6 1200 0.01894 294.7 1200 0.01893 294.8 1200 0.01893 295 1200 0.01894 295.1 1200 0.01896 295.2 1200 0.01894 295.3 1200 0.01894 295.5 1200 0.01895 295.6 1200 0.01896 295.7 1200 0.01896 295.8 1200 0.01898 296 1200 0.01895 296.1 1200 0.01893 296.2 1200 0.01893 296.3 1200 0.01895 296.5 1200 0.01893 296.6 1200 0.01891 296.7 1200 0.01891 296.8 1200 0.01891 297 1200 0.0189 297.1 1200 0.0189 297.2 1200 0.0189 297.3 1200 0.01889 297.5 1200 0.01888 297.6 1200 0.01888 297.7 1200 0.01888 297.8 1200 0.01888 298 1200 0.01888 298.1 1200 0.01888 298.2 1200 0.01885 298.3 1200 0.01885 298.5 1200 0.01887 298.6 1200 0.01885 298.7 1200 0.01884 298.8 1200 0.01884 299 1200 0.01883 299.1 1200 0.01883 299.2 1200 0.01883 299.3 1200 0.01883 299.5 1200 0.01883 299.6 1200 0.01883 299.7 1200 0.01883 299.8 1200 0.01883 300 1200 0.01883 300.1 1200 0.01882 300.2 1200 0.0188 300.3 1200 0.01879 300.4 1200 0.01878 300.6 1200 0.01879 300.7 1200 0.0188 300.8 1200 0.01879 300.9 1200 0.01878 301.1 1200 0.01879 301.2 1200 0.01882 301.3 1200 0.0188 301.4 1200 0.01878 301.6 1200 0.0188 301.7 1200 0.0188 301.8 1200 0.0188 301.9 1200 0.01882 302.1 1200 0.0188 302.2 1200 0.01879 302.3 1200 0.0188 302.4 1200 0.0188 302.6 1200 0.01879 302.7 1200 0.01879 302.8 1200 0.0188 302.9 1200 0.01882 303.1 1200 0.01879 303.2 1200 0.01878 303.3 1200 0.01879 303.4 1200 0.01878 303.6 1200 0.01878 303.7 1200 0.01878 303.8 1200 0.01878 303.9 1200 0.01879 304.1 1200 0.01879 304.2 1200 0.01879 304.3 1200 0.01879 304.4 1200 0.0188 304.6 1200 0.01879 304.7 1200 0.01878 304.8 1200 0.01878 304.9 1200 0.01878 305.1 1200 0.01879 305.2 1200 0.0188 305.3 1200 0.0188 305.4 1200 0.0188 305.6 1200 0.01879 305.7 1199 0.01879 305.8 1200 0.0188 305.9 1200 0.0188 306.1 1200 0.01882 306.2 1200 0.01882 306.3 1200 0.01882 306.4 1200 0.01882 306.6 1200 0.01882 306.7 1200 0.01882 306.8 1200 0.01883 306.9 1200 0.01883 307 1200 0.01883 307.2 1200 0.01884 307.3 1200 0.01883 307.4 1200 0.01883 307.5 1200 0.01882 307.7 1200 0.01882 307.8 1200 0.01882 307.9 1200 0.01883 308 1200 0.01884 308.2 1199 0.01884 308.3 1200 0.01883 308.4 1200 0.01883 308.5 1200 0.01883 308.7 1200 0.01884 308.8 1200 0.01884 308.9 1200 0.01884 309 1200 0.01884 309.2 1200 0.01883 309.3 1200 0.01883 309.4 1200 0.01883 309.5 1200 0.01882 309.7 1200 0.01883 309.8 1200 0.01882 309.9 1200 0.01883 310 1200 0.01882 310.2 1200 0.01882 310.3 1200 0.01883 310.4 1200 0.01883 310.5 1200 0.01883 310.7 1200 0.01884 310.8 1200 0.01884 310.9 1200 0.01884 311 1200 0.01884 311.2 1200 0.01884 311.3 1200 0.01884 311.4 1200 0.01884 311.5 1200 0.01884 311.7 1200 0.01883 311.8 1200 0.01884 311.9 1200 0.01884 312 1200 0.01884 312.2 1200 0.01884 312.3 1200 0.01883 312.4 1200 0.01883 312.5 1200 0.01883 312.7 1200 0.01883 312.8 1200 0.01883 312.9 1200 0.01883 313 1200 0.01883 313.2 1200 0.01883 313.3 1200 0.01882 313.4 1200 0.01883 313.5 1200 0.01882 313.6 1200 0.0188 313.8 1200 0.01882 313.9 1200 0.01882 314 1200 0.01879 314.1 1200 0.01879 314.3 1200 0.01879 314.4 1200 0.0188 314.5 1200 0.01879 314.6 1200 0.01879 314.8 1200 0.0188 314.9 1200 0.01879 315 1200 0.01879 315.1 1200 0.01878 315.3 1200 0.01878 315.4 1200 0.01878 315.5 1200 0.01878 315.6 1200 0.01878 315.8 1200 0.01878 315.9 1200 0.01878 316 1200 0.01878 316.1 1200 0.01878 316.3 1200 0.01878 316.4 1200 0.01878 316.5 1200 0.01878 316.6 1200 0.01878 316.8 1200 0.01878 316.9 1200 0.01878 317 1200 0.01877 317.1 1200 0.01875 317.3 1200 0.01875 317.4 1200 0.01875 317.5 1200 0.01875 317.6 1200 0.01874 317.8 1200 0.01873 317.9 1200 0.01872 318 1200 0.01872 318.1 1200 0.01872 318.3 1200 0.01873 318.4 1200 0.0187 318.5 1200 0.01872 318.6 1200 0.01873 318.8 1200 0.01873 318.9 1200 0.01873 319 1200 0.01873 319.1 1200 0.01873 319.3 1200 0.01873 319.4 1200 0.01873 319.5 1200 0.01872 319.6 1200 0.01872 319.7 1200 0.01873 319.9 1200 0.0187 320 1200 0.0187 320.1 1200 0.01872 320.2 1200 0.01873 320.4 1200 0.01872 320.5 1200 0.0187 320.6 1200 0.0187 320.7 1200 0.01872 320.9 1200 0.0187 321 1200 0.01869 321.1 1200 0.0187 321.2 1200 0.0187 321.4 1200 0.0187 321.5 1200 0.0187 321.6 1200 0.0187 321.7 1200 0.01872 321.9 1200 0.0187 322 1200 0.01869 322.1 1200 0.0187 322.2 1200 0.0187 322.4 1200 0.0187 322.5 1200 0.01872 322.6 1200 0.0187 322.7 1200 0.01872 322.9 1200 0.01872 323 1200 0.0187 323.1 1200 0.01869 323.2 1200 0.01869 323.4 1200 0.01868 323.5 1200 0.01868 323.6 1200 0.01868 323.7 1200 0.01868 323.9 1200 0.01868 324 1200 0.01867 324.1 1200 0.01868 324.2 1200 0.01868 324.4 1200 0.01868 324.5 1200 0.01868 324.6 1200 0.01868 324.7 1200 0.01868 324.9 1200 0.01868 325 1200 0.01868 325.1 1200 0.01869 325.2 1200 0.0187 325.4 1200 0.0187 325.5 1200 0.0187 325.6 1200 0.01872 325.7 1200 0.0187 325.9 1200 0.01872 326 1200 0.01872 326.1 1200 0.01872 326.2 1200 0.01872 326.3 1200 0.01872 326.5 1200 0.0187 326.6 1200 0.01868 326.7 1200 0.0187 326.8 1200 0.0187 327 1200 0.01872 327.1 1200 0.0187 327.2 1200 0.01872 327.3 1200 0.01872 327.5 1200 0.01872 327.6 1200 0.01872 327.7 1200 0.01873 327.8 1200 0.01872 328 1200 0.01873 328.1 1200 0.01875 328.2 1200 0.01873 328.3 1200 0.01873 328.5 1200 0.01873 328.6 1200 0.01873 328.7 1200 0.01873 328.8 1200 0.01872 329 1200 0.01872 329.1 1200 0.01873 329.2 1200 0.01874 329.3 1200 0.01875 329.5 1200 0.01875 329.6 1200 0.01875 329.7 1200 0.01873 329.8 1200 0.01874 330 1200 0.01875 330.1 1200 0.01875 330.2 1200 0.01874 330.3 1200 0.01875 330.5 1200 0.01878 330.6 1200 0.01878 330.7 1200 0.01879 330.8 1200 0.01879 331 1200 0.01878 331.1 1200 0.01879 331.2 1200 0.0188 331.3 1200 0.0188 331.5 1200 0.01882 331.6 1200 0.01883 331.7 1200 0.01884 331.8 1200 0.01884 332 1200 0.01883 332.1 1200 0.01883 332.2 1200 0.01883 332.3 1200 0.01884 332.4 1200 0.01884 332.6 1200 0.01887 332.7 1200 0.01887 332.8 1200 0.01887 332.9 1200 0.01888 333.1 1200 0.01887 333.2 1200 0.01888 333.3 1200 0.01888 333.4 1200 0.01888 333.6 1200 0.01888 333.7 1200 0.01888 333.8 1199 0.01888 333.9 1200 0.01888 334.1 1200 0.01888 334.2 1200 0.01888 334.3 1200 0.0189 334.4 1200 0.01889 334.6 1200 0.01888 334.7 1200 0.01889 334.8 1200 0.0189 334.9 1200 0.0189 335.1 1200 0.01891 335.2 1200 0.0189 335.3 1200 0.01893 335.4 1200 0.01891 335.6 1200 0.01893 335.7 1200 0.01893 335.8 1200 0.01891 335.9 1200 0.01893 336.1 1200 0.01895 336.2 1200 0.01895 336.3 1200 0.01896 336.4 1200 0.01896 336.6 1200 0.01898 336.7 1200 0.01898 336.8 1200 0.01898 336.9 1200 0.01894 337.1 1200 0.01894 337.2 1200 0.01893 337.3 1200 0.01893 337.4 1200 0.01898 337.6 1200 0.019 337.7 1200 0.01903 337.8 1200 0.01903 337.9 1200 0.01901 338.1 1200 0.01901 338.2 1200 0.01898 338.3 1200 0.01898 338.4 1200 0.01898 338.6 1200 0.01898 338.7 1200 0.01898 338.8 1200 0.01898 338.9 1200 0.01899 339 1200 0.01901 339.2 1200 0.01903 339.3 1200 0.01903 339.4 1200 0.01903 339.5 1200 0.01901 339.7 1200 0.01903 339.8 1200 0.01903 339.9 1200 0.01904 340 1200 0.01905 340.2 1200 0.01905 340.3 1200 0.01905 340.4 1200 0.01905 340.5 1200 0.01905 340.7 1200 0.01905 340.8 1200 0.01905 340.9 1200 0.01904 341 1200 0.01904 341.2 1200 0.01904 341.3 1200 0.01904 341.4 1200 0.01903 341.5 1200 0.01903 341.7 1200 0.01903 341.8 1200 0.01903 341.9 1200 0.01903 342 1200 0.01904 342.2 1200 0.01904 342.3 1200 0.01901 342.4 1200 0.019 342.5 1200 0.01901 342.7 1200 0.01899 342.8 1200 0.01899 342.9 1200 0.01899 343 1200 0.019 343.2 1200 0.01901 343.3 1200 0.019 343.4 1200 0.01899 343.5 1200 0.01899 343.7 1200 0.01898 343.8 1200 0.01898 343.9 1200 0.01898 344 1200 0.01896 344.2 1200 0.01895 344.3 1200 0.01895 344.4 1200 0.01894 344.5 1200 0.01895 344.7 1200 0.01896 344.8 1200 0.01896 344.9 1200 0.01898 345 1200 0.01898 345.2 1200 0.01896 345.3 1200 0.01895 345.4 1200 0.01895 345.5 1200 0.01895 345.6 1200 0.01894 345.8 1200 0.01893 345.9 1200 0.01893 346 1200 0.01891 346.1 1200 0.0189 346.3 1200 0.01893 346.4 1200 0.01891 346.5 1200 0.01893 346.6 1200 0.01893 346.8 1200 0.01893 346.9 1200 0.01891 347 1200 0.0189 347.1 1200 0.0189 347.3 1200 0.01891 347.4 1200 0.0189 347.5 1200 0.0189 347.6 1200 0.0189 347.8 1200 0.01888 347.9 1200 0.01888 348 1200 0.01888 348.1 1200 0.01888 348.3 1200 0.01888 348.4 1200 0.01887 348.5 1200 0.01885 348.6 1200 0.01887 348.8 1200 0.01885 348.9 1200 0.01885 349 1200 0.01884 349.1 1200 0.01884 349.3 1200 0.01883 349.4 1200 0.01883 349.5 1200 0.01883 349.6 1200 0.01884 349.8 1200 0.01884 349.9 1200 0.01884 350 1200 0.01884 350.1 1200 0.01883 350.3 1200 0.01883 350.4 1200 0.01884 350.5 1200 0.01884 350.6 1200 0.01884 350.8 1200 0.01883 350.9 1200 0.01882 351 1200 0.01882 351.1 1200 0.01882 351.3 1200 0.01882 351.4 1200 0.01883 351.5 1200 0.01882 351.6 1200 0.01882 351.7 1200 0.01883 351.9 1200 0.01882 352 1200 0.01882 352.1 1200 0.01883 352.2 1200 0.01882 352.4 1200 0.01883 352.5 1200 0.01883 352.6 1200 0.01883 352.7 1200 0.01883 352.9 1200 0.01882 353 1200 0.01883 353.1 1200 0.01883 353.2 1200 0.01882 353.4 1200 0.01883 353.5 1200 0.01884 353.6 1200 0.01884 353.7 1200 0.01884 353.9 1200 0.01883 354 1200 0.01883 354.1 1200 0.01883 354.2 1200 0.01882 354.4 1200 0.0188 354.5 1200 0.01882 354.6 1200 0.01882 354.7 1200 0.01882 354.9 1200 0.01882 355 1200 0.01882 355.1 1200 0.01882 355.2 1200 0.01882 355.4 1200 0.01882 355.5 1200 0.01883 355.6 1200 0.01882 355.7 1200 0.01882 355.9 1200 0.01883 356 1200 0.01883 356.1 1200 0.01883 356.2 1200 0.01884 356.4 1200 0.01884 356.5 1200 0.01884 356.6 1200 0.01884 356.7 1200 0.01884 356.9 1200 0.01884 357 1200 0.01884 357.1 1200 0.01883 357.2 1200 0.01884 357.4 1200 0.01883 357.5 1200 0.01884 357.6 1200 0.01884 357.7 1200 0.01884 357.9 1200 0.01883 358 1200 0.01883 358.1 1200 0.01884 358.2 1200 0.01885 358.3 1200 0.01884 358.5 1200 0.01883 358.6 1200 0.01884 358.7 1200 0.01883 358.8 1200 0.01884 359 1200 0.01884 359.1 1200 0.01884 359.2 1200 0.01885 359.3 1200 0.01884 359.5 1200 0.01884 359.6 1200 0.01884 359.7 1200 0.01883 359.8 1200 0.01884 360 1200 0.01885 360.1 1200 0.01885 360.2 1200 0.01885 360.3 1200 0.01888 360.5 1200 0.01888 360.6 1200 0.01888 360.7 1200 0.01887 360.8 1200 0.01885 361 1200 0.01885 361.1 1200 0.01883 361.2 1200 0.01884 361.3 1200 0.01884 361.5 1200 0.01885 361.6 1200 0.01885 361.7 1200 0.01887 361.8 1200 0.01887 362 1200 0.01887 362.1 1200 0.01884 362.2 1200 0.01883 362.3 1200 0.01883 362.5 1200 0.01882 362.6 1200 0.01883 362.7 1200 0.01884 362.8 1200 0.01883 363 1200 0.01884 363.1 1200 0.01884 363.2 1200 0.01884 363.3 1200 0.01884 363.5 1200 0.01883 363.6 1200 0.01883 363.7 1200 0.01884 363.8 1200 0.01884 364 1200 0.01884 364.1 1200 0.01884 364.2 1200 0.01883 364.3 1200 0.01883 364.4 1200 0.01882 364.6 1200 0.0188 364.7 1200 0.0188 364.8 1200 0.01878 364.9 1200 0.01879 365.1 1200 0.01882 365.2 1200 0.0188 365.3 1200 0.0188 365.4 1200 0.0188 365.6 1200 0.01879 365.7 1200 0.0188 365.8 1200 0.0188 365.9 1200 0.0188 366.1 1200 0.01883 366.2 1200 0.01882 366.3 1200 0.01882 366.4 1200 0.01883 366.6 1200 0.01882 366.7 1200 0.01883 366.8 1200 0.01882 366.9 1200 0.0188 367.1 1200 0.0188 367.2 1200 0.01878 367.3 1200 0.01878 367.4 1200 0.01878 367.6 1200 0.01878 367.7 1200 0.01878 367.8 1200 0.01877 367.9 1200 0.01875 368.1 1200 0.01875 368.2 1200 0.01875 368.3 1200 0.01877 368.4 1200 0.01878 368.6 1200 0.01875 368.7 1200 0.01874 368.8 1200 0.01874 368.9 1200 0.01873 369.1 1200 0.01873 369.2 1200 0.01873 369.3 1200 0.01873 369.4 1200 0.01873 369.6 1200 0.01872 369.7 1200 0.0187 369.8 1200 0.0187 369.9 1200 0.0187 370.1 1200 0.0187 370.2 1200 0.01869 370.3 1200 0.01868 370.4 1200 0.01868 370.6 1200 0.01868 370.7 1200 0.01868 370.8 1200 0.01868 370.9 1200 0.01868 371 1200 0.01868 371.2 1200 0.01869 371.3 1200 0.0187 371.4 1200 0.0187 371.5 1200 0.0187 371.7 1200 0.0187 371.8 1200 0.01872 371.9 1200 0.0187 372 1200 0.0187 372.2 1200 0.0187 372.3 1200 0.0187 372.4 1200 0.0187 372.5 1200 0.01869 372.7 1200 0.01868 372.8 1200 0.01868 372.9 1200 0.01868 373 1200 0.01868 373.2 1200 0.01868 373.3 1200 0.01868 373.4 1200 0.01868 373.5 1200 0.01868 373.7 1200 0.01867 373.8 1200 0.01868 373.9 1200 0.01868 374 1200 0.01868 374.2 1200 0.01868 374.3 1200 0.01868 374.4 1200 0.01867 374.5 1200 0.01868 374.7 1200 0.01864 374.8 1199 0.01865 374.9 1199 0.01865 375 1197 0.01865 375.2 1197 0.01864 375.3 1196 0.0186 375.4 1194 0.01859 375.5 1190 0.01856 375.7 1176 0.01853 375.8 1175 0.01856 375.9 1176 0.01858 376 1176 0.01857 376.2 1176 0.01858 376.3 1175 0.01853 376.4 1173 0.01851 376.5 1172 0.01847 376.7 1171 0.01843 376.8 1169 0.01839 376.9 1167 0.01836 377 1165 0.01832 377.1 1164 0.01829 377.3 1162 0.01825 377.4 1161 0.01821 377.5 1159 0.01816 377.6 1157 0.01811 377.8 1154 0.01805 377.9 1153 0.01802 378 1151 0.01797 378.1 1149 0.01794 378.3 1147 0.01789 378.4 1145 0.01784 378.5 1143 0.01779 378.6 1141 0.01772 378.8 1138 0.01769 378.9 1136 0.01764 379 1134 0.01758 379.1 1132 0.01751 379.3 1129 0.01746 379.4 1128 0.0174 379.5 1126 0.01735 379.6 1123 0.01729 379.8 1122 0.01724 379.9 1119 0.01719 380 1117 0.01713 380.1 1115 0.01708 380.3 1113 0.01703 380.4 1111 0.01698 380.5 1109 0.01694 380.6 1108 0.01689 380.8 1106 0.01684 380.9 1104 0.01679 381 1103 0.01676 381.1 1101 0.0167 381.3 1100 0.01667 381.4 1097 0.0166 381.5 1097 0.01655 381.6 1094 0.01652 381.8 1093 0.01651 381.9 1092 0.0165 382 1090 0.0165 382.1 1087 0.01642 382.3 1082 0.01637 382.4 1079 0.01634 382.5 1076 0.0163 382.6 1072 0.01627 382.8 1070 0.01625 382.9 1067 0.0162 383 1065 0.01617 383.1 1062 0.01615 383.3 1061 0.01613 383.4 1058 0.01606 383.5 1057 0.01603 383.6 1054 0.016 383.7 1051 0.01598 383.9 1051 0.01591 384 1046 0.01588 384.1 1048 0.01583 384.2 1041 0.01579 384.4 1043 0.01573 384.5 1039 0.01568 384.6 1037 0.01567 384.7 1039 0.01564 384.9 1031 0.0156 385 1035 0.01555 385.1 1028 0.01549 385.2 1029 0.01546 385.4 1026 0.01543 385.5 1022 0.01541 385.6 1026 0.01541 385.7 1017 0.01536 385.9 1021 0.01531 386 1014 0.01528 386.1 1014 0.01527 386.2 1015 0.01523 386.4 1008 0.0152 386.5 1012 0.01515 386.6 1003 0.01508 386.7 1005 0.01503 386.9 1003 0.01497 387 1000 0.01493 387.1 1003 0.01489 387.2 993 0.01486 387.4 997 0.01482 387.5 990 0.01476 387.6 990 0.01471 387.7 990 0.01467 387.9 984 0.01464 388 989 0.01459 388.1 979 0.01454 388.2 983 0.01451 388.4 978 0.01448 388.5 975 0.01444 388.6 978 0.01441 388.7 968 0.01439 388.9 975 0.01436 389 967 0.01429 389.1 968 0.01424 389.2 965 0.01422 389.4 961 0.01418 389.5 965 0.01413 389.6 954 0.01408 389.7 961 0.01405 389.9 952 0.01402 390 954 0.01396 390.1 951 0.01392 390.2 947 0.01387 390.3 950 0.01383 390.5 940 0.01382 390.6 947 0.01379 390.7 937 0.01376 390.8 940 0.01372 391 936 0.01368 391.1 932 0.01363 391.2 936 0.01356 391.3 927 0.0135 391.5 932 0.01346 391.6 923 0.01341 391.7 925 0.01337 391.8 922 0.01334 392 918 0.0133 392.1 922 0.01327 392.2 912 0.01326 392.3 918 0.01322 392.5 909 0.0132 392.6 912 0.01315 392.7 907 0.0131 392.8 904 0.01305 393 906 0.01299 393.1 898 0.01293 393.2 904 0.01289 393.3 893 0.01283 393.5 900 0.01278 393.6 892 0.01276 393.7 893 0.01275 393.8 892 0.0127 394 886 0.0127 394.1 890 0.01267 394.2 880 0.01264 394.3 886 0.01257 394.5 878 0.0125 394.6 879 0.01244 394.7 876 0.01239 394.8 872 0.01233 395 875 0.01228 395.1 866 0.01221 395.2 873 0.01216 395.3 862 0.0121 395.5 868 0.01206 395.6 860 0.01201 395.7 861 0.01197 395.8 859 0.01193 396 854 0.01188 396.1 857 0.01183 396.2 848 0.01179 396.3 855 0.01175 396.4 844 0.0117 396.6 851 0.01166 396.7 843 0.01162 396.8 844 0.01159 396.9 840 0.01154 397.1 838 0.01149 397.2 839 0.01146 397.3 831 0.01143 397.4 836 0.01139 397.6 827 0.01134 397.7 832 0.01129 397.8 824 0.01125 397.9 827 0.0112 398.1 821 0.01115 398.2 820 0.01112 398.3 819 0.01108 398.4 813 0.01102 398.6 817 0.01098 398.7 809 0.01093 398.8 814 0.01088 398.9 806 0.01086 399.1 809 0.01083 399.2 803 0.01078 399.3 803 0.01073 399.4 801 0.01068 399.6 801 0.01064 399.7 801 0.0106 399.8 795 0.01055 399.9 799 0.01051 400.1 793 0.01046 400.2 792 0.01045 400.3 790 0.01041 400.4 787 0.01036 400.6 786 0.01032 400.7 782 0.01025 400.8 783 0.01021 400.9 780 0.01017 401.1 779 0.01011 401.2 775 0.01009 401.3 775 0.01005 401.4 773 0.009987 401.6 769 0.009925 401.7 768 0.009901 401.8 767 0.009851 401.9 765 0.009801 402.1 762 0.009764 402.2 761 0.009727 402.3 759 0.00969 402.4 757 0.00964 402.6 756 0.009591 402.7 753 0.009529 402.8 750 0.009504 402.9 749 0.009454 403 746 0.009405 403.2 744 0.009355 403.3 743 0.009293 403.4 740 0.009219 403.5 739 0.009157 403.7 736 0.009107 403.8 734 0.009058 403.9 732 0.009008 404 729 0.008971 404.2 728 0.008934 404.3 726 0.008872 404.4 723 0.008822 404.5 721 0.008772 404.7 719 0.008735 404.8 718 0.008661 404.9 715 0.008611 405 714 0.008586 405.2 711 0.008549 405.3 710 0.008487 405.4 707 0.00845 405.5 706 0.008413 405.7 703 0.008388 405.8 703 0.008301 405.9 700 0.008239 406 698 0.008165 406.2 694 0.00814 406.3 694 0.00809 406.4 691 0.008041 406.5 690 0.007991 406.7 687 0.007966 406.8 685 0.007904 406.9 684 0.007867 407 682 0.007818 407.2 679 0.007793 407.3 678 0.007706 407.4 675 0.007656 407.5 674 0.007619 407.7 671 0.007582 407.8 670 0.007545 407.9 668 0.007508 408 667 0.007446 408.2 664 0.007396 408.3 662 0.007371 408.4 660 0.007297 408.5 658 0.007222 408.7 656 0.007173 408.8 654 0.007123 408.9 652 0.007074 409 650 0.007024 409.1 647 0.006974 409.3 645 0.006937 409.4 643 0.0069 409.5 642 0.006851 409.6 639 0.006813 409.8 637 0.006764 409.9 635 0.006702 410 634 0.006665 410.1 631 0.006603 410.3 629 0.006553 410.4 628 0.006503 410.5 625 0.006454 410.6 623 0.006379 410.8 621 0.006342 410.9 619 0.006317 411 617 0.006305 411.1 615 0.006243 411.3 614 0.006206 411.4 611 0.006156 411.5 609 0.006094 411.6 607 0.006057 411.8 604 0.00602 411.9 604 0.005958 412 601 0.005896 412.1 601 0.005846 412.3 598 0.005809 412.4 596 0.005747 412.5 593 0.00571 412.6 592 0.00566 412.8 590 0.005623 412.9 588 0.005586 413 585 0.005536 413.1 584 0.005487 413.3 582 0.005449 413.4 579 0.0054 413.5 578 0.005338 413.6 576 0.005288 413.8 574 0.005226 413.9 571 0.005164 414 569 0.005115 414.1 568 0.005065 414.3 565 0.005028 414.4 564 0.004978 414.5 562 0.004941 414.6 560 0.004891 414.8 558 0.004842 414.9 556 0.004792 415 554 0.004755 415.1 551 0.004718 415.3 549 0.004681 415.4 547 0.004643 415.5 546 0.004594 415.6 543 0.004557 415.7 542 0.004507 415.9 540 0.00447 416 537 0.004395 416.1 535 0.004346 416.2 534 0.004284 416.4 532 0.004234 416.5 530 0.004185 416.6 528 0.004135 416.7 526 0.004086 416.9 524 0.004048 417 521 0.004011 417.1 520 0.003974 417.2 518 0.003924 417.4 515 0.003887 417.5 514 0.003825 417.6 512 0.003788 417.7 510 0.003751 417.9 508 0.003701 418 506 0.003652 418.1 504 0.003614 418.2 503 0.003552 418.4 500 0.003503 418.5 499 0.003441 418.6 496 0.003379 418.7 494 0.003329 418.9 492 0.00328 419 490 0.00323 419.1 489 0.003205 419.2 486 0.003156 419.4 484 0.003106 419.5 482 0.003069 419.6 480 0.003007 419.7 478 0.002957 419.9 476 0.002908 420 474 0.002858 420.1 472 0.002808 420.2 470 0.002759 420.4 468 0.002709 420.5 466 0.002672 420.6 464 0.002635 420.7 462 0.002573 420.9 460 0.002523 421 459 0.002486 421.1 456 0.002436 421.2 454 0.002387 421.4 453 0.002312 421.5 449 0.002238 421.6 449 0.002176 421.7 446 0.002126 421.9 444 0.002064 422 442 0.002027 422.1 440 0.001965 422.2 438 0.001916 422.3 437 0.001866 422.5 435 0.001816 422.6 433 0.001754 422.7 431 0.001717 422.8 429 0.001668 423 428 0.00163 423.1 425 0.001556 423.2 423 0.001494 423.3 421 0.00142 423.5 419 0.001358 423.6 417 0.001296 423.7 415 0.001221 423.8 413 0.001147 424 410 0.001085 424.1 409 0.001048 424.2 406 0.001011 424.3 404 0.0009609 424.5 403 0.0009113 424.6 401 0.0008493 424.7 399 0.0007997 424.8 396 0.0007377 425 395 0.0006881 425.1 393 0.000651 425.2 390 0.000589 425.3 388 0.0005394 425.5 387 0.0004774 425.6 384 0.0004402 425.7 381 0.0003782 425.8 381 0.0003286 426 378 0.0002666 426.1 377 0.000217 426.2 374 0.0001674 426.3 373 0.0001302 426.5 370 8.059e-05 426.6 368 5.58e-05 426.7 367 6.2e-06 426.8 365 6.2e-06 427 363 -1.86e-05 427.1 360 -5.58e-05 427.2 359 -0.0001178 427.3 356 -0.0001674 427.5 355 -0.0002046 427.6 353 -0.0002542 427.7 351 -0.0003162 427.8 349 -0.0003658 428 347 -0.0004154 428.1 345 -0.0004526 428.2 343 -0.0005146 428.3 342 -0.0005642 428.4 340 -0.000589 428.6 338 -0.0006014 428.7 336 -0.0006634 428.8 335 -0.0006758 428.9 334 -0.0007129 429.1 332 -0.0007253 429.2 331 -0.0007501 429.3 329 -0.0007873 429.4 328 -0.0008121 429.6 326 -0.0008245 429.7 324 -0.0008245 429.8 323 -0.0008245 429.9 322 -0.0008245 430.1 320 -0.0008245 430.2 319 -0.0008245 430.3 318 -0.0008245 430.4 317 -0.0007997 430.6 315 -0.0007625 430.7 313 -0.0007377 430.8 312 -0.0006881 430.9 310 -0.000651 431.1 309 -0.0006014 431.2 306 -0.000527 431.3 306 -0.0004402 431.4 302 -0.0003782 431.6 301 -0.0002914 431.7 299 -0.000217 431.8 298 -0.0001302 431.9 296 -4.34e-05 432.1 295 6.2e-06 432.2 293 5.58e-05 432.3 291 0.000155 432.4 289 0.0002542 432.6 288 0.0003782 432.7 286 0.0004774 432.8 285 0.000589 432.9 284 0.0007005 433.1 281 0.0008245 433.2 279 0.0009113 433.3 278 0.001011 433.4 277 0.001085 433.6 274 0.001184 433.7 274 0.001259 433.8 271 0.001345 433.9 270 0.001395 434.1 268 0.001494 434.2 267 0.001568 434.3 264 0.00163 434.4 262 0.001692 434.6 260 0.001767 434.7 259 0.001816 434.8 256 0.001866 434.9 255 0.001916 435 252 0.001978 435.2 251 0.002015 435.3 248 0.002064 435.4 246 0.002102 435.5 245 0.002139 435.7 242 0.002164 435.8 242 0.002188 435.9 238 0.002226 436 238 0.002238 436.2 235 0.00225 436.3 234 0.002263 436.4 231 0.002263 436.5 229 0.002275 436.7 227 0.002275 436.8 226 0.002275 436.9 224 0.002288 437 221 0.002288 437.2 220 0.002312 437.3 217 0.002325 437.4 215 0.00235 437.5 214 0.002362 437.7 212 0.002362 437.8 209 0.002374 437.9 207 0.002374 438 206 0.002362 438.2 204 0.002362 438.3 202 0.00235 438.4 201 0.00235 438.5 199 0.00235 438.7 196 0.00235 438.8 195 0.00235 438.9 193 0.002337 439 191 0.002325 439.2 189 0.002312 439.3 187 0.002312 439.4 185 0.002288 439.5 184 0.002275 439.7 181 0.00225 439.8 179 0.002238 439.9 177 0.002238 440 176 0.002238 440.2 174 0.002226 440.3 173 0.002213 440.4 171 0.002213 440.5 168 0.002201 440.7 166 0.002188 440.8 165 0.002164 440.9 163 0.002164 441 161 0.002151 441.1 159 0.002139 441.3 157 0.002126 441.4 156 0.002114 441.5 154 0.002102 441.6 152 0.002089 441.8 150 0.002064 441.9 149 0.00204 442 147 0.00204 442.1 146 0.00204 442.3 144 0.002015 442.4 142 0.00199 442.5 141 0.001965 442.6 139 0.001928 442.8 138 0.001916 442.9 136 0.001916 443 135 0.001916 443.1 134 0.001916 443.3 132 0.001891 443.4 131 0.001866 443.5 129 0.001841 443.6 127 0.001816 443.8 127 0.001816 443.9 126 0.001816 444 123 0.001816 444.1 123 0.001804 444.3 121 0.001779 444.4 120 0.001767 444.5 118 0.001767 444.6 118 0.001754 444.8 116 0.001742 444.9 116 0.001742 445 114 0.00173 445.1 113 0.001717 445.3 112 0.001692 445.4 111 0.001668 445.5 109 0.001668 445.6 109 0.001668 445.8 109 0.001692 445.9 106 0.001692 446 106 0.001668 446.1 106 0.001668 446.3 104 0.001643 446.4 103 0.001618 446.5 102 0.001618 446.6 101 0.001606 446.8 100 0.001593 446.9 99 0.001581 447 98 0.001568 447.1 98 0.001556 447.3 96 0.001556 447.4 96 0.001556 447.5 95 0.001568 447.6 94 0.001556 447.7 93 0.001556 447.9 93 0.001544 448 91 0.001531 448.1 91 0.001519 448.2 91 0.001519 448.4 90 0.001519 448.5 89 0.001519 448.6 88 0.001506 448.7 88 0.001506 448.9 87 0.001482 449 87 0.001469 449.1 85 0.001457 449.2 84 0.001432 449.4 84 0.001432 449.5 84 0.001432 449.6 83 0.00142 449.7 82 0.001395 449.9 81 0.001382 450 81 0.00137 450.1 81 0.001358 450.2 80 0.001345 450.4 79 0.001345 450.5 79 0.001345 450.6 77 0.001333 450.7 77 0.001333 450.9 77 0.001321 451 77 0.001308 451.1 76 0.001283 451.2 75 0.001271 451.4 74 0.001271 451.5 74 0.001259 451.6 73 0.001246 451.7 73 0.001234 451.9 73 0.001221 452 73 0.001221 452.1 72 0.001221 452.2 71 0.001221 452.4 71 0.001221 452.5 70 0.001221 452.6 70 0.001209 452.7 69 0.001197 452.9 68 0.001197 453 68 0.001172 453.1 68 0.001159 453.2 68 0.001159 453.4 67 0.001172 453.5 66 0.001159 453.6 66 0.001159 453.7 66 0.001147 453.8 65 0.001135 454 65 0.001147 454.1 65 0.001122 454.2 65 0.001122 454.3 64 0.00111 454.5 63 0.001085 454.6 63 0.001073 454.7 63 0.001073 454.8 63 0.001073 455 62 0.001073 455.1 62 0.001073 455.2 62 0.001073 455.3 61 0.001073 455.5 61 0.00106 455.6 60 0.001048 455.7 60 0.001048 455.8 59 0.001048 456 59 0.001023 456.1 59 0.0009981 456.2 59 0.0009981 456.3 59 0.0009857 456.5 59 0.0009857 456.6 58 0.0009733 456.7 57 0.0009609 456.8 57 0.0009485 457 56 0.0009609 457.1 56 0.0009609 457.2 56 0.0009733 457.3 55 0.0009609 457.5 55 0.0009485 457.6 55 0.0009361 457.7 55 0.0009361 457.8 55 0.0009237 458 55 0.0009113 458.1 55 0.0008989 458.2 54 0.0008865 458.3 54 0.0008741 458.5 54 0.0008741 458.6 53 0.0008741 458.7 52 0.0008741 458.8 53 0.0008741 459 52 0.0008741 459.1 52 0.0008617 459.2 52 0.0008493 459.3 52 0.0008493 459.5 52 0.0008617 459.6 51 0.0008493 459.7 51 0.0008369 459.8 51 0.0008493 460 50 0.0008493 460.1 50 0.0008369 460.2 49 0.0008369 460.3 49 0.0008369 460.4 49 0.0008245 460.6 49 0.0008245 460.7 49 0.0008245 460.8 48 0.0008245 460.9 48 0.0008245 461.1 48 0.0008245 461.2 48 0.0008121 461.3 48 0.0007997 461.4 48 0.0007997 461.6 48 0.0007749 461.7 48 0.0007749 461.8 47 0.0007749 461.9 46 0.0007749 462.1 46 0.0007749 462.2 46 0.0007625 462.3 46 0.0007749 462.4 46 0.0007625 462.6 46 0.0007625 462.7 46 0.0007749 462.8 46 0.0007625 462.9 45 0.0007625 463.1 45 0.0007625 463.2 45 0.0007625 463.3 45 0.0007749 463.4 45 0.0007625 463.6 45 0.0007501 463.7 44 0.0007377 463.8 44 0.0007501 463.9 43 0.0007501 464.1 43 0.0007377 464.2 43 0.0007253 464.3 43 0.0007253 464.4 43 0.0007253 464.6 43 0.0007253 464.7 43 0.0007129 464.8 42 0.0007253 464.9 42 0.0007253 465.1 42 0.0007253 465.2 41 0.0007253 465.3 41 0.0007253 465.4 41 0.0007253 465.6 41 0.0007253 465.7 41 0.0007253 465.8 41 0.0007253 465.9 41 0.0007129 466.1 41 0.0007129 466.2 40 0.0007129 466.3 41 0.0007253 466.4 40 0.0007129 466.6 40 0.0007129 466.7 40 0.0007253 466.8 40 0.0007129 466.9 40 0.0007129 467 40 0.0007129 467.2 40 0.0007253 467.3 39 0.0007129 467.4 38 0.0007005 467.5 39 0.0006881 467.7 38 0.0007005 467.8 38 0.0007005 467.9 38 0.0007005 468 38 0.0007005 468.2 38 0.0006881 468.3 38 0.0006881 468.4 37 0.0007005 468.5 38 0.0007005 468.7 38 0.0007005 468.8 37 0.0007005 468.9 37 0.0006881 469 37 0.0006758 469.2 37 0.0006758 469.3 37 0.0006758 469.4 37 0.0006881 469.5 37 0.0006758 469.7 37 0.0006758 469.8 37 0.0006758 469.9 36 0.0006758 470 36 0.0006758 470.2 36 0.0006634 470.3 36 0.0006634 470.4 36 0.0006634 470.5 35 0.0006634 470.7 35 0.0006634 470.8 35 0.0006634 470.9 34 0.0006634 471 35 0.0006634 471.2 35 0.0006634 471.3 34 0.0006634 471.4 34 0.0006634 471.5 34 0.0006634 471.7 34 0.0006634 471.8 34 0.0006634 471.9 34 0.0006634 472 34 0.000651 472.2 34 0.000651 472.3 34 0.000651 472.4 34 0.000651 472.5 34 0.000651 472.7 34 0.000651 472.8 34 0.0006634 472.9 34 0.000651 473 33 0.000651 473.1 34 0.0006386 473.3 33 0.000651 473.4 33 0.000651 473.5 32 0.000651 473.6 32 0.000651 473.8 32 0.000651 473.9 32 0.0006386 474 32 0.0006262 474.1 32 0.0006262 474.3 32 0.0006262 474.4 31 0.0006262 474.5 31 0.0006262 474.6 31 0.0006138 474.8 31 0.0006138 474.9 30 0.0006138 475 31 0.0006138 475.1 31 0.0006014 475.3 30 0.000589 475.4 30 0.000589 475.5 30 0.0005766 475.6 30 0.0005766 475.8 30 0.0005766 475.9 30 0.0005766 476 30 0.0005642 476.1 30 0.0005766 476.3 30 0.0005766 476.4 30 0.0005766 476.5 30 0.0005766 476.6 30 0.0005766 476.8 30 0.0005642 476.9 30 0.0005766 477 30 0.0005642 477.1 29 0.0005642 477.3 29 0.0005642 477.4 29 0.0005642 477.5 29 0.0005642 477.6 29 0.0005642 477.8 29 0.0005642 477.9 29 0.0005642 478 29 0.0005642 478.1 29 0.0005642 478.3 28 0.0005642 478.4 29 0.0005642 478.5 28 0.0005642 478.6 28 0.0005518 478.8 28 0.0005394 478.9 28 0.000527 479 27 0.000527 479.1 28 0.000527 479.3 27 0.000527 479.4 27 0.0005146 479.5 27 0.0005146 479.6 27 0.0005146 479.7 27 0.0005146 479.9 27 0.0005022 480 27 0.0004774 480.1 27 0.0004774 480.2 27 0.0004774 480.4 27 0.000465 480.5 27 0.000465 480.6 27 0.000465 480.7 27 0.000465 480.9 27 0.0004774 481 27 0.0004898 481.1 27 0.0004898 481.2 26 0.0005022 481.4 27 0.0005022 481.5 27 0.0005022 481.6 26 0.0005022 481.7 26 0.0005146 481.9 26 0.0005022 482 26 0.0005022 482.1 26 0.0005146 482.2 26 0.0005022 482.4 26 0.0005022 482.5 26 0.0005022 482.6 26 0.0004898 482.7 26 0.000465 482.9 26 0.0004526 483 26 0.0004402 483.1 26 0.0004278 483.2 25 0.0004278 483.4 25 0.0004278 483.5 25 0.0004154 483.6 25 0.0004154 483.7 25 0.0004154 483.9 24 0.000403 484 24 0.000403 484.1 24 0.000403 484.2 24 0.000403 484.4 24 0.0004154 484.5 24 0.000403 484.6 24 0.000403 484.7 24 0.000403 484.9 24 0.0004154 485 24 0.000403 485.1 24 0.000403 485.2 24 0.000403 485.4 24 0.000403 485.5 24 0.000403 485.6 24 0.000403 485.7 23 0.000403 485.8 24 0.0004154 486 23 0.0004278 486.1 23 0.0004278 486.2 23 0.0004278 486.3 23 0.0004154 486.5 23 0.0004154 486.6 23 0.000403 486.7 23 0.0003906 486.8 23 0.0003906 487 23 0.0003782 487.1 23 0.0003782 487.2 23 0.0003658 487.3 23 0.0003658 487.5 23 0.0003658 487.6 23 0.0003534 487.7 23 0.0003658 487.8 23 0.0003658 488 23 0.0003782 488.1 23 0.0003782 488.2 23 0.0003782 488.3 23 0.0003658 488.5 22 0.0003658 488.6 23 0.0003658 488.7 22 0.0003534 488.8 22 0.0003534 489 22 0.0003286 489.1 22 0.000341 489.2 21 0.000341 489.3 21 0.0003534 489.5 22 0.0003534 489.6 21 0.0003534 489.7 21 0.0003534 489.8 21 0.0003658 490 22 0.0003782 490.1 21 0.0003534 490.2 22 0.000341 490.3 21 0.0003534 490.5 21 0.0003534 490.6 21 0.0003534 490.7 21 0.0003534 490.8 21 0.0003534 491 21 0.0003534 491.1 21 0.0003658 491.2 21 0.0003782 491.3 21 0.0003658 491.5 21 0.0003658 491.6 21 0.0003658 491.7 21 0.0003658 491.8 21 0.0003658 492 21 0.0003658 492.1 21 0.0003658 492.2 21 0.0003534 492.3 21 0.0003658 492.4 21 0.0003534 492.6 20 0.0003658 492.7 21 0.0003658 492.8 21 0.0003782 492.9 21 0.0003782 493.1 21 0.0003782 493.2 20 0.0003782 493.3 20 0.0003782 493.4 20 0.0003906 493.6 21 0.000403 493.7 20 0.000403 493.8 20 0.000403 493.9 20 0.000403 494.1 20 0.0004278 494.2 20 0.0004278 494.3 20 0.0004154 494.4 20 0.000403 494.6 20 0.0003906 494.7 20 0.000403 494.8 20 0.000403 494.9 20 0.000403 495.1 19 0.000403 495.2 20 0.000403 495.3 20 0.000403 495.4 20 0.000403 495.6 19 0.000403 495.7 19 0.0004154 495.8 20 0.0004278 495.9 19 0.0004402 496.1 19 0.0004402 496.2 19 0.0004278 496.3 19 0.0004278 496.4 19 0.0004278 496.6 19 0.0004402 496.7 19 0.0004526 496.8 19 0.0004526 496.9 19 0.0004526 497.1 19 0.0004526 497.2 19 0.0004526 497.3 19 0.0004526 497.4 18 0.0004526 497.6 18 0.0004526 497.7 19 0.0004526 497.8 19 0.0004526 497.9 18 0.0004526 498.1 19 0.0004526 498.2 18 0.0004526 498.3 18 0.000465 498.4 18 0.0004774 498.6 19 0.0004774 498.7 18 0.000465 498.8 18 0.000465 498.9 18 0.000465 499 19 0.0004774 499.2 18 0.0004774 499.3 18 0.0004774 499.4 18 0.000465 499.5 18 0.0004774 499.7 18 0.0004774 499.8 18 0.0004898 499.9 18 0.0005022 500 18 0.0005022 500.2 18 0.0005022 500.3 18 0.0005022 500.4 18 0.0005022 500.5 18 0.0005146 500.7 18 0.000527 500.8 18 0.0005394 500.9 18 0.0005518 501 18 0.0005518 501.2 18 0.0005518 501.3 18 0.0005518 501.4 18 0.0005518 501.5 18 0.0005642 501.7 17 0.0005518 501.8 17 0.0005394 501.9 18 0.000527 502 18 0.000527 502.2 18 0.000527 502.3 17 0.0005146 502.4 17 0.000527 502.5 17 0.000527 502.7 17 0.000527 502.8 17 0.0005518 502.9 17 0.0005518 503 17 0.0005518 503.2 16 0.0005518 503.3 17 0.0005518 503.4 16 0.0005642 503.5 16 0.0005642 503.7 17 0.0005642 503.8 16 0.0005642 503.9 17 0.0005642 504 17 0.0005642 504.2 16 0.0005642 504.3 16 0.0005518 504.4 17 0.0005642 504.5 16 0.0005642 504.7 16 0.0005642 504.8 16 0.0005642 504.9 16 0.0005518 505 16 0.0005394 505.1 16 0.0005394 505.3 16 0.0005518 505.4 16 0.0005518 505.5 16 0.0005518 505.6 16 0.0005642 505.8 16 0.0005766 505.9 16 0.000589 506 16 0.000589 506.1 16 0.0006014 506.3 16 0.0006014 506.4 16 0.0006262 506.5 16 0.0006262 506.6 16 0.0006262 506.8 16 0.0006262 506.9 16 0.0006138 507 16 0.0006138 507.1 16 0.000589 507.3 16 0.0005766 507.4 16 0.0005766 507.5 16 0.0005642 507.6 16 0.0005642 507.8 16 0.0005642 507.9 16 0.0005766 508 16 0.0005766 508.1 16 0.000589 508.3 16 0.0006014 508.4 16 0.0006014 508.5 16 0.000589 508.6 16 0.0005766 508.8 16 0.000589 508.9 16 0.000589 509 16 0.000589 509.1 16 0.0005766 509.3 16 0.0005766 509.4 16 0.0005766 509.5 32 0.29 0.09 0.74 0.002 0.007 0.66 1.3 1.02 0.292 0 0 0.001 0.0041 0 5 6.79e-05 0 8 6.79e-05 0.106 9 5.556e-05 0.2119 7 4.321e-05 0.3179 8 3.086e-05 0.4238 8 3.086e-05 0.5298 9 3.086e-05 0.6357 9 3.086e-05 0.7417 10 1.852e-05 0.8477 12 3.086e-05 0.9536 14 3.086e-05 1.06 16 4.321e-05 1.166 19 6.79e-05 1.271 22 8.025e-05 1.377 26 0.0001296 1.483 29 0.000179 1.589 33 0.0002161 1.695 37 0.0002654 1.801 41 0.0003025 1.907 46 0.0003642 2.013 49 0.0004012 2.119 54 0.000463 2.225 59 0.0005247 2.331 63 0.0005864 2.437 68 0.0006358 2.543 72 0.0006852 2.649 77 0.0007593 2.755 81 0.0008087 2.861 85 0.0008704 2.967 90 0.0009198 3.073 94 0.0009691 3.179 99 0.001031 3.285 102 0.00108 3.391 107 0.001142 3.497 111 0.001191 3.603 115 0.001253 3.709 119 0.001302 3.814 123 0.00134 3.92 127 0.001377 4.026 131 0.001438 4.132 134 0.001463 4.238 138 0.001488 4.344 141 0.001549 4.45 146 0.001586 4.556 149 0.001636 4.662 152 0.001685 4.768 156 0.001722 4.874 160 0.001759 4.98 163 0.001796 5.086 167 0.001833 5.192 170 0.001846 5.298 174 0.001907 5.404 177 0.001944 5.51 181 0.001994 5.616 184 0.002031 5.722 187 0.00208 5.828 191 0.002117 5.934 194 0.002142 6.04 197 0.002191 6.146 201 0.002228 6.252 203 0.002265 6.357 207 0.002302 6.463 210 0.002352 6.569 213 0.002426 6.675 217 0.002475 6.781 220 0.002537 6.887 224 0.002574 6.993 227 0.002636 7.099 231 0.002673 7.205 234 0.002747 7.311 238 0.002784 7.417 242 0.002833 7.523 245 0.002895 7.629 249 0.002944 7.735 252 0.003006 7.841 256 0.003043 7.947 259 0.003105 8.053 263 0.003167 8.159 266 0.003216 8.265 269 0.00329 8.371 273 0.003327 8.477 277 0.003389 8.583 280 0.003438 8.689 284 0.003512 8.795 287 0.003574 8.9 291 0.003623 9.006 294 0.003685 9.112 297 0.003722 9.218 301 0.003796 9.324 304 0.003846 9.43 308 0.003907 9.536 312 0.003969 9.642 315 0.004031 9.748 318 0.004093 9.854 322 0.004154 9.96 326 0.004216 10.07 329 0.004253 10.17 332 0.004315 10.28 335 0.004377 10.38 339 0.004426 10.49 343 0.004475 10.6 346 0.004525 10.7 349 0.004586 10.81 353 0.004636 10.91 357 0.004685 11.02 360 0.004735 11.13 363 0.004809 11.23 367 0.004907 11.34 371 0.004969 11.44 374 0.005019 11.55 378 0.005056 11.66 381 0.00508 11.76 385 0.005117 11.87 388 0.005142 11.97 392 0.005167 12.08 395 0.005191 12.19 399 0.005216 12.29 401 0.005241 12.4 404 0.005278 12.5 408 0.005327 12.61 411 0.005364 12.71 415 0.005389 12.82 418 0.005438 12.93 421 0.005475 13.03 424 0.005512 13.14 428 0.005562 13.24 431 0.005599 13.35 435 0.005636 13.46 438 0.005673 13.56 442 0.005722 13.67 446 0.005784 13.77 449 0.005833 13.88 453 0.005895 13.99 456 0.005932 14.09 459 0.005982 14.2 462 0.006031 14.3 466 0.006093 14.41 469 0.006142 14.52 473 0.006204 14.62 476 0.006253 14.73 480 0.006315 14.83 484 0.006352 14.94 487 0.006401 15.05 489 0.006463 15.15 493 0.006512 15.26 497 0.006574 15.36 501 0.006636 15.47 504 0.006685 15.58 507 0.006747 15.68 510 0.006809 15.79 514 0.00687 15.89 517 0.006907 16 521 0.006969 16.11 524 0.007019 16.21 528 0.007068 16.32 532 0.007105 16.42 535 0.007142 16.53 539 0.007216 16.64 542 0.007266 16.74 546 0.007327 16.85 549 0.007389 16.95 553 0.007438 17.06 556 0.0075 17.17 559 0.007537 17.27 563 0.007611 17.38 566 0.007673 17.48 569 0.00771 17.59 573 0.007759 17.69 576 0.007796 17.8 580 0.007858 17.91 584 0.007907 18.01 587 0.007957 18.12 590 0.008006 18.22 594 0.008068 18.33 597 0.008117 18.44 601 0.008167 18.54 603 0.008216 18.65 607 0.008253 18.75 610 0.008303 18.86 614 0.008352 18.97 617 0.008414 19.07 621 0.008463 19.18 625 0.008512 19.28 628 0.008562 19.39 632 0.008624 19.5 635 0.008673 19.6 639 0.008722 19.71 642 0.008784 19.81 645 0.008833 19.92 649 0.008895 20.03 653 0.008957 20.13 656 0.009006 20.24 659 0.009068 20.34 662 0.009117 20.45 666 0.009167 20.56 669 0.009228 20.66 672 0.00929 20.77 676 0.00934 20.87 679 0.009401 20.98 683 0.009463 21.09 686 0.009512 21.19 690 0.009574 21.3 693 0.009611 21.4 696 0.009685 21.51 700 0.009735 21.62 703 0.009809 21.72 706 0.009883 21.83 709 0.009932 21.93 712 0.01001 22.04 714 0.01006 22.15 717 0.01013 22.25 718 0.01015 22.36 721 0.01024 22.46 723 0.0103 22.57 726 0.01038 22.68 728 0.01044 22.78 730 0.01049 22.89 732 0.01056 22.99 734 0.01061 23.1 737 0.01067 23.2 740 0.01072 23.31 743 0.0108 23.42 746 0.01085 23.52 749 0.01091 23.63 750 0.01098 23.73 753 0.01104 23.84 756 0.01109 23.95 759 0.01115 24.05 761 0.01123 24.16 764 0.01129 24.26 766 0.01136 24.37 769 0.01146 24.48 772 0.01154 24.58 775 0.01164 24.69 779 0.01171 24.79 782 0.01181 24.9 787 0.01188 25.01 791 0.01198 25.11 795 0.01206 25.22 799 0.01213 25.32 801 0.01223 25.43 803 0.01231 25.54 806 0.01241 25.64 811 0.01246 25.75 814 0.01249 25.85 818 0.01248 25.96 821 0.01241 26.07 826 0.0123 26.17 831 0.0122 26.28 837 0.01198 26.38 843 0.01181 26.49 849 0.01157 26.6 856 0.01138 26.7 861 0.01119 26.81 867 0.01102 26.91 872 0.0109 27.02 878 0.0108 27.13 884 0.01075 27.23 889 0.01073 27.34 893 0.01075 27.44 900 0.0108 27.55 903 0.01086 27.66 907 0.01092 27.76 912 0.01099 27.87 915 0.01106 27.97 920 0.01114 28.08 922 0.01122 28.18 926 0.0113 28.29 930 0.01139 28.4 933 0.01148 28.5 936 0.01157 28.61 940 0.01165 28.71 943 0.01175 28.82 946 0.01182 28.93 949 0.01191 29.03 951 0.01198 29.14 955 0.01207 29.24 957 0.01215 29.35 961 0.01222 29.46 964 0.0123 29.56 967 0.01238 29.67 970 0.01245 29.77 973 0.01254 29.88 976 0.01261 29.99 979 0.01265 30.09 983 0.01267 30.2 986 0.01276 30.3 989 0.01282 30.41 992 0.01291 30.52 995 0.01297 30.62 998 0.01304 30.73 1001 0.01311 30.83 1004 0.01317 30.94 1007 0.01325 31.05 1010 0.01333 31.15 1013 0.01343 31.26 1017 0.01351 31.36 1020 0.0136 31.47 1023 0.01369 31.58 1026 0.01376 31.68 1029 0.01386 31.79 1033 0.01393 31.89 1036 0.01401 32 1040 0.01408 32.11 1043 0.01417 32.21 1046 0.01424 32.32 1049 0.01433 32.42 1053 0.0144 32.53 1056 0.01449 32.64 1059 0.01455 32.74 1062 0.01462 32.85 1065 0.0147 32.95 1069 0.01477 33.06 1072 0.01486 33.16 1076 0.01493 33.27 1080 0.01502 33.38 1083 0.01512 33.48 1086 0.01519 33.59 1090 0.01527 33.69 1094 0.01531 33.8 1097 0.01541 33.91 1101 0.01549 34.01 1104 0.01557 34.12 1108 0.01566 34.22 1111 0.01573 34.33 1115 0.01582 34.44 1119 0.01591 34.54 1122 0.01599 34.65 1126 0.01608 34.75 1129 0.01617 34.86 1133 0.01624 34.97 1136 0.01633 35.07 1140 0.01641 35.18 1144 0.0165 35.28 1147 0.0166 35.39 1151 0.0167 35.5 1154 0.01677 35.6 1157 0.01687 35.71 1161 0.01694 35.81 1165 0.01702 35.92 1169 0.01711 36.03 1172 0.01719 36.13 1175 0.01728 36.24 1179 0.01739 36.34 1183 0.01748 36.45 1186 0.01757 36.56 1189 0.01766 36.66 1193 0.01773 36.77 1197 0.01781 36.87 1200 0.0179 36.98 1201 0.01799 37.09 1203 0.01806 37.19 1205 0.01812 37.3 1207 0.01815 37.4 1208 0.01819 37.51 1209 0.0182 37.62 1210 0.01825 37.72 1212 0.01827 37.83 1212 0.01829 37.93 1212 0.0183 38.04 1212 0.0183 38.14 1213 0.0183 38.25 1212 0.0183 38.36 1213 0.0183 38.46 1213 0.0183 38.57 1213 0.0183 38.67 1213 0.01825 38.78 1212 0.01824 38.89 1212 0.01822 38.99 1212 0.01819 39.1 1212 0.01817 39.2 1212 0.01815 39.31 1211 0.01815 39.42 1210 0.01813 39.52 1209 0.01812 39.63 1209 0.01808 39.73 1209 0.01806 39.84 1209 0.01803 39.95 1208 0.01801 40.05 1208 0.01797 40.16 1207 0.01796 40.26 1206 0.01796 40.37 1206 0.01793 40.48 1205 0.01792 40.58 1205 0.01791 40.69 1204 0.01791 40.79 1204 0.0179 40.9 1203 0.01788 41.01 1203 0.01786 41.11 1203 0.01785 41.22 1202 0.01782 41.32 1201 0.01781 41.43 1201 0.0178 41.54 1201 0.01778 41.64 1201 0.01776 41.75 1201 0.01776 41.85 1201 0.01773 41.96 1200 0.01771 42.07 1200 0.0177 42.17 1200 0.01769 42.28 1200 0.01767 42.38 1200 0.01766 42.49 1200 0.01766 42.6 1199 0.01764 42.7 1199 0.01764 42.81 1199 0.01762 42.91 1198 0.01761 43.02 1199 0.01761 43.12 1199 0.0176 43.23 1198 0.01759 43.34 1198 0.01757 43.44 1198 0.01756 43.55 1198 0.01756 43.65 1198 0.01756 43.76 1198 0.01756 43.87 1198 0.01756 43.97 1198 0.01756 44.08 1198 0.01755 44.18 1197 0.01754 44.29 1198 0.01754 44.4 1198 0.01752 44.5 1198 0.01751 44.61 1198 0.01749 44.71 1199 0.0175 44.82 1198 0.01751 44.93 1199 0.01751 45.03 1199 0.0175 45.14 1199 0.01751 45.24 1198 0.01751 45.35 1199 0.01751 45.46 1199 0.01751 45.56 1199 0.01752 45.67 1199 0.01752 45.77 1199 0.01754 45.88 1199 0.01754 45.99 1199 0.01755 46.09 1200 0.01756 46.2 1199 0.01756 46.3 1200 0.01756 46.41 1200 0.01757 46.52 1200 0.01757 46.62 1200 0.01759 46.73 1200 0.0176 46.83 1200 0.01759 46.94 1200 0.01761 47.05 1200 0.01761 47.15 1200 0.01761 47.26 1200 0.01764 47.36 1200 0.01765 47.47 1200 0.01765 47.58 1200 0.01766 47.68 1200 0.01769 47.79 1200 0.0177 47.89 1200 0.01771 48 1200 0.01771 48.1 1200 0.01771 48.21 1200 0.01771 48.32 1200 0.01772 48.42 1200 0.01773 48.53 1200 0.01775 48.63 1200 0.01775 48.74 1199 0.01775 48.85 1200 0.01775 48.95 1200 0.01776 49.06 1200 0.01778 49.16 1200 0.01778 49.27 1200 0.01778 49.38 1200 0.01781 49.48 1200 0.01781 49.59 1200 0.01783 49.69 1200 0.01783 49.8 1200 0.01783 49.91 1200 0.01781 50.01 1200 0.01781 50.12 1200 0.01781 50.22 1200 0.01781 50.33 1200 0.01781 50.44 1200 0.01781 50.54 1200 0.0178 50.65 1200 0.01778 50.75 1200 0.01778 50.86 1200 0.01776 50.97 1200 0.01776 51.07 1200 0.01775 51.18 1200 0.01773 51.28 1200 0.01772 51.39 1200 0.01772 51.5 1200 0.01772 51.6 1200 0.01771 51.71 1200 0.01769 51.81 1200 0.01769 51.92 1200 0.01769 52.03 1200 0.01769 52.13 1200 0.01771 52.24 1200 0.01771 52.34 1200 0.0177 52.45 1200 0.01769 52.56 1200 0.01767 52.66 1200 0.01767 52.77 1200 0.01769 52.87 1200 0.01771 52.98 1200 0.01771 53.08 1200 0.01769 53.19 1200 0.01769 53.3 1200 0.01769 53.4 1200 0.01767 53.51 1200 0.01767 53.61 1200 0.01769 53.72 1200 0.01769 53.83 1200 0.01767 53.93 1200 0.01769 54.04 1200 0.01767 54.14 1200 0.01769 54.25 1200 0.01769 54.36 1200 0.0177 54.46 1200 0.0177 54.57 1200 0.01769 54.67 1200 0.01769 54.78 1200 0.0177 54.89 1200 0.01771 54.99 1200 0.01771 55.1 1200 0.0177 55.2 1200 0.01769 55.31 1200 0.01767 55.42 1200 0.01766 55.52 1200 0.01766 55.63 1200 0.01766 55.73 1200 0.01766 55.84 1200 0.01766 55.95 1200 0.01766 56.05 1200 0.01766 56.16 1200 0.01765 56.26 1200 0.01765 56.37 1200 0.01764 56.48 1200 0.01764 56.58 1200 0.01762 56.69 1200 0.01761 56.79 1200 0.01761 56.9 1200 0.01761 57.01 1200 0.01761 57.11 1200 0.01761 57.22 1200 0.0176 57.32 1200 0.01759 57.43 1200 0.01759 57.54 1200 0.01761 57.64 1200 0.0176 57.75 1200 0.01761 57.85 1200 0.01761 57.96 1200 0.01761 58.06 1200 0.01761 58.17 1200 0.01761 58.28 1200 0.0176 58.38 1200 0.0176 58.49 1200 0.01761 58.59 1200 0.0176 58.7 1200 0.0176 58.81 1200 0.01759 58.91 1200 0.01759 59.02 1200 0.01759 59.12 1200 0.01759 59.23 1200 0.01759 59.34 1200 0.01759 59.44 1200 0.01757 59.55 1200 0.01759 59.65 1200 0.0176 59.76 1200 0.0176 59.87 1200 0.0176 59.97 1200 0.0176 60.08 1200 0.01761 60.18 1200 0.01761 60.29 1200 0.01761 60.4 1200 0.01761 60.5 1200 0.01762 60.61 1200 0.01764 60.71 1200 0.01764 60.82 1200 0.01766 60.93 1200 0.01766 61.03 1200 0.01767 61.14 1200 0.01769 61.24 1200 0.01769 61.35 1200 0.01771 61.46 1200 0.01771 61.56 1200 0.01771 61.67 1200 0.01771 61.77 1200 0.01771 61.88 1200 0.01772 61.99 1200 0.01772 62.09 1200 0.01772 62.2 1200 0.01772 62.3 1200 0.01773 62.41 1200 0.01773 62.52 1200 0.01773 62.62 1200 0.01773 62.73 1200 0.01775 62.83 1200 0.01776 62.94 1200 0.01778 63.05 1200 0.01777 63.15 1200 0.01776 63.26 1200 0.01776 63.36 1200 0.01775 63.47 1200 0.01773 63.57 1200 0.01773 63.68 1200 0.01771 63.79 1200 0.01771 63.89 1200 0.0177 64 1200 0.01769 64.1 1200 0.01769 64.21 1200 0.01767 64.32 1200 0.01766 64.42 1200 0.01766 64.53 1200 0.01766 64.63 1200 0.01766 64.74 1200 0.01766 64.85 1200 0.01766 64.95 1200 0.01766 65.06 1200 0.01766 65.16 1200 0.01766 65.27 1200 0.01765 65.38 1200 0.01764 65.48 1200 0.01764 65.59 1200 0.01764 65.69 1200 0.01764 65.8 1200 0.01764 65.91 1200 0.01764 66.01 1200 0.01764 66.12 1200 0.01764 66.22 1200 0.01764 66.33 1200 0.01762 66.44 1200 0.01764 66.54 1200 0.01764 66.65 1200 0.01764 66.75 1200 0.01764 66.86 1200 0.01762 66.97 1200 0.01761 67.07 1200 0.01761 67.18 1200 0.01764 67.28 1200 0.01764 67.39 1200 0.01764 67.5 1200 0.01764 67.6 1200 0.01764 67.71 1200 0.01764 67.81 1200 0.01764 67.92 1200 0.01764 68.03 1200 0.01764 68.13 1200 0.01764 68.24 1200 0.01765 68.34 1200 0.01765 68.45 1200 0.01764 68.55 1200 0.01764 68.66 1200 0.01761 68.77 1200 0.01761 68.87 1200 0.01764 68.98 1200 0.01764 69.08 1200 0.01764 69.19 1200 0.01761 69.3 1200 0.01761 69.4 1200 0.01761 69.51 1200 0.01761 69.61 1200 0.01761 69.72 1200 0.0176 69.83 1200 0.0176 69.93 1200 0.01759 70.04 1200 0.01759 70.14 1200 0.01757 70.25 1200 0.01757 70.36 1200 0.01757 70.46 1200 0.01756 70.57 1200 0.01756 70.67 1200 0.01756 70.78 1200 0.01756 70.89 1200 0.01756 70.99 1200 0.01756 71.1 1200 0.01755 71.2 1200 0.01755 71.31 1200 0.01754 71.42 1200 0.01752 71.52 1200 0.01751 71.63 1200 0.01752 71.73 1200 0.01751 71.84 1200 0.01751 71.95 1200 0.01751 72.05 1200 0.01751 72.16 1200 0.01749 72.26 1200 0.01749 72.37 1200 0.01749 72.48 1200 0.01751 72.58 1200 0.01751 72.69 1200 0.01751 72.79 1200 0.01751 72.9 1200 0.01752 73.01 1200 0.01752 73.11 1200 0.01752 73.22 1200 0.01754 73.32 1200 0.01752 73.43 1200 0.01754 73.53 1200 0.01755 73.64 1200 0.01755 73.75 1200 0.01756 73.85 1200 0.01757 73.96 1200 0.01757 74.06 1200 0.01756 74.17 1200 0.01757 74.28 1200 0.01757 74.38 1200 0.01759 74.49 1200 0.01757 74.59 1200 0.01759 74.7 1200 0.0176 74.81 1200 0.0176 74.91 1200 0.01761 75.02 1200 0.01761 75.12 1200 0.01764 75.23 1200 0.01765 75.34 1200 0.01766 75.44 1200 0.01766 75.55 1200 0.01766 75.65 1200 0.01766 75.76 1200 0.01766 75.87 1200 0.01767 75.97 1200 0.01766 76.08 1200 0.01769 76.18 1200 0.01769 76.29 1200 0.01766 76.4 1200 0.01767 76.5 1200 0.01769 76.61 1200 0.01769 76.71 1200 0.0177 76.82 1200 0.01769 76.93 1200 0.01769 77.03 1200 0.0177 77.14 1200 0.0177 77.24 1200 0.01769 77.35 1200 0.01769 77.46 1200 0.01767 77.56 1200 0.01766 77.67 1200 0.01766 77.77 1200 0.01766 77.88 1200 0.01766 77.99 1200 0.01764 78.09 1200 0.01764 78.2 1200 0.01761 78.3 1200 0.01762 78.41 1200 0.01761 78.51 1200 0.01761 78.62 1200 0.0176 78.73 1200 0.01759 78.83 1200 0.01759 78.94 1200 0.01757 79.04 1200 0.01757 79.15 1200 0.01757 79.26 1200 0.01757 79.36 1200 0.01756 79.47 1200 0.01756 79.57 1200 0.01756 79.68 1200 0.01756 79.79 1200 0.01756 79.89 1200 0.01755 80 1200 0.01754 80.1 1200 0.01752 80.21 1200 0.01752 80.32 1200 0.01754 80.42 1200 0.01754 80.53 1200 0.01754 80.63 1200 0.01755 80.74 1200 0.01755 80.85 1200 0.01756 80.95 1200 0.01756 81.06 1200 0.01756 81.16 1200 0.01756 81.27 1200 0.01756 81.38 1200 0.01756 81.48 1200 0.01756 81.59 1200 0.01756 81.69 1200 0.01756 81.8 1200 0.01756 81.91 1200 0.01756 82.01 1200 0.01756 82.12 1200 0.01756 82.22 1200 0.01756 82.33 1200 0.01756 82.44 1200 0.01756 82.54 1200 0.01756 82.65 1200 0.01756 82.75 1200 0.01756 82.86 1200 0.01756 82.97 1200 0.01756 83.07 1200 0.01756 83.18 1200 0.01756 83.28 1200 0.01755 83.39 1200 0.01755 83.49 1200 0.01755 83.6 1201 0.01755 83.71 1200 0.01755 83.81 1200 0.01754 83.92 1200 0.01752 84.02 1200 0.01752 84.13 1200 0.01752 84.24 1200 0.01751 84.34 1200 0.01752 84.45 1200 0.01751 84.55 1200 0.01751 84.66 1200 0.01751 84.77 1200 0.01749 84.87 1200 0.01749 84.98 1200 0.01749 85.08 1200 0.01749 85.19 1200 0.01748 85.3 1200 0.01746 85.4 1200 0.01746 85.51 1200 0.01748 85.61 1200 0.01746 85.72 1200 0.01746 85.83 1200 0.01746 85.93 1200 0.01746 86.04 1200 0.01746 86.14 1200 0.01746 86.25 1200 0.01746 86.36 1200 0.01746 86.46 1200 0.01744 86.57 1200 0.01744 86.67 1200 0.01745 86.78 1200 0.01745 86.89 1199 0.01744 86.99 1200 0.01745 87.1 1200 0.01745 87.2 1200 0.01745 87.31 1200 0.01746 87.42 1200 0.01745 87.52 1200 0.01745 87.63 1200 0.01746 87.73 1200 0.01746 87.84 1200 0.01746 87.95 1200 0.01748 88.05 1200 0.01749 88.16 1200 0.01749 88.26 1200 0.01749 88.37 1200 0.01751 88.47 1200 0.01752 88.58 1200 0.01754 88.69 1200 0.01754 88.79 1200 0.01754 88.9 1200 0.01755 89 1200 0.01756 89.11 1200 0.01757 89.22 1200 0.01757 89.32 1200 0.01757 89.43 1200 0.01759 89.53 1200 0.01759 89.64 1200 0.0176 89.75 1200 0.0176 89.85 1200 0.0176 89.96 1200 0.01761 90.06 1200 0.01761 90.17 1200 0.01761 90.28 1200 0.01761 90.38 1200 0.01762 90.49 1200 0.01762 90.59 1200 0.01762 90.7 1200 0.01761 90.81 1200 0.01761 90.91 1200 0.01761 91.02 1200 0.01761 91.12 1200 0.01761 91.23 1200 0.01761 91.34 1200 0.01761 91.44 1200 0.01761 91.55 1200 0.01761 91.65 1200 0.01761 91.76 1200 0.01761 91.87 1200 0.01759 91.97 1200 0.01757 92.08 1200 0.01756 92.18 1200 0.01756 92.29 1200 0.01756 92.4 1200 0.01756 92.5 1200 0.01755 92.61 1200 0.01755 92.71 1200 0.01755 92.82 1200 0.01755 92.93 1200 0.01755 93.03 1200 0.01754 93.14 1200 0.01754 93.24 1200 0.01754 93.35 1200 0.01754 93.45 1200 0.01754 93.56 1200 0.01754 93.67 1200 0.01754 93.77 1200 0.01752 93.88 1200 0.01751 93.98 1200 0.01751 94.09 1200 0.0175 94.2 1200 0.0175 94.3 1200 0.01751 94.41 1200 0.0175 94.51 1200 0.0175 94.62 1200 0.01751 94.73 1200 0.01751 94.83 1200 0.01751 94.94 1200 0.0175 95.04 1200 0.01749 95.15 1200 0.01749 95.26 1200 0.01749 95.36 1200 0.0175 95.47 1200 0.01751 95.57 1200 0.01751 95.68 1200 0.01751 95.79 1200 0.01751 95.89 1200 0.01751 96 1200 0.01751 96.1 1200 0.01751 96.21 1200 0.01751 96.32 1200 0.01751 96.42 1200 0.0175 96.53 1200 0.01749 96.63 1200 0.0175 96.74 1200 0.01749 96.85 1200 0.01751 96.95 1200 0.01751 97.06 1200 0.01752 97.16 1200 0.01752 97.27 1200 0.01751 97.38 1200 0.01752 97.48 1200 0.01751 97.59 1200 0.01751 97.69 1200 0.0175 97.8 1200 0.01749 97.91 1200 0.01749 98.01 1200 0.01748 98.12 1200 0.01749 98.22 1200 0.01749 98.33 1200 0.01749 98.43 1200 0.01749 98.54 1200 0.01748 98.65 1200 0.01746 98.75 1200 0.01746 98.86 1200 0.01746 98.96 1200 0.01746 99.07 1200 0.01746 99.18 1200 0.01744 99.28 1200 0.01744 99.39 1200 0.01743 99.49 1200 0.01743 99.6 1200 0.01743 99.71 1200 0.01741 99.81 1200 0.01741 99.92 1200 0.01741 100 1200 0.01741 100.1 1200 0.01741 100.2 1200 0.01741 100.3 1200 0.01739 100.4 1200 0.01739 100.6 1200 0.01738 100.7 1200 0.01739 100.8 1200 0.01739 100.9 1200 0.01739 101 1200 0.01739 101.1 1200 0.01741 101.2 1200 0.01741 101.3 1200 0.01741 101.4 1200 0.01741 101.5 1200 0.01741 101.6 1200 0.01744 101.7 1200 0.01744 101.8 1200 0.01745 101.9 1200 0.01745 102 1200 0.01745 102.1 1200 0.01745 102.2 1200 0.01745 102.4 1200 0.01745 102.5 1200 0.01746 102.6 1200 0.01748 102.7 1200 0.01748 102.8 1200 0.01749 102.9 1200 0.01749 103 1200 0.0175 103.1 1200 0.01751 103.2 1200 0.01751 103.3 1200 0.01751 103.4 1200 0.01752 103.5 1200 0.01752 103.6 1200 0.01752 103.7 1200 0.01755 103.8 1200 0.01756 103.9 1200 0.01756 104.1 1200 0.01756 104.2 1200 0.01756 104.3 1200 0.01757 104.4 1200 0.01757 104.5 1200 0.01759 104.6 1200 0.01759 104.7 1200 0.0176 104.8 1200 0.01761 104.9 1200 0.01761 105 1200 0.0176 105.1 1200 0.0176 105.2 1200 0.01761 105.3 1200 0.01761 105.4 1200 0.01759 105.5 1200 0.01759 105.6 1200 0.01757 105.7 1200 0.01757 105.9 1200 0.01757 106 1200 0.01757 106.1 1200 0.01757 106.2 1200 0.01756 106.3 1200 0.01754 106.4 1200 0.01755 106.5 1200 0.01756 106.6 1200 0.01755 106.7 1200 0.01754 106.8 1200 0.01754 106.9 1200 0.01752 107 1200 0.01752 107.1 1200 0.01752 107.2 1200 0.01751 107.3 1200 0.01751 107.4 1200 0.0175 107.5 1200 0.0175 107.7 1200 0.0175 107.8 1200 0.0175 107.9 1200 0.01749 108 1200 0.01749 108.1 1200 0.01749 108.2 1200 0.01748 108.3 1200 0.01748 108.4 1199 0.01746 108.5 1200 0.01746 108.6 1200 0.01745 108.7 1200 0.01744 108.8 1200 0.01744 108.9 1200 0.01745 109 1200 0.01745 109.1 1200 0.01745 109.2 1200 0.01746 109.3 1200 0.01745 109.5 1200 0.01746 109.6 1200 0.01746 109.7 1200 0.01746 109.8 1200 0.01746 109.9 1200 0.01748 110 1200 0.01748 110.1 1200 0.01748 110.2 1200 0.01746 110.3 1200 0.01746 110.4 1200 0.01746 110.5 1200 0.01746 110.6 1200 0.01746 110.7 1200 0.01746 110.8 1200 0.01746 110.9 1200 0.01746 111 1200 0.01748 111.1 1200 0.01749 111.3 1200 0.01749 111.4 1200 0.01748 111.5 1200 0.01746 111.6 1200 0.01749 111.7 1200 0.01749 111.8 1200 0.01749 111.9 1200 0.01748 112 1200 0.01746 112.1 1200 0.01746 112.2 1200 0.01746 112.3 1200 0.01746 112.4 1200 0.01746 112.5 1200 0.01746 112.6 1200 0.01746 112.7 1200 0.01745 112.8 1200 0.01744 113 1200 0.01744 113.1 1200 0.01743 113.2 1200 0.01741 113.3 1200 0.01741 113.4 1200 0.01741 113.5 1200 0.01741 113.6 1200 0.01741 113.7 1200 0.01741 113.8 1200 0.01739 113.9 1200 0.01739 114 1200 0.01739 114.1 1200 0.01739 114.2 1200 0.0174 114.3 1200 0.0174 114.4 1200 0.01739 114.5 1200 0.01739 114.6 1200 0.01738 114.8 1200 0.01738 114.9 1200 0.01738 115 1200 0.01739 115.1 1200 0.01739 115.2 1200 0.01738 115.3 1200 0.01738 115.4 1200 0.01738 115.5 1200 0.01736 115.6 1200 0.01738 115.7 1200 0.01738 115.8 1200 0.01739 115.9 1201 0.0174 116 1200 0.01739 116.1 1200 0.01739 116.2 1200 0.01738 116.3 1200 0.01739 116.4 1200 0.01741 116.6 1200 0.01741 116.7 1200 0.01741 116.8 1200 0.01741 116.9 1200 0.01741 117 1200 0.01741 117.1 1200 0.01743 117.2 1200 0.01743 117.3 1200 0.01745 117.4 1200 0.01744 117.5 1200 0.01744 117.6 1200 0.01745 117.7 1200 0.01745 117.8 1200 0.01746 117.9 1200 0.01746 118 1200 0.01748 118.1 1200 0.01746 118.2 1200 0.01749 118.4 1200 0.0175 118.5 1200 0.01751 118.6 1200 0.01751 118.7 1200 0.01751 118.8 1200 0.01751 118.9 1200 0.01751 119 1200 0.01751 119.1 1200 0.01751 119.2 1200 0.01754 119.3 1200 0.01754 119.4 1200 0.01755 119.5 1200 0.01755 119.6 1200 0.01754 119.7 1200 0.01752 119.8 1200 0.01754 119.9 1200 0.01755 120.1 1200 0.01754 120.2 1200 0.01752 120.3 1200 0.01751 120.4 1200 0.01752 120.5 1200 0.01751 120.6 1200 0.01751 120.7 1200 0.01751 120.8 1200 0.0175 120.9 1200 0.01749 121 1200 0.01749 121.1 1200 0.01749 121.2 1200 0.01749 121.3 1200 0.01749 121.4 1200 0.01749 121.5 1200 0.01749 121.6 1200 0.01748 121.7 1200 0.01746 121.9 1200 0.01745 122 1200 0.01744 122.1 1200 0.01746 122.2 1200 0.01745 122.3 1200 0.01746 122.4 1200 0.01746 122.5 1200 0.01744 122.6 1200 0.01744 122.7 1200 0.01744 122.8 1200 0.01741 122.9 1200 0.01743 123 1200 0.01741 123.1 1200 0.01741 123.2 1200 0.01744 123.3 1200 0.01744 123.4 1200 0.01744 123.5 1200 0.01743 123.7 1200 0.01741 123.8 1200 0.01741 123.9 1200 0.01741 124 1200 0.01741 124.1 1200 0.01741 124.2 1200 0.01741 124.3 1200 0.01744 124.4 1200 0.01744 124.5 1200 0.01744 124.6 1200 0.01741 124.7 1200 0.01743 124.8 1200 0.01741 124.9 1200 0.01743 125 1200 0.01744 125.1 1200 0.01744 125.2 1200 0.01744 125.3 1200 0.01743 125.5 1200 0.01744 125.6 1200 0.01744 125.7 1200 0.01744 125.8 1200 0.01744 125.9 1200 0.01744 126 1200 0.01744 126.1 1200 0.01744 126.2 1200 0.01745 126.3 1200 0.01745 126.4 1200 0.01744 126.5 1200 0.01743 126.6 1201 0.01744 126.7 1200 0.01744 126.8 1200 0.01744 126.9 1200 0.01744 127 1200 0.01744 127.1 1200 0.01741 127.3 1200 0.01741 127.4 1200 0.0174 127.5 1200 0.01739 127.6 1200 0.01739 127.7 1200 0.01739 127.8 1200 0.01739 127.9 1200 0.01739 128 1200 0.01738 128.1 1200 0.01738 128.2 1200 0.01738 128.3 1200 0.01736 128.4 1200 0.01736 128.5 1200 0.01736 128.6 1200 0.01736 128.7 1200 0.01736 128.8 1200 0.01736 129 1200 0.01736 129.1 1200 0.01735 129.2 1200 0.01734 129.3 1200 0.01734 129.4 1200 0.01732 129.5 1200 0.01732 129.6 1200 0.01732 129.7 1200 0.01732 129.8 1200 0.01732 129.9 1199 0.01732 130 1200 0.01732 130.1 1200 0.01733 130.2 1200 0.01733 130.3 1200 0.01733 130.4 1200 0.01733 130.5 1200 0.01734 130.6 1200 0.01734 130.8 1200 0.01734 130.9 1200 0.01735 131 1200 0.01735 131.1 1200 0.01735 131.2 1200 0.01735 131.3 1200 0.01735 131.4 1200 0.01735 131.5 1200 0.01736 131.6 1200 0.01736 131.7 1200 0.01736 131.8 1200 0.01736 131.9 1200 0.01736 132 1200 0.01736 132.1 1200 0.01736 132.2 1200 0.01738 132.3 1200 0.01739 132.4 1200 0.0174 132.6 1200 0.01741 132.7 1200 0.01741 132.8 1200 0.01744 132.9 1200 0.01744 133 1200 0.01744 133.1 1200 0.01744 133.2 1200 0.01746 133.3 1200 0.01746 133.4 1200 0.01749 133.5 1200 0.01749 133.6 1200 0.01749 133.7 1200 0.01749 133.8 1200 0.0175 133.9 1200 0.01751 134 1200 0.01751 134.1 1200 0.01751 134.2 1200 0.01751 134.4 1200 0.01751 134.5 1200 0.01752 134.6 1200 0.01754 134.7 1200 0.01754 134.8 1200 0.01755 134.9 1200 0.01754 135 1200 0.01754 135.1 1200 0.01752 135.2 1200 0.01752 135.3 1200 0.01751 135.4 1200 0.01751 135.5 1200 0.01751 135.6 1200 0.01749 135.7 1200 0.01745 135.8 1200 0.01744 135.9 1200 0.01741 136.1 1200 0.01741 136.2 1200 0.01741 136.3 1200 0.01741 136.4 1200 0.01739 136.5 1200 0.01739 136.6 1200 0.01738 136.7 1200 0.01738 136.8 1200 0.01736 136.9 1200 0.01735 137 1200 0.01734 137.1 1200 0.01735 137.2 1200 0.01735 137.3 1200 0.01735 137.4 1200 0.01734 137.5 1200 0.01733 137.6 1200 0.01732 137.7 1200 0.01732 137.9 1200 0.01732 138 1200 0.01732 138.1 1200 0.01732 138.2 1200 0.01732 138.3 1200 0.01732 138.4 1200 0.01732 138.5 1200 0.01732 138.6 1200 0.01732 138.7 1200 0.01732 138.8 1200 0.0173 138.9 1200 0.01732 139 1200 0.01732 139.1 1201 0.01732 139.2 1200 0.01732 139.3 1200 0.01729 139.4 1200 0.01729 139.5 1200 0.01729 139.7 1200 0.01729 139.8 1200 0.0173 139.9 1200 0.0173 140 1200 0.0173 140.1 1200 0.0173 140.2 1200 0.01732 140.3 1200 0.01732 140.4 1200 0.01732 140.5 1200 0.01732 140.6 1200 0.01733 140.7 1200 0.01734 140.8 1200 0.01734 140.9 1200 0.01734 141 1200 0.01734 141.1 1200 0.01733 141.2 1200 0.01732 141.3 1200 0.01732 141.5 1200 0.01732 141.6 1200 0.0173 141.7 1200 0.01729 141.8 1200 0.01728 141.9 1200 0.01727 142 1200 0.01727 142.1 1200 0.01727 142.2 1200 0.01727 142.3 1200 0.01727 142.4 1200 0.01727 142.5 1200 0.01727 142.6 1200 0.01727 142.7 1200 0.01727 142.8 1200 0.01725 142.9 1200 0.01727 143 1200 0.01728 143.1 1200 0.01727 143.3 1200 0.01725 143.4 1200 0.01725 143.5 1200 0.01725 143.6 1200 0.01724 143.7 1200 0.01724 143.8 1200 0.01724 143.9 1200 0.01723 144 1200 0.01722 144.1 1200 0.01722 144.2 1200 0.01722 144.3 1200 0.01722 144.4 1200 0.01722 144.5 1200 0.01722 144.6 1200 0.01722 144.7 1200 0.0172 144.8 1200 0.0172 145 1200 0.01722 145.1 1200 0.01722 145.2 1200 0.01722 145.3 1200 0.0172 145.4 1200 0.01722 145.5 1200 0.01722 145.6 1200 0.01722 145.7 1200 0.01722 145.8 1200 0.0172 145.9 1200 0.0172 146 1200 0.01722 146.1 1200 0.01722 146.2 1200 0.01724 146.3 1200 0.01722 146.4 1200 0.01722 146.5 1199 0.01722 146.6 1200 0.01723 146.8 1200 0.01724 146.9 1200 0.01724 147 1200 0.01725 147.1 1200 0.01724 147.2 1200 0.01723 147.3 1200 0.01724 147.4 1200 0.01724 147.5 1200 0.01724 147.6 1200 0.01727 147.7 1200 0.01727 147.8 1200 0.01728 147.9 1200 0.01729 148 1200 0.01729 148.1 1200 0.01729 148.2 1200 0.0173 148.3 1200 0.01732 148.4 1200 0.01733 148.6 1200 0.01734 148.7 1200 0.01734 148.8 1200 0.01735 148.9 1200 0.01736 149 1200 0.01738 149.1 1200 0.01739 149.2 1200 0.01738 149.3 1200 0.01738 149.4 1200 0.01738 149.5 1200 0.01738 149.6 1200 0.01736 149.7 1200 0.01738 149.8 1200 0.01738 149.9 1200 0.01739 150 1200 0.01739 150.1 1200 0.01739 150.2 1200 0.01739 150.4 1200 0.01739 150.5 1200 0.0174 150.6 1200 0.0174 150.7 1200 0.01741 150.8 1200 0.01741 150.9 1200 0.01741 151 1200 0.01739 151.1 1200 0.01739 151.2 1200 0.01739 151.3 1200 0.01739 151.4 1200 0.01739 151.5 1200 0.01738 151.6 1200 0.01738 151.7 1200 0.01736 151.8 1200 0.01736 151.9 1200 0.01736 152 1200 0.01736 152.2 1200 0.01735 152.3 1200 0.01735 152.4 1200 0.01734 152.5 1200 0.01733 152.6 1200 0.01733 152.7 1200 0.01732 152.8 1200 0.01729 152.9 1200 0.01729 153 1200 0.01728 153.1 1200 0.01728 153.2 1200 0.01729 153.3 1200 0.01729 153.4 1200 0.01729 153.5 1200 0.01729 153.6 1200 0.01729 153.7 1200 0.01732 153.9 1200 0.0173 154 1200 0.0173 154.1 1200 0.0173 154.2 1200 0.0173 154.3 1200 0.01732 154.4 1200 0.01728 154.5 1200 0.01727 154.6 1200 0.01727 154.7 1200 0.01727 154.8 1200 0.01727 154.9 1200 0.01727 155 1200 0.01727 155.1 1200 0.01725 155.2 1200 0.01727 155.3 1200 0.01727 155.4 1200 0.01728 155.5 1200 0.01729 155.7 1200 0.01729 155.8 1200 0.01729 155.9 1200 0.0173 156 1200 0.0173 156.1 1200 0.01729 156.2 1200 0.01728 156.3 1200 0.01728 156.4 1200 0.01727 156.5 1200 0.01728 156.6 1200 0.0173 156.7 1200 0.01732 156.8 1200 0.01732 156.9 1200 0.01732 157 1200 0.01732 157.1 1200 0.01732 157.2 1200 0.01732 157.3 1200 0.01729 157.5 1200 0.01728 157.6 1200 0.01729 157.7 1200 0.01729 157.8 1200 0.01729 157.9 1200 0.01729 158 1200 0.01728 158.1 1200 0.01729 158.2 1200 0.01729 158.3 1200 0.01729 158.4 1200 0.01728 158.5 1200 0.01727 158.6 1200 0.01725 158.7 1200 0.01725 158.8 1200 0.01725 158.9 1200 0.01725 159 1200 0.01725 159.1 1200 0.01725 159.3 1200 0.01724 159.4 1200 0.01724 159.5 1200 0.01723 159.6 1200 0.01723 159.7 1200 0.01722 159.8 1200 0.01722 159.9 1200 0.01722 160 1200 0.01722 160.1 1200 0.01722 160.2 1200 0.01722 160.3 1200 0.0172 160.4 1200 0.01722 160.5 1200 0.01722 160.6 1200 0.01722 160.7 1200 0.01722 160.8 1200 0.01722 161 1200 0.01722 161.1 1200 0.01723 161.2 1200 0.01722 161.3 1200 0.01722 161.4 1200 0.0172 161.5 1200 0.01719 161.6 1200 0.0172 161.7 1200 0.01719 161.8 1200 0.0172 161.9 1200 0.0172 162 1200 0.01722 162.1 1200 0.0172 162.2 1200 0.0172 162.3 1200 0.0172 162.4 1200 0.01722 162.5 1200 0.01722 162.6 1200 0.0172 162.8 1200 0.01722 162.9 1200 0.01722 163 1200 0.01723 163.1 1200 0.01724 163.2 1200 0.01724 163.3 1200 0.01724 163.4 1200 0.01725 163.5 1200 0.01727 163.6 1200 0.01728 163.7 1200 0.01729 163.8 1200 0.01729 163.9 1200 0.01734 164 1200 0.01736 164.1 1200 0.01738 164.2 1200 0.01739 164.3 1200 0.01738 164.4 1200 0.01738 164.6 1200 0.01738 164.7 1200 0.01739 164.8 1201 0.01739 164.9 1200 0.01738 165 1200 0.01735 165.1 1200 0.01736 165.2 1200 0.01738 165.3 1200 0.01738 165.4 1200 0.01738 165.5 1200 0.01738 165.6 1200 0.01736 165.7 1200 0.01736 165.8 1200 0.01738 165.9 1200 0.01741 166 1200 0.01741 166.1 1200 0.01739 166.2 1200 0.01739 166.4 1200 0.01738 166.5 1200 0.01736 166.6 1200 0.01738 166.7 1200 0.01738 166.8 1200 0.01736 166.9 1200 0.01736 167 1200 0.01736 167.1 1200 0.01736 167.2 1200 0.01736 167.3 1200 0.01734 167.4 1200 0.01734 167.5 1200 0.01734 167.6 1200 0.01734 167.7 1200 0.01734 167.8 1200 0.01732 167.9 1200 0.01732 168 1199 0.01729 168.2 1200 0.01729 168.3 1200 0.01728 168.4 1200 0.01728 168.5 1200 0.01727 168.6 1200 0.01727 168.7 1200 0.01727 168.8 1200 0.01727 168.9 1200 0.01727 169 1200 0.01727 169.1 1200 0.01728 169.2 1200 0.01728 169.3 1200 0.01727 169.4 1200 0.01727 169.5 1200 0.01727 169.6 1200 0.01727 169.7 1200 0.01727 169.9 1200 0.01727 170 1200 0.01727 170.1 1200 0.01728 170.2 1200 0.01729 170.3 1200 0.01728 170.4 1200 0.01728 170.5 1200 0.01728 170.6 1200 0.01729 170.7 1200 0.01729 170.8 1200 0.01728 170.9 1200 0.01728 171 1200 0.01727 171.1 1200 0.01727 171.2 1200 0.01727 171.3 1200 0.01727 171.4 1200 0.01727 171.5 1200 0.01727 171.7 1200 0.01727 171.8 1200 0.01727 171.9 1200 0.01727 172 1200 0.01727 172.1 1200 0.01728 172.2 1200 0.01729 172.3 1200 0.01729 172.4 1200 0.0173 172.5 1200 0.01732 172.6 1200 0.0173 172.7 1200 0.01732 172.8 1200 0.0173 172.9 1200 0.01729 173 1200 0.01729 173.1 1200 0.01728 173.2 1200 0.01727 173.3 1200 0.01728 173.5 1200 0.01729 173.6 1200 0.01729 173.7 1200 0.01728 173.8 1200 0.01727 173.9 1200 0.01727 174 1200 0.01727 174.1 1200 0.01727 174.2 1200 0.01727 174.3 1200 0.01727 174.4 1200 0.01727 174.5 1200 0.01725 174.6 1200 0.01724 174.7 1200 0.01724 174.8 1200 0.01723 174.9 1200 0.01722 175 1200 0.01722 175.1 1200 0.01722 175.3 1200 0.01722 175.4 1200 0.01722 175.5 1200 0.01722 175.6 1200 0.01722 175.7 1200 0.01722 175.8 1200 0.0172 175.9 1200 0.01719 176 1200 0.01718 176.1 1200 0.01718 176.2 1200 0.01719 176.3 1200 0.01719 176.4 1200 0.0172 176.5 1200 0.0172 176.6 1200 0.0172 176.7 1200 0.0172 176.8 1200 0.0172 176.9 1200 0.0172 177.1 1200 0.01719 177.2 1200 0.01718 177.3 1200 0.01718 177.4 1200 0.01718 177.5 1200 0.01718 177.6 1200 0.0172 177.7 1200 0.0172 177.8 1200 0.0172 177.9 1200 0.0172 178 1200 0.0172 178.1 1200 0.0172 178.2 1200 0.01722 178.3 1200 0.01722 178.4 1200 0.0172 178.5 1200 0.0172 178.6 1200 0.0172 178.8 1200 0.01722 178.9 1200 0.01722 179 1200 0.01722 179.1 1200 0.01722 179.2 1200 0.01724 179.3 1200 0.01724 179.4 1200 0.01724 179.5 1200 0.01724 179.6 1200 0.01723 179.7 1200 0.01724 179.8 1200 0.01724 179.9 1200 0.01725 180 1200 0.01727 180.1 1200 0.01727 180.2 1200 0.01728 180.3 1200 0.01729 180.4 1200 0.01729 180.6 1200 0.0173 180.7 1200 0.01732 180.8 1200 0.01732 180.9 1200 0.01733 181 1200 0.01733 181.1 1200 0.01734 181.2 1200 0.01734 181.3 1200 0.01733 181.4 1200 0.01734 181.5 1200 0.01734 181.6 1200 0.01734 181.7 1200 0.01735 181.8 1200 0.01735 181.9 1200 0.01735 182 1200 0.01735 182.1 1200 0.01736 182.2 1200 0.01738 182.4 1200 0.01739 182.5 1200 0.01739 182.6 1200 0.01739 182.7 1200 0.01738 182.8 1200 0.01738 182.9 1200 0.01738 183 1200 0.01738 183.1 1200 0.01736 183.2 1200 0.01736 183.3 1200 0.01736 183.4 1200 0.01735 183.5 1200 0.01734 183.6 1200 0.01733 183.7 1200 0.01732 183.8 1200 0.01732 183.9 1200 0.01732 184 1200 0.01732 184.2 1200 0.01734 184.3 1200 0.01734 184.4 1200 0.01733 184.5 1200 0.01732 184.6 1200 0.01732 184.7 1200 0.01732 184.8 1200 0.01732 184.9 1200 0.01732 185 1200 0.01732 185.1 1200 0.0173 185.2 1200 0.01729 185.3 1200 0.01729 185.4 1200 0.01728 185.5 1200 0.01727 185.6 1200 0.01727 185.7 1200 0.01727 185.9 1200 0.01727 186 1200 0.01727 186.1 1200 0.01727 186.2 1200 0.01725 186.3 1200 0.01727 186.4 1200 0.01727 186.5 1200 0.01725 186.6 1200 0.01724 186.7 1200 0.01724 186.8 1200 0.01724 186.9 1200 0.01724 187 1200 0.01724 187.1 1200 0.01724 187.2 1200 0.01723 187.3 1200 0.01724 187.4 1200 0.01724 187.5 1200 0.01724 187.7 1200 0.01725 187.8 1200 0.01725 187.9 1200 0.01725 188 1200 0.01727 188.1 1200 0.01725 188.2 1200 0.01727 188.3 1200 0.01727 188.4 1200 0.01727 188.5 1200 0.01727 188.6 1200 0.01725 188.7 1200 0.01725 188.8 1200 0.01727 188.9 1200 0.01725 189 1200 0.01727 189.1 1200 0.01727 189.2 1201 0.01727 189.3 1200 0.01727 189.5 1200 0.01725 189.6 1199 0.01724 189.7 1200 0.01723 189.8 1200 0.01723 189.9 1200 0.01722 190 1200 0.01722 190.1 1200 0.01722 190.2 1200 0.01722 190.3 1200 0.01722 190.4 1200 0.01722 190.5 1200 0.01724 190.6 1200 0.01724 190.7 1200 0.01724 190.8 1200 0.01724 190.9 1200 0.01724 191 1200 0.01725 191.1 1200 0.01725 191.3 1200 0.01725 191.4 1200 0.01724 191.5 1200 0.01724 191.6 1200 0.01723 191.7 1200 0.01722 191.8 1200 0.0172 191.9 1200 0.01718 192 1200 0.01718 192.1 1200 0.01718 192.2 1200 0.01719 192.3 1200 0.01719 192.4 1200 0.01718 192.5 1200 0.01718 192.6 1200 0.01718 192.7 1200 0.01718 192.8 1200 0.01719 192.9 1200 0.01719 193.1 1200 0.01719 193.2 1200 0.01718 193.3 1200 0.01718 193.4 1200 0.01717 193.5 1200 0.01717 193.6 1200 0.01717 193.7 1200 0.01717 193.8 1200 0.01717 193.9 1200 0.01715 194 1200 0.01717 194.1 1200 0.01715 194.2 1200 0.01717 194.3 1200 0.01715 194.4 1200 0.01715 194.5 1200 0.01717 194.6 1200 0.01717 194.8 1200 0.01718 194.9 1200 0.01717 195 1200 0.01717 195.1 1200 0.01718 195.2 1200 0.01718 195.3 1200 0.01718 195.4 1200 0.01719 195.5 1200 0.01718 195.6 1200 0.01718 195.7 1200 0.01718 195.8 1200 0.01717 195.9 1200 0.01717 196 1200 0.01717 196.1 1200 0.01718 196.2 1200 0.01719 196.3 1200 0.01722 196.4 1200 0.01722 196.6 1200 0.01724 196.7 1200 0.01724 196.8 1200 0.01725 196.9 1200 0.01727 197 1200 0.01728 197.1 1200 0.01729 197.2 1200 0.01728 197.3 1200 0.01727 197.4 1200 0.01728 197.5 1200 0.01729 197.6 1200 0.01729 197.7 1200 0.01729 197.8 1200 0.01729 197.9 1200 0.0173 198 1201 0.0173 198.1 1200 0.01732 198.2 1200 0.01732 198.4 1200 0.01732 198.5 1200 0.01733 198.6 1200 0.01732 198.7 1200 0.01732 198.8 1200 0.01734 198.9 1200 0.01734 199 1200 0.01734 199.1 1200 0.01735 199.2 1200 0.01735 199.3 1200 0.01735 199.4 1200 0.01736 199.5 1200 0.01738 199.6 1200 0.01736 199.7 1200 0.01736 199.8 1200 0.01736 199.9 1200 0.01738 200 1200 0.01736 200.2 1200 0.01736 200.3 1200 0.01736 200.4 1200 0.01736 200.5 1200 0.01735 200.6 1200 0.01734 200.7 1200 0.01733 200.8 1200 0.01733 200.9 1200 0.01732 201 1200 0.01732 201.1 1200 0.01732 201.2 1200 0.0173 201.3 1200 0.01729 201.4 1200 0.01728 201.5 1200 0.01727 201.6 1200 0.01727 201.7 1200 0.01728 201.8 1200 0.01727 202 1200 0.01727 202.1 1200 0.01727 202.2 1200 0.01727 202.3 1200 0.01727 202.4 1200 0.01725 202.5 1200 0.01724 202.6 1200 0.01722 202.7 1200 0.01723 202.8 1200 0.01722 202.9 1200 0.01722 203 1200 0.01722 203.1 1200 0.01722 203.2 1200 0.01722 203.3 1200 0.0172 203.4 1200 0.01722 203.5 1200 0.01722 203.7 1200 0.01722 203.8 1200 0.01722 203.9 1200 0.01722 204 1200 0.01722 204.1 1200 0.01722 204.2 1200 0.0172 204.3 1200 0.0172 204.4 1200 0.0172 204.5 1200 0.01722 204.6 1200 0.01722 204.7 1200 0.01722 204.8 1200 0.01722 204.9 1200 0.01723 205 1200 0.01724 205.1 1200 0.01724 205.2 1200 0.01725 205.3 1200 0.01725 205.5 1200 0.01725 205.6 1200 0.01725 205.7 1200 0.01725 205.8 1200 0.01727 205.9 1200 0.01725 206 1200 0.01725 206.1 1200 0.01725 206.2 1200 0.01725 206.3 1200 0.01727 206.4 1200 0.01727 206.5 1200 0.01725 206.6 1200 0.01725 206.7 1200 0.01725 206.8 1200 0.01727 206.9 1200 0.01727 207 1200 0.01724 207.1 1200 0.01724 207.3 1200 0.01724 207.4 1200 0.01724 207.5 1200 0.01724 207.6 1200 0.01724 207.7 1200 0.01722 207.8 1200 0.01722 207.9 1200 0.01722 208 1200 0.01722 208.1 1200 0.01722 208.2 1200 0.01722 208.3 1200 0.01722 208.4 1200 0.01722 208.5 1200 0.01723 208.6 1200 0.01723 208.7 1200 0.01722 208.8 1200 0.01719 208.9 1200 0.01718 209.1 1200 0.01718 209.2 1200 0.01718 209.3 1200 0.01718 209.4 1200 0.01717 209.5 1200 0.01717 209.6 1200 0.01717 209.7 1200 0.01717 209.8 1200 0.01717 209.9 1200 0.01714 210 1200 0.01713 210.1 1200 0.01713 210.2 1200 0.01714 210.3 1200 0.01714 210.4 1200 0.01715 210.5 1200 0.01714 210.6 1200 0.01714 210.8 1201 0.01715 210.9 1200 0.01715 211 1200 0.01717 211.1 1199 0.01715 211.2 1200 0.01715 211.3 1200 0.01715 211.4 1200 0.01715 211.5 1200 0.01715 211.6 1200 0.01717 211.7 1200 0.01717 211.8 1200 0.01718 211.9 1200 0.01718 212 1200 0.01719 212.1 1200 0.01719 212.2 1200 0.01719 212.3 1200 0.01719 212.4 1200 0.01719 212.6 1200 0.0172 212.7 1200 0.01722 212.8 1200 0.0172 212.9 1200 0.01722 213 1200 0.01722 213.1 1200 0.01722 213.2 1200 0.01723 213.3 1200 0.01723 213.4 1200 0.01724 213.5 1200 0.01724 213.6 1200 0.01725 213.7 1200 0.01725 213.8 1200 0.01727 213.9 1200 0.01727 214 1200 0.01727 214.1 1200 0.01727 214.2 1200 0.01727 214.4 1200 0.01728 214.5 1200 0.01729 214.6 1200 0.01729 214.7 1200 0.01729 214.8 1200 0.01732 214.9 1200 0.01733 215 1200 0.01733 215.1 1200 0.01734 215.2 1200 0.01734 215.3 1200 0.01735 215.4 1200 0.01735 215.5 1200 0.01735 215.6 1200 0.01735 215.7 1200 0.01736 215.8 1200 0.01735 215.9 1200 0.01736 216 1200 0.01738 216.2 1200 0.01738 216.3 1200 0.01738 216.4 1200 0.01738 216.5 1200 0.01736 216.6 1200 0.01736 216.7 1200 0.01738 216.8 1200 0.01736 216.9 1200 0.01736 217 1200 0.01735 217.1 1200 0.01734 217.2 1200 0.01734 217.3 1200 0.01732 217.4 1200 0.01733 217.5 1200 0.01732 217.6 1200 0.01732 217.7 1200 0.01732 217.8 1200 0.01732 218 1200 0.0173 218.1 1200 0.01729 218.2 1200 0.01729 218.3 1200 0.0173 218.4 1200 0.01729 218.5 1200 0.01729 218.6 1200 0.01728 218.7 1200 0.01728 218.8 1200 0.01727 218.9 1200 0.01727 219 1200 0.01727 219.1 1200 0.01727 219.2 1200 0.01727 219.3 1200 0.01727 219.4 1200 0.01725 219.5 1200 0.01724 219.7 1200 0.01725 219.8 1200 0.01724 219.9 1200 0.01725 220 1200 0.01725 220.1 1200 0.01725 220.2 1200 0.01724 220.3 1200 0.01723 220.4 1200 0.01722 220.5 1200 0.01722 220.6 1200 0.01722 220.7 1200 0.01722 220.8 1200 0.01722 220.9 1200 0.01722 221 1200 0.01722 221.1 1200 0.01722 221.2 1200 0.01724 221.3 1200 0.01722 221.5 1200 0.01722 221.6 1200 0.01722 221.7 1200 0.01722 221.8 1200 0.01722 221.9 1200 0.01722 222 1200 0.01722 222.1 1200 0.01722 222.2 1200 0.01723 222.3 1200 0.01724 222.4 1200 0.01724 222.5 1200 0.01724 222.6 1200 0.01724 222.7 1200 0.01725 222.8 1200 0.01725 222.9 1200 0.01725 223 1200 0.01725 223.1 1200 0.01727 223.3 1200 0.01725 223.4 1200 0.01725 223.5 1200 0.01727 223.6 1200 0.01727 223.7 1200 0.01725 223.8 1200 0.01725 223.9 1200 0.01725 224 1200 0.01725 224.1 1200 0.01724 224.2 1200 0.01724 224.3 1200 0.01724 224.4 1200 0.01724 224.5 1200 0.01724 224.6 1200 0.01724 224.7 1200 0.01722 224.8 1200 0.01722 224.9 1200 0.01722 225.1 1200 0.01722 225.2 1200 0.01722 225.3 1200 0.0172 225.4 1200 0.01718 225.5 1200 0.01718 225.6 1200 0.01718 225.7 1200 0.01717 225.8 1200 0.01717 225.9 1200 0.01717 226 1200 0.01717 226.1 1200 0.01717 226.2 1200 0.01717 226.3 1200 0.01717 226.4 1200 0.01715 226.5 1200 0.01714 226.6 1200 0.01713 226.8 1200 0.01712 226.9 1200 0.01712 227 1200 0.01712 227.1 1200 0.01712 227.2 1200 0.01712 227.3 1200 0.01712 227.4 1200 0.01712 227.5 1200 0.01712 227.6 1200 0.01712 227.7 1200 0.01712 227.8 1200 0.01712 227.9 1200 0.01713 228 1200 0.01714 228.1 1200 0.01714 228.2 1200 0.01714 228.3 1200 0.01714 228.4 1200 0.01714 228.6 1200 0.01714 228.7 1200 0.01714 228.8 1200 0.01713 228.9 1200 0.01713 229 1200 0.01713 229.1 1200 0.01714 229.2 1200 0.01714 229.3 1200 0.01714 229.4 1200 0.01715 229.5 1200 0.01717 229.6 1200 0.01717 229.7 1200 0.01717 229.8 1200 0.01717 229.9 1200 0.01718 230 1200 0.01718 230.1 1200 0.01718 230.2 1200 0.01719 230.4 1200 0.01719 230.5 1200 0.01719 230.6 1200 0.0172 230.7 1200 0.0172 230.8 1200 0.0172 230.9 1200 0.01722 231 1200 0.01723 231.1 1200 0.01724 231.2 1200 0.01724 231.3 1200 0.01724 231.4 1200 0.01724 231.5 1200 0.01725 231.6 1200 0.01725 231.7 1200 0.01725 231.8 1200 0.01727 231.9 1200 0.01728 232 1200 0.01728 232.2 1200 0.01729 232.3 1200 0.0173 232.4 1200 0.01732 232.5 1200 0.01732 232.6 1200 0.01733 232.7 1200 0.01734 232.8 1200 0.01734 232.9 1200 0.01733 233 1200 0.01732 233.1 1200 0.01732 233.2 1200 0.01732 233.3 1200 0.01732 233.4 1200 0.01732 233.5 1200 0.01733 233.6 1200 0.01733 233.7 1200 0.01734 233.8 1200 0.01734 234 1200 0.01735 234.1 1200 0.01735 234.2 1200 0.01735 234.3 1200 0.01734 234.4 1200 0.01734 234.5 1200 0.01734 234.6 1200 0.01733 234.7 1200 0.01732 234.8 1200 0.01732 234.9 1200 0.01732 235 1200 0.01732 235.1 1200 0.01732 235.2 1200 0.01732 235.3 1200 0.01729 235.4 1200 0.01729 235.5 1200 0.01729 235.7 1200 0.0173 235.8 1200 0.01729 235.9 1200 0.01728 236 1200 0.01727 236.1 1200 0.01728 236.2 1200 0.01727 236.3 1200 0.01725 236.4 1200 0.01724 236.5 1200 0.01723 236.6 1200 0.01723 236.7 1200 0.01722 236.8 1200 0.01722 236.9 1200 0.01722 237 1200 0.01724 237.1 1200 0.01723 237.2 1200 0.01722 237.3 1200 0.01722 237.5 1200 0.01722 237.6 1200 0.01722 237.7 1200 0.01722 237.8 1200 0.01722 237.9 1200 0.01722 238 1200 0.01722 238.1 1200 0.01722 238.2 1200 0.01722 238.3 1200 0.01723 238.4 1200 0.01722 238.5 1200 0.01722 238.6 1200 0.01722 238.7 1200 0.01722 238.8 1200 0.01722 238.9 1200 0.01722 239 1200 0.01722 239.1 1200 0.01722 239.3 1200 0.01722 239.4 1200 0.0172 239.5 1200 0.01722 239.6 1200 0.0172 239.7 1200 0.01722 239.8 1200 0.01722 239.9 1200 0.01722 240 1200 0.0172 240.1 1200 0.01722 240.2 1200 0.01723 240.3 1200 0.01724 240.4 1200 0.01724 240.5 1200 0.01724 240.6 1200 0.01723 240.7 1200 0.01722 240.8 1200 0.01722 240.9 1200 0.01722 241.1 1200 0.01723 241.2 1200 0.01723 241.3 1200 0.01724 241.4 1200 0.01724 241.5 1200 0.01725 241.6 1200 0.01724 241.7 1200 0.01723 241.8 1200 0.01723 241.9 1200 0.01722 242 1200 0.01722 242.1 1200 0.01724 242.2 1200 0.01724 242.3 1200 0.01723 242.4 1200 0.01722 242.5 1200 0.01722 242.6 1200 0.01722 242.7 1200 0.01723 242.9 1200 0.01723 243 1200 0.01724 243.1 1200 0.01723 243.2 1201 0.01723 243.3 1200 0.01722 243.4 1200 0.01722 243.5 1200 0.01722 243.6 1200 0.01722 243.7 1200 0.01722 243.8 1200 0.0172 243.9 1200 0.01718 244 1200 0.01718 244.1 1200 0.01717 244.2 1200 0.01718 244.3 1200 0.01717 244.4 1200 0.01717 244.6 1200 0.01717 244.7 1200 0.01717 244.8 1200 0.01717 244.9 1200 0.01717 245 1200 0.01717 245.1 1200 0.01715 245.2 1200 0.01715 245.3 1200 0.01714 245.4 1200 0.01713 245.5 1200 0.01714 245.6 1200 0.01714 245.7 1200 0.01713 245.8 1200 0.01712 245.9 1200 0.01712 246 1200 0.01712 246.1 1200 0.01712 246.2 1200 0.01712 246.4 1200 0.01711 246.5 1200 0.01709 246.6 1200 0.01709 246.7 1200 0.01709 246.8 1200 0.01712 246.9 1200 0.01712 247 1200 0.01712 247.1 1200 0.01713 247.2 1200 0.01714 247.3 1200 0.01714 247.4 1200 0.01714 247.5 1200 0.01714 247.6 1200 0.01714 247.7 1200 0.01715 247.8 1200 0.01715 247.9 1200 0.01715 248 1200 0.01715 248.2 1200 0.01717 248.3 1200 0.01717 248.4 1200 0.01719 248.5 1200 0.0172 248.6 1200 0.01722 248.7 1200 0.01722 248.8 1200 0.01724 248.9 1200 0.01724 249 1200 0.01724 249.1 1200 0.01724 249.2 1200 0.01725 249.3 1200 0.01724 249.4 1200 0.01724 249.5 1200 0.01724 249.6 1200 0.01724 249.7 1200 0.01724 249.8 1200 0.01724 250 1200 0.01725 250.1 1200 0.01727 250.2 1200 0.01727 250.3 1200 0.01728 250.4 1200 0.01728 250.5 1200 0.01729 250.6 1200 0.01729 250.7 1200 0.01728 250.8 1200 0.01728 250.9 1200 0.01729 251 1200 0.01729 251.1 1200 0.01732 251.2 1200 0.01733 251.3 1200 0.01733 251.4 1200 0.01734 251.5 1200 0.01734 251.7 1200 0.01735 251.8 1200 0.01735 251.9 1200 0.01735 252 1200 0.01735 252.1 1200 0.01735 252.2 1200 0.01735 252.3 1200 0.01736 252.4 1200 0.01736 252.5 1200 0.01735 252.6 1200 0.01734 252.7 1200 0.01734 252.8 1200 0.01733 252.9 1201 0.01733 253 1200 0.01732 253.1 1200 0.01732 253.2 1200 0.01732 253.3 1200 0.01732 253.5 1200 0.01732 253.6 1200 0.01732 253.7 1200 0.01732 253.8 1200 0.01732 253.9 1200 0.01732 254 1200 0.01732 254.1 1200 0.01732 254.2 1200 0.0173 254.3 1200 0.01729 254.4 1200 0.01729 254.5 1200 0.01728 254.6 1200 0.01728 254.7 1200 0.01727 254.8 1200 0.01727 254.9 1200 0.01727 255 1200 0.01725 255.1 1200 0.01724 255.3 1200 0.01723 255.4 1200 0.01723 255.5 1200 0.01724 255.6 1200 0.01724 255.7 1200 0.01724 255.8 1200 0.01724 255.9 1200 0.01722 256 1200 0.01722 256.1 1200 0.01722 256.2 1200 0.01722 256.3 1200 0.01722 256.4 1200 0.01722 256.5 1200 0.01722 256.6 1200 0.01722 256.7 1200 0.01722 256.8 1200 0.01722 256.9 1200 0.01722 257.1 1200 0.01722 257.2 1200 0.01719 257.3 1200 0.01718 257.4 1200 0.01719 257.5 1200 0.01719 257.6 1200 0.0172 257.7 1200 0.01722 257.8 1200 0.01722 257.9 1200 0.01722 258 1200 0.01722 258.1 1200 0.01722 258.2 1200 0.01723 258.3 1200 0.01724 258.4 1200 0.01724 258.5 1200 0.01725 258.6 1200 0.01724 258.7 1200 0.01724 258.9 1200 0.01724 259 1200 0.01724 259.1 1200 0.01724 259.2 1200 0.01725 259.3 1200 0.01725 259.4 1200 0.01725 259.5 1200 0.01725 259.6 1200 0.01725 259.7 1200 0.01727 259.8 1200 0.01727 259.9 1200 0.01725 260 1200 0.01725 260.1 1200 0.01725 260.2 1200 0.01727 260.3 1200 0.01724 260.4 1200 0.01724 260.6 1200 0.01724 260.7 1200 0.01724 260.8 1200 0.01724 260.9 1200 0.01724 261 1200 0.01724 261.1 1200 0.01722 261.2 1200 0.01722 261.3 1200 0.01722 261.4 1200 0.01722 261.5 1200 0.01722 261.6 1201 0.01722 261.7 1200 0.01722 261.8 1200 0.01719 261.9 1200 0.01718 262 1200 0.01718 262.1 1200 0.01718 262.2 1200 0.01718 262.4 1200 0.01718 262.5 1200 0.01718 262.6 1200 0.01718 262.7 1200 0.01718 262.8 1200 0.01715 262.9 1200 0.01714 263 1200 0.01713 263.1 1200 0.01713 263.2 1200 0.01713 263.3 1200 0.01712 263.4 1200 0.01712 263.5 1200 0.01712 263.6 1200 0.01713 263.7 1200 0.01714 263.8 1200 0.01714 263.9 1200 0.01713 264 1200 0.01713 264.2 1200 0.01712 264.3 1200 0.01712 264.4 1200 0.01712 264.5 1200 0.01712 264.6 1200 0.01712 264.7 1200 0.01712 264.8 1200 0.01713 264.9 1200 0.01713 265 1200 0.01713 265.1 1200 0.01713 265.2 1200 0.01713 265.3 1200 0.01712 265.4 1200 0.01712 265.5 1200 0.01713 265.6 1200 0.01714 265.7 1200 0.01714 265.8 1200 0.01714 266 1200 0.01714 266.1 1200 0.01715 266.2 1200 0.01714 266.3 1200 0.01715 266.4 1200 0.01715 266.5 1200 0.01717 266.6 1200 0.01717 266.7 1200 0.01718 266.8 1200 0.01717 266.9 1200 0.01718 267 1200 0.01718 267.1 1200 0.01718 267.2 1200 0.01719 267.3 1200 0.0172 267.4 1201 0.01722 267.5 1200 0.01722 267.6 1200 0.01722 267.8 1200 0.01724 267.9 1200 0.01724 268 1200 0.01725 268.1 1200 0.01725 268.2 1200 0.01725 268.3 1201 0.01725 268.4 1200 0.01725 268.5 1200 0.01727 268.6 1200 0.01727 268.7 1200 0.01725 268.8 1200 0.01727 268.9 1200 0.01729 269 1200 0.01732 269.1 1200 0.01732 269.2 1200 0.0173 269.3 1200 0.0173 269.5 1200 0.01732 269.6 1200 0.01732 269.7 1200 0.01732 269.8 1200 0.01732 269.9 1200 0.01732 270 1200 0.01732 270.1 1200 0.01732 270.2 1200 0.01734 270.3 1200 0.01734 270.4 1201 0.01734 270.5 1200 0.01735 270.6 1200 0.01735 270.7 1201 0.01736 270.8 1200 0.01735 270.9 1200 0.01735 271 1200 0.01735 271.1 1200 0.01736 271.3 1200 0.01735 271.4 1200 0.01734 271.5 1200 0.01734 271.6 1200 0.01734 271.7 1200 0.01735 271.8 1200 0.01735 271.9 1200 0.01735 272 1200 0.01735 272.1 1200 0.01734 272.2 1200 0.01734 272.3 1200 0.01734 272.4 1200 0.01735 272.5 1200 0.01734 272.6 1200 0.01734 272.7 1200 0.01732 272.8 1200 0.01732 272.9 1200 0.0173 273.1 1200 0.0173 273.2 1200 0.0173 273.3 1200 0.0173 273.4 1200 0.01728 273.5 1200 0.01728 273.6 1200 0.01727 273.7 1200 0.01727 273.8 1200 0.01727 273.9 1200 0.01727 274 1200 0.01724 274.1 1200 0.01724 274.2 1200 0.01724 274.3 1200 0.01724 274.4 1200 0.01722 274.5 1200 0.01722 274.6 1200 0.01722 274.7 1200 0.01722 274.9 1200 0.01722 275 1200 0.01722 275.1 1200 0.01722 275.2 1200 0.01722 275.3 1200 0.01723 275.4 1200 0.01723 275.5 1200 0.01724 275.6 1200 0.01724 275.7 1200 0.01724 275.8 1200 0.01722 275.9 1200 0.01722 276 1200 0.01722 276.1 1200 0.01722 276.2 1200 0.01722 276.3 1200 0.01722 276.4 1200 0.01722 276.6 1200 0.01722 276.7 1200 0.01722 276.8 1200 0.01722 276.9 1200 0.01722 277 1200 0.01722 277.1 1200 0.01724 277.2 1200 0.01724 277.3 1200 0.01724 277.4 1200 0.01724 277.5 1200 0.01722 277.6 1200 0.01724 277.7 1200 0.01724 277.8 1200 0.01724 277.9 1200 0.01724 278 1200 0.01724 278.1 1200 0.01724 278.2 1200 0.01724 278.4 1200 0.01724 278.5 1200 0.01722 278.6 1200 0.01723 278.7 1200 0.01724 278.8 1200 0.01724 278.9 1200 0.01725 279 1200 0.01725 279.1 1200 0.01725 279.2 1200 0.01725 279.3 1200 0.01724 279.4 1200 0.01724 279.5 1200 0.01724 279.6 1200 0.01722 279.7 1200 0.01722 279.8 1200 0.01723 279.9 1200 0.01724 280 1200 0.01724 280.2 1200 0.01725 280.3 1200 0.01724 280.4 1200 0.01724 280.5 1200 0.01723 280.6 1200 0.01723 280.7 1200 0.01722 280.8 1200 0.01722 280.9 1200 0.01722 281 1200 0.01722 281.1 1200 0.01719 281.2 1200 0.01719 281.3 1200 0.01719 281.4 1200 0.01719 281.5 1200 0.01718 281.6 1200 0.01718 281.7 1200 0.01718 281.8 1200 0.01718 282 1200 0.01718 282.1 1200 0.01718 282.2 1200 0.01718 282.3 1200 0.01717 282.4 1200 0.01717 282.5 1200 0.01717 282.6 1200 0.01715 282.7 1200 0.01717 282.8 1200 0.01715 282.9 1200 0.01717 283 1200 0.01715 283.1 1200 0.01715 283.2 1200 0.01714 283.3 1200 0.01713 283.4 1200 0.01713 283.5 1200 0.01714 283.6 1200 0.01714 283.8 1200 0.01714 283.9 1200 0.01714 284 1200 0.01713 284.1 1200 0.01713 284.2 1200 0.01712 284.3 1200 0.01712 284.4 1200 0.01712 284.5 1200 0.01713 284.6 1200 0.01713 284.7 1200 0.01714 284.8 1200 0.01714 284.9 1200 0.01714 285 1200 0.01714 285.1 1200 0.01714 285.2 1200 0.01715 285.3 1200 0.01715 285.5 1200 0.01715 285.6 1200 0.01715 285.7 1200 0.01715 285.8 1200 0.01717 285.9 1200 0.01717 286 1200 0.01717 286.1 1200 0.01718 286.2 1200 0.01718 286.3 1200 0.01719 286.4 1200 0.01719 286.5 1200 0.0172 286.6 1200 0.01719 286.7 1200 0.0172 286.8 1200 0.0172 286.9 1200 0.01722 287 1200 0.01724 287.1 1200 0.01724 287.3 1200 0.01724 287.4 1200 0.01725 287.5 1200 0.01727 287.6 1200 0.01728 287.7 1200 0.01728 287.8 1200 0.01729 287.9 1200 0.0173 288 1200 0.01729 288.1 1200 0.01732 288.2 1200 0.01732 288.3 1200 0.01732 288.4 1201 0.0173 288.5 1200 0.01732 288.6 1200 0.01732 288.7 1200 0.01734 288.8 1200 0.01734 288.9 1200 0.01734 289.1 1200 0.01735 289.2 1200 0.01735 289.3 1200 0.01735 289.4 1200 0.01736 289.5 1200 0.01735 289.6 1200 0.01736 289.7 1200 0.01735 289.8 1200 0.01736 289.9 1200 0.01738 290 1200 0.01739 290.1 1200 0.01739 290.2 1200 0.01739 290.3 1200 0.01738 290.4 1200 0.01738 290.5 1200 0.01739 290.6 1200 0.01738 290.7 1200 0.01739 290.9 1200 0.01738 291 1200 0.01738 291.1 1200 0.01736 291.2 1200 0.01735 291.3 1200 0.01735 291.4 1200 0.01735 291.5 1200 0.01735 291.6 1200 0.01734 291.7 1200 0.01733 291.8 1200 0.01732 291.9 1200 0.0173 292 1200 0.0173 292.1 1200 0.01732 292.2 1199 0.01729 292.3 1200 0.01729 292.4 1200 0.01728 292.6 1200 0.01728 292.7 1200 0.01727 292.8 1200 0.01727 292.9 1200 0.01727 293 1200 0.01727 293.1 1200 0.01727 293.2 1200 0.01727 293.3 1200 0.01727 293.4 1200 0.01727 293.5 1200 0.01727 293.6 1200 0.01727 293.7 1200 0.01725 293.8 1200 0.01725 293.9 1200 0.01727 294 1200 0.01727 294.1 1200 0.01727 294.2 1200 0.01725 294.4 1200 0.01725 294.5 1200 0.01725 294.6 1200 0.01727 294.7 1200 0.01725 294.8 1200 0.01724 294.9 1200 0.01724 295 1200 0.01723 295.1 1200 0.01723 295.2 1200 0.01722 295.3 1200 0.01719 295.4 1200 0.01719 295.5 1200 0.01719 295.6 1200 0.01722 295.7 1200 0.0172 295.8 1200 0.01719 295.9 1200 0.01719 296 1200 0.01718 296.2 1200 0.01718 296.3 1200 0.01719 296.4 1200 0.0172 296.5 1200 0.01719 296.6 1200 0.0172 296.7 1200 0.01722 296.8 1200 0.01724 296.9 1200 0.01724 297 1200 0.01727 297.1 1200 0.01727 297.2 1200 0.01728 297.3 1200 0.01728 297.4 1200 0.01729 297.5 1200 0.01727 297.6 1200 0.01727 297.7 1200 0.01727 297.8 1200 0.01727 298 1200 0.01727 298.1 1200 0.01727 298.2 1200 0.01728 298.3 1200 0.01729 298.4 1200 0.01729 298.5 1200 0.01729 298.6 1200 0.0173 298.7 1200 0.01729 298.8 1200 0.0173 298.9 1200 0.0173 299 1200 0.01732 299.1 1200 0.01732 299.2 1200 0.01732 299.3 1200 0.01729 299.4 1200 0.01729 299.5 1200 0.01728 299.6 1200 0.01728 299.8 1200 0.01727 299.9 1200 0.01725 300 1200 0.01724 300.1 1200 0.01724 300.2 1200 0.01723 300.3 1200 0.01723 300.4 1200 0.01722 300.5 1200 0.01722 300.6 1200 0.01722 300.7 1200 0.01722 300.8 1200 0.01722 300.9 1200 0.01722 301 1200 0.01722 301.1 1200 0.0172 301.2 1200 0.01722 301.3 1200 0.01722 301.5 1200 0.01722 301.6 1200 0.0172 301.7 1200 0.0172 301.8 1200 0.01719 301.9 1200 0.01718 302 1200 0.01718 302.1 1200 0.01718 302.2 1200 0.01717 302.3 1200 0.01717 302.4 1200 0.01717 302.5 1200 0.01718 302.6 1200 0.01718 302.7 1200 0.01718 302.8 1200 0.01717 302.9 1200 0.01717 303 1200 0.01717 303.1 1200 0.01717 303.3 1200 0.01717 303.4 1200 0.01717 303.5 1200 0.01715 303.6 1200 0.01715 303.7 1200 0.01715 303.8 1200 0.01717 303.9 1200 0.01717 304 1200 0.01717 304.1 1200 0.01718 304.2 1200 0.01717 304.3 1200 0.01717 304.4 1200 0.01718 304.5 1200 0.01718 304.6 1200 0.01718 304.7 1200 0.01719 304.8 1200 0.0172 304.9 1200 0.0172 305.1 1200 0.01719 305.2 1200 0.01719 305.3 1200 0.0172 305.4 1200 0.01722 305.5 1200 0.01722 305.6 1200 0.01722 305.7 1200 0.0172 305.8 1200 0.0172 305.9 1200 0.01722 306 1200 0.01722 306.1 1200 0.01722 306.2 1200 0.01722 306.3 1200 0.01722 306.4 1200 0.01722 306.5 1200 0.01724 306.6 1200 0.01724 306.7 1200 0.01724 306.9 1200 0.01724 307 1200 0.01724 307.1 1200 0.01725 307.2 1200 0.01727 307.3 1200 0.01727 307.4 1200 0.01728 307.5 1200 0.01729 307.6 1200 0.01732 307.7 1200 0.01732 307.8 1200 0.01733 307.9 1200 0.01734 308 1200 0.01734 308.1 1200 0.01735 308.2 1200 0.01735 308.3 1200 0.01736 308.4 1200 0.01738 308.5 1200 0.01738 308.7 1200 0.01739 308.8 1200 0.01739 308.9 1200 0.01738 309 1200 0.01739 309.1 1200 0.01739 309.2 1200 0.01739 309.3 1200 0.01739 309.4 1200 0.0174 309.5 1200 0.01741 309.6 1200 0.01741 309.7 1200 0.0174 309.8 1200 0.01739 309.9 1200 0.01739 310 1200 0.01741 310.1 1200 0.01741 310.2 1200 0.01741 310.4 1200 0.01741 310.5 1200 0.01741 310.6 1200 0.01744 310.7 1200 0.01744 310.8 1200 0.01741 310.9 1200 0.01741 311 1200 0.01738 311.1 1200 0.01736 311.2 1200 0.01736 311.3 1200 0.01736 311.4 1200 0.01735 311.5 1200 0.01735 311.6 1200 0.01734 311.7 1200 0.01735 311.8 1200 0.01735 311.9 1200 0.01735 312 1200 0.01735 312.2 1200 0.01736 312.3 1200 0.01734 312.4 1200 0.01734 312.5 1200 0.01734 312.6 1200 0.01734 312.7 1200 0.01734 312.8 1200 0.01734 312.9 1200 0.01733 313 1200 0.01733 313.1 1200 0.01732 313.2 1200 0.01732 313.3 1200 0.01732 313.4 1200 0.01732 313.5 1200 0.01732 313.6 1200 0.01732 313.7 1199 0.01729 313.8 1200 0.01729 314 1200 0.01728 314.1 1200 0.01728 314.2 1200 0.01728 314.3 1200 0.01727 314.4 1200 0.01727 314.5 1200 0.01727 314.6 1200 0.01727 314.7 1200 0.01727 314.8 1200 0.01727 314.9 1200 0.01725 315 1200 0.01724 315.1 1200 0.01724 315.2 1200 0.01725 315.3 1200 0.01725 315.4 1200 0.01725 315.5 1200 0.01725 315.6 1200 0.01724 315.8 1200 0.01725 315.9 1200 0.01727 316 1200 0.01725 316.1 1200 0.01725 316.2 1200 0.01725 316.3 1200 0.01725 316.4 1200 0.01727 316.5 1200 0.01727 316.6 1200 0.01725 316.7 1200 0.01725 316.8 1200 0.01727 316.9 1200 0.01725 317 1200 0.01727 317.1 1200 0.01727 317.2 1200 0.01725 317.3 1200 0.01725 317.5 1200 0.01725 317.6 1200 0.01727 317.7 1200 0.01728 317.8 1200 0.01728 317.9 1200 0.01729 318 1200 0.01729 318.1 1200 0.01729 318.2 1200 0.01732 318.3 1201 0.0173 318.4 1200 0.01732 318.5 1200 0.0173 318.6 1200 0.01729 318.7 1200 0.01729 318.8 1200 0.01729 318.9 1200 0.01727 319 1200 0.01727 319.1 1200 0.01727 319.3 1200 0.01727 319.4 1200 0.01727 319.5 1200 0.01727 319.6 1200 0.01727 319.7 1200 0.01727 319.8 1200 0.01727 319.9 1200 0.01727 320 1200 0.01727 320.1 1200 0.01727 320.2 1200 0.01727 320.3 1200 0.01727 320.4 1200 0.01728 320.5 1200 0.01728 320.6 1200 0.01727 320.7 1200 0.01727 320.8 1200 0.01727 320.9 1200 0.01727 321.1 1200 0.01727 321.2 1200 0.01727 321.3 1200 0.01725 321.4 1200 0.01724 321.5 1200 0.01725 321.6 1200 0.01725 321.7 1200 0.01725 321.8 1200 0.01725 321.9 1200 0.01725 322 1200 0.01724 322.1 1200 0.01724 322.2 1200 0.01723 322.3 1200 0.01723 322.4 1200 0.01722 322.5 1200 0.01722 322.6 1200 0.0172 322.7 1200 0.01719 322.9 1200 0.01718 323 1200 0.01719 323.1 1200 0.0172 323.2 1200 0.01719 323.3 1200 0.0172 323.4 1200 0.01719 323.5 1200 0.01718 323.6 1200 0.01718 323.7 1200 0.01717 323.8 1200 0.01717 323.9 1200 0.01718 324 1200 0.01718 324.1 1200 0.01719 324.2 1200 0.0172 324.3 1200 0.01719 324.4 1200 0.0172 324.5 1200 0.01719 324.7 1200 0.0172 324.8 1200 0.01722 324.9 1200 0.01722 325 1200 0.01722 325.1 1200 0.01722 325.2 1200 0.01722 325.3 1200 0.01722 325.4 1200 0.01722 325.5 1200 0.01722 325.6 1200 0.01722 325.7 1200 0.01722 325.8 1200 0.01722 325.9 1200 0.01722 326 1200 0.01724 326.1 1200 0.01722 326.2 1200 0.01722 326.4 1200 0.01724 326.5 1200 0.01725 326.6 1200 0.01727 326.7 1200 0.01728 326.8 1200 0.01728 326.9 1200 0.01727 327 1200 0.01727 327.1 1200 0.01728 327.2 1200 0.0173 327.3 1200 0.01729 327.4 1200 0.01729 327.5 1200 0.0173 327.6 1200 0.0173 327.7 1200 0.01732 327.8 1200 0.01732 327.9 1200 0.01733 328 1200 0.01733 328.2 1200 0.01734 328.3 1200 0.01735 328.4 1200 0.01735 328.5 1200 0.01735 328.6 1200 0.01735 328.7 1200 0.01735 328.8 1200 0.01736 328.9 1200 0.01736 329 1200 0.01736 329.1 1200 0.01738 329.2 1200 0.01738 329.3 1200 0.01739 329.4 1200 0.01739 329.5 1200 0.01739 329.6 1200 0.01738 329.7 1200 0.01739 329.8 1200 0.01739 330 1200 0.01739 330.1 1200 0.01741 330.2 1200 0.01744 330.3 1200 0.01744 330.4 1200 0.01744 330.5 1200 0.01744 330.6 1200 0.01745 330.7 1200 0.01745 330.8 1200 0.01746 330.9 1200 0.01746 331 1200 0.01746 331.1 1200 0.01746 331.2 1200 0.01746 331.3 1200 0.01746 331.4 1200 0.01746 331.5 1200 0.01744 331.6 1200 0.01744 331.8 1200 0.01741 331.9 1200 0.01741 332 1201 0.0174 332.1 1200 0.01739 332.2 1200 0.01739 332.3 1200 0.01739 332.4 1200 0.01739 332.5 1200 0.01739 332.6 1200 0.01738 332.7 1200 0.01738 332.8 1200 0.01736 332.9 1200 0.01736 333 1200 0.01736 333.1 1200 0.01736 333.2 1200 0.01736 333.3 1200 0.01736 333.4 1200 0.01735 333.6 1200 0.01734 333.7 1200 0.01733 333.8 1200 0.01733 333.9 1200 0.01733 334 1200 0.01732 334.1 1200 0.01732 334.2 1200 0.01733 334.3 1200 0.01734 334.4 1200 0.01734 334.5 1200 0.01733 334.6 1200 0.01732 334.7 1200 0.01732 334.8 1200 0.01732 334.9 1200 0.01732 335 1200 0.01732 335.1 1200 0.01732 335.3 1199 0.01732 335.4 1200 0.01732 335.5 1200 0.01732 335.6 1200 0.01732 335.7 1200 0.01729 335.8 1200 0.01729 335.9 1200 0.01728 336 1200 0.01727 336.1 1200 0.01728 336.2 1200 0.01729 336.3 1200 0.01729 336.4 1200 0.01729 336.5 1200 0.0173 336.6 1200 0.0173 336.7 1200 0.0173 336.8 1199 0.01732 336.9 1198 0.01729 337.1 1197 0.01727 337.2 1196 0.01723 337.3 1194 0.01718 337.4 1194 0.01715 337.5 1194 0.01712 337.6 1192 0.01709 337.7 1181 0.01704 337.8 1172 0.01702 337.9 1173 0.01699 338 1174 0.01698 338.1 1173 0.01697 338.2 1172 0.01691 338.3 1170 0.01687 338.4 1168 0.0168 338.5 1165 0.01675 338.6 1162 0.01667 338.7 1156 0.0166 338.9 1148 0.01655 339 1142 0.01646 339.1 1134 0.01639 339.2 1128 0.01633 339.3 1122 0.01628 339.4 1117 0.01623 339.5 1112 0.0162 339.6 1109 0.01614 339.7 1104 0.01608 339.8 1100 0.01603 339.9 1096 0.01596 340 1094 0.01591 340.1 1090 0.01583 340.2 1085 0.01577 340.3 1081 0.01571 340.4 1076 0.01562 340.5 1072 0.01556 340.7 1069 0.01549 340.8 1065 0.01543 340.9 1062 0.01534 341 1059 0.01525 341.1 1056 0.01518 341.2 1053 0.01509 341.3 1050 0.01501 341.4 1047 0.01491 341.5 1043 0.01485 341.6 1039 0.01475 341.7 1036 0.01469 341.8 1033 0.01462 341.9 1029 0.01452 342 1025 0.01448 342.1 1022 0.01438 342.2 1018 0.0143 342.4 1014 0.0142 342.5 1011 0.01411 342.6 1008 0.01402 342.7 1004 0.01393 342.8 1001 0.01385 342.9 998 0.01373 343 994 0.01366 343.1 992 0.01357 343.2 988 0.0135 343.3 984 0.0134 343.4 981 0.01331 343.5 978 0.01322 343.6 974 0.01314 343.7 970 0.01307 343.8 967 0.01294 343.9 964 0.01286 344 959 0.01277 344.2 956 0.0127 344.3 953 0.01265 344.4 950 0.01257 344.5 947 0.0125 344.6 943 0.01239 344.7 939 0.01231 344.8 936 0.0122 344.9 932 0.01211 345 929 0.01202 345.1 926 0.01193 345.2 922 0.01185 345.3 918 0.01176 345.4 915 0.01171 345.5 912 0.0116 345.6 907 0.01151 345.7 904 0.01143 345.8 901 0.01136 346 898 0.01129 346.1 893 0.0112 346.2 891 0.01114 346.3 887 0.01104 346.4 884 0.01097 346.5 881 0.01088 346.6 877 0.0108 346.7 874 0.0107 346.8 870 0.0106 346.9 866 0.0105 347 864 0.0104 347.1 859 0.01033 347.2 856 0.01024 347.3 853 0.01015 347.4 849 0.01007 347.5 847 0.009982 347.6 842 0.009908 347.8 839 0.009833 347.9 836 0.009759 348 832 0.009661 348.1 829 0.009599 348.2 826 0.009512 348.3 821 0.009463 348.4 818 0.009389 348.5 814 0.009303 348.6 811 0.009216 348.7 807 0.00913 348.8 803 0.009043 348.9 801 0.008969 349 800 0.008883 349.1 799 0.008796 349.2 793 0.008722 349.3 792 0.008648 349.4 787 0.008562 349.6 784 0.008488 349.7 781 0.008414 349.8 776 0.008327 349.9 775 0.008253 350 769 0.008167 350.1 768 0.008093 350.2 762 0.008006 350.3 762 0.007945 350.4 756 0.00787 350.5 753 0.007784 350.6 750 0.00771 350.7 746 0.007636 350.8 743 0.007562 350.9 739 0.007451 351 736 0.007389 351.1 732 0.007303 351.3 728 0.007241 351.4 726 0.007142 351.5 721 0.00708 351.6 718 0.006994 351.7 715 0.006907 351.8 712 0.006846 351.9 709 0.006772 352 704 0.006698 352.1 701 0.006611 352.2 698 0.006549 352.3 694 0.006451 352.4 691 0.006377 352.5 688 0.006303 352.6 684 0.006204 352.7 681 0.006117 352.8 677 0.006006 352.9 675 0.005932 353.1 670 0.005858 353.2 667 0.005784 353.3 664 0.005698 353.4 660 0.005599 353.5 657 0.005525 353.6 653 0.005438 353.7 650 0.005389 353.8 646 0.00529 353.9 642 0.005204 354 639 0.005117 354.1 635 0.005019 354.2 632 0.004932 354.3 628 0.004846 354.4 626 0.004796 354.5 621 0.00471 354.6 618 0.004648 354.7 615 0.004549 354.9 611 0.004451 355 609 0.004377 355.1 604 0.004278 355.2 601 0.004204 355.3 598 0.004105 355.4 594 0.004031 355.5 591 0.003932 355.6 587 0.003846 355.7 584 0.003759 355.8 581 0.003685 355.9 578 0.003611 356 574 0.003512 356.1 571 0.003414 356.2 567 0.00334 356.3 564 0.003253 356.4 560 0.003179 356.5 557 0.003093 356.7 554 0.003031 356.8 550 0.002944 356.9 547 0.00287 357 544 0.002772 357.1 540 0.002698 357.2 537 0.002599 357.3 534 0.0025 357.4 531 0.002426 357.5 528 0.00234 357.6 524 0.002253 357.7 521 0.002154 357.8 517 0.002068 357.9 514 0.001982 358 510 0.001907 358.1 506 0.001809 358.2 503 0.00171 358.3 500 0.001636 358.5 496 0.001525 358.6 493 0.001451 358.7 490 0.001352 358.8 487 0.001265 358.9 483 0.001154 359 480 0.001068 359.1 476 0.0009691 359.2 472 0.0008704 359.3 469 0.0007963 359.4 466 0.0007099 359.5 462 0.0006358 359.6 459 0.0005494 359.7 456 0.0004753 359.8 452 0.0004012 359.9 449 0.0003025 360 445 0.0002284 360.2 442 0.0001543 360.3 438 8.025e-05 360.4 435 6.173e-06 360.5 431 -6.173e-06 360.6 428 -0.0001049 360.7 424 -0.0002037 360.8 421 -0.0002778 360.9 417 -0.0003889 361 413 -0.0004753 361.1 410 -0.0005864 361.2 407 -0.0006728 361.3 403 -0.0007593 361.4 401 -0.000858 361.5 398 -0.0009321 361.6 394 -0.001043 361.7 390 -0.001117 361.8 387 -0.001228 362 384 -0.001315 362.1 381 -0.001401 362.2 377 -0.001488 362.3 373 -0.001574 362.4 370 -0.001673 362.5 367 -0.001747 362.6 363 -0.001846 362.7 359 -0.001907 362.8 356 -0.002006 362.9 353 -0.00208 363 349 -0.002167 363.1 346 -0.002241 363.2 343 -0.002315 363.3 340 -0.002377 363.4 337 -0.002438 363.5 334 -0.0025 363.6 331 -0.002574 363.8 329 -0.002623 363.9 328 -0.002685 364 324 -0.002722 364.1 323 -0.002759 364.2 320 -0.002784 364.3 318 -0.002796 364.4 317 -0.002796 364.5 315 -0.002784 364.6 313 -0.002784 364.7 312 -0.002759 364.8 310 -0.002722 364.9 309 -0.002685 365 307 -0.002636 365.1 306 -0.002599 365.2 304 -0.002068 365.3 302 -0.001512 365.4 301 -0.001389 365.6 300 -0.001537 365.7 299 -0.001648 365.8 298 -0.001698 365.9 296 -0.001735 366 295 -0.001722 366.1 293 -0.001698 366.2 293 -0.001673 366.3 292 -0.001623 366.4 290 -0.001574 366.5 288 -0.0015 366.6 287 -0.001451 366.7 286 -0.001352 366.8 285 -0.001278 366.9 282 -0.001179 367 281 -0.001105 367.1 281 -0.001043 367.3 278 -0.0009815 367.4 277 -0.0009198 367.5 276 -0.0008333 367.6 274 -0.0007593 367.7 273 -0.0006852 367.8 271 -0.0006235 367.9 270 -0.0005617 368 268 -0.0005 368.1 267 -0.0004383 368.2 265 -0.0003765 368.3 263 -0.0003395 368.4 262 -0.0002778 368.5 260 -0.0002284 368.6 259 -0.0002037 368.7 256 -0.0001543 368.8 256 -0.0001173 368.9 254 -6.79e-05 369.1 251 -3.086e-05 369.2 249 6.173e-06 369.3 248 6.173e-06 369.4 246 6.173e-06 369.5 244 6.173e-06 369.6 243 1.852e-05 369.7 242 4.321e-05 369.8 238 6.79e-05 369.9 237 0.0001049 370 235 0.0001296 370.1 234 0.0001296 370.2 232 0.000142 370.3 230 0.0001667 370.4 228 0.000179 370.5 226 0.0002161 370.6 224 0.0002284 370.7 223 0.0002531 370.9 221 0.0002654 371 218 0.0002778 371.1 217 0.0002901 371.2 215 0.0002901 371.3 213 0.0003025 371.4 212 0.0003272 371.5 209 0.0003272 371.6 207 0.0003272 371.7 206 0.0003395 371.8 204 0.0003395 371.9 202 0.0003395 372 201 0.0003272 372.1 199 0.0003272 372.2 197 0.0003272 372.3 195 0.0003025 372.4 193 0.0002901 372.5 191 0.0002778 372.7 190 0.0002778 372.8 188 0.0002654 372.9 187 0.0002407 373 184 0.0002284 373.1 182 0.0002284 373.2 181 0.0002161 373.3 179 0.0002037 373.4 177 0.0002037 373.5 176 0.0001914 373.6 174 0.000179 373.7 171 0.0001667 373.8 170 0.000142 373.9 168 0.0001296 374 166 0.0001296 374.1 165 0.0001173 374.2 162 0.0001049 374.3 160 9.259e-05 374.5 159 6.79e-05 374.6 157 5.556e-05 374.7 156 3.086e-05 374.8 154 6.173e-06 374.9 152 6.173e-06 375 150 6.173e-06 375.1 149 6.173e-06 375.2 148 6.173e-06 375.3 146 6.173e-06 375.4 144 6.173e-06 375.5 143 6.173e-06 375.6 141 -1.852e-05 375.7 140 -3.086e-05 375.8 138 -3.086e-05 375.9 137 -6.79e-05 376 135 -8.025e-05 376.2 134 -0.0001049 376.3 132 -0.0001296 376.4 131 -0.0001543 376.5 130 -0.0001667 376.6 129 -0.000179 376.7 127 -0.0002037 376.8 126 -0.0002161 376.9 124 -0.0002407 377 123 -0.0002654 377.1 122 -0.0002778 377.2 121 -0.0002901 377.3 120 -0.0003025 377.4 118 -0.0003395 377.5 118 -0.0003519 377.6 116 -0.0003765 377.7 115 -0.0004012 377.8 115 -0.0004136 378 113 -0.0004259 378.1 112 -0.0004506 378.2 112 -0.000463 378.3 110 -0.0004877 378.4 109 -0.0005124 378.5 109 -0.0005124 378.6 107 -0.0005247 378.7 106 -0.000537 378.8 106 -0.000537 378.9 105 -0.0005617 379 104 -0.0005864 379.1 102 -0.0005864 379.2 102 -0.0005988 379.3 101 -0.0006111 379.4 100 -0.0006358 379.5 99 -0.0006605 379.6 99 -0.0006728 379.8 98 -0.0006852 379.9 97 -0.0006975 380 96 -0.0007099 380.1 96 -0.0007099 380.2 95 -0.0007222 380.3 94 -0.0007346 380.4 93 -0.0007469 380.5 92 -0.0007593 380.6 91 -0.0007593 380.7 91 -0.0007593 380.8 90 -0.000784 380.9 90 -0.000784 381 89 -0.000784 381.1 88 -0.0007963 381.2 88 -0.0007963 381.3 87 -0.0007963 381.4 87 -0.0007963 381.6 86 -0.0007963 381.7 85 -0.0008087 381.8 84 -0.000821 381.9 84 -0.000821 382 84 -0.0008333 382.1 84 -0.0008457 382.2 83 -0.000858 382.3 82 -0.000858 382.4 81 -0.000858 382.5 81 -0.0008704 382.6 81 -0.0008704 382.7 80 -0.0008704 382.8 79 -0.0008827 382.9 79 -0.0008827 383 78 -0.0008827 383.1 77 -0.0008827 383.3 77 -0.0008951 383.4 77 -0.0008951 383.5 76 -0.0009074 383.6 76 -0.0009074 383.7 76 -0.0009074 383.8 74 -0.0009198 383.9 74 -0.0009321 384 74 -0.0009321 384.1 73 -0.0009321 384.2 73 -0.0009445 384.3 73 -0.0009568 384.4 72 -0.0009568 384.5 71 -0.0009691 384.6 71 -0.0009815 384.7 71 -0.0009938 384.8 70 -0.001006 384.9 70 -0.001006 385.1 70 -0.001031 385.2 69 -0.001031 385.3 69 -0.001031 385.4 68 -0.001043 385.5 68 -0.001043 385.6 68 -0.001043 385.7 68 -0.001056 385.8 66 -0.001056 385.9 66 -0.001068 386 66 -0.00108 386.1 66 -0.00108 386.2 65 -0.001105 386.3 65 -0.001105 386.4 65 -0.001117 386.5 65 -0.00113 386.6 65 -0.00113 386.7 63 -0.001142 386.9 64 -0.001142 387 63 -0.001142 387.1 63 -0.001154 387.2 63 -0.001154 387.3 62 -0.001154 387.4 62 -0.001154 387.5 62 -0.001167 387.6 62 -0.001179 387.7 61 -0.001179 387.8 60 -0.001179 387.9 60 -0.001191 388 60 -0.001204 388.1 59 -0.001204 388.2 59 -0.001216 388.3 59 -0.001216 388.4 59 -0.001216 388.5 59 -0.001216 388.7 59 -0.001204 388.8 59 -0.001216 388.9 58 -0.001216 389 57 -0.001228 389.1 57 -0.001228 389.2 57 -0.001241 389.3 57 -0.001241 389.4 56 -0.001253 389.5 55 -0.001253 389.6 55 -0.001241 389.7 55 -0.001228 389.8 55 -0.001241 389.9 55 -0.001241 390 55 -0.001241 390.1 55 -0.001253 390.2 55 -0.001253 390.3 55 -0.001253 390.5 54 -0.001253 390.6 54 -0.001253 390.7 54 -0.001253 390.8 53 -0.001253 390.9 52 -0.001253 391 52 -0.001253 391.1 52 -0.001253 391.2 52 -0.001253 391.3 52 -0.001253 391.4 52 -0.001253 391.5 52 -0.001253 391.6 52 -0.001253 391.7 52 -0.001253 391.8 52 -0.001278 391.9 51 -0.001278 392 51 -0.001278 392.2 50 -0.001278 392.3 50 -0.001265 392.4 50 -0.001265 392.5 49 -0.001253 392.6 49 -0.001253 392.7 50 -0.001241 392.8 49 -0.001228 392.9 49 -0.001228 393 49 -0.001228 393.1 48 -0.001241 393.2 48 -0.001253 393.3 48 -0.001253 393.4 48 -0.001253 393.5 48 -0.001253 393.6 48 -0.001228 393.7 48 -0.001216 393.8 48 -0.001216 394 48 -0.001216 394.1 47 -0.001204 394.2 46 -0.001216 394.3 46 -0.001204 394.4 46 -0.001204 394.5 46 -0.001204 394.6 46 -0.001179 394.7 46 -0.001179 394.8 46 -0.001179 394.9 46 -0.001167 395 46 -0.001179 395.1 45 -0.001154 395.2 45 -0.001167 395.3 45 -0.001154 395.4 45 -0.001179 395.5 45 -0.001204 395.6 45 -0.001204 395.8 44 -0.001191 395.9 44 -0.001179 396 44 -0.001179 396.1 43 -0.001191 396.2 44 -0.001179 396.3 43 -0.001179 396.4 43 -0.001179 396.5 43 -0.001167 396.6 43 -0.001179 396.7 43 -0.001179 396.8 43 -0.001179 396.9 42 -0.001179 397 42 -0.001179 397.1 41 -0.001179 397.2 41 -0.001179 397.3 42 -0.001191 397.4 41 -0.001204 397.6 41 -0.001216 397.7 41 -0.001216 397.8 41 -0.001228 397.9 41 -0.001241 398 41 -0.001241 398.1 41 -0.001253 398.2 41 -0.001253 398.3 40 -0.001253 398.4 41 -0.001253 398.5 40 -0.001253 398.6 40 -0.001265 398.7 40 -0.001278 398.8 40 -0.001278 398.9 40 -0.00129 399 40 -0.001302 399.1 40 -0.001302 399.2 40 -0.001302 399.4 40 -0.001302 399.5 39 -0.001302 399.6 39 -0.001315 399.7 39 -0.001315 399.8 38 -0.001327 399.9 38 -0.001315 400 38 -0.001315 400.1 38 -0.001327 400.2 38 -0.00134 400.3 38 -0.001327 400.4 38 -0.001327 400.5 38 -0.001327 400.6 38 -0.001327 400.7 38 -0.00134 400.8 38 -0.001352 400.9 38 -0.001352 401.1 38 -0.001352 401.2 37 -0.001352 401.3 37 -0.001352 401.4 37 -0.001377 401.5 37 -0.001389 401.6 37 -0.001389 401.7 37 -0.001401 401.8 37 -0.001401 401.9 37 -0.001401 402 37 -0.001401 402.1 36 -0.001401 402.2 36 -0.001401 402.3 35 -0.001401 402.4 35 -0.001401 402.5 36 -0.001401 402.6 35 -0.001401 402.7 35 -0.001414 402.9 35 -0.001438 403 35 -0.001426 403.1 35 -0.001426 403.2 35 -0.001426 403.3 34 -0.001414 403.4 35 -0.001414 403.5 34 -0.001414 403.6 34 -0.001414 403.7 34 -0.001414 403.8 34 -0.001414 403.9 34 -0.001414 404 34 -0.001414 404.1 34 -0.001414 404.2 34 -0.001401 404.3 34 -0.001414 404.4 34 -0.001401 404.5 34 -0.001401 404.7 34 -0.001414 404.8 34 -0.001414 404.9 34 -0.001414 405 34 -0.001426 405.1 34 -0.001438 405.2 33 -0.001426 405.3 34 -0.001426 405.4 32 -0.001426 405.5 34 -0.001438 405.6 32 -0.001438 405.7 33 -0.001451 405.8 32 -0.001451 405.9 32 -0.001451 406 32 -0.001451 406.1 32 -0.001451 406.2 32 -0.001451 406.3 32 -0.001451 406.5 32 -0.001451 406.6 32 -0.001451 406.7 32 -0.001451 406.8 31 -0.001438 406.9 31 -0.001438 407 31 -0.001426 407.1 31 -0.001426 407.2 30 -0.001438 407.3 30 -0.001451 407.4 30 -0.001438 407.5 30 -0.001438 407.6 30 -0.001426 407.7 30 -0.001426 407.8 30 -0.001426 407.9 30 -0.001438 408 30 -0.001451 408.2 30 -0.001451 408.3 30 -0.001451 408.4 30 -0.001451 408.5 30 -0.001451 408.6 30 -0.001463 408.7 30 -0.001475 408.8 30 -0.001488 408.9 30 -0.001488 409 30 -0.0015 409.1 30 -0.0015 409.2 30 -0.0015 409.3 29 -0.0015 409.4 30 -0.0015 409.5 29 -0.001512 409.6 29 -0.001512 409.7 29 -0.001512 409.8 29 -0.001525 410 29 -0.001537 410.1 29 -0.001549 410.2 29 -0.001549 410.3 29 -0.001549 410.4 29 -0.001549 410.5 29 -0.001549 410.6 29 -0.001562 410.7 28 -0.001562 410.8 28 -0.001574 410.9 28 -0.001574 411 28 -0.001574 411.1 28 -0.001574 411.2 28 -0.001574 411.3 27 -0.001574 411.4 27 -0.001574 411.5 27 -0.001574 411.6 27 -0.001586 411.8 27 -0.001586 411.9 27 -0.001599 412 27 -0.001599 412.1 27 -0.001599 412.2 27 -0.001586 412.3 27 -0.001574 412.4 27 -0.001574 412.5 27 -0.001574 412.6 27 -0.001586 412.7 27 -0.001586 412.8 27 -0.001586 412.9 27 -0.001574 413 27 -0.001574 413.1 27 -0.001574 413.2 27 -0.001562 413.3 27 -0.001549 413.4 27 -0.001549 413.6 27 -0.001549 413.7 27 -0.001549 413.8 26 -0.001549 413.9 26 -0.001549 414 26 -0.001549 414.1 26 -0.001574 414.2 26 -0.001562 414.3 26 -0.001574 414.4 26 -0.001549 414.5 26 -0.001549 414.6 26 -0.001549 414.7 26 -0.001549 414.8 26 -0.001549 414.9 26 -0.001549 415 26 -0.001549 415.1 26 -0.001549 415.2 26 -0.001549 415.4 25 -0.001537 415.5 25 -0.001525 415.6 26 -0.001525 415.7 24 -0.001525 415.8 25 -0.001525 415.9 24 -0.001525 416 24 -0.001525 416.1 24 -0.001525 416.2 24 -0.001525 416.3 24 -0.001525 416.4 24 -0.001512 416.5 24 -0.001525 416.6 24 -0.0015 416.7 24 -0.0015 416.8 24 -0.001488 416.9 24 -0.001488 417.1 24 -0.001475 417.2 24 -0.001475 417.3 24 -0.001475 417.4 24 -0.001475 417.5 24 -0.001475 417.6 24 -0.001475 417.7 24 -0.001475 417.8 23 -0.001463 417.9 24 -0.001463 418 24 -0.001463 418.1 23 -0.001475 418.2 23 -0.001463 418.3 23 -0.001475 418.4 23 -0.001463 418.5 23 -0.001475 418.6 23 -0.001488 418.7 23 -0.001488 418.9 23 -0.001475 419 23 -0.001451 419.1 23 -0.001451 419.2 23 -0.001451 419.3 23 -0.001451 419.4 23 -0.001451 419.5 23 -0.001463 419.6 23 -0.001451 419.7 23 -0.001451 419.8 23 -0.001426 419.9 23 -0.001426 420 23 -0.001426 420.1 23 -0.001426 420.2 23 -0.001414 420.3 23 -0.001426 420.4 23 -0.001414 420.5 23 -0.001414 420.7 22 -0.001414 420.8 22 -0.001414 420.9 22 -0.001414 421 22 -0.001414 421.1 22 -0.001414 421.2 21 -0.001414 421.3 22 -0.001401 421.4 22 -0.001401 421.5 22 -0.001426 421.6 21 -0.001438 421.7 21 -0.001438 421.8 21 -0.001426 421.9 22 -0.001426 422 21 -0.001438 422.1 21 -0.001438 422.2 21 -0.001451 422.3 21 -0.001451 422.5 21 -0.001451 422.6 21 -0.001451 422.7 21 -0.001451 422.8 21 -0.001451 422.9 21 -0.001451 423 21 -0.001463 423.1 21 -0.001451 423.2 21 -0.001475 423.3 21 -0.001475 423.4 21 -0.001488 423.5 21 -0.0015 423.6 21 -0.0015 423.7 21 -0.0015 423.8 21 -0.0015 423.9 21 -0.0015 424 21 -0.001512 424.1 21 -0.001512 424.3 21 -0.001512 424.4 21 -0.001512 424.5 21 -0.001512 424.6 21 -0.001512 424.7 20 -0.001512 424.8 21 -0.001512 424.9 20 -0.001512 425 21 -0.001525 425.1 21 -0.001537 425.2 20 -0.001549 425.3 21 -0.001549 425.4 20 -0.001562 425.5 20 -0.001574 425.6 20 -0.001574 425.7 20 -0.001586 425.8 21 -0.001586 426 20 -0.001574 426.1 20 -0.001574 426.2 20 -0.001574 426.3 20 -0.001574 426.4 20 -0.001574 426.5 20 -0.001574 426.6 20 -0.001574 426.7 20 -0.001574 426.8 19 -0.001562 426.9 20 -0.001549 427 20 -0.001549 427.1 20 -0.001549 427.2 20 -0.001549 427.3 20 -0.001549 427.4 20 -0.001549 427.5 20 -0.001562 427.6 20 -0.001549 427.8 20 -0.001549 427.9 19 -0.001562 428 20 -0.001562 428.1 20 -0.001562 428.2 19 -0.001574 428.3 20 -0.001574 428.4 19 -0.001562 428.5 19 -0.001562 428.6 19 -0.001574 428.7 18 -0.001574 428.8 18 -0.001562 428.9 19 -0.001574 429 19 -0.001562 429.1 19 -0.001549 429.2 18 -0.001549 429.3 18 -0.001549 429.4 18 -0.001549 429.6 19 -0.001549 429.7 18 -0.001537 429.8 18 -0.001549 429.9 18 -0.001549 430 19 -0.001549 430.1 18 -0.001549 430.2 18 -0.001549 430.3 18 -0.001549 430.4 18 -0.001537 430.5 18 -0.001549 430.6 18 -0.001549 430.7 18 -0.001549 430.8 18 -0.001549 430.9 18 -0.001549 431 18 -0.001549 431.1 18 -0.001562 431.2 18 -0.001562 431.4 18 -0.001562 431.5 18 -0.001562 431.6 18 -0.001562 431.7 18 -0.001562 431.8 18 -0.001574 431.9 18 -0.001562 432 18 -0.001562 432.1 18 -0.001562 432.2 18 -0.001562 432.3 18 -0.001562 432.4 18 -0.001574 432.5 18 -0.001574 432.6 18 -0.001586 432.7 18 -0.001599 432.8 18 -0.001599 432.9 18 -0.001599 433.1 18 -0.001599 433.2 17 -0.001611 433.3 18 -0.001611 433.4 18 -0.001611 433.5 18 -0.001611 433.6 18 -0.001599 433.7